KR20200012350A - Ethnic wood and its manufacturing method - Google Patents

Ethnic wood and its manufacturing method Download PDF

Info

Publication number
KR20200012350A
KR20200012350A KR1020180087524A KR20180087524A KR20200012350A KR 20200012350 A KR20200012350 A KR 20200012350A KR 1020180087524 A KR1020180087524 A KR 1020180087524A KR 20180087524 A KR20180087524 A KR 20180087524A KR 20200012350 A KR20200012350 A KR 20200012350A
Authority
KR
South Korea
Prior art keywords
wood
natural
timber
ethnic
present
Prior art date
Application number
KR1020180087524A
Other languages
Korean (ko)
Inventor
이욱재
이종우
Original Assignee
주식회사 자인우드
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 주식회사 자인우드 filed Critical 주식회사 자인우드
Priority to KR1020180087524A priority Critical patent/KR20200012350A/en
Publication of KR20200012350A publication Critical patent/KR20200012350A/en

Abstract

The present invention provides ethnic wood and a manufacturing method thereof. The present invention utilizes domestic timber, preserves the texture and feel of natural timber which hardwood has while making vegetable natural oil permeate thereto to preserve the wood grain of the timber, and improves the durability, waterproofness, and antiseptic properties which the timber lacks. The present invention upgrades to an eco-friendly, natural and emotional material. The vegetable natural oil mixed with a pigment penetrates the timber such that the color is not uniform or opaque. The present invention improves various colors, functionality, and aesthetics and upgrades domestic timber to high-quality materials such as interior finishing materials, small furniture, and accessories. According to the present invention, the manufacturing method of ethnic wood comprises: a step of lumbering hardwood into a plank; a step of drying the lumbered plank; a step of processing the dried plank by planning four sides; and a step of coloring depending on the natural knot or wood grain of the timber of the processed plank planed at four sides.

Description

에스닉우드 및 그 제조방법{Ethnic wood and its manufacturing method}Ethnic wood and its manufacturing method

본 발명은 에스닉우드(ethnic wood)에 관한 것으로, 보다 상세하게는, 원목이 갖고 있는 천연목재의 질감과 느낌을 그대로 살리면서 식물성 천연오일로 마감하여 친환경적이고 감성적인 인테리어 마감재 및 소가구와 소품의 소재로 사용되는 에스닉우드 및 그 제조방법에 관한 것이다.The present invention relates to an ethnic wood, and more particularly, eco-friendly interior finishing materials and materials of small furniture and accessories by finishing with natural vegetable oil while maintaining the texture and feel of natural wood as it is. It relates to ethnic wood and its manufacturing method used as.

통상적으로 건축물에 사용되는 마감재는 다양한 미적 효과를 얻을 수 있도록 특정 무늬를 형성한 필름지나 무늬판부재를 부착하여 사용해 오다가, 인테리어에 대한 관심이 많아지면서 인테리어용 마감재 또는 소품의 소재로 원목을 사용하게 되었는데, 원목을 사용할 때는 천연 목재가 갖는 칼라와 나무결을 살리기 위해 목재에 투명한 오일 또는 니스를 칠하여 사용하게 되었고, 국산 목재는 수령(樹齡)도 작고 성장의 속도도 느려서 직경이 작고 더군다나 옹이와 같은 목재로서의 결함이 많으며, 옹이, 송진, 청태, 병충해 등의 발생 때문에 고가의 목재로서는 부족함이 많기 때문에 특히 고가(高價)의 원목은 대부분 수입목을 사용하고 있다. 한편, 원목은 나이테에 의한 자연스런 모양과 색감의 무늬가 형성되어 있어서 미적 측면에서는 우수하다 할 수 있으나 고가이기 때문에 원목을 얇게 켜서 만든 무늬목을 MDF와 같은 판재에 부착시켜 사용한 경우가 많았다.Normally, finishing materials used in buildings are used by attaching film or pattern plate member with a specific pattern to obtain various aesthetic effects, and using wood as an interior finishing material or accessory material with increasing interest in interiors. When using solid wood, natural wood was used by applying transparent oil or varnish to the color and wood texture of natural wood. Domestic timber has a small diameter and slow growth rate, so it is smaller and more like knots. There are many defects as wood, and because of the occurrence of knots, rosin, cherries, pests, etc., there are many shortages of expensive wood, and especially expensive wood is mostly imported wood. On the other hand, solid wood has a natural shape and color pattern formed by rings, which can be said to be excellent in terms of aesthetics. However, it is often used to attach a pattern made of thin wood to a plate such as MDF.

