KR20050039892A - A painting method for removing scars on automobiles using low-pressured spray gun - Google Patents
A painting method for removing scars on automobiles using low-pressured spray gun Download PDFInfo
- Publication number
- KR20050039892A KR20050039892A KR1020030074961A KR20030074961A KR20050039892A KR 20050039892 A KR20050039892 A KR 20050039892A KR 1020030074961 A KR1020030074961 A KR 1020030074961A KR 20030074961 A KR20030074961 A KR 20030074961A KR 20050039892 A KR20050039892 A KR 20050039892A
- Authority
- KR
- South Korea
- Prior art keywords
- coating
- paint
- transparent coating
- transparent
- distance
- Prior art date
Abstract
본 발명은 저압 스프레이건을 이용한 자동차 흠집 도장방법에 관한 것으로서, 더욱 상세하게는 자동차 표면의 흠집을 제거하고 저압 스프레이건을 이용하여 페인트와 투명코팅제를 코팅함에 있어 기존의 페인트와 새로 도포된 페인트가 균일하고 색상의 편차를 없도록 함과 아울러 도장부위가 파손되지 않도록 도장두께를 보상하고 작업성을 향상시킨 저압 스프레이건을 이용한 자동차 흠집 도장방법에 관한 것이다.The present invention relates to a method for painting a car scratch using a low pressure spray gun, and more particularly, to remove scratches on the surface of a car and to coat paint and a transparent coating agent using a low pressure spray gun. The present invention relates to a method for painting a scratch on a car using a low pressure spray gun which compensates the coating thickness and improves workability so as to prevent uniformity and color variation and to prevent damage to the painted portion.
이에 본 발명은 자동차의 도장할 부위를 컴파운드를 이용하여 이물질을 제거하는 1차 이물질 제거공정(10); 상기 1차 이물질 제거공정(10)을 거친 흠집부분을 샌드페이퍼로 연마하고 고형화물질을 도포한 후, 재차 샌드페이퍼로 연마하는 흠집제거 공정(11); 상기 흠집제거 공정(11)을 거쳐 흠집이 제거된 부분을 일정거리에서 페인트로 분사도장하는 1차 도장공정(12); 상기 1차 도장공정(12)을 거친 페인트 부분을 열건조기로 일정시간 건조한 후 냉각시키는 1차 열처리공정(13); 상기 1차 열처리공정(13)을 거쳐 건조되고 냉각된 페인트 부분을 샌드페이퍼로 연마하여 이물질을 제거하는 2차 이물질 제거공정(14); 상기 2차 이물질 제거공정(14)을 거져 이물질이 제거된 부분을 상기 1차 도장공정(12)시 보다 먼 도장거리에서 페인트로 분사도장하는 2차 도장공정(15); 상기 2차 도장공정(15)을 거친 페인트 부분을 일정거리에서 투명코팅제로 코팅하는 1차 투명코팅공정(16); 상기 1차 투명코팅공정(16)시 보다 짧은 거리에서 투명코팅제로 코팅하는 2차 투명코팅공정(17); 상기 2차 투명코팅공정(17)시 보다 짧은 거리에서 투명코팅제로 코팅하는 3차 투명코팅공정(18); 상기 3차 투명코팅공정(18)을 거쳐 코팅된 부분을 열건조기로 일정시간 건조한 후 냉각시키는 2차 열처리공정(19); 상기 2차 열처리공정(19)을 거쳐 건조되고 냉각된 코팅 부분을 컴파운드로 광택처리하는 광택공정(20)으로 이루어지는 것을 특징으로 한다.Accordingly, the present invention provides a first foreign matter removing step (10) of removing foreign matter by using a compound to be painted on the vehicle; A scratch removal step (11) of polishing the scratches which have passed through the first foreign matter removing step (10) with sand paper and applying a solidifying material, and then again polishing with sand paper; A primary coating process (12) for spray-coating a portion where the scratches are removed through the scratch removing step (11) with paint at a predetermined distance; A first heat treatment step 13 of cooling the paint portion that has undergone the first coating step 12 after drying for a predetermined time with a heat dryer; A secondary foreign material removal step (14) of removing the foreign matter by polishing the dried and cooled paint portion by sand paper through the primary heat treatment step (13); A secondary coating step (15) of spraying and coating a portion from which the foreign matter is removed by the secondary foreign material removing step (14) with paint at a farther coating distance than the first coating step (12); A first transparent coating step 16 of coating the paint part that has passed through the second coating step 15 with a transparent coating agent at a predetermined distance; A second transparent coating process 17 for coating with a transparent coating agent at a shorter distance than the first transparent coating process 16; A third transparent coating process 18 of coating a transparent coating agent at a shorter distance than the second transparent coating process 17; A second heat treatment step 19 of cooling the coated portion through the third transparent coating process 18 after drying for a predetermined time with a heat dryer; It characterized in that it comprises a gloss process (20) for polishing the dried and cooled coating portion with a compound through the secondary heat treatment process 19.
