NL7603181A - Synthetic rubbers of high green strength - prepd by crosslinking tert amino-modified conj diolefin (co)polymers with bis-halomethyl aromatics - Google Patents
Synthetic rubbers of high green strength - prepd by crosslinking tert amino-modified conj diolefin (co)polymers with bis-halomethyl aromaticsInfo
- Publication number
- NL7603181A NL7603181A NL7603181A NL7603181A NL7603181A NL 7603181 A NL7603181 A NL 7603181A NL 7603181 A NL7603181 A NL 7603181A NL 7603181 A NL7603181 A NL 7603181A NL 7603181 A NL7603181 A NL 7603181A
- Authority
- NL
- Netherlands
- Prior art keywords
- green strength
- diphenyl
- conj
- prepd
- aryl
- Prior art date
Abstract
A new synthetic rubber compsn. with improved green strength is prepd. by reacting a rubbery polymer of a 4-6C conj. olefin (I) (opt. copolymerised with an 8-10C aromatic vinyl(idene) hydrocarbon or a 3-5C vinyl nitrile) which has 0.5-10 mmoles tert. amine gps/100g polymer with a halogen cpd. of formula (II) X X CG2 x R x CH2 x Y (X and Y are each Cl, Br or I; R = mononuclear aryl substd. by CH2X or CH3O; or polynuclear aryl chosen from diphenyl, diphenyl (thio) ether, diphenyl (1-4C) alkane or naphthalene; all aryls opt. substd. by >=1 lower (halo) alkyl x aryl or lower alkenyl, and CH2X and CH2Y are directly bonded to different rings when R is polynuclear). (II) provide labile crosslinks which improve the green strength but which are broken on heating etc. so the compsns. can be treated like ordinary rubbers e.g. formed into tyres. Compared with the dihalo cpds. described in the parent patent. (II) have a less irritating odour; lower vapour press x so are easily handled with less loss of matl. and can be added to the polymer latex at the coagulation stage.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
NL7603181A NL182884C (en) | 1976-03-26 | 1976-03-26 | METHOD FOR PREPARING A SYNTHETIC RUBBER PRODUCT WITH IMPROVED GREEN STRENGTH |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
NL7603181A NL182884C (en) | 1976-03-26 | 1976-03-26 | METHOD FOR PREPARING A SYNTHETIC RUBBER PRODUCT WITH IMPROVED GREEN STRENGTH |
Publications (3)
Publication Number | Publication Date |
---|---|
NL7603181A true NL7603181A (en) | 1977-09-28 |
NL182884B NL182884B (en) | 1988-01-04 |
NL182884C NL182884C (en) | 1988-06-01 |
Family
ID=19825883
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
NL7603181A NL182884C (en) | 1976-03-26 | 1976-03-26 | METHOD FOR PREPARING A SYNTHETIC RUBBER PRODUCT WITH IMPROVED GREEN STRENGTH |
Country Status (1)
Country | Link |
---|---|
NL (1) | NL182884C (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4454304A (en) * | 1981-04-22 | 1984-06-12 | Copolymer Rubber & Chemical Corp. | Method and material for producing high green strength rubber compounds |
-
1976
- 1976-03-26 NL NL7603181A patent/NL182884C/en not_active IP Right Cessation
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4454304A (en) * | 1981-04-22 | 1984-06-12 | Copolymer Rubber & Chemical Corp. | Method and material for producing high green strength rubber compounds |
Also Published As
Publication number | Publication date |
---|---|
NL182884C (en) | 1988-06-01 |
NL182884B (en) | 1988-01-04 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS54132647A (en) | Vulcanizable rubber composition having improved ozon crack and oil resistance | |
ATE201036T1 (en) | RUBBER BLEND BASED ON A DIENE POLYMER WITH A SILANOL GROUP WHICH CONTAINS AN ORGANOSILANDE DERIVATIVE | |
KR950032408A (en) | Tire tread reinforced with quantitative amount of silica | |
DE3689229D1 (en) | Manufacture of rubber compounds. | |
JPS57195105A (en) | Preparation of modified cis-1,4-polyisoprene rubber | |
GB968756A (en) | Butadiene polymer and blends and compositions containing same | |
US3821134A (en) | Vulcanizable polymer blends of diene rubbers and grafted epdm polymers | |
US3062696A (en) | Pneumatic tires | |
FR2345468A2 (en) | Synthetic rubbers of high green strength - prepd by crosslinking tert amino-modified conj diolefin (co)polymers with bis-halomethyl aromatics | |
NL7603181A (en) | Synthetic rubbers of high green strength - prepd by crosslinking tert amino-modified conj diolefin (co)polymers with bis-halomethyl aromatics | |
KR950032410A (en) | Pneumatic tires with inner liner of cured rubber compound containing trans 1,4-polybutadiene rubber | |
SE7906077L (en) | VEHICLE TIRES WITH SEALING PUNKING COATING | |
IT1058767B (en) | Synthetic rubbers of high green strength - prepd by crosslinking tert amino-modified conj diolefin (co)polymers with bis-halomethyl aromatics | |
NO813684L (en) | POLYMER BLEND. | |
US2490518A (en) | N-thio amine vulcanization agents for butadiene copolymers | |
DK0486914T3 (en) | Thermoplastic mixtures based on polyolefin and vinyl aromatic polymer | |
IT1057806B (en) | Synthetic rubbers of high green strength - prepd by crosslinking amino-modified conj diolefin (co)polymers with di-haloacetyl cpds | |
NL7603182A (en) | Synthetic rubbers of high green strength - prepd by crosslinking amino-modified conj diolefin (co)polymers with di-haloacetyl cpds | |
FR2345469A2 (en) | Synthetic rubbers of high green strength - prepd by crosslinking amino-modified conj diolefin (co)polymers with di-haloacetyl cpds | |
GB835639A (en) | Brominated rubbery polymers | |
IE41566L (en) | Tyre tread polymer | |
GB1058641A (en) | A mixture for improving the physical and cord-adhesion properties of natural and synthetic rubbers | |
US2892805A (en) | Vulcanizing furnace black stocks with dithio secondary amines | |
GB1001352A (en) | Improvements relating to modified polymers | |
GB1303138A (en) |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
BA | A request for search or an international-type search has been filed | ||
BB | A search report has been drawn up | ||
BC | A request for examination has been filed | ||
A85 | Still pending on 85-01-01 | ||
V1 | Lapsed because of non-payment of the annual fee |