내, 외장석재용 방수, 방청 및 광택처리제의 제조방법Manufacturing method of waterproofing, rustproofing and varnish treatment for interior and exterior stone
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.
Claims (1)
실시예 세락 100부에 대하여 메타놀 150부를 1차 혼합하여 세락을 용해시켜 세락용해 조성물(A)을 조성한 다음, 이 조성물 100부에 대하여 다시 트리크로로 에탄 75부를 첨가하여 상온에서 12시간 교반함을 특징으로 하는 내, 외장석재용 방수, 방청 및 광택처리제의 제조방법.EXAMPLES 150 parts of methanol were firstly mixed with 100 parts of cerac to dissolve the cerac to form a composition for dissolving the cerac, and then, 75 parts of ethane was added again with trichloro to 100 parts of the composition, followed by stirring at room temperature for 12 hours. Method for producing a waterproof, rust-preventive and polished agent for interior and exterior stone, characterized in that.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.