Prior art keywords
welding
current
welding method
gas
torch
Prior art date
Application number
KR1019960003818A
Other languages
Korean (ko)
Other versions
KR100193800B1 (en
Inventor
미츠아키 오토구로
가즈오 나가토모
도시오 아오키
노부유키 아오키
Original Assignee
기무라 다츠야
닛데츠 요세츠 고교 가부시키가이샤
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 기무라 다츠야, 닛데츠 요세츠 고교 가부시키가이샤 filed Critical 기무라 다츠야
Publication of KR960031045A publication Critical patent/KR960031045A/en
Application granted granted Critical
Publication of KR100193800B1 publication Critical patent/KR100193800B1/en

Links

Landscapes

  • Arc Welding In General (AREA)
  • Butt Welding And Welding Of Specific Article (AREA)
  • Arc Welding Control (AREA)

Abstract

(purpose)

In the transverse gas-sealed arc welding, a good welded portion without any undercut is formed and a good welded portion free from dissolution defects is obtained and the welding efficiency is improved.

(Configuration)

In the gas shielded arc welding in the transverse posture, the solid backing material is brought into contact with the back side of the improvement made by the upper and lower base materials, and the welding current is repeatedly welded The welded torch is pivoted in the thickness direction of the upper and lower base materials by bringing the remaining improvement parts into contact with the slidable copper support parts on the front side and finishing by the electrosurgical gas welding method do.

Description

Lateral welding method and apparatus

Since this is a trivial issue, I did not include the contents of the text.

1 (a) is a cross-sectional view showing a first-layer bead by a current-change welding method, (b) is a longitudinal sectional view,

Fig. 2 is an improved cross-sectional view showing a finished bead by an electro-gas welding method, wherein Fig. 2 (a) is a cross-sectional view, Fig. 2

FIG. 3 is a cross-sectional view illustrating a front end portion of a welding torch used in an embodiment of the present invention, wherein half of the tube remains an outer appearance, (B) is a cross-sectional view showing the welding torch tip end portion when performing the electro-gas welding method; Fig.

FIG. 4 is a perspective view illustrating the appearance of a sliding copper support 9 used in an embodiment of the present invention. FIG.

FIG. 5 is a flow chart illustrating knitting of an electrical element of an embodiment of the inventive apparatus. FIG.

Claims (3)

In the gas shielded arc welding in the transverse posture, the solid backing material is brought into contact with the back side of the improvement formed by the upper and lower base materials, and the welding current is repeatedly increased The welded torch is shaken by the plate thickness method of the upper and lower base materials by forming the beads first by welding by the change welding method and bringing the remaining improvement parts into contact with the slidable copper support parts on the surface side and finishing by the electrosurgical gas welding method Wherein the lateral welding method is characterized by: The welding method according to claim 1, further comprising: a first welding step of forming a first bead by a current change welding method in which a welding current is periodically repeatedly welded with a large current and a small current; Wherein the welding is performed using the same wire feeder and the same welding torch. A switching timer for periodically and repeatedly switching the welding current to a large current and a small current, a switch for switching the current change welding method and the electro-gas welding method, a detector for detecting a welding current, a reference current setting device, A circuit for controlling the welding speed so as to keep the distance between the welding tip and the molten metal free surface substantially constant by receiving the output of the comparator and a circuit for controlling the welding torch in the thickness direction of the base plate in the direction substantially perpendicular to the welding line, A detector for detecting an improvement edge of at least one of the upper base material and the lower base material, and an improved imitation control circuit for improving and controlling the position of the welding torch with respect to the improved edge by the output of the detector And a lateral direction welding device. ※ Note: It is disclosed by the contents of the first application.
KR1019960003818A 1995-02-21 1996-02-16 Transverse Welding Method and Apparatus KR100193800B1 (en)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP3195495A JPH08215840A (en) 1995-02-21 1995-02-21 Horizontal position welding method and equipment therefor
JP95-31954 1995-02-21

Publications (2)

Publication Number Publication Date
KR960031045A true KR960031045A (en) 1996-09-17
KR100193800B1 KR100193800B1 (en) 1999-06-15

Family

ID=12345357

Family Applications (1)

Application Number Title Priority Date Filing Date
KR1019960003818A KR100193800B1 (en) 1995-02-21 1996-02-16 Transverse Welding Method and Apparatus

Country Status (3)

Country Link
JP (1) JPH08215840A (en)
KR (1) KR100193800B1 (en)
CN (1) CN1135948A (en)

Families Citing this family (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR100466365B1 (en) * 2001-12-29 2005-01-13 대우조선해양 주식회사 Method of electro gas welding with soild wire
JP2013184220A (en) * 2012-03-12 2013-09-19 Daihen Corp Arc welding device
CN102922153B (en) * 2012-11-27 2014-10-15 哈尔滨工业大学 Laser guide GMAW (Gas Metal Arc Welding) electric arc compound transverse welding method
CN103521991A (en) * 2013-09-26 2014-01-22 天津大学 Horizontal position welding clamping device for workpiece to be welded
CN104801876B (en) * 2015-04-28 2017-04-19 上海气焊机厂有限公司 Horizontal welding method
JP7161903B2 (en) * 2018-09-28 2022-10-27 株式会社小松製作所 Welding equipment and welding method
CN113770522A (en) * 2021-07-06 2021-12-10 中国船舶重工集团公司第七二五研究所 Laser ultra-narrow gap welding method for titanium alloy thick plate pre-filled wire

Also Published As

Publication number Publication date
JPH08215840A (en) 1996-08-27
KR100193800B1 (en) 1999-06-15
CN1135948A (en) 1996-11-20

Similar Documents

Publication Publication Date Title
DE50115753D1 (en) Method for setting a welding device
DE69717132D1 (en) DEVICE FOR OSCILLATING FRICTION WELDING
KR960031045A (en) Lateral welding method and apparatus
JPH10113771A (en) Device for feeding wire for plural electrode gas shield arc weldings
HU9901831D0 (en) Apparatus and method for seaung foil material
ATE296705T1 (en) WELDING DEVICE WITH A FIELD GENERATION
JPS54126646A (en) Welder
US3999035A (en) Lay down arc welding method
JPS5970469A (en) Dc arc welding device
US2387864A (en) Starting device for gravity arc welders
KR19980014526A (en) METHOD FOR CONTROLLING STICK-OUT OF ARC WELDING ROBOT
JPS6415278A (en) Back bead control method for automatic gas shielded arc one-side welding
JPH069765U (en) Stud welder gun head
JPS577375A (en) Nonconsumable electrode arc welding method
JP3009820U (en) Gas arc welder
JPH09314360A (en) Ultrasonic welding
KR960009628Y1 (en) Stud welding machine
KR970020275A (en) Arc sensing method of automatic welding process
JPS5419443A (en) Bead welding method
JP2000153358A (en) Automatic welding start control method
JPS56148473A (en) Position control method for weaving welding
JPH08138631A (en) Arc welding device for tubular bulb and its method
JPS551953A (en) Arc welding method
JPS5689377A (en) Starting method of welding arc
Rajasekaran et al. Effect of parameters of pulsed current on droplet detachment and effect of different types of droplet detachements on weld bead geometry

Legal Events

Date Code Title Description
A201 Request for examination
E902 Notification of reason for refusal
E701 Decision to grant or registration of patent right
GRNT Written decision to grant
LAPS Lapse due to unpaid annual fee