하지만 메마른 도시환경 속에서 살아가는 대다수의 현대인들은 주거환경을 자연의 숨결이 느껴지도록 바꾸기를 원하고 있고, 최근들어 삶의 질에 대한 욕구가 증가하면서 웰빙(Well-being) 의식의 확대 및 경제 수준의 향상으로 친환경적이고 친자연적이며 감성적인 소재에 대한 관심이 점점 증가하고 있다. 이러한 추세에 맞춰 실내에서 화분을 가꾸거나 정원에 나무를 심는 것은 물론 주거공간의 바닥재와 인테리어 마감재로 원목을 사용하는 경향이 점차로 늘고 있다.However, most modern people living in barren urban environments want to change their living environments to feel the breath of nature. Recently, as the desire for quality of life has increased, well-being awareness and economic Increasingly, there is a growing interest in environmentally friendly, natural and emotional materials. In line with these trends, there is an increasing tendency to use wood as a flooring and interior finishing material in residential spaces, as well as planting pots or planting trees in the garden.

상기와 같은 추세에 맞춰 출현한 기술을 예로 들면, 특허등록 제1466250호 "인테리어 및 건축용 목재와 그 제조방법"은 원목을 얇게 켜서 무늬목을 형성하고 무늬목의 일면에 편백나무 추출물을 함침시킨 후에 MDF에 접합시켜서 만든 인테리어 및 건축용 목재에 관한 기술이다. 또한, 공개특허 제2015-122495호 "편백나무 추출 원액과 오일 혼합액이 첨가된 가구 보드 원목 인테리어 건축 마감재 제조방법 및 그 마감재"는 편백나무 추출 원액 및 편백나무 오일을 수용성 방염제와 혼합하여 캡슐화하여 다양한 무늬가 인쇄된 크라프트지에 함침시켜 다양한 무늬를 갖게 한 시트지를 MDF 또는 PB 보드에 부착하여 만든 인테리어 및 건축용 마감재에 관한 것이다.Taking the technology that appeared in accordance with the above trend, for example, Patent Registration No. 1466250 "Interior and architectural wood and its manufacturing method" is to turn the wood thinly to form a veneer, impregnated with a cypress extract on one side of the veneer in MDF It is a technology about interior and building wood made by joining. In addition, Korean Patent Publication No. 2015-122495 "Current board wood interior construction finishing material manufacturing method and the finishing material is added to the cypress extract stock and oil mixture liquid" is a variety of encapsulated by mixing the cypress extract stock and cypress oil with a water-soluble flame retardant The present invention relates to interior and building finishing materials made by attaching sheet paper, which is impregnated with printed kraft paper, to various patterns, to MDF or PB boards.

상기 기술 뿐만 아니라 지금까지 국내에서 출현했던 소위 친환경적이고 친자연적이라고 불리어지는 인테리어 소재는 대부분 MDF 또는 PB 보드와 같은 판재에 얇게 켜서 만든 무늬목을 부착하여 외관만 원목처럼 보이게 하여 무늬만 원목이거나, 원목 표면에 단순히 오일 또는 니스를 칠한 정도의 것이고 원목 소재도 대부분 수입목을 사용하고 있다는 문제가 있다. 물론 국산 목재의 경우는 대부분 굵기가 가늘고 질이 떨어질 뿐만 아니라 수종이 제한적이고 목재를 건조하는 기술수준이 매우 낮다는 문제도 있다.In addition to the above technology, the so-called interior and environmentally friendly interior materials that have emerged in Korea so far are mostly attached to thin plates such as MDF or PB boards to make the exterior look like solid wood, so that only the pattern is solid wood, or the surface of wood There is a problem that oil or varnish is simply applied, and the wood materials are mostly imported wood. Of course, in the case of domestic timber, most of them are not only thin and poor in quality, but also have a limited number of species and a very low level of technology for drying wood.

