KR20060124360A KR1020050046249A KR20050046249A KR20060124360A KR 20060124360 A KR20060124360 A KR 20060124360A KR 1020050046249 A KR1020050046249 A KR 1020050046249A KR 20050046249 A KR20050046249 A KR 20050046249A KR 20060124360 A KR20060124360 A KR 20060124360A
Authority
KR
South Korea
Prior art keywords
mixture
ocher
mold
conveyor
hopper
Prior art date
Application number
KR1020050046249A
Other languages
Korean (ko)
Other versions
KR100674429B1 (en
Inventor
박용수
Original Assignee
박용수
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 박용수 filed Critical 박용수
Priority to KR1020050046249A priority Critical patent/KR100674429B1/en
Publication of KR20060124360A publication Critical patent/KR20060124360A/en
Application granted granted Critical
Publication of KR100674429B1 publication Critical patent/KR100674429B1/en

Links

Images

Classifications

    • BPERFORMING OPERATIONS; TRANSPORTING
    • B28WORKING CEMENT, CLAY, OR STONE
    • B28BSHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER
    • B28B1/00Producing shaped prefabricated articles from the material
    • B28B1/14Producing shaped prefabricated articles from the material by simple casting, the material being neither forcibly fed nor positively compacted
    • B28B1/16Producing shaped prefabricated articles from the material by simple casting, the material being neither forcibly fed nor positively compacted for producing layered articles
    • BPERFORMING OPERATIONS; TRANSPORTING
    • B28WORKING CEMENT, CLAY, OR STONE
    • B28BSHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER
    • B28B1/00Producing shaped prefabricated articles from the material
    • B28B1/08Producing shaped prefabricated articles from the material by vibrating or jolting
    • BPERFORMING OPERATIONS; TRANSPORTING
    • B28WORKING CEMENT, CLAY, OR STONE
    • B28BSHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER
    • B28B23/00Arrangements specially adapted for the production of shaped articles with elements wholly or partly embedded in the moulding material; Production of reinforced objects
    • B28B23/02Arrangements specially adapted for the production of shaped articles with elements wholly or partly embedded in the moulding material; Production of reinforced objects wherein the elements are reinforcing members
    • BPERFORMING OPERATIONS; TRANSPORTING
    • B28WORKING CEMENT, CLAY, OR STONE
    • B28BSHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER
    • B28B5/00Producing shaped articles from the material in moulds or on moulding surfaces, carried or formed by, in, or on conveyors irrespective of the manner of shaping
    • B28B5/04Producing shaped articles from the material in moulds or on moulding surfaces, carried or formed by, in, or on conveyors irrespective of the manner of shaping in moulds moved in succession past one or more shaping stations

Abstract

A yellow loess panel manufacturing method and a device are provided to automatically produce light and firm yellow loess panels and to install the yellow loess panels on the ceiling by reducing the weight. The yellow loess panel manufacturing method comprises the steps of: producing a square yellow loess panel mold by using light materials like copper sheets or aluminum; attaching a mesh fabric to the inside of the mold; attaching a light aluminum mesh net on the upper side of the mesh fabric; putting yellow loess and limestone forming a yellow loess panel into a first hopper(20); putting light aggregates forming the yellow loess panel into a second hopper(21); inserting water and a nontoxic adhesive agent forming the yellow loess panel into a third hopper(22); putting the predetermined amount of the yellow loess, limestone, water, and nontoxic adhesive agent filled in the first, second, and third hoppers by a measuring device(23a) and blending the mixture in a circular roll mixer(23); supplying the mixture to a feeder(24); inputting the mold attached with the mesh fabric and the mesh net to a conveyor(30) and putting the mixture from the feeder into the mold; generating vibration by a vibrating table(31) installed at the lower side of the conveyor to repress bubbles with keeping the mixture filled into the mold horizontal; firstly drying the mold containing the mixture horizontally kept, at the natural temperature of 15-18 deg.C by using a blower(33); secondly drying the mold by the hot air of 35-40 deg.C by passing the mold through a drying compartment(34); and automatically stacking the completely dried yellow loess panels by supplying the yellow loess panels to an automatic masonry device(35) by the conveyor.

Description

황토판넬 제작방법과 장치 및 황토판넬{A Yellow Earth Panel Of The Method Manufacturing and An Apparatus and A Yellow Earth Panel}A yellow earth panel of the method manufacturing and an apparatus and a yellow earth panel

도 1은 본 발명 황토판넬을 제작하는 방법을 보인 플로우챠트,1 is a flow chart showing a method for manufacturing the present invention ocher panel,

도 2는 본 발명 황토판넬을 제작하는 장치를 보인 평면도,Figure 2 is a plan view showing an apparatus for manufacturing the present invention loess panel,

도 3은 본 발명 황토판넬을 제작하는 장치를 보인 정면도,Figure 3 is a front view showing the device for manufacturing the present invention ocher panel,

도 4는 본 발명 황토판넬의 사시도,Figure 4 is a perspective view of the ocher panel of the present invention,

도 5는 본 발명에 따른 황토판넬을 제작하기 위한 구성을 보인 분해사시도,5 is an exploded perspective view showing a configuration for manufacturing the ocher panel according to the present invention,

도 6은 본 발명 황토판넬의 단면도.Figure 6 is a cross-sectional view of the present invention ocher panel.

<도면의 주요부분에 대한 부호의 설명><Description of the symbols for the main parts of the drawings>

1 - 황토판넬 2 - 틀1-ocher panel 2-frame

3 - 통공 4 - 망사원단3-Aeration 4-Mesh

5 - 매쉬망 20,21,22 - 제1·제2·제3호퍼5-Mesh Network 20,21,22-First, Second, Third Hopper

23 - 원형 롤 믹서 24 - 공급기23-round roll mixer 24-feeder

30 - 컨베이어 31 - 진동테이블30-Conveyor 31-Vibration Table

32 - 무늬성형롤러 33 - 송풍기32-Pattern Molding Roller 33-Blower

34 - 건조실 35 - 자동조적기34-Drying Room 35-Automatic Loading Machine

본 발명을 황토를 이용하여 황토판넬을 제작하는 황토판넬 제작방법과 장치 및 황토판넬에 관한 것이다. 더욱 상세하게는 중량이 가볍고, 휨성이 없으며, 설치하였을 때 미적 아름다움을 강조할 수 있도록 황토판넬을 제작하여 실내의 벽이나 천장, 바닥 등에 용이하게 설치할 수 있도록 하는 황토판넬 제작방법과 장치 및 황토판넬을 제공하는 것이다.The present invention relates to a loess panel manufacturing method and apparatus for producing loess panel using loess and loess panel. More specifically, the ocher panel manufacturing method and apparatus and the ocher panel which make it easy to install on the wall, ceiling or floor of the room by making ocher panel to emphasize the aesthetic beauty when it is light in weight, not warp and installed. To provide.

일반적으로 벽체나 바닥의 장식용 내장판재로는 베니아판이나 목재에 무늬목이 붙여진 장식판 등이 사용되고 있다. 이때 이들은 경량성이고 응용성이 많은 건축용 내장판재이기는 하나 내열성이 약하고 경제적이지 않으며 방음 및 방습에 취약하고 파손되기 쉽다는 단점이 있다.In general, decorative boards for walls and floors are used as veneer boards and decorative boards with wood veneer. At this time, although they are light weight and have high applicability, they are disadvantageous in that they are weak in heat resistance, not economical, vulnerable to sound insulation and moisture proofing, and easy to break.

그리고, 상기 장식용 내장판재로 난연성이 우수한 석고보드를 사용하고 있으나, 이 또한 무겁고 조그마한 충격에도 파손되기 쉬우며 환경을 오염시키는 석면과 석고로 되어 있어 폐기시 분해되어 썩지 아니하고, 인체에 유해한 물질을 내포하여 암 등을 유발시킬 수 있는 단점을 가지고 있다.In addition, although the gypsum board is excellent in flame retardancy as the decorative interior material, it is also made of asbestos and gypsum which are easy to be damaged by heavy and small impacts and pollute the environment. It has the disadvantage that can cause cancer.

