KR960027089A - How to make graphite brush for automobile electric motor - Google Patents

How to make graphite brush for automobile electric motor Download PDF

Info

Publication number
KR960027089A
KR960027089A KR1019940036186A KR19940036186A KR960027089A KR 960027089 A KR960027089 A KR 960027089A KR 1019940036186 A KR1019940036186 A KR 1019940036186A KR 19940036186 A KR19940036186 A KR 19940036186A KR 960027089 A KR960027089 A KR 960027089A
Authority
KR
South Korea
Prior art keywords
powder
graphite
electric motor
automobile electric
brush
Prior art date
Application number
KR1019940036186A
Other languages
Korean (ko)
Other versions
KR100231066B1 (en
Inventor
김일두
김성수
Original Assignee
정몽원
만도기계 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 정몽원, 만도기계 주식회사 filed Critical 정몽원
Priority to KR1019940036186A priority Critical patent/KR100231066B1/en
Publication of KR960027089A publication Critical patent/KR960027089A/en
Application granted granted Critical
Publication of KR100231066B1 publication Critical patent/KR100231066B1/en

Abstract

브러시에 함유되는 동분말의 함량을 증대시킴이 없이 전동기의 출력 특성을 향상시킬 수 있을 뿐만 아니라 소음 특성 및 내마모 특성을 향상시키기 위하여 본 발명은 섬유 입자상의 동분말을 첨가시켜서 브러시를 제작하는 방법을 제공한다.In order to improve the output characteristics of the motor without increasing the content of the copper powder contained in the brush, as well as to improve the noise characteristics and abrasion resistance, the present invention provides a method of manufacturing a brush by adding copper powder on fiber particles. To provide.

Description

자동차 전동기용 흑연 브러시 제작 방법How to make graphite brush for automobile electric motor

본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.

제1도는 정류자상에 회전가능하도록 접촉되어 있는 브러시를 구비하고 있는 전동기를 일부 절개시켜 도시한 측면도, 제2도는 본 발명에 따라서 제작되는 흑연 브러시의 제조 순서도.1 is a side view partially cut away of an electric motor having a brush rotatably contacted on a commutator, and FIG. 2 is a manufacturing flowchart of a graphite brush manufactured according to the present invention.

Claims (2)

흑연 분말에 결합제를 첨가시켜서 제작된 괴상의 흑연을 오븐에서 50 내지 80℃의 온도로 가열시켜 용매성분을 증발시키는 제1단계와, 상기 괴상의 흑연을 분쇄시켜서 소정 크기의 입도를 갖는 수지 함유 흑연 분말을 생성시키는 제2단계와, 상기 수지 함유 흑연 분말에 동분말 및 분말 형태의 첨가제를 혼합시킨 혼합물을 가압 성형시키는 제3단계와, 상기 가압 성형처리된 혼합물을 600 내지 800℃의 고온에서 소성변형시키는 제4단계로 이루어지는 자동차 전동기용 흑연 브러시 제작 방법에 있어서, 상기 동분말은 섬유 입자상으로 이루어져 있는 것을 특징으로 하는 자동차 전동기용 흑연 브러시 제작 방법.The first step of evaporating the solvent component by heating the bulk graphite prepared by adding the binder to the graphite powder at a temperature of 50 to 80 ℃ in the oven, and the graphite containing a resin having a particle size of a predetermined size by grinding A second step of producing a powder, a third step of press molding a mixture of copper powder and an additive in powder form to the resin-containing graphite powder, and firing the pressure-molded mixture at a high temperature of 600 to 800 ° C. The method of manufacturing a graphite brush for an automobile electric motor, comprising the fourth step of deforming, wherein the copper powder is formed of fiber particles. 제1항에 있어서, 상기 첨가제는 1 내지 5 중량%의 이염화 몰리브데늄으로 이루어져 있는 것을 특징으로 하는 자동차 전동기용 흑연 브러시 제작 방법.The method of claim 1, wherein the additive is molybdenum dichloride of 1 to 5% by weight. ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.
KR1019940036186A 1994-12-23 1994-12-23 Method of manufacturing graphite brush for electric motor KR100231066B1 (en)