Description
본 발명은 저압 스프레이건을 이용한 자동차 흠집 도장방법에 관한 것으로서, 더욱 상세하게는 자동차 표면의 흠집을 제거하고 저압 스프레이건을 이용하여 페인트와 투명코팅제를 코팅함에 있어 기존의 페인트와 새로 도포된 페인트가 균일하고 색상의 편차를 없도록 함과 아울러 도장부위가 파손되지 않도록 도장두께를 보상하고 작업성을 향상시킨 저압 스프레이건을 이용한 자동차 흠집 도장방법에 관한 것이다.The present invention relates to a method for painting a car scratch using a low pressure spray gun, and more particularly, to remove scratches on the surface of a car and to coat paint and a transparent coating agent using a low pressure spray gun. The present invention relates to a method for painting a scratch on a car using a low pressure spray gun which compensates the coating thickness and improves workability so as to prevent uniformity and color variation and to prevent damage to the painted portion.
일반적으로 자동차 제조공장에서 출고된 차량은 운행하다가 접촉 또는 추돌 사고로 인하거나, 못, 칼, 기타 뾰족한 물체 등에 의해 긁혀서 차량의 도색에 흠집 및 상처가 나는 일이 빈번히 발생하며, 노후로 인하여 차량 도색이 박리 되기도 하는데, 이러한 자동차의 외관 특히 차량 표면은 자동차 품위나 수명에 미치는 영향이 클 뿐 아니라, 금속의 부식 방지를 위해서라도 차량 외부가 손상되면 정비업소를 찾아가 많은 비용을 들여 재 도색하고 있는 실정이다.In general, a vehicle released from a car manufacturing factory is frequently caused by contact or collision while driving, scratches and scratches due to nails, knives, or other sharp objects. The paint may be peeled off, and the appearance of such a car, especially the surface of the car, has a great effect on the quality and life of the car, and in order to prevent corrosion of metals, when the outside of the car is damaged, it visits a repair shop and repaints it at a high cost. It is true.
통상, 이와 같은 목적을 위해 사용되어 온 종래의 차량 도색 장치는 컴프레서에서 생성된 고압의 압축공기를 스프레이 건에 공급하여 도료를 내뿜여 분사도장하는 것으로서, 이때, 컴프레서는 동력, 즉 발동기 또는 모터로 임펠러형 로터를 회전시키거나 피스톤을 왕복운동시켜 기체를 압송하는 것으로서, 압력비 2 이상, 송출압력 1kgf/cm2 이상의 것을 말한다.Conventionally, a conventional vehicle paint apparatus which has been used for this purpose is to supply high pressure compressed air generated by a compressor to a spray gun to spray paint by spraying paint, wherein the compressor is a power, that is, a motor or a motor. It rotates an impeller-type rotor or reciprocates a piston, and conveys gas, and it means a pressure ratio of 2 or more and a delivery pressure of 1 kgf / cm <2> or more.
한편, 분사도장시 분진 등으로 인해 주변 환경에 도료가 날려 환경 공해 문제가 초래되어 최근에는 환경규제에 대처하기 위하여, 도료를 저압 에어의 고체적 흐름으로 분무시키는 저압 스프레이건의 사용에 대하여 관심이 증대되고 있다.On the other hand, the spraying of paint on the surrounding environment due to dust, etc. during spray coating causes environmental pollution problems. Recently, in order to cope with environmental regulations, interest in the use of a low pressure spray gun that sprays the paint with a solid flow of low pressure air is increasing. It is becoming.