한편, 국내산 목재는 건축자재로 사용 가능한 것이 거의 없기 때문에 건축자재로 사용되는 목재는 거의 수입에 의존하고 있는 실정이며, 우리나라에서는 벌목 허가도 받기 어렵지만 간벌(間伐)하여 나온 목재도 폐목재로 버려지거나 화목(火木)으로 사용되는 경우가 많고, 또한, 간벌한 목재에 흠결이 있는 경우가 많아서 활용되지 못하고 버려지는 경우가 많기 때문에 국가적인 차원에서도 이들을 활용할 수 있는 방안을 찾는 일이 절실하고 시급하다고 하겠다.On the other hand, since domestic timber is rarely used as a building material, timber used as a building material is almost dependent on imports. In Korea, logging permits are difficult to obtain, but thinned wood is discarded as waste wood. It is often used as a firewood, and because there are many defects in thin timber, it is not used and is often discarded. Therefore, it is urgent and urgent to find a way to use them at the national level. would.

본 발명은 상기와 같은 문제를 해결하기 위하여 안출된 것으로, 본 발명의 목적은, 국내산 목재를 활용하여 원목이 갖고 있는 천연목재의 질감과 느낌을 그대로 살리면서 식물성 천연오일을 침투시켜 목재의 무늬결을 살리면서 목재에 부족한 내구성과 방수성 및 방부성 등을 향상시키고, 친환경적이고 친자연적이며 감성적인 소재로 업그레이드시킨 에스닉우드 및 그 제조방법을 제공하기 위한 것이다.The present invention has been made to solve the above problems, the object of the present invention, by utilizing the domestic wood while maintaining the texture and feel of the natural wood has a natural wood infiltrate the natural oil infiltrate the texture of the wood It is to provide ethnic wood and its manufacturing method that are upgraded with environmentally friendly, natural and emotional materials while improving the durability, waterproofness, and antiseptic properties, which are lacking in wood.

본 발명의 다른 목적은, 안료를 혼합한 식물성 천연오일을 목재에 침투시켜 색상이 획일적이거나 불투명하지 않고 다양한 색상과 기능성 및 심미성을 향상시켜 국산 목재를 인테리어 마감재와 소가구 및 소품 등의 고급 소재로 업그레이드시킨 에스닉우드 및 그 제조방법을 제공하기 위한 것이다.Another object of the present invention, by infiltrating the natural vegetable oil mixed with the pigment to the wood is not uniform or opaque to improve a variety of colors, functionality and aesthetics to upgrade the domestic wood to high-quality materials such as interior finishing materials and small furniture and accessories To provide ethnic wood and a method for producing the same.

본 발명에 따른 에스닉우드 제조방법은, 원목을 판재(板材)로 제재(製材)하는 단계; 제재한 판재를 건조시키는 단계; 건조시킨 판재를 사면대패하여 가공하는 단계; 사면대패하여 가공한 판재가 갖고 있는 목재 본연의 옹이나 나무결에 맞춰 컬러링하는 단계를 거쳐서 제조하는 것을 특징으로 한다.Ethnic wood manufacturing method according to the invention, the step of lumbering the wood into a sheet (재); Drying the plated material; Processing the sloped plate by drying the plate; It is characterized by manufacturing through the step of coloring according to the natural wood or wood texture of the plate processed by the slope planer.

