KR20130122292A - A manufacturing method of salt comprising quantum energy occurrence material - Google Patents

A manufacturing method of salt comprising quantum energy occurrence material Download PDF

Info

Publication number
KR20130122292A
KR20130122292A KR1020120045494A KR20120045494A KR20130122292A KR 20130122292 A KR20130122292 A KR 20130122292A KR 1020120045494 A KR1020120045494 A KR 1020120045494A KR 20120045494 A KR20120045494 A KR 20120045494A KR 20130122292 A KR20130122292 A KR 20130122292A
Authority
KR
South Korea
Prior art keywords
salt
quantum energy
generating material
energy generating
quantum
Prior art date
Application number
KR1020120045494A
Other languages
Korean (ko)
Inventor
이순일
Original Assignee
이순일
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 이순일 filed Critical 이순일
Priority to KR1020120045494A priority Critical patent/KR20130122292A/en
Publication of KR20130122292A publication Critical patent/KR20130122292A/en

Abstract

The present invention comprises the steps of preparing a drinking water containing a quantum energy generating material; Preparing salt; Injecting drinking water containing the quantum energy generating material into the salt and adhering to the salt; And a method for producing a salt including a quantum energy generating material comprising drying the salt to which the drinking water containing the quantum energy generating material is attached. It is effective to take energy generating substance.

Description

A manufacturing method of salt comprising quantum energy occurrence material

The present invention relates to a method for preparing a salt containing a quantum energy generating material, and more particularly, to prepare a salt containing a quantum energy generating material, which allows a consumer to easily consume and absorb the quantum energy generating material. It is about a method.

In general, in the field of energy medicine of alternative medicine, many efforts have been made to treat diseases of the human body by making microenergy, and various methods of making microenergy have been developed.

In particular, various foreign quantum energy generators have been invented for the treatment of patients with cancer, skin cancer, diabetes, etc. by applying the principle of quantum mechanics in foreign countries. There are various cases that can be used to cure patients with facial cancer, cancer, arthritis, skin cancer and diabetes.

The following shows the method of generating quantum energy in quantum mechanics of the energy medicine of the great medicine.

1. How to use Self-Canceling Coil.

Most Sub-Energy (SE) generators use a 180-degree interaction of two electromagnetic fields to generate an SE, a self-dissipating coil discovered by Tesla at the beginning of the 20th century.

It is also called Tesla Coil, Inductive Toroid Coil, and the principle of Tesla Coil is to wind the wire in a certain direction to make a coil, and then to wind the wire in the opposite direction from the first one. When a current flows in the field, the right and left windings make magnetic fields opposite to each other, so the two magnetic fields cancel each other and become magnetic fields. This energy is called non-Hertzian energy. .

2. How to use a variant of an inductive toroidal coil (Tesla Coil).

Modified Tesla coils are called Moebius Coil or Caduceus Coil, which are topological variations of Tesla coils, and the field of studying the energy in such phased coils is called phase electronics. .

Mobius coils have a toroidal model in their inner spiral, which is similar to a toroid, but the difference between Tesla and Mobius coils is that the electrons have the same spectral current as the SE input. It has frequency information, and the latter has a whole new complex harmonic vibration.

In addition, by synthesizing a new waveform by mixing several waves using a method mainly used in nonlinear optics, an SE is generated by mixing four waves without using a self-extinguishing coil, according to Abram. The SE generated by the method is larger than the amplitude of the first introduced electromagnetic field so that a high strength SE can be obtained.

3. How to use phase matching

This method is also commonly used in nonlinear optics, which is called phase-matching to make an SE without the use of a self-destroying coil. According to Pepper, when an electromagnetic field is reflected on a nonlinear mirror, the SE energy, which is the original source of the electromagnetic vector, is paired in phase. In other words, the replicated energy is time-reversed, returning to the original energy from which the electromagnetic vector originated, or SE energy, a technique that Raymond Rife used in the 1930s to create high-power life microscopes. It is also.