이러한 저압 스프레이건은 0.7kgf/cm2 이하의 저압에어를 사용함으로서 분무 작업시 고속 및 고압 에어를 사용하는 일반 스프레이건 보다 과분무가 적다.This low pressure spray gun uses less than 0.7kgf / cm 2 low pressure air, so there is less overspray than general spray guns using high speed and high pressure air in spraying operations.
그러나, 상기 저압 스프레이건의 도료 분사용 기체는 저압이며, 이러한 저압의 공기로 도료를 분사해 도장할 경우 도장 작업이 더디고, 도료의 도장강도가 낮아 수명이 짧을 뿐 아니라, 특히 저압 스프레이건은 토출량이 적어 일반 스프레이건을 사용할 때의 도장두께를 따라갈 수 없으며, 이에 따라 나뭇가지 등의 스침에도 도장이 파손되는 문제가 있다.However, the gas for spraying the paint of the low pressure spray gun is low pressure, and when spraying the paint with such low pressure air, the painting work is slow, the paint strength of the paint is short, and the life is short. It is not possible to follow the coating thickness when using a general spray gun, there is a problem that the coating is damaged even when grazing, such as twigs.
또한, 도장작업시 외부에서 들어오는 공기와 함께 흙먼지 등의 이물질이 유입되어 도장면에 부착되어 도장품질이 저하되는 문제도 있었다.In addition, there was a problem in that the coating quality is degraded due to the inflow of foreign matters such as dust and dirt with the air coming from the outside during the painting work.
상기한 종래의 문제점을 해결하기 위한 본 발명의 목적은 자동차 표면의 흠집을 제거하기 위해 저압 스프레이건을 이용하여 페인트와 투명코팅제를 코팅함에 있어 도장두께를 보상하여 도장부위가 파손되지 않도록 함과 아울러 기존의 페인트와 새로 도포된 페인트가 균일하고 색상의 편차를 없도록 하며 작업성을 향상시킨 저압 스프레이건을 이용한 자동차 흠집 도장방법을 제공하는데 있다.An object of the present invention for solving the above-mentioned problems is to compensate for the coating thickness in coating the paint and the transparent coating agent using a low pressure spray gun to remove scratches on the surface of the vehicle and to prevent the coating site from being damaged. The present invention provides a method of painting a scratch on a car using a low pressure spray gun that improves workability and prevents uniformity of color between existing paint and newly applied paint.
상기한 목적을 달성하기 위한 본 발명은 자동차의 도장할 부위를 컴파운드를 이용하여 이물질을 제거하는 1차 이물질 제거공정; 상기 1차 이물질 제거공정을 거친 흠집부분을 샌드페이퍼로 연마하고 고형화물질을 도포한 후, 재차 샌드페이퍼로 연마하는 흠집제거 공정; 상기 흠집제거 공정을 거쳐 흠집이 제거된 부분을 일정거리에서 페인트로 분사도장하는 1차 도장공정; 상기 1차 도장공정을 거친 페인트 부분을 열건조기로 일정시간 건조한 후 냉각시키는 1차 열처리공정; 상기 1차 열처리공정을 거쳐 건조되고 냉각된 페인트 부분을 샌드페이퍼로 연마하여 이물질을 제거하는 2차 이물질 제거공정; 상기 2차 이물질 제거공정을 거져 이물질이 제거된 부분을 상기 1차 도장공정시 보다 먼 도장거리에서 페인트로 분사도장하는 2차 도장공정; 상기 2차 도장공정을 거친 페인트 부분을 일정거리에서 투명코팅제로 코팅하는 1차 투명코팅공정; 상기 1차 투명코팅공정시 보다 짧은 거리에서 투명코팅제로 코팅하는 2차 투명코팅공정; 상기 2차 투명코팅공정시 보다 짧은 거리에서 투명코팅제로 코팅하는 3차 투명코팅공정; 상기 3차 투명코팅공정을 거쳐 코팅된 부분을 열건조기로 일정시간 건조한 후 냉각시키는 2차 열처리공정; 상기 2차 열처리공정을 거쳐 건조되고 냉각된 코팅 부분을 컴파운드로 광택처리하는 광택공정으로 이루어지는 것을 특징으로 한다.The present invention for achieving the above object is the first foreign matter removal step of removing the foreign matter by using a compound to the painted portion of the vehicle; A scratch removal step of polishing the scratched portion that has been subjected to the first foreign matter removing process by sand paper and applying a solidifying material, and then again by sand paper; A primary coating process of spray-coating a portion where the scratch is removed through the scratch removing process with paint at a predetermined distance; A primary heat treatment step of cooling the paint portion which has undergone the primary coating process by drying with a heat dryer for a predetermined time; A secondary foreign material removal step of removing foreign matters by polishing the dried and cooled paint part by sand paper through the primary heat treatment process; A secondary coating step of spray coating the portion from which the foreign matter is removed by the second foreign matter removing step with paint at a farther coating distance than the first coating step; A first transparent coating process of coating the paint part that has undergone the second coating process with a transparent coating agent at a predetermined