바람직하게는, 건조시키는 단계에서는, 응달에서 3∼5개월 동안 자연건조시키는 공정을 거친 후, 자연건조시킨 판재를 내부온도가 100∼150℃인 컨테이너 형상의 킬른(kiln) 내에 적층시켜 3∼10일 동안 인공건조시키는 공정을 거친다.Preferably, in the drying step, after the natural drying process for 3 to 5 months in the shade, the naturally dried sheet is laminated in a kiln of a container shape having an internal temperature of 100 to 150 ° C. for 3 to 10 months. The process is artificially dried for days.

바람직하게는, 컬러링하는 단계에서는 식물성 천연오일을 판재에 도포하며, 특정 컬러를 내기 위해서는 안료를 혼합한다.Preferably, in the coloring step, the vegetable natural oil is applied to the plate, and the pigment is mixed to give a specific color.

본 발명에 따른 에스닉우드는 국내산 목재를 벽재, 아트월(art wall), 가구, 장난감, 바닥재, 생활소품 및 인테리어 등의 소재로 사용하도록 하여 벌목이나 간벌재로 나온 목재를 폐기시키거나 화목(火木)으로 사용하지 않고 실용적으로 사용할 수 있게 하여 국내산 목재의 활용도를 높였다는 점만으로도 국가적 차원에서 목재수입을 줄이면서 우리 산림자원의 경제적·산업적 활용이라는 측면에서 충분한 가치가 있고 우수한 평가를 받을 수 있다.Ethnic wood according to the present invention is to use domestic timber as a wall material, art wall (art wall), furniture, toys, flooring materials, living goods and interior materials, such as timber from timber felling or thinning materials or firewood (火 木By increasing the utilization of domestic timber by making it practically available instead of using it, it is worth noting that it is worthwhile and excellent in terms of economic and industrial use of our forest resources while reducing timber imports at the national level.

또한, 본 발명에 따른 에스닉우드는 원목을 자연건조와 인공건조를 시킨 후에 가공한 것이기 때문에 틀어짐이나 변형 등이 발생하지 않고, 목재에 있는 옹이 또는 나이테, 일부 흠결 등의 모양을 그대로 살려 가공을 하고 컬러링을 하기 때문에 나무가 갖고 있는 우아하고 은은하며 자연스러운 천연목재 본연의 질감과 느낌이 그대로 살아 있고, 식물성 천연오일을 침투시켜 은은한 향(香)과 목재가 갖는 자연미를 최대한 살리면서 기능성, 내구성, 방수성 및 방부성을 향상시킨 친환경적이고 친자연적이며 감성적인 인테리어 마감재와 소가구 및 소품 등의 소재로 업그레이드시켜 매우 유용하게 사용될 수 있으며, 건조과정에서 원목에 함유되어 있던 송진이 완전히 제거되기 때문에 원목 자체가 뽀송뽀송하여 제품화 된 에스닉우드에 먼지가 앉더라도 먼지만 닦아내면 처음과 같이 뽀송뽀송한 상태로 된다. 특히, 최근 빈티지(vintage) 스타일의 인테리어가 많은 관심을 끌고 있는 점을 감안했을 때, 이런 시류에 가장 적합하고 업그레이드된 인테리어 소재이다.In addition, the ethnic wood according to the present invention is processed after the natural wood and artificial drying, so that there is no distortion or deformation, and processing by utilizing the shape of knots or rings, some scratches, etc. in the wood as it is Because of the coloring, the wood's natural texture and feel is elegant, soft and natural. The natural texture and feel of the wood remain intact, and it penetrates natural vegetable oils to maximize the subtle fragrance and natural beauty of wood, while maintaining functionality, durability and waterproofness. And eco-friendly, natural and emotional interior finishing materials with improved antiseptic properties, and upgraded to materials such as small furniture and props, which can be used very usefully. As the rosin contained in the wood is completely removed during the drying process, the wood itself is smooth. Even if dust sits on commercialized ethnic wood But inside is a pposong one pposong status as the first wipe. In particular, given the recent interest in vintage-style interiors, it is the most suitable and upgraded interior material for this series.

