유리면에 서리무늬형성방법How to Form Frost Patterns on Glass Surface
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.
Claims (2)
유리면에 샌딩가공함에 있어서, 아크릴에멀죤 350cc, 포리비닐알콜 5G, 카복시메칠세루로오즈 20G을 혼합 교반하여 110℃에 30분간 가열한 제1액과, 아크릴에멀죤 600cc, 분말탈크 30G, 중크롬산암모니아소 3cc를 혼합진탕한 제2액을 강제 혼합하여서된 점성조성물로 유리면에 보호피막을 형성함을 특징으로하는 유리면에 서리무늬 형성방법.In the sanding process of glass surface, the first liquid heated by mixing and stirring acrylic emulsion 350cc, polyvinyl alcohol 5G, carboxymethylcellulose 20G for 30 minutes at 110 ° C, acrylic emulsion 600cc, powder talc 30G, ammonia dichromate A method of forming a frost pattern on a glass surface, characterized by forming a protective film on the glass surface with a viscous composition obtained by forcibly mixing a second liquid mixed with bovine 3cc.제1항에 있어서 조성된 점성조성물을 스크린인쇄도포법에 의하여 유리면에 보호피막을 형성하는 공정.The process of forming a protective film on the glass surface by the screen printing coating method of the viscous composition formed in Claim 1.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.
KR1019820000946A1982-03-051982-03-05
How to Form Frost Patterns on Glass Surface