KR910001829A - 고체 전해 콘덴서의 제조방법 - Google Patents

고체 전해 콘덴서의 제조방법 Download PDF

Info

Publication number
KR910001829A
KR910001829A KR1019890009282A KR890009282A KR910001829A KR 910001829 A KR910001829 A KR 910001829A KR 1019890009282 A KR1019890009282 A KR 1019890009282A KR 890009282 A KR890009282 A KR 890009282A KR 910001829 A KR910001829 A KR 910001829A
Authority
KR
South Korea
Prior art keywords
electrolytic capacitor
solid electrolytic
manufacturing
solution
producing
Prior art date
Application number
KR1019890009282A
Other languages
English (en)
Inventor
박철우
Original Assignee
서주인
삼성전기 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 서주인, 삼성전기 주식회사 filed Critical 서주인
Priority to KR1019890009282A priority Critical patent/KR910001829A/ko
Publication of KR910001829A publication Critical patent/KR910001829A/ko

Abstract

내용 없음

Description

고체 전해 콘덴서의 제조방법
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음

Claims (2)

  1. 탄탈륨을 사용한 고체전해 콘덴서의 제조방법에 있어서, 탄탈륨 펠릿 함침 조건을 질산망간(Mn(NO3)2)의 농도에 따라 침적회수를 조절하고, 재화성액을 NH4HSO4를 쓰는 것을 특징으로 하는 고체 전해 콘덴서의 제조방법.
  2. 제1항에 있어서, 상기 함침조건을20% Mn(NO3)2용액에서 2회, 40%Mn(NO3)2용액에서 1회 60%, Mn(NO3)2용액에서 4회를 하는 것을 특징으로 하는 고체 전해 콘덴서의 제조방법.
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019890009282A 1989-06-30 1989-06-30 고체 전해 콘덴서의 제조방법 KR910001829A (ko)