도 1 내지 도 4는 본 발명에 따른 에스닉우드를 다양한 색상으로 도포하여 제조한 실물 사진이다.
도 5는 에스닉우드의 제조방법을 개략적으로 나타낸 순서도이다.
1 to 4 are real photos produced by applying ethnic wood according to the present invention in various colors.
5 is a flowchart schematically showing a method of manufacturing ethnic wood.

본 발명에 따른 에스닉우드의 가장 큰 기술적 특징은, 우아하고 은은하며 자연스러운 원목 본연의 질감과 느낌을 살리면서 안료를 혼합한 식물성 천연오일로 마감하여 목재에 부족한 내구성과 방수성 및 방부성을 향상시키며 다양한 색상과 기능성 및 심미성을 갖는 친환경적이고 감성적인 마감재를 구현했다는 점이다.The biggest technical feature of ethnic wood according to the present invention is to finish with natural natural vegetable oil mixed with pigments while utilizing the natural texture and feel of elegant, soft and natural wood to improve the durability and waterproofness and antiseptic property that wood lacks, and various colors. It is an eco-friendly and emotional finish with functional and aesthetic.

본 명세서에서 에스닉우드(ethnic wood)란 국산 목재, 특히 소나무과에 속하는 목재를 일정 두께(30㎜ 이하)의 판재로 제재(製材)하여 본 발명에 따른 제조방법으로 제조하여 자연스러운 천연목재 본연의 질감과 느낌을 가지면서 내구성과 방수성 및 방부성을 갖는 목재로, 벽재, 아트월(art wall), 가구, 장난감, 바닥재, 생활소품 등으로 사용되는 목재를 말한다. 일반적인 나무의 구조를 살펴보면, 중앙에 단단하고 색이 진한 심재, 이를 원주 방향으로 둘러싸는 색이 옅은 부분인 변재 및 이를 둘러싸는 껍질로 구성되어 있으며, 성장이 빠른 봄과 여름에는 세포막이 얇고 색이 연한 춘재와, 성장이 더딘 가을과 겨울에는 세포막이 두껍고 단단하며 짙은 추재가 반복되어 나이테를 생성하며, 나무의 줄기에서 가지가 뻗어나와 목질이 구성된 옹이를 형성하게 되며, 일부에는 벌레가 먹거나 흠결이 있는 부분이 있을 수도 있는데, 에스닉우드는 이와 같은 원목이 갖는 본연의 무늬를 그대로 살리고 기능성과 내구성을 가미한 목재이다.In this specification, ethnic wood (ethnic wood) is produced by the manufacturing method according to the present invention by the domestic wood, in particular wood belonging to the pine family with a plate of a certain thickness (30 mm or less) and natural natural wood and natural texture and It is a wood that has a feeling of durability, waterproofness and antiseptic, and is used as a wall material, art wall, furniture, toys, flooring, household goods, and the like. Looking at the structure of a general tree, it is composed of a hard and dark heartwood in the center, a sapwood that is a light part surrounding the circumferential direction, and a bark surrounding it. In soft autumn and winter, slow and slow growth, the cell membranes are thick, hard, and dense woodwoods, which produce rings, with branches extending from the trunks of trees, forming woody knots. There may be a part of it, and ethnic wood is a wood that preserves the original pattern of the wood and adds functionality and durability.

본 발명의 에스닉우드의 제조방법은, 원목을 판재(板材)로 제재(製材)하는 단계(S1)와, 제재한 판재를 건조시키는 단계(S2)와, 건조시킨 판재를 사면대패하여 가공하는 단계(S3)와, 사면대패하여 가공한 판재가 갖고 있는 목재 본연의 옹이나 나무결에 맞춰 컬러링하는 단계(S4)를 기본적으로 거쳐서 제조하게 된다.In the method of manufacturing ethnic wood of the present invention, the step (S1) of lumbering the wood into a plate (S), the step of drying the banung board (S2), and the step of processing the sloped plate of the dried board (S3) and the step of coloring according to the natural wood or wood grains of the plate processed by the slope planer (S4) is basically produced through.