4. How to use plasma tube

This method generates SE waves in nonlinear plasma physics. According to Well in 1970, the plasma suddenly pulses. Plasma is a complex structure that contains SE energy such as various types of electromagnetic fields, light, circularly polarized Alven Wave, and ionic acoustic waves, and the vortex ring structure of the plasma is generated by Bostick. It has already been foreseen that the SE energy is released from the plasma tube because it has been observed experimentally. Using this technique, Prior of France and Rife of the United States have been used to treat cancer.

Through the method of generating the quantum energy, the terms of the term such as quantum energy = super quantum energy = Scalar energy = non-Hertzian energy are different, but the meaning can be interpreted as the same meaning. Able to know.

However, a quantum energy generator for the purpose of healing the human body has been developed using the above-described quantum energy generating method, which artificially generates quantum energy by a current device to penetrate the human body. The production cost and installation cost is expensive, there is a problem that is not efficient because it is restricted by time and place.

Therefore, various studies to overcome the constraints of the time and place of the quantum energy generating device must be carried out, and in particular, various studies are required to penetrate into the human skin by receiving quantum energy even in real life.

A problem to be solved by the present invention is to process a quantum energy generating material in which natural quantum energy is generated and amplified by using an artificial hemochromatite, which is collected in the region of 0 Gauss and in which natural quantum energy is generated.

In addition, an object of the present invention is to enable consumers to easily consume the quantum energy generating material.

The objects of the present invention are not limited to the above-mentioned objects, and other objects not mentioned can be clearly understood by those skilled in the art from the following description.

In order to solve the above problems, the present invention comprises the steps of preparing a drinking water containing a quantum energy generating material; Preparing salt; Injecting drinking water containing the quantum energy generating material into the salt and adhering to the salt; And it provides a method for producing a salt comprising a quantum energy generating material comprising the step of drying the salt is adhered to the drinking water containing the quantum energy generating material.

In addition, the present invention provides a method for producing a salt containing a quantum energy generating material, characterized in that the heating step comprises removing the impurities by heating at a temperature of 500 ° or more for 5 hours or more.

The present invention also provides a method for preparing a salt comprising a quantum energy generating material comprising the step of preparing the salt, heating the salt to remove impurities and grinding the salt from which the impurities are removed by heating. do.

In another aspect, the present invention provides a method for producing a salt comprising a quantum energy generating material, characterized in that the grinding of the salt, the salt diameter is pulverized to 20 to 100 mesh.

According to the salt production method including the quantum energy generating material of the present invention as described above, there is an effect that consumers can easily ingest the quantum energy generating material through the intake of salt.

1 is a flow chart illustrating a process for preparing a quantum energy generating material powder using a multicolored blood soil according to the present invention.
Figure 2 is a flow chart illustrating a manufacturing process of drinking water containing a quantum energy generating material according to the present invention.
Figure 3 is a flow chart showing the manufacturing process of salt containing a quantum energy generating material according to the present invention.

Advantages and features of the present invention and methods for achieving them will be apparent with reference to the embodiments described below in detail with the accompanying drawings. The present invention may, however, be embodied in many different forms and should not be construed as being limited to the embodiments set forth herein. Rather, these embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the scope of the invention to those skilled in the art. Is provided to fully convey the scope of the invention to those skilled in the art, and the invention is only defined by the scope of the claims.

DETAILED DESCRIPTION Hereinafter, exemplary embodiments of the present invention will be described in detail with reference to the accompanying drawings. &Quot; and / or "include each and every combination of one or more of the mentioned items. ≪ RTI ID = 0.0 >

Although the first, second, etc. are used to describe various components, it goes without saying that these components are not limited by these terms. These terms are used only to distinguish one component from another. Therefore, it goes without saying that the first component mentioned below may be the second component within the technical scope of the present invention.

The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting of the invention. In the present specification, the singular form includes plural forms unless otherwise specified in the specification. The terms " comprises "and / or" comprising "used in the specification do not exclude the presence or addition of one or more other elements in addition to the stated element.