또한, 상기 장식용 내장판재를 사용하지 않고 시멘트로 마감 처리할 수 있으나, 이는 여름철에는 열을 흡수하여 실내의 온도를 상승시키고 겨울철에는 열을 쉽게 방출하여 실내의 온도를 하강시켜 냉, 난방비가 많이 소요되고, 인체에 유해한 물질이 방출되며, 여름에는 냉기 및 습기가 잘 스며드는 단점을 가지고 있다.In addition, it can be finished with cement without using the decorative interior plate, but it absorbs heat in summer to increase the temperature of the room, and in the winter to easily release heat to lower the temperature of the room to take a lot of cooling and heating costs And harmful substances are emitted to the human body, and cold and moisture have a disadvantage in the summer.

이에 따라, 최근 황토가 단열과 방음성이 우수하고, 항균효과 및 다량의 원적외선을 방출하며, 뛰어난 습도 조절 능력 등이 확인됨에 따라 각종 건축재료로서 각광을 받고 있다. 즉 일반 흙이 가지고 있는 2층판상구조와는 달리 황토는 3층벌집구조를 가지고 있으므로, 실내의 유해가스나 악취 등을 흡착하고 담배나 콘크리트 냄새 등을 제거하는 탈취 효과가 뛰어나다.Accordingly, in recent years, yellow clay has been in the spotlight as various building materials as it has excellent thermal insulation and sound insulation, antibacterial effect and a large amount of far infrared rays, and excellent humidity control ability. In other words, unlike the two-layered plate structure of ordinary soil, loess has a three-layer honeycomb structure, so it is excellent in deodorizing effect of adsorbing harmful gases and odors in the room and removing tobacco and concrete smells.

또한, 카탈라제, 디페놀, 옥시티아제, 시카라제, 프로테아제 등의 분해 효소가 풍부해 몸에 해로운 미생물의 번식을 억제하는 항균기능도 가지고 있으며, 여름철에는 열을 차단하여 실내를 시원하게 하고, 겨울철에는 열을 흡수하여 실내를 따뜻하게 하여 냉·난방비를 절감할 수 있는 효과도 있다.In addition, it is rich in degrading enzymes such as catalase, diphenol, oxycytase, cicarase, and protease, and has an antibacterial function that suppresses the growth of harmful microorganisms.In summer, it cools the room by blocking heat. It also has the effect of reducing heat and cooling costs by absorbing heat to warm the room.

그리고, 방음 및 방습 효과가 우수하고, 화재시에는 난연성이 우수하여 화재의 피해를 최소화시킬 수 있으며, 반영구적으로 재사용이 가능하고 일정기간 사용한 후에는 폐기하여도 환경오염이 없는 장점을 가지고 있다.In addition, the soundproof and moisture-proof effect is excellent, and in the case of fire, the flame retardancy is excellent to minimize the damage of the fire, semi-permanently reusable, and after a certain period of use has the advantage that there is no environmental pollution even if discarded.

그러나, 상기 황토를 건축 내장재로 사용하는 종래 기술은, 접착제와 보강제 등 첨가제를 첨가하여 적당하게 반죽을 한 후 바닥이나 벽면 및 천정 등에 흙손을 사용하여 바르거나 붓으로 얇게 칠하는 방법을 사용하였다. 이에 상기 황토가 가진 특성상 바닥이나 벽면 및 천장에서 균열이 발생하여 건축물의 미관을 해치며, 시공과정상 많은 인력이 필요하고 시공기간이 오래 걸리는 문제점이 있었다.However, in the prior art using the loess as a building interior material, by adding additives such as adhesives and reinforcing agents, the dough is appropriately kneaded, and a method of applying thinly with a trowel to a floor, a wall, a ceiling, or the like is used. Therefore, due to the characteristics of the loess, cracks are generated on the floor, walls, and ceilings, thereby impairing the aesthetics of the building.

또한, 상기 황토를 판넬로 제작하여 사용하는 종래 기술은, 황토판넬의 중량이 무거워 벽에 고정시키는 데에도 상당히 어려웠으며, 천장에 설치하는 것은 중량 관계로 인해 아예 설치할 수 없었다.In addition, the prior art of manufacturing the ocher as a panel, the heavy weight of the ocher panel was very difficult to fix to the wall, it was not possible to install at all because of the weight relationship to the ceiling.

따라서, 상기 바닥이나 벽은 황토판넬을 설치하고, 천장은 황토벽지를 도배하여 일체감을 주고 있으나, 실질적으로 설치후 상태를 보면 일체감이 없어 실내 인테리어가 미려해지지 않게 되는 큰 문제점을 가지고 있었다.Therefore, the floor or the wall is to install the ocher panel, the ceiling is to give a sense of unity by wallpapering the ocher wall, but there is a big problem that the interior interior is not beautiful because there is no sense of unity when looking at the state after the installation.

본 발명은 상술한 문제점들을 해소하기 위한 것으로, 황토를 이용하여 황토판넬을 제작하되, 그 중량을 가볍게 하여 황토판넬을 벽에 간편하게 설치함은 물론, 천장에 용이하게 설치하여 실내 인테리어의 일체감으로 인해 미려한 실내 디자인을 얻을 수 있고, 황토의 효능을 극대화시킬 수 있는 황토판넬 제작방법과 장치 및 황토판넬을 제공하는데 그 목적이 있다. The present invention is to solve the above-mentioned problems, but to manufacture the ocher panel using the ocher, light weight of the ocher panel is easily installed on the wall, as well as easily installed on the ceiling due to the unity of the interior interior The purpose of the present invention is to provide an ocher panel manufacturing method and apparatus and an ocher panel that can obtain a beautiful interior design and maximize the efficacy of ocher.

본 발명의 목적과 부수되는 많은 효과는 다음의 상세한 설명에 의해서 용이하게 이해될 것이다.Many of the objects and accompanying effects of the present invention will be readily understood by the following detailed description.

상기 목적을 달성하기 위한 본 발명의 특징은 황토를 이용하여 황토판넬을 제작하는 통상의 황토판넬 제작방법에 있어서, 황토판넬의 사각의 틀을 동(銅)판 또는 알루미늄 등의 경량재를 이용하여 제작하는 틀 제작단계와; 상기 단계에서 제작된 틀의 내부에 망사원단을 부착하는 원단 부착단계와; 상기 단계에서 망사원단의 상부에 경량 알루미늄 매쉬망을 부착하는 매쉬망 부착단계와; 상기 황토판넬을 제작하기 위한 황토와 석회석을 제1호퍼에 넣는 제1호퍼단계와; 상기 황토판넬을 제작하기 위한 경량골재를 제2호퍼에 넣는 제2호퍼단계와; 상기 황토판넬을 제작하기 위한 물 및 무독성 접착제를 제3호퍼에 넣는 제3호퍼단계와; 상기 제1호퍼단계와 제2호퍼단계 및 제3호퍼단계에서 제1·제2·제3호퍼에 넣어진 황토와 석회석 및 경량골재, 물과 무독성 접착제를 원형 롤 믹서에 계량장치를 통해 일정량을 각각 투입하여 혼합하는 원형 롤 믹서단계와; 상기 단계에서 혼합된 혼합물을 공급기에 공급하는 공급단계와; 상기 단계에서 망사원단과 매쉬망이 부착된 틀을 컨베이어에 투입하고 상기 투입된 틀의 내부에 혼합물을 충진시키는 컨베이어 투입단계와; 상기 단계에서 틀의 내부에 충진된 혼합물의 수평을 유지시키며 기포발생을 억제시키기 위해 컨베이어의 하부에 설치된 진동테이블에 의해 진동을 부여하는 진동테이블 통과단계와; 상기 단계에서 혼합물이 수평으로 유지된 틀에 컨베이어의 하부에 설치된 송풍기를 이용하여 15 ~ 18℃의 자연온도로 1차건조시키는 1차 자연풍 건조단계와; 상기 단계에서 1차 건조된 틀을 컨베이어에 의해 이송시켜 건조실을 통과시키며 35 ~ 40℃의 열풍으로 완전건조시키는 2차 열풍건조단계와; 상기 단계에서 완전건조된 황토판넬을 컨베이어에 의해 자동조적기로 공급하여 자동으로 조적되도록 하는 자동조적기 단계로 이루어진 것을 특징으로 한다.A characteristic of the present invention for achieving the above object is in a conventional ocher panel manufacturing method for producing ocher panels using ocher, using a lightweight material such as copper plate or aluminum in the rectangular frame of the ocher panel A production step of producing a frame; A fabric attachment step of attaching a mesh fabric to the inside of the frame manufactured in the step; A mesh net attachment step of attaching a lightweight aluminum mesh net to the upper portion of the mesh fabric in the step; A first hopper step of putting ocher and limestone in the first hopper for manufacturing the ocher panel; A second hopper step of putting a light weight aggregate for manufacturing the ocher panel in a second hopper; A third hopper step of putting water and a non-toxic adhesive for manufacturing the ocher panel into a third hopper; Ocher, limestone, lightweight aggregate, water and non-toxic adhesives put in the first, second and third hoppers in the first hopper stage, the second hopper stage and the third hopper stage, water and non-toxic adhesives were measured in a circular roll mixer through a measuring device. A circular roll mixer step of injecting and mixing each; A feeding step of feeding the mixture mixed in the step to a feeder; A conveyor feeding step of inserting the frame attached with the mesh fabric and the mesh net into the conveyor in the step and filling the mixture into the introduced mold; A vibrating table passing step of applying vibration by a vibrating table installed at the lower part of the conveyor to maintain horizontality of the mixture filled in the mold in the above step and suppress bubble generation; A first natural wind drying step of first drying at a natural temperature of 15 to 18 ° C. by using a blower installed at a lower part of the conveyor in a mold in which the mixture is horizontally maintained in the step; A second hot air drying step of transferring the first dried mold in the step by a conveyor to pass through the drying chamber and completely drying the hot air at 35 to 40 ° C .; In the above step is characterized by consisting of an automatic masonry step to supply the fully dried ocher panel by automatic conveyor to the automatic masonry.

