KR900014267A - 잉크를 이용한 스크린 인쇄에 의한 유리표면 에칭 방법 - Google Patents

잉크를 이용한 스크린 인쇄에 의한 유리표면 에칭 방법 Download PDF

Info

Publication number
KR900014267A
KR900014267A KR1019890003746A KR890003746A KR900014267A KR 900014267 A KR900014267 A KR 900014267A KR 1019890003746 A KR1019890003746 A KR 1019890003746A KR 890003746 A KR890003746 A KR 890003746A KR 900014267 A KR900014267 A KR 900014267A
Authority
KR
South Korea
Prior art keywords
weight
screen printing
glass surface
ink
etching method
Prior art date
Application number
KR1019890003746A
Other languages
English (en)
Other versions
KR910003091B1 (ko
Inventor
김중형
Original Assignee
김중형
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 김중형 filed Critical 김중형
Priority to KR1019890003746A priority Critical patent/KR910003091B1/ko
Publication of KR900014267A publication Critical patent/KR900014267A/ko
Application granted granted Critical
Publication of KR910003091B1 publication Critical patent/KR910003091B1/ko

Abstract

내용 없음

Description

잉크로 이용한 스크린 인쇄에 의한 유리표면 에칭 방법
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음

Claims (1)

  1. 증류수를 교반기에 투입하고 이 증류수 100중량%에 대하여 글리세린90-120중량%와, 300메쉬이상의 전분분말 55-65중량%와 불화암몬 약80중량%를 서서히 투입하면서 교반하고, 이를 약90-100℃로 20-25분간 중량한후, 상온에서 자연 냉각시켜주고 이에 다시 230메쉬 이상의 산화 알루미늄 분말을 상기 조성물 100중량%에 대하여 33-60중량%을 투입하여 충분히 교반하여 크림상의 조성물을 얻은다음, 이를 통상의 스크린 인쇄방법에 의하여 유리표면에 스크린 인쇄한후 2-5분후 수세처리함을 특징으로 하는 잉크를 이용한 스크린 인쇄에 의한 유리표면 에칭 방법.
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019890003746A 1989-03-24 1989-03-24 잉크를 이용한 스크린 인쇄에 의한 유리표면 에칭방법 KR910003091B1 (ko)