Unless otherwise defined, all terms (including technical and scientific terms) used in the present specification may be used in a sense that can be commonly understood by those skilled in the art. Also, commonly used predefined terms are not ideally or excessively interpreted unless explicitly defined otherwise.

The terms spatially relative, "below", "beneath", "lower", "above", "upper" And can be used to easily describe a correlation between an element and other elements. Spatially relative terms should be understood in terms of the directions shown in the drawings, including the different directions of components at the time of use or operation. For example, when inverting an element shown in the figures, an element described as "below" or "beneath" of another element may be placed "above" another element . Thus, the exemplary term "below" can include both downward and upward directions. The components can also be oriented in different directions, so that spatially relative terms can be interpreted according to orientation.

Hereinafter, exemplary embodiments of the present invention will be described in detail with reference to the accompanying drawings.

The quantum energy generating material of the present invention neutralizes and destroys harmful magnetic fields to 0 Gauss by generating and amplifying and dissipating warm heat and scalar waves at room temperature without adding electrical devices or chemical components, and penetrate into human skin by vascularization. A substance that not only promotes metabolism but also repairs wound skin, regenerates wounds, and regenerates dead skin due to black necrosis of bedsores.It is a zero (zero) gauge that emits energy naturally without a coil or current device. Neutralizing and extinguishing, eliminating inconveniences such as supplying coil device current of quantum energy generating device, eliminating constraints on space, and maximizing amplification of quantum energy generation, effectively treating patients Would be possible.

Here, the harmful magnetic field is harmful to the human body naturally generated in the spaces where people live, such as homes, offices, workplaces, rice fields, fields, and mountains. The supermagnetism field is superimposed to block the generation of quantum energy to penetrate more than 1.0 Gauss. It is strong and refers to a high value magnetic field such as water waves, electrons, and current waves causing human diseases.

The quantum energy generating material detects whether the Gauss corresponding to the area of the detected location is 0 Gauss by detecting a quantum energy emitted from the ground through a Gaussian measuring device, aka probe, When it is cut, a vein composed of five natural colors of five-colored hemosphere appears, and the pure five-colored hemosphere, which is 2m underground, is collected and processed from the vein composed of the five-colored hemosphere.

Here, the 0 Gauss region is a space where healthy people, animals, and plants grow and have been stopped for a long time (the place where plants grow, where people and animals sleep), where energy is formed in the form of circles. Is characterized.

In other words, natural quantum energy is generated and amplified in the 0 Gauss region, and quantum energy for healthy activation of life is generated in the boundary region of the circle. 4, the surface temperature higher than the space where diseased organisms grow with high magnetic fields? It can be confirmed that it is high and free of moisture, and that moss and fungus dies and disappears and is clean and clear. Especially, the quantum energy generated in the 0 Gauss region is zero harmful magnetic field which is harmful to life in nature without coil or current device. As it occurs at the moment of extinction, it can be seen that natural quantum energy is generated even in the natural state.

In other words, in the 0 Gauss region, the superquantum field in the air overlaps with the center point, and the quantum energy is generated and amplified, the quantum energy in the air is concentrated at the center point, the magnetic field is measured at zero, and the surface temperature is 4? It is a region where it is confirmed that it is high and free of moisture, and the area is clean, moss fungi do not grow, and life is healthy.

In addition, the 1.0 Gauss area is a space where diseased people, animals, and plants grow, and have stopped for a long time. This space contains harmful magnetic fields (water waves, electrons, current waves, etc.) that have a high value of 1.0 Gauss or more at intervals of about 20 cm. A film is formed, which prevents protons from entering the space, preventing the production of quantum energy, having a high magnetic field, and a temperature of 4? Above the surface of the 0 Gauss region. Low, high humidity, moss and mold grow wild, and life is diseased.

