KR840000023Y1 - 브라스팅(Blasting)용 탄소봉 - Google Patents
브라스팅(Blasting)용 탄소봉 Download PDFInfo
- Publication number
- KR840000023Y1 KR840000023Y1 KR2019810007469U KR810007469U KR840000023Y1 KR 840000023 Y1 KR840000023 Y1 KR 840000023Y1 KR 2019810007469 U KR2019810007469 U KR 2019810007469U KR 810007469 U KR810007469 U KR 810007469U KR 840000023 Y1 KR840000023 Y1 KR 840000023Y1
- Authority
- KR
- South Korea
- Prior art keywords
- carbon
- carbon electrode
- blasting
- carbon rods
- rods
- Prior art date
Abstract
내용 없음.
Description
제1도는 일부 절개한 본 고안의 사시도.
제2도는 A-A선 확대 단면도.
본 고안은 두터운 철판의 용접, 절단, 가우징하는데 사용하는 탄소봉에 관한 것이다.
종래의 탄소봉은 구리가 피막되어 있어 용접기에 연결된 도치에 탄소봉(길이 35.5cm)을 끼우고 용접이나 절단을 하고 나면 타다 남은 탄소봉의 토막(도치에 물려 있던 4cm 가량의 토막)은 재사용이 불가능하여 폐기 처분하였었다.
그 이유는 구리로 탄소봉이 피막되여 있기 때문에 이를 재사용하기 위해 용광로에 녹이면 알미늄, 망간등은 탄소봉을 구성하는 요소로서 아무런 지장이 없지만 구리만은 용광로에 녹고 있는 다른 물질과 화학반응을 일으켜 재질을 변경시키기 때문이다.
그러므로 타다남은 탄소봉에 피막된 구리를 일일이 벗겨서 탄소알맹이만 가탄제로 사용하려고 하면 피막된 구리를 벗기는 작업에 소요되는 인건비가 많아 비경제적인 결점이 있고, 또 구리로 피막된 탄소봉은 장기간 보관으로 구리가 산화되여 생기는 찌꺼기가 탄소봉과 함께 용접이 되므로 용접부가 잘 떨어지는 폐단이 있었다.
본 고안은 이러한 제결점을 제거하고져 내식성이 좋고, 강도가 있으며, 비중이 가벼운 알미늄으로 탄소봉을 피막하여서 용접이 잘되고, 또 알미늄은 탄소봉을 구성하는 재질로 되어 있기 때문에 용접을 하다가 남은 탄소봉의 토막을 용광로에서 녹여 재사용이 가능하도록 한 것으로 첨부도면에 의거 상술하면 다음과 같다.
공지의 탄소봉(1)에 내식성이 좋고 강도가 있으며 비중이 가벼운 알미늄층(2)을 피막하여서 된 것이다.
이와 같이 구성된 본 고안은 쓰고 남은 탄소봉 토막을 용광로에 투입하면 알미늄층은 녹아 망간과 철등과 같이 탄소봉을 만드는 요소로 재사용되고, 알미늄 피막이 녹여진 탄소봉은 가탄제 역활을 하여 용광로의 용융 온도를 높여주게 되는 것이다.
이와 같이 된 본고안은 종래와 같이 탄소봉 토막에 피복된 구리를 일일이 벗기지 않아도 탄소봉의 재사용이 가능하므로 인건비를 절약하는 경제적인 이점이 있으며, 내식성인 알미늄층으로 피막이 되여 있기 때문에 장소에 구애됨이 없이 장기간 보관이 가능하여, 또 용접활 때 알미늄층도 같이 용해되어 용접부를 더욱 견고히 하는 등의 이점이 있다.
Claims (1)
- 도시한 바와 같이 공지의 탄소봉(1)에 내식성이 좋고 강도가 있으며 비중이 가벼운 알미늄층(2)을 피막함을 특징으로 하는 브라스팅(Blasting)용 탄소봉.