distance; A second transparent coating process of coating with a transparent coating agent at a shorter distance than the first transparent coating process; A third transparent coating process of coating with a transparent coating agent at a shorter distance during the second transparent coating process; A secondary heat treatment step of cooling the coated portion after drying for a predetermined time with a heat dryer through the third transparent coating process; It characterized by consisting of a gloss process to polish the coating portion dried and cooled through the secondary heat treatment process with a compound.
또한, 자동차의 도장할 부위를 컴파운드를 이용하여 이물질을 제거하는 1차 이물질 제거공정; 상기 1차 이물질 제거공정을 거친 흠집부분을 샌드페이퍼로 연마하고 고형화물질을 도포한 후, 재차 샌드페이퍼로 연마하는 흠집제거 공정; 상기 흠집제거 공정을 거쳐 흠집이 제거된 부분을 일정거리에서 페인트로 분사도장하되 상기 고형화물질의 경계선 보다 4∼6cm 넘겨서 도장하는 1차 도장공정; 상기 1차 도장공정을 거친 페인트 부분을 열건조기로 일정시간 건조한 후 냉각시키는 1차 열처리공정; 상기 1차 열처리공정을 거쳐 건조되고 냉각된 페인트 부분을 샌드페이퍼로 연마하여 이물질을 제거하는 2차 이물질 제거공정; 상기 2차 이물질 제거공정을 거져 이물질이 제거된 부분을 상기 1차 도장공정시 보다 먼 도장거리에서 페인트로 분사도장하되 상기 1차 도장공정에서 도장된 폐인트 경계선 보다 2∼4cm 넘겨서 도장하는 2차 도장공정; 상기 2차 도장공정을 거친 페인트 부분을 일정거리에서 투명코팅제로 코팅하되 상기 폐인트 부분의 경계선 보다 4∼6cm 넘겨서 코팅하는 1차 투명코팅고정; 상기 1차 투명코팅공정시 보다 짧은 거리에서 투명코팅제로 코팅하되 상기 1차 투명코팅공정에서 코팅된 코팅 경계선 보다 1∼2cm 작게 코팅하는 2차 투명코팅공정; 상기 2차 투명코팅공정시 보다 짧은 거리에서 투명코팅제로 코팅하되 상기 2차 투명코팅공정에서 코팅된 코팅 경계선 보다 1∼2cm 작게 코팅하는 3차 투명코팅공정; 상기 3차 투명코팅공정을 거쳐 코팅된 부분을 열건조기로 일정시간 건조한 후 냉각시키는 2차 열처리공정; 상기 2차 열처리공정을 거쳐 건조되고 냉각된 코팅 부분을 컴파운드로 광택처리하는 광택공정으로 이루어지는 것을 특징으로 한다.In addition, the first foreign matter removing step of removing the foreign matter by using the compound to the painted portion of the vehicle; A scratch removal step of polishing the scratched portion that has been subjected to the first foreign matter removing process by sand paper and applying a solidifying material, and then again by sand paper; A first coating process of spray-coating a portion of which the scratch is removed through the scratch removing process with paint at a predetermined distance, but coating 4-6 cm beyond the boundary of the solidifying material; A primary heat treatment step of cooling the paint portion which has undergone the primary coating process by drying with a heat dryer for a predetermined time; A secondary foreign material removal step of removing foreign matters by polishing the dried and cooled paint part by sand paper through the primary heat treatment process; The second foreign material is coated by spraying the part where foreign material is removed by the second foreign material removal process with paint at a farther coating distance than in the first painting process, but it is coated 2-4 cm beyond the border of the painted ingot in the first painting process. Painting process; A first transparent coating fixing the paint part which has undergone the second coating process with a transparent coating agent at a predetermined distance, but coating 4 to 6 cm beyond the boundary line of the waste insert part; A second transparent coating process of coating with a transparent coating agent at a shorter distance than the first transparent coating process but coating 1 to 2 cm smaller than the coating boundary line coated in the first transparent coating process; A third transparent coating process of coating with a transparent coating agent at a shorter distance than the second transparent coating process but coating 1 to 2 cm smaller than a coating boundary coated in the second transparent coating process; A secondary heat treatment step of cooling the coated portion after drying for a predetermined time with a heat dryer through the third transparent coating process; It characterized by consisting of a gloss process to polish the coating portion dried and cooled through the secondary heat treatment process with a compound.