In other words, the 1.0 Gauss region has a high permeability of harmful magnetic fields (water veins, electrons, current waves, etc.) with a strong permeability of more than 1.0 Gauss, which is formed at intervals of about 20 cm in the space where diseased people, animals, and plants grow and have been stopped for a long time. ) Acts as a membrane to block the concentration of protons in the air to the center of the space, preventing the centralization of the proton field and the amplification of the generation of quantum energy. Than 4? Low, high humidity, high permeability, high magnetic field continuously penetrates while the body stops, causing mold and bacteria to grow, causing disease, no quantum energy, high humidity, low temperature This is deepening.

The quantum energy generating material of the present invention permanently dissipates natural warm heat and quantum energy without the addition of electric devices or external chemicals, neutralizes and destroys harmful magnetic fields of 1.0 Gauss or more to 0 Gauss, It penetrates into and promotes vascular metabolism to activate the human body, regenerates and cures necrotic dead skin, inhibits and eradicates cancer cells, etc., and has an excellent effect on arthritis.

1 is a flow chart illustrating a process for preparing a quantum energy generating material powder using a multicolored blood soil according to the present invention.

Referring to FIG. 1, the quantum energy generating material of the present invention is manufactured by using the multicolored hemoglobin collected from the 0 Gauss region. In the ground, it collects clear five-colored blood soil with five colors that are hard as high-purity stones and broken like soil. (S110)

Here, the extraction of multicolored hemoglobin is performed by using a Gauss probe and a geomagnetic measuring instrument, and cutting the ground of the place where the Gauss is 0 Gauss on the ground by about 50 cm. Only harvest five-colored hemospheres that are more than 2m deep.

The multicolored hemoglobin collected through the above process is pulverized until the size of 320 mesh by using a grinder, and removes heavy metals and harmful components contained in the crushed multicolored hemoglobin (S120).

Here, the crushed multicolored hematite is generally shredded to a size of 320 mesh since the specific gravity to air is significantly lower than that of mineral ores such as gold, silver, copper, iron, germanium, elvan, zeolite, bentonite, and jade. Is injected into the tablet drum through a conveyor equipped with strong magnets to remove heavy metals and harmful components contained in the multicolored blood soil by strong magnetic force.

In addition, through the sedimentation method of the five-colored hemoglobin administered to the tablet drum, particles having a high particle size and high specific gravity are precipitated to the bottom of the purification drum, and particles of low specific gravity are suspended to collect only high-quality hemoglobin.

In addition, sterilize the multicolored hemoglobin administered to the tablet drum with high temperature heat, and perform the first sterilization and drying step to dry naturally until the high temperature heat cools down (S130).

This is because 400 to 400? Rotate for 150 minutes while applying ~ 500 ° C to perform the first sterilization step of the multicolored hemoglobin using high temperature heat, and naturally dry the multicolored hemoglobin.

Then, pure distilled water is added to a purification drum to purify impurities contained in the multicolored hemoglobin, which has been sterilized and dried, and 40% wt of powder powder is mixed.

Here, pure distilled water is introduced into the purification drum in the ratio of 1: 1 with sterilized and dried multicolored hemoglobin, and 40% wt of the powder powder composed of multi-colored hemoglobin in which the 2nd sterilization and drying steps are completely finished. will be.

Then, to remove the impurities contained in the multicolored hemoglobin mixed by impeller mixing method so that the mixed multicolored hemoglobin is formed in the form of a slurry by distilled water, the mixed red blood hemoglobin in the slurry form for a predetermined time layer of the slurry Separation occurs so that the five-colored hemoglobin is separated from the lower part of the purification drum, and the impurities are separated into the upper layer of the five-colored hemoglobin, thereby removing impurities from the five-colored hemoglobin. (S150)

On the other hand, the multicolored hemoglobin in the form of slurry from which impurities are removed is homogeneous by classifying the particles, and collects only the multicolored hemoglobin composed of finer particles by filtering the collected multicolored hemoglobin.