원목은 국산 목재를 사용하는데, 특히 소나무과(학명: Pinaceae)에 속하는 목재가 적합하며, 70년생 이상의 나무를 사용하는 것이 바람직하고, 벌레가 먹거나 곰팡이가 슨 목재도 사용할 수 있다. 원목을 판재로 제재할 때는 건조시키는 단계에서 수축될 것을 감안하여 약간 크기의 여유를 두고 제재하여야 한다.Logs use domestic timber, especially those belonging to the pine family (Pinaceae), suitable for trees over 70 years old, and insect-eaten or moldy wood. When lumber is lumbered, it should be lumbered with some size to allow for shrinkage during drying.

건조시키는 단계(S2)에서는 자연건조와 인공건조 모두를 거치는 것이 바람직하며, 이 과정에서 판재가 건조되어 나무 고유의 색상이 나타나면서 내재되어 있던 수분과 송진 등이 제거되게 된다. 자연건조는 응달에서 3∼5개월 동안 자연건조시켜 함수율 30∼40% 정도로 건조키는 공정인데, 건조과정에서 급작스런 온도 및 습도 변화가 있으면 제재된 판재가 뒤틀리거나 갈라지고 옹이가 탈거하게 되어 원목 본연의 질감과 느낌이 없어지므로 주의하여야 한다. 제재된 판재를 자연건조만 시킬 경우에는 나중에 컬러링 공정에서 식물성 천연오일을 도포할 경우 오일이 판재에 침투하지 못하고 표면에서 얼룩지기 때문에 자연건조시킨 후에 인공건조를 시켜 주어야 한다.In the drying step (S2), it is preferable to go through both natural drying and artificial drying, and in this process, the board is dried to remove the moisture and rosin that are inherent while the color of the wood appears. Natural drying is the process of drying in the shade for 3 to 5 months and drying it at about 30 to 40% of moisture content. If there is a sudden change in temperature and humidity during the drying process, the board is warped or cracked and knots are removed. Care must be taken as the texture and feel of the product will disappear. In case of only natural drying of the sanctioned plate, when applying vegetable natural oil in the coloring process, oil should not penetrate into the plate and stain on the surface, so it must be artificially dried after natural drying.

인공건조는 자연건조시킨 판재를 열풍과 압력에 의해 스팀에 의해 습식으로 건조시키는 컨테이너 형상의 킬른(kiln) 내에 일정 간격을 갖도록 적층시켜서 내부온도가 100∼150℃ 상태에서 3∼10일 동안 건조시켜서 목재의 함수율이 10∼20% 정도가 되도록 건조시킨다. 이때 컨테이너 형상의 킬른 내부에 스팀을 공급하면서 열풍과 압력을 가하면 스팀이 킬른 내부에 적층된 판재 사이를 대류 현상에 의해 순환하게 되면서 판재에 함유된 수분과 송진이 제거되게 된다. 만일 스팀에 열풍과 압력을 가하지 않으면 목재 내부의 송진이 완전히 제거되지 않고 잔류하게 되어 에스닉우드로 만들어진 제품에서 계속 송진 등이 흘러내리면서 표면이 끈적끈적하게 되고 이물질이 달라붙게 되는 문제가 있다.Artificial drying is laminated in a container-shaped kiln to dry the plate dried naturally by steam with hot air and pressure at regular intervals, and dried for 3 to 10 days at an internal temperature of 100 ~ 150 ℃ It is dried so that the moisture content of wood is about 10-20%. In this case, when hot air and pressure are applied while supplying steam into the kiln of the container shape, steam is circulated between the plates stacked in the kiln by convection, thereby removing moisture and rosin contained in the plate. If the hot air and pressure are not applied to the steam, the rosin inside the wood is not completely removed and remains, and the rosin and the like continue to flow down from the product made of ethnic wood, and the surface becomes sticky and foreign matters stick.

