Claims (1)
열전도율이 높은 전열시멘트 몰탈을 제조함에 있어, 흑연 50-6-%, 규산소다 36-4-%, 경탄 5-8%, 보강섬유 0.5-1%의 중량비로 배합함을 특징으로 하는 전열시멘트 몰탈 조성물.In manufacturing the electrothermal cement mortar with high thermal conductivity, the electrothermal cement mortar is blended at a weight ratio of 50-6-% graphite, 36-4-% sodium silicate, 5-8% hard coal, and 0.5-1% reinforcing fiber. Composition.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.