MX165847B - Mejoras a derretimiento de vidrio con calentamiento sumergido en etapas - Google Patents

Mejoras a derretimiento de vidrio con calentamiento sumergido en etapas

Info

Publication number
MX165847B
MX165847B MX206028A MX20602885A MX165847B MX 165847 B MX165847 B MX 165847B MX 206028 A MX206028 A MX 206028A MX 20602885 A MX20602885 A MX 20602885A MX 165847 B MX165847 B MX 165847B
Authority
MX
Mexico
Prior art keywords
liquefied
melt container
stages
glass melting
submerged heating
Prior art date
Application number
MX206028A
Other languages
English (en)
Inventor
Kwang Jong Won
George Anthony Pecoraro
Henry Peter Hanneken
Original Assignee
Ppg Industries Inc
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Priority claimed from US06/632,507 external-priority patent/US4539034A/en
Priority claimed from US06/632,506 external-priority patent/US4545800A/en
Application filed by Ppg Industries Inc filed Critical Ppg Industries Inc
Publication of MX165847B publication Critical patent/MX165847B/es

Abstract

La presente invención se refiere a mejoras a método para derretir material que comprende licuar en un recipiente de derretido primario materiales de carga a un estado fluible y drenar los materiales licuados desde el recipiente de derretido hacia adentro de un recipiente del derretido secundario, mantener en el recipiente de derretido secundario un cuerpo del material licuado e inyectar gas radiante debajo de la superficie del cuerpo licuado a una tasa suficiente para calentar el cuerpo licuado y para avanzar el material licuado hacia el estado fundido.
MX206028A 1984-07-19 1985-07-18 Mejoras a derretimiento de vidrio con calentamiento sumergido en etapas MX165847B (es)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
US06/632,507 US4539034A (en) 1984-07-19 1984-07-19 Melting of glass with staged submerged combustion
US06/632,506 US4545800A (en) 1984-07-19 1984-07-19 Submerged oxygen-hydrogen combustion melting of glass

Publications (1)

Publication Number Publication Date
MX165847B true MX165847B (es) 1992-12-07

Family

ID=27091651

Family Applications (1)

Application Number Title Priority Date Filing Date
MX206028A MX165847B (es) 1984-07-19 1985-07-18 Mejoras a derretimiento de vidrio con calentamiento sumergido en etapas

Country Status (12)

Country Link
KR (1) KR930001962B1 (es)
AU (1) AU558646B2 (es)
BR (1) BR8503434A (es)
DK (1) DK327185A (es)
EG (1) EG17145A (es)
FI (1) FI78282C (es)
IL (1) IL75734A0 (es)
IN (1) IN164105B (es)
MX (1) MX165847B (es)
NZ (1) NZ212345A (es)
PT (1) PT80819B (es)
TR (1) TR22614A (es)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
FR2991759B1 (fr) * 2012-06-12 2014-06-20 Saint Gobain Isover Installation de fusion de verre

Also Published As

Publication number Publication date
EG17145A (en) 1991-11-30
FI852819L (fi) 1986-01-20
AU558646B2 (en) 1987-02-05
NZ212345A (en) 1987-02-20
IL75734A0 (en) 1985-11-29
KR860001013A (ko) 1986-02-22
FI78282B (fi) 1989-03-31
KR930001962B1 (ko) 1993-03-20
IN164105B (es) 1989-01-14
FI78282C (fi) 1989-07-10
TR22614A (tr) 1988-01-08
PT80819B (pt) 1987-09-30
DK327185D0 (da) 1985-07-18
AU4318785A (en) 1986-01-23
DK327185A (da) 1986-01-20
BR8503434A (pt) 1986-04-15
FI852819A0 (fi) 1985-07-18
PT80819A (en) 1985-08-01

Similar Documents

Publication Publication Date Title
GB1137513A (en) Improvements in and relating to processes for the manufacture of heat-recoverable articles
MX166953B (es) Mejoras en metodo para derretir vidrio
ZA854058B (en) Melting of glass with staged submerged heating
ES2142594T3 (es) Metodo para envasar adhesivos de fusion en caliente en un proceso continuo.
EP0194020A3 (en) A fitting
MX165847B (es) Mejoras a derretimiento de vidrio con calentamiento sumergido en etapas
JPS57177745A (en) Container for generating heat with controlled temperature
DE3673626D1 (de) Oberflaechenschmelzen mit thermischem schutz.
ES2064300T3 (es) Crisol de soporte de multiples partes.
GB1249422A (en) Improvements in thermal insulation of pipes and the like and method of forming same
EP0507265A3 (en) Procedure of and device for thermally cutting workpieces
JPS5693412A (en) Superthin quartz oscillator
ES8500770A1 (es) Aparato estarcidor para aplicar polvo fusible segun una configuracion tridimensional sobre una superficie receptora
JPS5513932A (en) Transfer mold for semiconductor device
SE7712389L (sv) Forfarande for forvermning av delar till behallare for smelta metaller
JPS5519553A (en) Method of repairing damage arising on covering layer
GB1188555A (en) Improvements in or relating to ampoules and like glass containers
SG1092G (en) Ablation melting with composite lining
JPS56156599A (en) Upper cool keeping construction of sprayed foamed urethane cool keeping layer for low temperature tank
JPS54135093A (en) Contraction packing method
JPS6465787A (en) Silicon carbide heater
JPS56977A (en) Method of repairing part of container lined with refractory material
JPS5733676A (en) Application of heat insulator for tank for liquified natural gas or the like
Pribytkov Thermal Effects in the Interaction of a Solid Metal With a Metallic Melt
JPS6449520A (en) Production of metal thermos