이하, 본 발명의 바람직한 실시예들을 첨부된 도면을 참조하여 설명하면 다음과 같다.Hereinafter, preferred embodiments of the present invention will be described with reference to the accompanying drawings.
도 1 은 본 발명에 따른 저압 스프레이건을 이용한 자동차 흠집 도장방법을 나타내는 공정도이다.1 is a process chart showing a scratch coating method for a vehicle using a low pressure spray gun according to the present invention.
실시예 1Example 1
본 발명의 제 1 실시예에 따른 저압 스프레이건을 이용한 자동차 흠집 도장방법은, 1차 이물질 제거공정(10), 흠집제거 공정(11), 1차 도장공정(12), 1차 열처리공정(13), 2차 이물질 제거공정(14), 2차 도장공정(15), 1차 투명코팅공정(16), 2차 투명코팅공정(17), 3차 투명코팅공정(18), 2차 열처리공정(19), 광택공정(20)으로 이루어진다.Automobile scratch coating method using a low-pressure spray gun according to the first embodiment of the present invention, the first foreign matter removal step 10, the scratch removal step (11), the primary coating step (12), the first heat treatment step (13) ), Secondary foreign material removal process (14), secondary coating process (15), primary transparent coating process (16), secondary transparent coating process (17), tertiary transparent coating process (18), secondary heat treatment process 19, the gloss process 20 is carried out.
먼저, 1차 이물질 제거공정(10)은 자동차에 발생된 흠집부분 즉, 도장할 부위를 1000메쉬 컴파운드를 이용하여 이물질 등을 제거하는 공정이다.First, the first foreign matter removing step 10 is a process of removing foreign matters, etc. using a 1000 mesh compound on the scratches, that is, the portions to be painted, on the automobile.
흠집제거 공정(11)은 상기 1차 이물질 제거공정(10)을 거쳐 이물질 등이 제거된 흠집부분을 샌드페이퍼로 연마하고 난 후, 상기 흠집부분에 석고 또는 진흙과 같은 고형화물질을 도포하여 흠집을 제거하게 된다. 그리고, 상기 흠집에 도포된 고형화물질을 재차 샌드페이퍼로 연마하여 주변면과 평탄면이 되도록 한다.The scratch removal step 11 is to remove the scratches by polishing the scratched portion from which the foreign matter and the like has been removed by sand paper, and then applying a solidified material such as gypsum or mud to the scratched portion. Done. Then, the solidified material applied to the scratch is polished again with sandpaper so as to be the peripheral surface and the flat surface.
1차 도장공정(12)은 상기 흠집제거 공정(11)을 거쳐 흠집이 제거된 부분을 저압 스프레이건을 사용하여 도장할 면으로부터 9∼11cm 바람직하게는 10cm 거리를 유지한 상태에서 차체에 도색된 동일한 색상의 페인트를 분사도장하는 공정이다. The primary painting step 12 is applied to the vehicle body while maintaining the distance of 9 to 11 cm, preferably 10 cm, from the surface to be scratched using the low pressure spray gun through the scratch removing step 11. Spray coating of the same color
이때, 상기 저압 스프레이건을 가로방향으로 도장하되 상,하 3cm 간격으로 이격하여 도장을 하며 전체적으로 2회 도포하는 것이 바람직하다.At this time, the low-pressure spray gun is coated in the horizontal direction, the upper and lower spaced apart 3cm intervals are preferably applied twice as a whole.
