KR970006574A - Manufacturing method of chlorinated composite twisted yarn - Google Patents

Manufacturing method of chlorinated composite twisted yarn Download PDF

Info

Publication number
KR970006574A
KR970006574A KR1019950021792A KR19950021792A KR970006574A KR 970006574 A KR970006574 A KR 970006574A KR 1019950021792 A KR1019950021792 A KR 1019950021792A KR 19950021792 A KR19950021792 A KR 19950021792A KR 970006574 A KR970006574 A KR 970006574A
Authority
KR
South Korea
Prior art keywords
twisted yarn
yarn
yarns
producing
composite twisted
Prior art date
Application number
KR1019950021792A
Other languages
Korean (ko)
Inventor
서원
온형일
Original Assignee
이명환
동양폴리에스터 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 이명환, 동양폴리에스터 주식회사 filed Critical 이명환
Priority to KR1019950021792A priority Critical patent/KR970006574A/en
Publication of KR970006574A publication Critical patent/KR970006574A/en

Abstract

본 발명은 길이방향으로 여러형태의 권축구조 및 섬도가 불규칙적으로 배열되어 길이방향으로 이염(異染)효과를 발현시켜 방적사풍의 염색효과를 낼 수 있는 복합 가연사의 제조방법에 관한 것이다.The present invention relates to a method for producing a composite twisted yarn which can produce various types of crimp structure and fineness irregularly in the longitudinal direction to express a dyeing effect in the longitudinal direction, thereby producing a dyeing effect of spun yarn wind.

본 발명의 이염성 복합 가연사의 제조방법은 신도차가 100% 이상되는 2종의원사를 사용하되 내층부에 위치할 원사의 신도가 100∼150%인 원사를 이용하여 오버피이드율 1.5∼2.5%의 조건하에서 강한 공기압을 이용하여 교락하고, 오버피이드율을 1.5∼2.5%로 하여 연신 가연하는 것을 특징으로 한다.In the method of manufacturing a bleeding composite false twisted yarn of the present invention, two kinds of yarns having an elongation difference of 100% or more are used, but yarns having an elongation of 100 to 150% of yarns to be placed in the inner layer have an overfeed rate of 1.5 to 2.5%. Under the conditions, it entangles using strong air pressure, and it extends and combusts by setting overfeed rate to 1.5 to 2.5%.

본 발명에 따르면 기존의 방식에 의해 제조된 복합 가연사가 발현하고 있는 방적사풍의 촉감을 나타내는 동시에, 방적사 특유의 이염효과를 발현시켜 Wool의 효과를 나타내는 폴리에스터 필라멘트사가 제공되는 효과가 있다.According to the present invention, a polyester filament yarn having a wool effect can be provided by expressing a feeling of spinning yarn wind expressed by a composite twisted yarn manufactured by a conventional method, and expressing a dyeing effect peculiar to a yarn.

Description

이염성 복합가연사의 제조방법Manufacturing method of chlorinated composite twisted yarn

본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.

Claims (3)

신도가 다른 두원사를 복합 가연함에 있어서, 신도차가 100% 이상되는 2종의 원사를 사용하되 내층부에 위치할 원사의 신도가 100∼150%이고, 오버피이드율 1.5∼2.5%의 조건하에서 강한 공기압을 이용하여 교락하고, 오버피이드율을 1.5∼2.5%로 하여 연신 가연하여 제조됨을 특징으로 하는 이염성(異染性) 복합가연사의 제조방법.In the composite flame retardation of two yarns with different elongation, use two kinds of yarns with a difference in elongation of 100% or more, but have a strong elongation under the condition of 100-150% of the yarn to be placed in the inner layer and 1.5 ~ 2.5% of overfeed rate. A method for producing a chlorinated composite twisted yarn, characterized in that it is entangled using air pressure and is stretched and flammable with an overfeed ratio of 1.5 to 2.5%. 제1항에 있어서, 상기 연신 가연 공정에서 가연처리 가열판의 온도를 160℃ 미만으로 하여 연신 가연하는 것을 특징으로 하는 이염성 복합가연사의 제조방법.The method for producing a dichroic composite twisted yarn according to claim 1, wherein said stretched twist is carried out by setting the temperature of the flammable heating plate to less than 160 DEG C in said stretch twisting process. 제1항에 있어서, 교락시 공기압을 2.5㎏/㎤ 이상으로 하여 제조함을 특징으로 하는 이염성 복합가연사의 제조방법.The method for producing a dichroic composite twisted yarn according to claim 1, wherein the entangled air pressure is 2.5 kg / cm 3 or more. ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.
KR1019950021792A 1995-07-22 1995-07-22 Manufacturing method of chlorinated composite twisted yarn KR970006574A (en)