가공단계(S3)에서는 건조시킨 판재를 일정 형상으로 가공하는 공정으로, 원형 톱이나 대패를 사용하여 사면대패(four side plaining moulding)를 하여 필요로 하는 두께와 폭으로 가공한다. 이때 제재한 판재(板材)의 두께가 10㎜ 이하인 것은 일면을 벽에 부착하고 일면을 컬러링 처리하여 벽재나 마감재로 주로 사용되고, 그 이상의 두께로 제재된 판재는 양면 모두를 컬러링 처리하여 양면 모두를 사용하게 된다. 컬러링 단계에서 두께가 10㎜ 이하로 얇은 판재는 일면만 오일을 도포하여 컬러링 하고, 그 이상으로 두꺼운 판재는 일면만 컬러링하면 원목(판재)이 휘거나 뒤틀어질 수 있으므로 양면 모두에 오일을 도포하여 컬러링을 하여야 한다.In the processing step (S3) is a process of processing the dried sheet material to a certain shape, using a circular saw or a planer using a four side plaining moulding to process the required thickness and width. At this time, the thickness of the plated material (10) is less than 10㎜ is used mainly as a wall material or finishing material by attaching one surface to the wall and coloring one surface, and the plated material with more thickness is used by coloring both sides. Done. In the coloring step, thin plates with a thickness less than 10 mm are colored by applying oil on one side only, and thicker plates may be bent or distorted by coloring only one side. Should be done.

가공공정이 끝나면 판재의 옹이나 무늬의 모양에 맞춰 일정 폭마다 길이방향을 따라 라인(line)을 넣거나, 면 전체에 오일을 도포하거나 오일에 적절한 안료를 혼합하여 골드, 블랙, 블루 등 적절한 컬러를 발현하게 하는 컬러링 단계(S4)를 거치게 된다(도 1 내지 4 참조). 컬러링하는 단계에서는 식물성 천연오일 또는 식물성 오일에 안료를 혼합하여 판재에 도포하는 공정이다. 오일은 천연수지로 만들어 진 것으로, 도포후 매우 빠르게 건조되는 특성이 있고, 목재에 도포된 후에는 도막을 형성하고 물기에 대한 내구성을 가진 표면을 형성하기 위해 목재의 기공을 채우면서 목재 깊은 곳까지 침투하게 되며, 양생된 표면은 강력한 도막과 내수성(耐水性)을 갖게 해주며, 보호층이 두껍게 형성되기 때문에 외부 충격이 가해지더라도 목재의 손상을 막아주게 되어 내구성이 현저하게 향상된다.After finishing the process, put a line along the length direction every width according to the shape of the plate's knot or pattern, apply oil on the whole surface or mix the appropriate pigment in oil to get proper color such as gold, black, blue Through the coloring step (S4) to be expressed (see Figures 1 to 4). In the coloring step, a pigment is mixed with vegetable natural oil or vegetable oil and applied to a plate. The oil is made of natural resin, which dries very quickly after application, and after it is applied to wood, it fills the pores of the wood to form a coating and to form a surface that is durable against moisture. Penetrated, the cured surface has a strong coating and water resistance (막 水性), and because the protective layer is formed thick to prevent damage to wood even if an external impact is applied, durability is significantly improved.