In addition, the multicolored hemoglobin (sample) of the fine particles is mixed with distilled water and stored in the sample storage container. In the 0 Gauss region, the multicolored hemoglobin is mixed at a ratio of 1: 1, 50% and 50% distilled water, and stored in a closed sample storage container. In addition, the stored sample reservoir is aged and fermented for 80 to 90 hours in the 2 m underground vein of 0 Gauss region where the best quantum energy is generated (S170).

As such, when the aging and fermentation process for a certain period of time in the 0 Gauss region, the cold properties of natural mineral ores or soils disappear, and the cationic warm properties are changed. It constantly reacts with protons or photons to produce warm heat for a person to feel.

Then, the samples aged and fermented in the 0 Gauss region (australian hemoglobin in the form of fine particles consisting of at least 320 mesh) were dried in the sun and 650? Into the thermal calciner of ~ 750? To be sterilized and dried for 3 to 4 hours, so as to be composed of a powder form such as powder. (S180)

The quantum energy generating material produced through such a step is composed of a powder form pulverized into 320 mesh or a quantum energy generating material formed into a powder form of 1.8 ~ 2mm pulverized into 320 mesh to form a 1200, this is 1200 By firing through a thermal calciner of?, It may be produced in the form of ceramic balls.

As described above, the quantum energy generating material is a substance transformed into an organic organism in which microorganisms grow by aging and fermenting the multicolored hemosphere, which is a natural inorganic ore that does not absorb protons in the air without life, as described above. .

Such materials are commonly referred to as Yangmyeongseok, and life-saving Yangmyeongseok absorbs and superposes quantum in the air, such as electrons, positrons, protons, and other elements necessary to maintain life such as light and moisture in the air. By releasing or releasing it, it continuously generates and emits quantum energy on its own.

The quantum energy thus produced and dissipated continuously has the following effects and functions.

First, it automatically adjusts temperature and humidity to increase heat as it gets colder, and to cool down as it gets hotter, keeping humidity optimally.

Second, Yang Myung-seok, an organic organism with microorganisms itself, kills harmful bacteria such as pneumococci and staphylococcus, and thirdly, it reacts with both of them in the air to maintain life and releases harmful gases, odors and odors. Keep it.

Fourth, neutralize and extinguish harmful magnetic fields such as water waves, electromagnetic waves, and current waves to 0 Gauss to keep life healthy.

Fifth, it penetrates into human skin to promote vascular metabolism, cures skin diseases such as herpes and atopy, treats wound and burn skin painlessly, regenerates and repairs necrotic decubitus skin, maintains immunity to normal Prevent it.

Accordingly, the present inventor intends to manufacture Yang Myeongseok having such an effect and function so that a consumer can easily purchase and take it, and may be prepared with a salt containing the quantum energy generating material powder in the form of the high concentration powder prepared above.

To this end, first, the quantum energy generating material powder is prepared in drinking water, and then, after the step of adhering the drinking water containing the quantum energy generating material to salt, the salt containing the quantum energy generating material according to the present invention is finally obtained. It can manufacture.

Figure 2 is a flow chart illustrating a manufacturing process of drinking water containing a quantum energy generating material according to the present invention.

Referring to Figure 2, to prepare a drinking water containing a quantum energy generating material according to the present invention to prepare a first solution by mixing the quantum energy generating material in the form of powder and water (S210).

More specifically, mixing the quantum energy generating material with water is easy for the consumer to take, so that the first solution is mixed with water so as to contain 3 to 5% by mass of the quantum energy generating material. That is, the first solution is prepared such that the ratio of quantum energy generating material and water is 3:97 to 5:95.

At this time, in the case of the first solution, since the quantum energy generating material is contained in 3 to 5% by mass, since the amount of microorganisms is reduced by the amount of water, it is difficult to perform the effects and functions of the above-mentioned Yangmyeongseok.

Therefore, in order for the drinking water containing the quantum energy generating material according to the present invention to function and function as described above, it is necessary to multiply the amount of microorganisms.

