KR890002310A - 난연화 수지조성물 - Google Patents
난연화 수지조성물 Download PDFInfo
- Publication number
- KR890002310A KR890002310A KR1019870007951A KR870007951A KR890002310A KR 890002310 A KR890002310 A KR 890002310A KR 1019870007951 A KR1019870007951 A KR 1019870007951A KR 870007951 A KR870007951 A KR 870007951A KR 890002310 A KR890002310 A KR 890002310A
- Authority
- KR
- South Korea
- Prior art keywords
- resin composition
- flame retardant
- retardant resin
- weight
- flame
- Prior art date
Abstract
내용 없음
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
Claims (1)
- 난연화된 수지조성물에 있어서, 베이스 폴리며 97∼60중량%와 다음 일반식(Ⅰ)로 표시되는 인화합물이 난연제 3∼40중량%가 혼합되어 있고, 이 혼합물에 대해 열안정제가 0.01∼10중량% 함유된 것을 특징으로 하는 난연화 수지조성물.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.