즉, 상기 도장할 면으로부터 9∼11cm 거리를 유지하고, 상,하 3cm 간격으로 도장하는 것은 상기 흠집제거 공정(11)에서 흠집을 도포한 고형화물질이 안보이도록 페인트를 두껍고 진하게 도장하기 위함이다. 이때의 도장된 페인트면의 색상은 아직 주변색상과는 차이가 있다.That is, to maintain a 9 to 11cm distance from the surface to be painted, and to paint at an interval of 3cm up and down, to paint the thick and thick paint so that the solidified material applied to the scratch in the scratch removal step (11) is not visible. At this time, the color of the painted surface is still different from the surrounding color.
1차 열처리공정(13)은 상기 1차 도장공정(12)을 거쳐 도포된 페인트 부분을 열건조기로 대략 10분동안 가열한 후 대략 5분동안 냉각하는 공정이다.The primary heat treatment process 13 is a process of heating the paint portion applied through the primary coating process 12 with a heat dryer for about 10 minutes and then cooling for approximately 5 minutes.
즉, 상기 1차 도장공정(12)에서 페인트가 도포될 때 핀롤, 먼지 등의 이물질이 함께 부착될 경우 이러한 이물질을 제거하는 작업을 하기위해 상기 1차 도장공정(12)에서 페인트가 도포된 후에는 열건조기로 가열하여 신속히 건조하고 가열된 부분은 신속히 냉각하여 아래의 2차 이물질 제거공정(14)에서 샌드페이퍼 작업이 원활히 이루어지도록 하는 것이다.That is, when foreign matter such as a pin roll or dust is attached together when the paint is applied in the primary painting process 12, after the paint is applied in the primary painting process 12 to remove the foreign matter, Is heated quickly with a heat dryer to dry quickly and the heated portion is to cool the sandpaper work in the secondary foreign material removal process 14 below.
2차 이물질 제거공정(14)은 앞서 설명한 바와 같이, 상기 1차 도장공정(12)에서 페인트가 도포될 때 이물질 등이 함께 부착되는 경우 이러한 이물질을 제거하는 공정이다. 이때 1000메쉬 샌드페이퍼로 연마하여 이물질을 제거한다.As described above, the secondary foreign material removal process 14 is a process of removing such foreign matter when foreign matters are attached together when the paint is applied in the primary coating process 12. At this time, the foreign material is removed by grinding with 1000 mesh sandpaper.
2차 도장공정(15)은 상기 2차 이물질 제거공정(14)을 거쳐 이물질이 제거된 페인트 부분을 저압 스프레이건을 사용하여 상기 1차 도장공정(12)시 보다 먼 거리인 14∼16cm 바람직하게는 15cm 거리를 유지한 상태에서 차체에 도색된 동일한 색상의 페인트를 분사도장하는 공정이다. The secondary coating process 15 preferably uses a low pressure spray gun to remove the foreign matter removed through the secondary foreign material removal process 14, using a low pressure spray gun, which is 14 to 16 cm, which is farther away from the primary coating process 12. Is a process of spray coating the paint of the same color painted on the body while maintaining a distance of 15 cm.
이때, 상기 저압 스프레이건을 가로방향으로 도장하되 상,하 5cm 간격으로 이격하여 도장을 하며 전체적으로 3회 도포하는 것이 바람직하다.At this time, the low-pressure spray gun is applied in the horizontal direction, spaced apart at intervals of 5cm up and down, it is preferable to apply three times as a whole.
즉, 상기 1차 도장공정(12)시 보다 먼 거리인 14∼16cm 거리를 유지함으로서 상,하 간격도 5cm 를 유지하는 것이며 1차 도장공정(12)시 보다 먼 거리에서 하기 때문에 고운입자로 도장이 가능하며, 또한 입자들이 분산되기 때문에 3회 정도 도포하는 것이다.That is, by maintaining a distance of 14 to 16cm, which is farther than the first coating process 12, the upper and lower intervals are also maintained at 5cm, and because of the farther distance than the first coating process 12, the fine particles are coated. This is possible, and the particles are applied three times because they are dispersed.
