KR950032768A - Manufacturing method of multifilament low shrinkage yarn and its manufacturing apparatus - Google Patents
Manufacturing method of multifilament low shrinkage yarn and its manufacturing apparatus Download PDFInfo
- Publication number
- KR950032768A KR950032768A KR1019940009759A KR19940009759A KR950032768A KR 950032768 A KR950032768 A KR 950032768A KR 1019940009759 A KR1019940009759 A KR 1019940009759A KR 19940009759 A KR19940009759 A KR 19940009759A KR 950032768 A KR950032768 A KR 950032768A
- Authority
- KR
- South Korea
- Prior art keywords
- heat treatment
- manufacturing
- plate
- temperature
- treatment plate
- Prior art date
Abstract
본 발명은 70∼150℃의 온도대역을 갖는 제1열처리판(13), 160∼250℃의 온도대역을 갖는 제2열처리판(14), 열처리판(13,14)의 온도를 감지하여 온도를 조절하는 온도센서(15)로 구성되어지되, 열처리장치 몸체(16)에 열처리판 (13,14)을 서로 대으되게 형성하고 열처리판(13,14)의 내측으로 온도센서(15)를 내장시켜 구성한 이중열처리장치(6)를 구비한 것을 특징으로 하는 멀티필라멘트 저수축사의 제조장치 및 폴리에스테르 반연신사를 일정한 장력으로 공급하여 1차 연신을 행한 후 상기 열처리장치를 통과시켜 열처리를 행한다음, 2차 연신하고 권취하되 1차 연신비율은 3.15∼3.19로, 열처리를 2∼5회반복함을 특징으로 하는 멀티 필라멘트 저수축사의 제조방법에 관한 것으로,제조된 저수축사는 열수축을 1% 이하인 우수한 효과를 얻을 수 있다.The present invention senses the temperature of the first heat treatment plate 13 having a temperature range of 70 to 150 ° C., the second heat treatment plate 14 having a temperature range of 160 to 250 ° C., and the heat treatment plates 13 and 14. It is composed of a temperature sensor 15 for controlling the heat treatment plate 13, 14 formed on the heat treatment apparatus body 16 to be opposed to each other and the temperature sensor 15 inside the heat treatment plate (13, 14) built-in After the primary stretching by supplying the manufacturing apparatus and polyester semi-stretched yarn with a constant tension, characterized in that it comprises a double heat treatment device (6) configured to make a heat treatment by passing through the heat treatment device, The secondary stretching and winding, but the primary stretching ratio is 3.15 to 3.19, and the manufacturing method of the multi-filament low shrink yarn, characterized in that the heat treatment is repeated 2 to 5 times, the manufactured low shrink yarn is excellent in shrinkage of less than 1% The effect can be obtained.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.
제1도는 본 발명에 따른 멀티필라멘트 저수축사의 개략적인 제조공정도이고, 제2도는 본 발명의 일요부인 이중 열처리장치의 개략도이다.1 is a schematic manufacturing process diagram of a multifilament low shrinkage yarn according to the present invention, and FIG. 2 is a schematic diagram of a dual heat treatment apparatus which is an essential part of the present invention.
Claims (5)