이때, 상기 진동테이블 통과단계와 1차 자연풍 건조단계의 사이에 황토판넬의 표면에 무늬성형롤러를 이용하여 무늬를 형성시킬 수 있는 무늬성형단계를 더 포함시킴이 바람직하다.At this time, it is preferable to further include a pattern forming step capable of forming a pattern using a pattern forming roller on the surface of the ocher panel between the vibration table passing step and the first natural wind drying step.

또한, 황토를 이용하여 황토판넬을 제작하는 통상의 황토판넬 제작장치에 있 어서, 동판 또는 알루미늄 등의 경량재를 이용하여 제작된 사각의 틀에 망사원단과 경량 알루미늄 매쉬망을 부착하고, 각 공정으로 틀을 이송시키는 켄베이어와; 상기 컨베이어의 상부에 설치되어 황토와 석회석이 넣어지는 제1호퍼와; 상기 컨베이어의 상부에 설치되어 경량골재가 넣어지는 제2호퍼와; 상기 컨베이어의 상부에 설치되어 물 및 무독성 접착제가 넣어지는 제3호퍼와; 상기 제1·제2·제3호퍼와 연결되어 각각의 물질들을 계량장치로 부터 일정량씩 공급받아 이를 혼합하는 원형 롤 믹서와; 상기 원형 롤 믹서에서 혼합된 혼합물을 틀의 내부에 넣기위해 혼합물이 저장되는 컨베이어의 상부에 설치된 공급기와; 상기 컨베이어에 의해 이송되다가 공급기에서 틀의 내부에 혼합물이 충진되면 진동을 발생시켜 혼합물의 수평을 유지시키고 기포가 발생되는 것을 억제하는 컨베이어의 하부에 설치된 진동테이블과; 상기 진동테이블에 의해 틀에 충진된 혼합물이 수평으로 유지된 후 이를 15 ~ 18℃의 자연풍으로 1차건조시키는 컨베이어의 하부에 설치된 송풍기와; 상기 송풍기에 의해 1차건조된 틀에 35 ~ 40℃의 열풍을 공급하여 2차건조시키는 건조실과; 상기 건조실에서 완전건조된 황토판넬을 컨베이어에 의해 이송시켜 자동으로 조적하는 자동조적기로 이루어진 것을 특징으로 한다.In addition, in a conventional ocher panel manufacturing apparatus for producing ocher panels using ocher, attaching a fabric and a lightweight aluminum mesh net to a rectangular frame made of a copper plate or a lightweight material such as aluminum, each step Kenvey and conveying the mold; A first hopper installed at an upper portion of the conveyor and into which loess and limestone are put; A second hopper installed on an upper portion of the conveyor and including a light aggregate; A third hopper installed on the conveyor and into which water and non-toxic adhesive are put; A circular roll mixer connected to the first, second and third hoppers and receiving a predetermined amount of each substance from a metering device and mixing them; A feeder installed at the top of the conveyor in which the mixture is stored for placing the mixture mixed in the circular roll mixer into a mold; A vibration table which is transported by the conveyor and installed at the lower part of the conveyor to generate vibration when the mixture is filled in the mold in the feeder to maintain the level of the mixture and to prevent bubbles from being generated; A blower installed at a lower part of the conveyor for drying the mixture filled in the mold by the vibration table horizontally and firstly drying it with natural wind at 15 to 18 ° C .; A drying chamber for supplying hot air having a temperature of 35 to 40 ° C. to the mold dried primarily by the blower for secondary drying; It characterized by consisting of an automatic mason to transfer automatically by the conveyor the completely dried ocher panel in the drying chamber.

이때, 상기 진동테이블과 송풍기 사이의 컨베이어 상부에 설치되어 틀에 충진된 혼합물의 상면에 무늬를 형성시키는 무늬형성롤러를 더 구비함이 바람직하다.At this time, it is preferable to further include a pattern forming roller installed on the conveyor between the vibrating table and the blower to form a pattern on the upper surface of the mixture filled in the mold.

한편, 황토를 이용하여 제작된 통상의 황토판넬에 있어서, 상기 황토판넬의 테두리를 형성하기 위해 "ㄷ"자 형상으로 사면이 이루어지고, 경량재질의 알루미늄으로 제작되는 사각의 틀과; 상기 틀의 내부에 부착되는 망사원단과; 상기 망사원 단의 상면에 부착되는 경량재질의 알루미늄으로 제작되는 매쉬망과; 상기 망사원단과 매쉬망이 부착된 틀의 내부에 충진되는 황토층으로 이루어진다.On the other hand, in the conventional ocher panel manufactured using ocher, the rectangular frame is made of a "c" shape to form the border of the ocher panel, a rectangular frame made of lightweight aluminum; A mesh fabric attached to the inside of the frame; Mesh net made of lightweight aluminum attached to the upper surface of the mesh; It consists of an ocher layer filled in the inside of the frame attached to the mesh fabric and mesh.

이때, 상기 틀의 내부에 충진되어 황토층을 구성하는 혼합물은, 황토 70 ~ 75%와, 석회석 4 ~ 5%와, 경량골재 13 ~ 15%와, 물 및 접착제 8 ~ 10%를 혼합한 혼합물로 이루어진다.At this time, the mixture filling the inside of the frame constituting the loess layer is a mixture of 70 to 75% ocher, 4 to 5% limestone, 13 to 15% lightweight aggregate, and 8 to 10% water and adhesive Is done.

그리고, 상기 황토판넬에 의해 유해전자파와 수맥 등이 차단되도록 알루미늄 매쉬망 대신에 동(銅)으로 제작된 동메쉬망을 구비함도 바람직하다.It is also preferable to have a copper mesh net made of copper instead of an aluminum mesh net so that harmful electromagnetic waves and water veins are blocked by the ocher panel.

이하, 첨부된 도면을 참조하여 본 발명을 상세히 설명하도록 한다.Hereinafter, the present invention will be described in detail with reference to the accompanying drawings.

도 1은 본 발명 황토판넬을 제작하는 방법을 보인 플로우챠트이고, 도 2는 본 발명 황토판넬을 제작하는 장치를 보인 평면도이며, 도 3은 본 발명 황토판넬을 제작하는 장치를 보인 정면도이다.1 is a flowchart showing a method of manufacturing the loess panel of the present invention, Figure 2 is a plan view showing a device for manufacturing the loess panel of the present invention, Figure 3 is a front view showing a device for producing the loess panel of the present invention.

그리고, 도 4는 본 발명 황토판넬의 사시도이고, 도 5는 본 발명에 따른 황토판넬을 제작하기 위한 구성을 보인 분해사시도이며, 도 6은 본 발명 황토판넬의 단면도이다.And, Figure 4 is a perspective view of the loess panel of the present invention, Figure 5 is an exploded perspective view showing a configuration for manufacturing the loess panel according to the present invention, Figure 6 is a cross-sectional view of the loess panel of the present invention.

