KR900001771A - 드롭특성이 우수한 난연성, 저연 열수축 튜브의 수지조성물 - Google Patents

드롭특성이 우수한 난연성, 저연 열수축 튜브의 수지조성물 Download PDF

Info

Publication number
KR900001771A
KR900001771A KR1019880009307A KR880009307A KR900001771A KR 900001771 A KR900001771 A KR 900001771A KR 1019880009307 A KR1019880009307 A KR 1019880009307A KR 880009307 A KR880009307 A KR 880009307A KR 900001771 A KR900001771 A KR 900001771A
Authority
KR
South Korea
Prior art keywords
flame
weight
parts
retardant
low
Prior art date
Application number
KR1019880009307A
Other languages
English (en)
Inventor
관준연
Original Assignee
서주인
삼성전기 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 서주인, 삼성전기 주식회사 filed Critical 서주인
Priority to KR1019880009307A priority Critical patent/KR900001771A/ko
Publication of KR900001771A publication Critical patent/KR900001771A/ko

Abstract

내용 없음

Description

드롭특성이 우수한 난연성, 저연 열수축 튜브의 수지조성물
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음

Claims (1)

  1. 선형 저밀도 폴리에틸렌 40중량부와 초산비닐량이 5wt%~30wt%로 된 에틸렌 초산비닐 공중합 수지 60중량부에 수산화 무기 화합물을 50~200중량부, 테카르브로모 디페닐 옥사이드를 10~50중량부, 삼산화 안티몬을 5~25중량부로 되는 드롭특성이 우수한 난연성 저연 열수축 튜브의 수지조성물.
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019880009307A 1988-07-25 1988-07-25 드롭특성이 우수한 난연성, 저연 열수축 튜브의 수지조성물 KR900001771A (ko)