오일을 도포할 때는 필요에 따라 안료를 혼합하여 면 전체 또는 라인(line)을 따라 적절한 색상을 나타내도록 하는데, 컬러링할 때는 붓, 솜 또는 적절한 도구를 사용하여 칠하거나 분무하여 도포하는데, 1차로 도포한 다음 건조시킨 후에 수회에 걸쳐서 도포작업을 한다. 식물성 천연오일을 도포함으로써 에스닉우드에 친환경 기능성과 더불어 도막과 내수성(耐水性)을 부여하면서 클래식한 질감과 유니크한 색감을 발현할 수 있다. 또한, 모든 목재는 그 자체로 오일과 레진 성분을 가지고 있기 때문에 풍화나 흰개미와 같은 해충으로부터 스스로를 보호하는 특성이 있지만, 목재를 제재(製材)한 후에는 이런 오일에 의한 효과가 현저하게 감소하게 되는데, 본 발명에 따른 에스닉우드는 제재된 목재에 천연수지로 만든 오일을 도포하여 침투시켜서 목재를 보호하는 효과를 주게 된다.When applying the oil, mix the pigments as necessary to give the proper color along the entire surface or line.When coloring, apply with a brush, cotton or a suitable tool to paint or spray. After drying, apply several times. By applying natural vegetable oils, you can express classic textures and unique colors while giving ethnic wood coatings and water resistance. In addition, all woods have oil and resin properties that protect themselves from pests such as weathering and termites, but after they are lumbered, the effects of these oils are significantly reduced. The ethnic wood according to the present invention has an effect of protecting the wood by penetrating by applying the oil made of natural resin to the wood.

이상의 설명은 본 발명을 예시적으로 설명한 것이고, 명세서에 게시된 실시예는 본 발명의 기술사상을 한정하기 위한 것이 아니라 설명하기 위한 것이므로 본 발명이 속하는 기술분야에서 통상의 지식을 가진 자라면 본 발명의 기술사상을 벗어나지 않는 범위에서 다양한 수정 및 변형이 가능할 것이다. 그러므로 본 발명의 보호범위는 청구범위에 기재된 사항에 의해 해석되고, 그와 균등한 범위 내에 있는 기술적 사항도 본 발명의 권리범위에 포함되는 것으로 해석되어야 할 것이다.The above description illustrates the present invention by way of example, and the embodiments disclosed in the specification are not intended to limit the technical spirit of the present invention, but to explain the present invention, so that those skilled in the art to which the present invention pertains can understand the present invention. Various modifications and variations will be possible without departing from the spirit of the technology. Therefore, the protection scope of the present invention is to be interpreted by the matter described in the claims, it should be interpreted that the technical matters within the scope equivalent to that included in the scope of the present invention.

Claims (4)

원목을 판재(板材)로 제재(製材)하는 단계;
제재한 판재를 건조시키는 단계;
건조시킨 판재를 사면대패하여 가공하는 단계;
사면대패하여 가공한 판재가 갖고 있는 목재 본연의 옹이나 나무결에 맞춰 컬러링하는 단계;
를 거쳐서 제조하는 것을 특징으로 하는 에스닉우드 제조방법.
Lumbering wood with plate;
Drying the plated material;
Processing the sloped plate by drying the plate;
Coloring according to the natural wood or wood texture of the plate processed by the slope plane;
Ethnic wood manufacturing method characterized in that the manufacturing through.
제1항에 있어서, 상기 건조시키는 단계는,
응달에서 3∼5개월 동안 자연건조시키는 공정을 거친 후,
자연건조시킨 판재를 내부온도가 100∼150℃인 컨테이너 형상의 킬른(kiln) 내에 적층시켜 3∼10일 동안 인공건조시키는 공정을 거치는 것을 특징으로 하는 에스닉우드 제조방법.
The method of claim 1, wherein the drying step,
After 3 to 5 months of natural drying in the shade,
An ethnic wood manufacturing method comprising the step of laminating the naturally dried sheet material in a kiln (kiln) of the container shape having an internal temperature of 100 ~ 150 ℃ subjected to artificial drying for 3 to 10 days.
제1항에 있어서,
상기 컬러링하는 단계에서는 식물성 천연오일을 판재에 도포하는 것을 특징으로 하는 에스닉우드 제조방법.
The method of claim 1,
In the coloring step, ethnic wood manufacturing method, characterized in that the vegetable oil is applied to the plate.
제1항 내지 제3항 중 어느 하나의 항에 기재된 방법에 의해 제조된 것을 특징으로 하는 에스닉우드.Ethnic wood produced by the method according to any one of claims 1 to 3.
KR1020180087524A 2018-07-27 2018-07-27 Ethnic wood and its manufacturing method KR20200012350A (en)