우선, 도 5에서와 같이 "ㄷ"자 형상으로 내부가 파인 사각의 틀(2)을 제작하되, 황토판넬(1)의 설정크기에 맞추어 가벼운 경량 재질의 동판이나 알루미늄 등으로 제작하는 틀 제작단계(S10)를 실행한 후, 상기 틀 제작단계(S10)에서 제작된 사각의 틀(2) 내부에 망사원단(4)을 부착시키는 원단부착단계(S11)를 실행하게 되며, 상기 망사원단(4)을 부착한 그 상면에 다시 가벼운 경량 재질의 알루미늄으로 만든 매쉬망(5)을 부착하는 매쉬망 부착단계(S12)를 실행하게 된다.First, as shown in Figure 5, while producing a frame (2) of the inside is dug into a "c" shape, the frame manufacturing step of manufacturing a light weight copper plate or aluminum, etc. according to the set size of the ocher panel (1) After executing (S10), the fabric fabric attaching step (S11) for attaching the mesh fabric 4 to the inside of the rectangular frame (2) produced in the frame manufacturing step (S10), and the mesh fabric (4) The mesh net attaching step (S12) of attaching the mesh net 5 made of light weight aluminum again is performed on the upper surface to which is attached.

이때, 상기 망사원단(4)은 일반적인 망사로된 원단을 말하는 것으로, 통상 주변에서 손쉽게 구입할 수 있는 어떠한 재질의 망사원단(4)을 사용하여도 무방하나, 황토가 혼합된 혼합물을 충진시켰을 때 혼합물이 쉽게 빠져나갈 수 없는 망사로 이루어진 원단을 사용함이 바람직하다.At this time, the mesh fabric (4) refers to the fabric made of a common mesh, it is possible to use a mesh fabric (4) of any material that can be usually purchased easily around, when the mixture is filled with a mixture of ocher It is preferable to use a fabric made of a mesh that can not easily escape.

즉, 상기 망사원단(4)은 황토가 혼합된 혼합물이 틀(2) 내부에 충진되었을 때 쉽게 빠져나가지 못하도록 하여 틀(2)의 내부에 충진된 혼합물이 안정된 상태로 건조될 수 있도록 하는 목적으로 틀(2)의 내부에 부착된다.That is, the mesh fabric (4) is for the purpose of preventing the mixture mixed with ocher to be easily escaped when the mixture is filled in the frame (2) so that the mixture filled in the frame (2) can be dried in a stable state It is attached to the inside of the mold (2).

또한, 상기 매쉬망(5)은 통상 주변에서 손쉽게 구입할 수 있는 경량재질(동이나 알루미늄 등)로 제작된 매쉬망(5)을 사용하는 것이며, 구멍의 크기가 작거나 큰 것에 관계없이 사용할 수 있으나, 구멍이 너무 크면 매쉬망(5)을 사용하는 목적을 얻을 수 없으므로 너무 크지 않은 구멍으로 이루어진 매쉬망(5)을 사용함이 바람직하다.In addition, the mesh net 5 is to use a mesh net (5) made of a lightweight material (copper or aluminum, etc.) that can be easily purchased around the ordinary, can be used regardless of the size of the hole is small or large. If the hole is too large, the purpose of using the mesh net 5 cannot be obtained. Therefore, it is preferable to use the mesh net 5 made of a hole not too large.

즉, 상기 매쉬망(5)은 틀(2)의 내부에 부착되어 혼합물이 건조될 때 일체화가 됨으로써, 틀(2)의 내부에서 건조된 황토가 휘어지는 것을 방지하는 한편, 황토판넬(1)의 강도를 보강하는 목적으로 틀(2)의 내부에 부착된다.That is, the mesh net 5 is attached to the inside of the mold 2 to be integrated when the mixture is dried, thereby preventing warpage of the dried ocher in the interior of the mold 2, while It is attached to the inside of the frame 2 for the purpose of reinforcing strength.

한편, 상기와 같이 틀(2)의 내부에 망사원단(4)과 매쉬망(5)이 부착된 후에는 도 3과 같이 모터(미도시)에 의해 회전하는 다수개의 회전롤러를 따라 궤적운동을 하는 컨베이어(30)의 상부에 올려지는 컨베이어 투입단계(S30)를 진행하게 된다. Meanwhile, after the mesh fabric 4 and the mesh net 5 are attached to the inside of the mold 2 as described above, a trajectory motion is performed along a plurality of rotating rollers rotated by a motor (not shown) as shown in FIG. 3. The conveyor input step (S30) to be put on the upper portion of the conveyor 30 to proceed.

이때, 상기 컨베이어(30)의 상부에 올려진 틀(2)의 내부에 황토가 혼합된 혼합물이 충진되어야 하는바, 컨베이어(30)의 상부에는 제1·제2·제3호퍼(20)(21)(22)가 설치되고, 상기 제1·제2·제3호퍼(20)(21)(22)로 부터 각각의 물질을 공급받는 계량장치(23a)가 설치되며, 상기 계량장치(23a)로 부터 각각의 물질들의 일정량을 공급받아 이들을 혼합하는 원형 롤 믹서(23)가 설치된다. 이때 상기 원형 롤 믹서(23)는 통상적으로 물질들을 혼합하는데 사용되는 것으로 이에 대한 상세한 설명을 생략하기로 한다.At this time, the mixture of ocher mixed with the inside of the frame 2 placed on the conveyor 30 should be filled, the first, second and third hopper 20 (the top of the conveyor 30) ( 21, 22 are provided, and a metering device 23a for receiving respective substances from the first, second and third hoppers 20, 21, 22 is provided, and the metering device 23a is provided. A circular roll mixer 23 is installed to receive a certain amount of each material from the mixture and mix them. In this case, the circular roll mixer 23 is typically used to mix materials, and a detailed description thereof will be omitted.

즉, 상기 제1호퍼(20)에는 황토와 석회석이 충진되는 제1호퍼단계(S20)를 진행하게 되고, 제2호퍼(21)에는 작은 돌 등을 고온에서 구은 경량골재로 이루어진 부자재가 충진되는 제2호퍼단계(S21)를 진행하게 되며, 제3호퍼(22)에는 물과 무독성 접착제가 혼합되어 충진되는 제3호퍼단계(S23)를 진행하게 된다.That is, the first hopper 20 proceeds to the first hopper step (S20) is filled with ocher and limestone, and the second hopper 21 is filled with an auxiliary material made of lightweight aggregate baked at a high temperature small stones, etc. The second hopper step (S21) proceeds, and the third hopper 22 is a third hopper step (S23) is filled with a mixture of water and a non-toxic adhesive.

그리고, 상기 제1·제2·제3호퍼(20)(21)(22)로 부터 계량장치(23a)에서 각각의 물질들을 공급받아 각각 일정량을 원형 롤 믹서(23)에 공급하여 이들을 혼합하는 원형 롤 믹서단계(S23)를 진행하게 되고, 상기 혼합된 혼합물을 틀(2) 내부에 충진시킬 수 있는 공급기(24)로 공급하는 공급단계(S24)를 진행하게 된다.Then, the respective materials are supplied from the first, second, and third hoppers 20, 21, and 22 by the metering device 23a to supply a predetermined amount to the circular roll mixer 23 to mix them. The circular roll mixer step S23 is performed, and the feeding step S24 for supplying the mixed mixture to the feeder 24 capable of filling the mold 2 is performed.

이때, 상기 계량장치(23a)에 의해 원형 롤 믹서(23)로 공급되는 각각의 물질은, 황토가 70 ~ 75%, 석회석이 4 ~ 5%, 경량골재가 13 ~ 15%, 물 및 무독성 접착제 8 ~ 10%가 혼합되어 혼합물이 된다.At this time, each material supplied to the circular roll mixer 23 by the metering device (23a) is 70 to 75% ocher, 4 to 5% limestone, 13 to 15% lightweight aggregate, water and non-toxic adhesive 8 to 10% is mixed to form a mixture.

또한, 상기 황토와 석회석은 제1호퍼(20)에 충진되어 함께 계량장치(23a)에 공급되는 바, 상기 황토가 93.75 ~ 94.6%, 석회석이 5.4 ~ 6.25%로 혼합되어 제1호 퍼(20)에 충진된다.In addition, the ocher and limestone is filled in the first hopper 20 is supplied to the metering device (23a) together, the ocher is mixed 93.75 ~ 94.6%, limestone 5.4 ~ 6.25% of the first hopper 20 ) Is filled.