Subsequently, referring to FIG. 2, the lactic acid bacteria are cultured in a separate process from preparing the first solution by mixing the quantum energy generating material and water.

Lactic acid bacteria have long been used for the processing of many food products, such as fermented dairy products, cast products, pickled vegetables and fruits, for the purpose of storing and seasoning foods. As lactic acid bacteria used in the present invention, any lactic acid bacteria that can be used in food can be used without limitation. The lactic acid bacteria are classified into oil-based lactic acid bacteria, plant-based lactic acid bacteria, enteric lactic acid bacteria, and lactic acid bacteria derived from natural lakes in which algae grows depending on the growth environment derived. In addition, lactic acid bacteria are classified into mesophilic bacteria, thermophilic bacteria, flame resistant bacteria and the like according to their optimum growth conditions, and may be bacteria having any properties.

As lactic acid bacteria used in the present invention, Lactobacillus genus, Pediococcus genus, Teteragenococcus genus, Carnobacterium genus, Vagococcus genus, Genus Leuconostoc, Genus Weissella, Genus Oenococcus, Genus Atopobium, Genus Streptococcus, Genus Enterococcus, Genus Lactococcus (Lactococcus), Aerococcus (Aerococcus), Alloiococcus (Alloiococcus), Melissococcus (B), Bifidobacterium (Bifidobacterium), and the like. Lactobacillus delbrueckii, Lactobacillus plantarum, Lactobacillus acidophilus, Lactobacillus brevis, Lactococcus lactis, Lactococcus lactis Species such as Leuconostoc sp. And Enterococcus casseliflavus.

The lactic acid bacteria may be used alone, or may be used by mixing two or more kinds of bacteria. In the culturing step, the same type of bacteria may be cultured by dividing the bacteria into two or more stages, or different bacterial species may be divided into two or more stages and cultured.

Incidentally, the culture of the lactic acid bacteria may be carried out using a culture method that is generally used. For example, the lactic acid bacteria are ingested in a medium and cultured at a predetermined range of pH. As the culture method, batch culture, batch culture, oil culture, continuous culture, anaerobic culture, aeration culture, shaking culture, stationary culture, stirred culture, test tube culture, tank culture, flask culture, permanent culture It can be cultured by any method such as (fermentor culture), Jar fermentor culture (Jar fermentor culture). Therefore, the present invention does not limit the culturing method of lactic acid bacteria.

Subsequently, referring to FIG. 2, a second solution in which 3 to 10 parts by weight of the lactic acid bacteria culture medium is added per 100 parts by weight of the first solution prepared by mixing the quantum energy generating material and water is prepared (S230).

When the content of the cultured lactic acid bacteria is less than 3 parts by weight, the growth effect of microorganisms may be insignificant, and when the content of the lactic acid bacteria exceeds 10 parts by weight, the taste of drinking water may be reduced.

Subsequently, referring to FIG. 2, the second solution in which the lactic acid bacteria culture medium is added to the water in which the quantum energy generating material is mixed is incubated in the incubator.

Specifically, it is 22 to incubate the second solution in the incubator? Incubate for 30 to 48 hours at a temperature of 25 to 25 ℃, the incubator can be used on the general bacterial incubator on the market.

Thereby, drinking water containing the quantum energy generating material according to the present invention can be prepared.

As described above, since the quantum energy generating material is mixed with water, the amount of microorganisms is reduced by the amount of water, but the microorganisms are multiplied through the process of mixing the lactic acid bacteria culture medium and culturing in the incubator, The mixed water will also contain a sufficient amount of microorganisms.

In addition, by adding a culture of lactic acid bacteria to the water mixed with the quantum energy generating material and cultivating it, the amount of microorganisms can be multiplied to function and efficacy of Yangmyeongseok.

Next, the salt containing the quantum energy generating material may be prepared by sticking the drinking water including the prepared quantum energy generating material to salt.

