KR900007020A - How to strengthen part of shadow mask - Google Patents
How to strengthen part of shadow mask Download PDFInfo
- Publication number
- KR900007020A KR900007020A KR1019880014234A KR880014234A KR900007020A KR 900007020 A KR900007020 A KR 900007020A KR 1019880014234 A KR1019880014234 A KR 1019880014234A KR 880014234 A KR880014234 A KR 880014234A KR 900007020 A KR900007020 A KR 900007020A
- Authority
- KR
- South Korea
- Prior art keywords
- shadow mask
- strengthen part
- laser
- partially
- strengthen
- Prior art date
Abstract
내용 없음.No content.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.
제 2 도는 새도우마스크의 도밍현상을 보인 설명도.2 is an explanatory diagram showing the ming phenomenon of the shadow mask.
제 3 도는 본 발명의 부분강화방법의 실시예를 보인 설명도.3 is an explanatory view showing an embodiment of a partial strengthening method of the present invention.
Claims (2)