한편, 상기 무독성 접착제는 황토와 경량골재를 틀(2)과 망사원단(4) 및 매쉬망(5)에 견고하게 결합시킬 수 있도록 함과 동시에 황토판넬(1)의 강도를 보강하여 주는 것으로, 해초류 등 자연적인 재료로 만들어진 친환경적인 무독성 접착제가 널리 사용되고 있으며, 이들 중 하나를 선택하여 사용하면 된다.On the other hand, the non-toxic adhesive is to reinforce the strength of the ocher panel (1) while allowing the ocher and lightweight aggregate to be firmly coupled to the frame (2) and the mesh fabric (4) and mesh net (5), Eco-friendly non-toxic adhesives made of natural materials such as seaweed are widely used, and one of them can be selected and used.

상기와 같이 컨베이어(30)의 상부에 올려진 틀(2)은 컨베이어(30)에 의해 이송되며 공급기(24)의 하부를 지나게 되고, 상기 공급기(24)에서는 황토가 혼합된 혼합물을 틀(2)의 내부에 충진시키는 컨베이어 투입단계(S30)를 진행하게 된다.As described above, the mold 2 placed on the upper portion of the conveyor 30 is transported by the conveyor 30 and passes through the lower portion of the feeder 24. In the feeder 24, the mold mixture 2 is mixed with ocher. Into the conveyor filling step (S30) to fill in the interior.

이때, 상기 공급기(24)는 인접된 위치에 설치된 롤러(24a)의 사이로 혼합물을 떨어뜨림과 동시에 틀(2)에 충진되는 혼합물의 양을 제어하여 틀(2)에 적정량의 혼합물이 충진되도록 한다.At this time, the feeder 24 drops the mixture between the rollers 24a installed at adjacent positions and simultaneously controls the amount of the mixture filled in the mold 2 so that the mold 2 is filled with the appropriate amount of the mixture. .

또한, 상기 컨베이어 투입단계(S30)를 진행하며 컨베이어(30)상에서 혼합물이 충진된 틀(2)이 이송하게 되면, 컨베이어(30)의 하부에 결합된 진동테이블(31)이 진동을 발생시켜 진동테이블 통과단계(S31)를 진행하게 된다.In addition, when the conveying step (S30) is carried out and the mold 2 filled with the mixture is transferred on the conveyor 30, the vibration table 31 coupled to the lower portion of the conveyor 30 vibrates to generate vibration The table passing step S31 is performed.

이때, 상기 진동테이블(31)에 의해 진동이 발생되면 틀(2)에 충진된 혼합물의 상면이 빠르게 수평으로 펴지며 혼합물 내부에 공기가 포함되지 않도록 하게 된다. 한편 도 3에 도시된 바와 같이, 상기 공급기(24)의 하부에 진동테이블(31)을 설치하여 틀(2)의 내부로 공급기(24)에서 혼합물을 충진시킴과 동시에 진동테이블(31)이 동작하여 혼합물의 수평유지와 기포발생을 억제시킬 수 있도록 함이 바람직하다.At this time, when the vibration is generated by the vibrating table 31, the upper surface of the mixture filled in the mold 2 quickly spreads out horizontally so that no air is contained in the mixture. On the other hand, as shown in Figure 3, by installing the vibrating table 31 in the lower portion of the feeder 24 to fill the mixture in the feeder 24 into the interior of the frame 2 and at the same time the vibrating table 31 operates It is desirable to be able to suppress the leveling and bubble generation of the mixture.

그리고, 상기 진동테이블 통과단계(S31)를 진행한 후 컨베이어(30)에 의해 이송되던 틀(2)은 무늬성형롤러(32)에 의해 상면에 무늬가 형성되는 무늬성형단계(S32)를 진행하게 된다.Then, the frame 2 which is transferred by the conveyor 30 after the vibrating table passing step S31 is carried out to have a pattern forming step S32 in which a pattern is formed on the upper surface by the pattern forming roller 32. do.

따라서, 상기 틀(2)의 내부에 황토가 혼합된 혼합물이 충진되고, 그 상면에 다양한 무늬가 무늬성형롤러(32)에 의해 성형되어 자연적인 색상은 물론 무늬에 의한 미감을 극대화시킬 수 있게 된다.Therefore, the mixture is mixed with the ocher is filled in the interior of the frame (2), the various patterns on the upper surface is molded by the pattern forming roller 32 to be able to maximize the natural color as well as the aesthetics of the pattern. .

상기와 같이 무늬성형단계(S32)를 진행한 후에는 컨베이어(30)에 의해 이송되던 틀(2)이 송풍기(33)를 통과하며 1차건조가 되는 1차 자연풍 건조단계(S33)를 진행하게 된다.After proceeding with the pattern forming step (S32) as described above, the frame (2) conveyed by the conveyor 30 passes through the blower 33 to proceed to the first natural wind drying step (S33) to be the primary drying do.

즉, 상기 틀(2)에 충진된 혼합물이 갑자기 건조가 되면 황토의 특성에 의해 갈라지는 현상(크랙)이 발생되어, 이를 방지하기 위해 15 ~ 18℃의 대기중의 온도로 송풍기(33)를 이용하여 바람을 불어주면, 틀(2)에 충진된 혼합물이 적당하게 굳어지며 건조가 되어 갈라지는 현상이 발생되지 않게 된다.That is, when the mixture filled in the frame 2 is suddenly dried, a phenomenon (crack) occurs due to the characteristics of the loess, and the blower 33 is used at an air temperature of 15 to 18 ° C. to prevent this. When the wind is blown, the mixture filled in the mold (2) is properly hardened and dried to prevent the phenomenon of cracking.

또한, 도 3에서와 같이 컨베이어(30)의 하부에 송풍기(33)를 설치하여 틀(2)의 하부에서 자연바람을 불어줌으로서, 틀(2)의 내부 최하단을 구성하는 망사원단(4)이 물과 무독성 접착제에 의해 젖어있다가 우선적으로 마르게 되어 황토판넬(1) 최상단에 변형이 발생되는 것을 방지하게 된다. 즉 상기 망사원단(4)이 먼저 마르게 되면 황토가 혼합된 혼합물이 망사원단(4)을 통과할 수 없어 혼합물의 상면이 수평으로 유지될 수 있으나, 송풍기(33)를 컨베이어(30)의 상부에 설치하여 자연바람을 불어주면 혼합물의 상면만이 건조되고, 망사원단(4)은 젖어있는 상태로 컨베 이어(30)에 의해 진행하게 되어 적은 양이라도 혼합물이 망사원단(4)을 통과하게 되면, 건조된 상면의 하부에 공간이 발생되어 갈라지는 현상이 발생됨은 물론, 완성된 황토판넬(1)의 강도를 약하게 하는 매우 큰 문제점이 발생하게 된다.In addition, as shown in Figure 3 by installing a blower 33 in the lower portion of the conveyor 30 to blow natural wind from the lower portion of the frame 2, the mesh fabric (4) constituting the inner bottom of the frame (2) The water and the non-toxic adhesive wetted and preferentially dried to prevent deformation of the top of the ocher panel (1). That is, if the mesh fabric 4 is dried first, the mixture of ocher can not pass through the mesh fabric 4, so that the upper surface of the mixture can be maintained horizontally, but the blower 33 is placed on the upper portion of the conveyor 30. If you install and blow the natural wind, only the upper surface of the mixture is dried, the mesh fabric (4) is carried by the conveyor (30) in the wet state, even if a small amount of the mixture passes through the mesh fabric (4), Space is generated in the lower portion of the dried upper surface, as well as a phenomenon occurs, as well as a very large problem that weakens the strength of the finished ocher panel (1).

따라서, 도 3과 같이 송풍기(33)를 컨베이어(30)의 하부에 설치함이 매우 바람직하고, 필요에 따라 컨베이어(30)의 상부와 하부에 동시에 설치할 수도 있음은 물론이다.Therefore, it is very preferable to install the blower 33 in the lower part of the conveyor 30 as shown in FIG. 3, and of course, the upper part and the lower part of the conveyor 30 may be installed at the same time.

한편, 상기 1차 자연풍 건조단계(S33)를 진행한 후에는 열풍에 의해 황토판넬(1)을 완전건조시키는 건조실(34)을 틀(2)이 통과하는 2차 열풍 건조단계(S34)를 진행하게 되는 바, 상기 건조실(34)에서는 35 ~ 40℃의 고온의 열풍을 불어넣어 틀(2)의 내부에 충진된 혼합물을 완전 건조시키게 된다. 이때 상기 건조실(34)의 열풍을 발생시키는 히터 및 송풍기는 통상의 구조이므로 도면과 상세한 설명을 생략하기로 한다.On the other hand, after the first natural wind drying step (S33) proceeds to the second hot air drying step (S34) through which the mold 2 passes through the drying chamber 34 for completely drying the ocher panel 1 by hot air. In the drying chamber 34, a hot air of 35-40 ° C. is blown to completely dry the mixture filled in the mold 2. At this time, the heater and the blower for generating hot air of the drying chamber 34 will be omitted because of the conventional structure and the detailed description.