Figure 3 is a flow chart showing the manufacturing process of salt containing a quantum energy generating material according to the present invention.

First, the salt is put in a container and heated to 500 ° C or more for 5 hours or more to remove impurities. (S310)

The type of salt used as the raw material is crushed rock salt, sun salt containing various minerals beneficial to the body produced by evaporating seawater introduced into the evaporation paper by solar heat, electrolysis of seawater to remove impurities and heavy metals by ion resin membrane. Purified salts containing 99.5% or more of sodium chloride (NaCl) obtained, and processed salts obtained by washing, pulverizing, compressing, dissolving or melting the salts of the natural salts or refined salts, and the like, including the brine and the chloride gas contained in the salt through the heating process. Insoluble gas can be removed.

Next, the salt from which impurities are removed is pulverized through a heating step. (S320)

At this time, the particle size of the salt is preferably pulverized to 20 to 100 mesh so that the next step is to drink the drinking water containing the quantum energy generating material evenly.

Next, the drinking water in which the prepared quantum energy generating material is dissolved is sprayed onto the crushed salt and adhered. (S330)

At this time, since the surface of the salt particles are partially dissolved in water and undergo a recrystallization process during drying, the quantum energy generating material contained in the drinking water may adhere to the surface of the salt particles.

On the other hand, the drinking water containing the quantum energy generating material in the salt is sprayed in a state in which the salt is laid flat, so that the surface area to which the drinking water is sprayed to facilitate the adhesion, the quantum energy of drinking water containing the quantum energy generating material Although the molecular weight of the generating material is not particularly limited, the molecular weight is preferably 0.5 to 500 kDa in order to improve the binding strength of sodium chloride (NaCl) with chlorine ions (Cl?) At the time of spraying.

At this time, the injection of the drinking water containing the quantum energy generating material is sprayed to the salt enough to wet the salt, the content of the quantum energy generating material bound to the salt surface after the drying step of the next step is 0.1 to 5 It is preferable to make it%.

When the content of the quantum energy generating material is 5% or more relative to salt, the intrinsic taste of salt may be reduced.

Subsequently, the salt to which the drinking water containing the said quantum energy generating substance was stuck is dried. (S340)

At this time, the drying method may be dried at room temperature drying or heating the salt attached to the drinking water containing the quantum energy generating material in a sealed kiln to remove impurities.

Thus, it is possible to manufacture a salt containing a quantum energy generating material according to an embodiment of the present invention.

According to the method for producing drinking water including the quantum energy generating material of the present invention as described above, by mixing the quantum energy generating material with water, and spraying it on the salt as a raw material, the consumer through the intake of salt There is an effect that can easily absorb the quantum energy generated energy.

While the present invention has been described in connection with what is presently considered to be practical exemplary embodiments, it is to be understood that the invention is not limited to the disclosed embodiments, but, on the contrary, It will be understood. It is therefore to be understood that the above-described embodiments are illustrative in all aspects and not restrictive.

Claims (5)

Preparing drinking water containing a quantum energy generating material;
Preparing salt;
Injecting drinking water containing the quantum energy generating material into the salt and adhering to the salt; And
Method of producing a salt comprising a quantum energy generating material comprising the step of drying the salt to which the drinking water containing the quantum energy generating material is attached.
The method of claim 1,
The heating step is a method for producing a salt comprising a quantum energy generating material, characterized in that the heating is performed for more than 5 hours at a temperature of 500 ℃ or more.
The method of claim 1,
Preparing the salt,
Heating salt to remove impurities and pulverizing the salt from which the impurities are removed by heating.
The method of claim 3, wherein
Wherein the salt grinding step of producing a salt comprising a quantum energy generating material, characterized in that the particle size of the salt is ground to 20 to 100 mesh.
Salt prepared by the method for producing salt comprising the quantum energy generating material of any one of claims 1 to 4.
KR1020120045494A 2012-04-30 2012-04-30 A manufacturing method of salt comprising quantum energy occurrence material KR20130122292A (en)