Claims (1)
점토의 소결온도보다 용융온도 또는 분해온도가 높은 광물성섬유와 점토를 일정비율로 균분혼합하여 훈련하고 성형, 건조, 소결케함으로써 만들어진 섬유보강 도자기질물Fiber-reinforced porcelain made by mixing, training, forming, drying and sintering mineral fiber and clay at a certain ratio with higher melting or decomposition temperature than clay sintering temperature※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.