이와 같이, 상기 틀(2)에 황토가 혼합된 혼합물이 충진되어 2차 열풍 건조단계(S34)까지 완료되면, 도 4 및 도 6과 같은 완성된 황토판넬(1)이 제작되는 바, 완성된 황토판넬(1)은 자동조적기(35)에 의해 하나씩 차례대로 적재되는 자동조적기 단계(S35)가 진행되어 황토판넬(1)을 제작하는 모든 과정이 자동으로 완료된다.As such, when the mixture in which the ocher is mixed is filled in the mold 2 and the second hot air drying step S34 is completed, the completed ocher panel 1 as illustrated in FIGS. 4 and 6 is manufactured. The ocher panel 1 is automatically loaded by the automatic masonry 35 step by step the automatic masonry step (S35) proceeds to automatically complete all the process of manufacturing the ocher panel (1).

한편, 상기 황토판넬(1)을 완성시키는 대부분의 과정을 수행하는 컨베이어(30)는 분당 15 ~ 20m 의 속도로 틀(2)을 이송시키게 되는 바, 상기 컨베이어(30)의 속도가 너무 느리면 틀(2)에 혼합물이 충진된 후 1차 자연풍 건조단계(S33)를 실행하기 전에 많은 양의 혼합물이 망사원단(4)을 통과하여 불량품을 발생시키게 되고, 컨베이어(30)의 속도가 너무 빠르면 틀(2)에 충진된 혼합물이 완전히 건조되지 않은 상태에서 자동조적기(35)로 공급되어 이또한 불량품을 발생시키게 되는 문제점이 발생된다. On the other hand, the conveyor 30 performing most of the process to complete the ocher panel 1 is to transfer the mold 2 at a speed of 15 ~ 20m per minute, if the speed of the conveyor 30 is too slow After the mixture is filled in (2) and before the first natural wind drying step (S33), a large amount of the mixture passes through the mesh fabric 4 to generate defective products, and if the speed of the conveyor 30 is too high, The mixture filled in (2) is supplied to the automatic assembler 35 in a state where it is not completely dried, which also causes a problem of generating a defective product.

이에 따라, 상기 황토판넬(1)의 두께 및 크기 등을 고려하여 컨베이어(30)의 이송속도를 조절할 수 있도록 인버터모터에 의해 컨베이어(30)를 제어함이 바람직하고, 황토판넬(1)을 건조실(34)을 통과시키는 컨베이어(30)는 열에 강한 슬래트 컨베이어를 사용함이 바람직하다.Accordingly, in consideration of the thickness and size of the ocher panel 1 and the like, it is preferable to control the conveyor 30 by an inverter motor so that the conveying speed of the conveyor 30 can be adjusted, and the ocher panel 1 is dried in a drying room. Conveyor 30 passing through 34 preferably uses a slat conveyor resistant to heat.

또한, 상기 건조실(34)을 황토판넬(1)이 통과하는 대략적인 시간은 3 ~ 4 시간 정도로 하여 완전히 건조되어 자동조적기(35)에서 자동으로 조적되고, 이에 따라 자동으로 출고가 가능하도록 함이 바람직하다.In addition, the approximate time for the ocher panel 1 to pass through the drying chamber 34 is about 3 to 4 hours and is completely dried so that it is automatically assembled by the automatic assembler 35, so that the product can be automatically released. This is preferred.

한편, 상기 황토판넬(1)의 틀(2)에는 도면과 같이 통공(3)을 형성하여 측벽이나 천정에 용이하게 설치할 수 있도록 함이 바람직하다.On the other hand, it is preferable to form a through hole 3 in the frame 2 of the ocher panel 1 to be easily installed on the side wall or ceiling.

이때, 상기 통공(3)은 틀(2)을 제작하는 틀 제작단계(S10)에서 형성할 수도 있고, 황토판넬(1)이 완성된 후에 통공(3)을 별도로 형성시킬 수도 있다.At this time, the through hole 3 may be formed in the frame manufacturing step (S10) for producing the frame 2, or may be formed separately through the hole (3) after the ocher panel (1) is completed.

그리고, 상기 황토판넬(1)을 바닥에 설치하는 바닥재(황토구들장)로 형성할 경우에, 유해전자파나 수맥 등을 차단시킬 수 있도록 알루미늄 메쉬망(5) 대신에 동(銅)으로 제작된 동메쉬망을 설치하여 인체에 더욱 큰 이로움을 줄 수 있도록 해도 된다.In addition, when the ocher panel 1 is formed of a flooring material (ocher ball field) installed on the floor, copper is made of copper instead of the aluminum mesh net 5 to block harmful electromagnetic waves or veins. You can also install a mesh network to give greater benefit to the human body.

또한, 상기 동메쉬망을 설치함에 있어, 망사원단(4)의 상부에 동메쉬망을 설치하고, 그 상부에 알루미늄 메쉬망(5)을 설치하여 황토판넬(1)을 제작해도 됨은 물론이고, 틀(2)의 내부에 동메쉬망을 설치하는 위치가 가변될 수 있음은 물론이다.Further, in installing the copper mesh net, the copper mesh net may be installed on the upper part of the mesh fabric 4 and the aluminum mesh net 5 may be installed on the upper part of the mesh fabric 4 to manufacture the ocher panel 1 as well. Of course, the position of installing the moving mesh network inside the frame (2) can be varied.

이와 같이 본 발명 황토판넬 제작방법과 장치 및 황토판넬에 관하여, 본 발명의 범주 내에서 각 부품들의 여러 가지 설계변경은 모두 본 발명의 기술사상의 범위에 포함되는 것으로 간주된다. Thus, with regard to the method and apparatus for manufacturing the ocher panel of the present invention and the ocher panel, various design changes of the respective components within the scope of the present invention are all considered to be included in the technical spirit of the present invention.

따라서, 본 발명은 경량재질로 이루어진 사각의 틀 내부에 망사로된 원단을 부착시키고, 그 상부에 경량재질로 이루어진 매쉬망을 부착시킨 후 황토가 혼합된 혼합물을 충진시키고, 건조시키며, 자동으로 조적되는 모든 과정을 자동으로 진행되도록 함으로서, 무게가 가볍고 단단한 황토판넬을 자동으로 제작하여 고품질의 황토판넬을 대량생산할 수 있게 되는 효과가 있다.Therefore, the present invention is attached to the fabric of the mesh inside the rectangular frame made of lightweight materials, and then attached to the mesh mesh made of lightweight materials on the top of the mixture mixed with ocher, dried, and automatically masonry By automatically proceeding all the processes, the light weight and hard ocher panel is automatically produced to have an effect of mass production of high quality ocher panel.

또한, 상기 황토판넬이 경량화됨으로 인해, 천정에는 황토판넬을 설치할 수 없는 종래의 문제점을 해결하여 천정에도 본 발명 황토판넬을 용이하게 설치할 수 있음은 물론, 실내의 측벽과 바닥 및 천정의 통일된 인테리어를 구현할 수 있는 효과도 있고, 이에 따라 향상된 황토의 효능을 얻을 수 있어 인체의 건강에 매우 큰 이로움을 가져올 수 있게 된다.In addition, due to the light weight of the ocher panel, it is possible to easily install the ocher panel of the present invention on the ceiling by solving the conventional problem that the ocher panel can not be installed on the ceiling, as well as the unified interior of the side wall and floor of the room and the ceiling There is also an effect that can be implemented, and thus can obtain an improved ocher efficacy, which can bring a great benefit to the health of the human body.

그리고, 상기 황토판넬을 자동화하여 생산하게 되므로, 인력의 낭비를 방지할 수 있고, 이에 따른 비용의 절감을 얻을 수 있으며, 균일화된 최상의 황토판넬을 저렴하게 제작할 수 있는 매우 큰 효과가 있다.In addition, since the ocher panel is automatically produced, it is possible to prevent the waste of manpower, thereby reducing the cost, and have a very large effect of inexpensively producing the best uniformed ocher panel.

