KR950016954A - Low Fluorine Molding Solvent - Google Patents
Low Fluorine Molding Solvent Download PDFInfo
- Publication number
- KR950016954A KR950016954A KR1019930027034A KR930027034A KR950016954A KR 950016954 A KR950016954 A KR 950016954A KR 1019930027034 A KR1019930027034 A KR 1019930027034A KR 930027034 A KR930027034 A KR 930027034A KR 950016954 A KR950016954 A KR 950016954A
- Authority
- KR
- South Korea
- Prior art keywords
- less
- molding solvent
- fluorine
- cao
- sio
- Prior art date
Abstract
본 발명에 의하면 불소함유량이 낮으면서도 저탄소강의 고숙주조를 가능하게 하고 양호한 품질을 갖는 주편을 얻을 수 있는 주형용제에 관한 것이다. 이 주형용제는, 중량 %로 불소(F) 6%이하; LiO2; Al2O38%이하; B2O36$이하; MgO 9%이하; Na27∼12%; 및 염기도(%CaO%SiO2)가 0.8∼1.1 되는 CaO와 SiO2혼합물45∼60%; 로 조성되고, 13000℃에서의 점도가 0.1∼0.5poise이며 응고온도가 920∼970℃인 것이다.The present invention relates to a molding solvent capable of high-temperature casting of low-carbon steels with low fluorine content and obtaining casts having good quality. This molding solvent is 6% or less of fluorine (F) by weight%; LiO 2 ; Al 2 O 3 8% or less; B 2 O 3 6 $ and below; MgO 9% or less; Na 2 7-12%; And 45-60% of a mixture of CaO and SiO 2 having a basicity (% CaO% SiO 2 ) of 0.8-1.1; The viscosity is 1 to 0.5 poise and the solidification temperature is 920 to 970 ° C.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.
제1도(a) 및 (b)는 연속주조용 주형과 주편사이의 윤활기능 및 온도분포를 각각 모식적으로 나타낸 도면.1 (a) and (b) schematically show the lubrication function and temperature distribution between the continuous casting mold and the cast steel, respectively.
제2도(a) 및 (g)는 각종 몰드파우더의 화학성분과 점도 및 응고온도와의 관계를 나타내는 그래프.2 (a) and (g) are graphs showing the relationship between the chemical composition, viscosity, and solidification temperature of various mold powders.
제3도는 본 발명재와 비교재의 점도 및 응고온도와의 관계를 나타내는 그래프.3 is a graph showing the relationship between the viscosity of the present invention and the comparative material and the solidification temperature.
제4도는 본 발명재와 비교재의 불소용출시험시 30분 및 720분에서의 불소용출량을 나타내는 그래프.4 is a graph showing the amount of fluorine dissolution at 30 and 720 minutes in the fluorine dissolution test of the present invention and the comparative material.
Claims (1)