Claims (7)

황토를 이용하여 황토판넬(1)을 제작하는 통상의 황토판넬 제작방법에 있어서,In the conventional ocher panel manufacturing method for producing the ocher panel (1) using ocher, 황토판넬(1)의 사각의 틀(2)을 동(銅)판 또는 알루미늄 등의 경량재를 이용하여 제작하는 틀 제작단계(S10)와;Frame manufacturing step (S10) for producing a rectangular frame (2) of the ocher panel (1) by using a lightweight material such as copper plate or aluminum; 상기 단계(S10)에서 제작된 틀(2)의 내부에 망사원단(4)을 부착하는 원단 부착단계(S11)와;And fabric attachment step (S11) for attaching the fabric (4) to the inside of the frame (2) produced in the step (S10); 상기 단계(S11)에서 망사원단(4)의 상부에 경량 알루미늄 매쉬망(5)을 부착하는 매쉬망 부착단계(S12)와;A mesh net attaching step (S12) of attaching a lightweight aluminum mesh net (5) to the upper portion of the mesh fabric (4) in the step (S11); 상기 황토판넬(1)을 제작하기 위한 황토와 석회석을 제1호퍼(20)에 넣는 제1호퍼단계(S20)와;First hopper step (S20) for putting the loess and limestone in the first hopper 20 for producing the ocher panel (1); 상기 황토판넬(1)을 제작하기 위한 경량골재를 제2호퍼(21)에 넣는 제2호퍼단계(S21)와;A second hopper step (S21) for putting the light weight aggregate for producing the ocher panel 1 into the second hopper 21; 상기 황토판넬(1)을 제작하기 위한 물 및 무독성 접착제를 제3호퍼(22)에 넣는 제3호퍼단계(S22)와;A third hopper step (S22) of putting water and a non-toxic adhesive for producing the ocher panel 1 into the third hopper 22; 상기 제1호퍼단계(S20)와 제2호퍼단계(S21) 및 제3호퍼단계(S22)에서 제1·제2·제3호퍼(20)(21)(22)에 넣어진 황토와 석회석 및 경량골재, 물과 무독성 접착제를 원형 롤 믹서(23)에 계량장치(23a)를 통해 일정량을 각각 투입하여 혼합하는 원형 롤 믹서단계(S23)와;Ocher and limestone put into the first, second and third hoppers 20, 21, 22 in the first hopper stage (S20), the second hopper stage (S21) and the third hopper stage (S22); A circular roll mixer step S23 for mixing light aggregate, water and non-toxic adhesive into a circular roll mixer 23 by mixing a predetermined amount through a metering device 23a; 상기 단계(S23)에서 혼합된 혼합물을 공급기(24)에 공급하는 공급단계(S24)와;A supply step (S24) of supplying the mixture mixed in the step (S23) to the feeder (24); 상기 단계(S24)에서 망사원단(4)과 매쉬망(5)이 부착된 틀(2)을 컨베이어(30)에 투입하고 상기 투입된 틀(2)의 내부에 공급기(24)에서 혼합물을 충진시키는 컨베이어 투입단계(S30)와;In the step (S24) to insert the frame 2 attached to the mesh fabric 4 and the mesh 5 to the conveyor 30 and to fill the mixture in the feeder 24 inside the injected frame (2) Conveyor input step (S30) and; 상기 단계(S30)에서 틀(2)의 내부에 충진된 혼합물의 수평을 유지시키며 기포발생을 억제시키기 위해 컨베이어(30)의 하부에 설치된 진동테이블(31)에 의해 진동을 발생시키는 진동테이블 통과단계(S31)와;Vibration table passing step of generating vibration by vibrating table 31 installed in the lower part of the conveyor 30 to maintain the horizontal level of the mixture filled in the frame (2) in the step (S30) and to suppress bubble generation (S31); 상기 단계(S31)에서 혼합물이 수평으로 유지된 틀(2)에 송풍기(33)를 이용하여 15 ~ 18℃의 자연온도로 1차건조시키는 1차 자연풍 건조단계(S33)와;A first natural wind drying step (S33) of primary drying at a natural temperature of 15 to 18 ° C. by using a blower 33 in the mold 2 in which the mixture is horizontally maintained in the step S31; 상기 단계(S33)에서 1차건조된 틀(2)을 건조실(34)을 통과시키며 35 ~ 40℃의 열풍으로 건조시키는 2차 열풍건조단계(S34)와;A second hot air drying step (S34) of passing the mold (2) first dried in the step (S33) and drying it with hot air at 35 to 40 ° C; 상기 단계(S34)에서 완전건조된 황토판넬(1)을 컨베이어(30)에 의해 자동조적기(S35)로 공급하여 자동으로 조적되도록 하는 자동조적기 단계(S35)로 이루어진 것을 특징으로 하는 황토판넬 제작방법.The ocher panel, characterized in that made in the step (S34) is an automatic regulator step (S35) to be automatically supplied by supplying the fully dried ocher panel (1) to the automatic regulator (S35) by the conveyor (30) How to make. 제 1 항에 있어서,The method of claim 1, 상기 진동테이블 통과단계(S31)와 1차 자연풍 건조단계(S33)의 사이에 황토판넬(1)의 표면에 무늬성형롤러(32)를 이용하여 무늬를 형성시킬 수 있는 무늬성형 단계(S32)를 더 포함시킨 것을 특징으로 하는 황토판넬 제작방법.Between the vibrating table passing step (S31) and the first natural wind drying step (S33) a pattern forming step (S32) that can form a pattern using a pattern forming roller 32 on the surface of the ocher panel (1) Ocher panel manufacturing method characterized in that it further comprises. 황토를 이용하여 황토판넬(1)을 제작하는 통상의 황토판넬 제작장치에 있어서,In the conventional ocher panel manufacturing apparatus for producing the ocher panel (1) using the loess, 동판 또는 알루미늄 등의 경량재를 이용하여 제작된 틀(2)에 망사원단(4)과 경량 알루미늄 매쉬망(5)을 부착하고, 각 공정으로 틀(2)을 이송시키는 켄베이어(30)와;Kenvey 30, which attaches the mesh fabric 4 and the lightweight aluminum mesh net 5 to the mold 2 made of a lightweight material such as copper plate or aluminum, and transfers the mold 2 to each process. ; 상기 컨베이어(30)의 상부에 설치되어 황토와 석회석이 넣어지는 제1호퍼(20)와;A first hopper 20 installed at an upper portion of the conveyor 30 to which ocher and limestone are placed; 상기 컨베이어(30)의 상부에 설치되어 경량골재가 넣어지는 제2호퍼(21)와;A second hopper 21 installed at an upper portion of the conveyor 30 and into which lightweight aggregate is placed; 상기 컨베이어(30)의 상부에 설치되어 물 및 무독성 접착제가 넣어지는 제3호퍼(22)와;A third hopper 22 installed on the conveyor 30 and into which water and non-toxic adhesive are put; 상기 제1·제2·제3호퍼(20)(21)(22)와 연결되어 각각 물질들을 일정량 투입하는 계량장치(23a)로 부터 혼합물을 공급받아 이를 혼합하는 원형 롤 믹서(23)와;A circular roll mixer 23 which is connected to the first, second and third hoppers 20, 21 and 22 and receives a mixture from a metering device 23a for inputting a predetermined amount of substances, respectively, and mixes the mixture; 상기 원형 롤 믹서(23)에서 혼합된 혼합물을 틀(2)의 내부에 넣기위해 저장되는 공급기(24)와;A feeder (24) which is stored for putting the mixture mixed in the circular roll mixer (23) into the mold (2); 상기 컨베이어(30)에 의해 이송되다가 공급기(24)에서 틀(2)의 내부에 혼합물이 충진되면 진동을 발생시켜 혼합물의 수평을 유지시키고 기포가 발생되는 것을 억제하는 컨베이어(30)의 하부에 설치된 진동테이블(31)과;If the mixture is transported by the conveyor 30 and the mixture is filled in the mold 2 in the feeder 24, the vibration is generated and installed at the lower portion of the conveyor 30 to maintain the level of the mixture and to suppress the generation of bubbles. A vibration table 31; 상기 진동테이블(31)에 의해 틀(2)에 충진된 혼합물이 수평으로 유지된 후 이를 15 ~ 18℃의 자연풍으로 1차건조시키는 컨베이어(30)의 하부에 설치된 송풍기(33)와;A blower (33) installed in the lower part of the conveyor (30) for maintaining the mixture filled in the mold (2) by the vibration table (31) horizontally and then first drying it with natural wind at 15 to 18 ° C; 상기 송풍기(33)에 의해 1차건조된 틀(2)에 35 ~ 40℃의 열풍을 공급하여 2차건조시키는 건조실(34)과;A drying chamber 34 for supplying hot air having a temperature of 35 to 40 ° C. to the mold 2 primarily dried by the blower 33 for secondary drying; 상기 건조실(34)에서 완전건조된 황토판넬(1)을 컨베이어(30)에 의해 이송시켜 자동으로 조적하는 자동조적기(35)로 이루어진 것을 특징으로 하는 황토판넬 제작장치. The ocher panel manufacturing apparatus, characterized in that consisting of an automatic assembler (35) to transfer automatically by the conveyor 30 to the completely dried ocher panel (1) in the drying room (34). 제 3 항에 있어서,The method of claim 3, wherein 상기 진동테이블(31)과 송풍기(33)의 사이의 컨베이어(30) 상부에 설치되어 틀(2)에 충진된 혼합물의 상면에 무늬를 형성시키는 무늬형성롤러(32)를 더 구비한 것을 특징으로 하는 황토판넬 제작장치.It is characterized in that it further comprises a pattern forming roller 32 is installed on the conveyor 30 between the vibrating table 31 and the blower 33 to form a pattern on the upper surface of the mixture filled in the frame (2). Ocher panel manufacturing apparatus. 황토를 이용하여 제작된 통상의 황토판넬(1)에 있어서,In the conventional loess panel (1) made using loess, 상기 황토판넬(1)의 테두리를 형성하기 위해 "ㄷ"자 형상으로 사면이 이루어지고, 경량재질의 알루미늄으로 제작되는 사각의 틀(2)과;A rectangular frame (2) made of a slope having a "c" shape to form an edge of the ocher panel (1) and made of lightweight aluminum; 상기 틀(2)의 내부에 부착되는 망사원단(4)과;A mesh fabric (4) attached to the inside of the frame (2); 상기 망사원단(4)의 상면에 부착되는 경량재질의 알루미늄으로 제작되는 매쉬망(5)과;Mesh net (5) made of lightweight aluminum attached to the upper surface of the mesh fabric (4); 상기 망사원단(4)과 매쉬망(5)이 부착된 틀(1)의 내부에 충진되어 건조된 황토층(6)으로 이루어진 것을 특징으로 하는 황토판넬.Ocher panel, characterized in that made of the ocher layer (6) filled and dried inside the frame (1) to which the mesh fabric (4) and the mesh net (5) is attached. 제 5 항에 있어서,The method of claim 5, 상기 틀(2)의 내부에 충진되어 황토층(6)을 구성하는 혼합물은, 황토 70 ~ 75%와, 석회석 4 ~ 5%와, 경량골재 13 ~ 15%와, 물 및 무독성 접착제 8 ~ 10%를 혼합한 혼합물로 이루어진 것을 특징으로 하는 황토판넬.The mixture constituting the ocher layer 6 by filling the inside of the mold 2 is 70 to 75% of ocher, 4 to 5% of limestone, 13 to 15% of light aggregate, 8 to 10% of water and non-toxic adhesive. Ocher panel, characterized in that consisting of a mixture. 제 5 항에 있어서,The method of claim 5, 상기 황토판넬(1)에 의해 유해전자파와 수맥 등이 차단되도록 알루미늄 매쉬망(5) 대신에 동(銅)으로 제작된 동메쉬망을 구비시킨 것을 특징으로 하는 황토판넬.The ocher panel, characterized in that it is provided with a copper mesh net made of copper (대신) instead of the aluminum mesh net (5) to block harmful electromagnetic waves and veins by the ocher panel (1).
KR1020050046249A 2005-05-31 2005-05-31 The Method Manufacturing and An Apparatus of Yellow Earth Panel KR100674429B1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
KR1020050046249A KR100674429B1 (en) 2005-05-31 2005-05-31 The Method Manufacturing and An Apparatus of Yellow Earth Panel

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
KR1020050046249A KR100674429B1 (en) 2005-05-31 2005-05-31 The Method Manufacturing and An Apparatus of Yellow Earth Panel

Related Child Applications (1)

Application Number Title Priority Date Filing Date
KR20-2005-0015480U Division KR200396159Y1 (en) 2005-05-31 2005-05-31 A Yellow Earth Panel Of An Apparatus

Publications (2)

Publication Number Publication Date
KR20060124360A true KR20060124360A (en) 2006-12-05
KR100674429B1 KR100674429B1 (en) 2007-01-25

Family

ID=37729123

Family Applications (1)

Application Number Title Priority Date Filing Date
KR1020050046249A KR100674429B1 (en) 2005-05-31 2005-05-31 The Method Manufacturing and An Apparatus of Yellow Earth Panel

Country Status (1)

Country Link
KR (1) KR100674429B1 (en)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR101123301B1 (en) * 2010-06-18 2012-03-20 윤덕식 Finishing materials of building using yellow soils and apparatus for manufacturing the same
KR101219970B1 (en) * 2011-10-07 2013-01-09 노광우 Loess panel manufacture method and device
CN107263698A (en) * 2017-08-02 2017-10-20 安阳三乔环保科技有限公司 A kind of load bearing wall wall board forming equipment

Families Citing this family (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR20070108840A (en) 2007-10-24 2007-11-13 한상관 Method to execute interior works for nature friendly construction
KR101077743B1 (en) 2008-12-01 2011-10-27 이관석 A Movable House For Simplicity

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR101123301B1 (en) * 2010-06-18 2012-03-20 윤덕식 Finishing materials of building using yellow soils and apparatus for manufacturing the same
KR101219970B1 (en) * 2011-10-07 2013-01-09 노광우 Loess panel manufacture method and device
CN107263698A (en) * 2017-08-02 2017-10-20 安阳三乔环保科技有限公司 A kind of load bearing wall wall board forming equipment

Also Published As

Publication number Publication date
KR100674429B1 (en) 2007-01-25

Similar Documents

Publication Publication Date Title
ES2738525T3 (en) General purpose materials that incorporate a matrix of microparticles
US20090235600A1 (en) Stone work simulation system
US20230258001A1 (en) Cladding panel
KR100674429B1 (en) The Method Manufacturing and An Apparatus of Yellow Earth Panel
KR100695502B1 (en) Heat insulating material composition, heat insulating panel prepared using this and preparing method of heat insulating panel
KR100715253B1 (en) Hollow light weight block
KR20180031544A (en) Activated charcoal slurry preventing radon gas for building and its forming products
TW200631748A (en) Process for manufacturing sound absorbing cement tile
KR100359736B1 (en) A porosity building materials and its manufacturing method
US5765334A (en) Method of manufacturing porous building materials
KR102188082B1 (en) Sculpture panel for decorating the interior and exterior wall of the building
KR200396159Y1 (en) A Yellow Earth Panel Of An Apparatus
JP2006348479A (en) Construction method of backing material for construction
KR20010012022A (en) A building interior having loess
JP2004243748A (en) Production method for building material with surface layer integrated inside layer
KR101966149B1 (en) Multifunctional building wall structure including oxygen gas supplying line
KR100598868B1 (en) Loess panel with strength, method for producing the same and construction meterials using the panel
JP3819837B2 (en) Insulating panel manufacturing method, insulating panel, and insulating panel construction method
KR20040052778A (en) Method for manufacturing lightweight board and lightweight board thereof
CN216042310U (en) Gather rock flat board
KR101167581B1 (en) Loess panel and manufacturing method thereof
KR200393123Y1 (en) Hot Water Room Ground Panel made by Vermiculite
KR20050081568A (en) Inorganic sound absorbers, sound absorbing boards and manufacturing methods thereof
KR20110132005A (en) Method of manufacturing for loess tile
CN107524236A (en) A kind of environment-friendly waterproof sheet material and preparation method thereof

Legal Events

Date Code Title Description
A201 Request for examination
E902 Notification of reason for refusal
E701 Decision to grant or registration of patent right
GRNT Written decision to grant
FPAY Annual fee payment

Payment date: 20130119

Year of fee payment: 7

FPAY Annual fee payment

Payment date: 20140121

Year of fee payment: 8

FPAY Annual fee payment

Payment date: 20150119

Year of fee payment: 9

FPAY Annual fee payment

Payment date: 20160119

Year of fee payment: 10

FPAY Annual fee payment

Payment date: 20170119

Year of fee payment: 11

LAPS Lapse due to unpaid annual fee