아울러, 2차 도장공정(15) 후에는 도포된 페인트면의 색상과 주변색상이 균일하고 편차가 없게 된다.In addition, after the secondary coating process 15, the color and the surrounding color of the applied paint surface are uniform and there is no deviation.
그리고, 상기 2차 도장공정(15) 후에 저압 스프레이건을 사용하여 투명코팅공정(16)(17)(18)을 하게 되는데, 총 3차에 걸쳐서 진행하게 되며, 상기에서 도장된 페인트부분의 강도를 향상하여 도장부분이 일정한 외력에 의해 파손되는 것을 방지하고 광택의 효과를 얻을 수 있다.Then, after the secondary coating process (15) using a low pressure spray gun to perform a transparent coating process (16) (17) (18), which proceeds to a total of three times, the strength of the painted part It is possible to prevent the coating part from being broken by a constant external force and to obtain a gloss effect.
먼저, 1차 투명코팅공정(16)은 상기 2차 도장공정(15)을 거친 페인트 부분에 도장할 면으로부터 19∼21cm 바람직하게는 20cm 거리를 유지한 상태에서 투명코팅제를 분사하여 코팅하는 공정이다.First, the primary transparent coating process 16 is a process of spraying and coating a transparent coating agent while maintaining a distance of 19 to 21 cm, preferably 20 cm, from the surface to be coated on the part of the paint that has undergone the second coating process 15. .
이때, 상기 저압 스프레이건을 가로방향으로 분사하되 상,하 5cm 간격으로 이격하여 분사하며 전체적으로 2회 도포하는 것이 바람직하다.At this time, it is preferable to spray the low pressure spray gun in the horizontal direction, spaced apart at intervals of 5cm up and down, and to apply twice as a whole.
즉, 상기 도장할 면으로부터 19∼21cm 거리를 유지하고, 상,하 5cm 간격으로 도장하는 것은 저압 스프레이건을 사용하여 19∼21cm의 먼 거리에서 분사하게 되면 분사되는 동안 건조되어 상기 페인트 부분에 곧바로 붙게 되는 것이다.That is, to maintain a distance of 19 ~ 21cm from the surface to be painted, and to paint at 5cm intervals up and down, when spraying at a long distance of 19 ~ 21cm using a low pressure spray gun is dried while being sprayed immediately to the paint portion It is attached.
2차 투명코팅공정(17)은 상기 1차 투명코팅공정(16)시 보다 짧은 거리인 14∼16cm 바람직하게는 15cm 거리를 유지한 상태에서 투명코팅제를 분사하여 코팅하는 공정이다.The second transparent coating process 17 is a process of spraying and coating a transparent coating agent while maintaining a distance of 14 to 16 cm, preferably 15 cm, which is shorter than that of the first transparent coating process 16.
이때, 상기 저압 스프레이건을 가로방향으로 분사하되 상,하 3cm 간격으로 이격하여 분사하며 전체적으로 2회 도포하는 것이 바람직하다.At this time, it is preferable to spray the low pressure spray gun in the horizontal direction, spaced apart at intervals of 3cm up and down, and to apply twice as a whole.
즉, 상기 1차 투명코팅공정(16)시 보다 짧은 거리인 14∼16cm 거리를 유지하고, 상,하 3cm 간격으로 도장하는 것은 상기 1차 투명코팅공정(16)시 상기 페인트부분에 이미 투명코팅제가 1차적으로 부착되어 있어서 여기에 재차 투명코팅제를 분사하게 되면 상호간에 잡아주는 역할을 하여 부착력을 향상하게 되고, 가까운거리에서 분사할 때 발생할 수 있는 흘러내림이 방지된다.That is, maintaining a distance of 14 to 16 cm, which is a shorter distance than the first transparent coating process 16, and painting at intervals of 3 cm above and below is already transparent coating agent on the paint portion during the first transparent coating process 16. Is attached to the primary to be sprayed here again to the transparent coating agent serves to hold each other to improve the adhesive force, and to prevent the flow that can occur when spraying at close range.
3차 투명코팅공정(18)은 상기 2차 투명코팅공정(17)을 거친 후 2∼4분 바람직하게는 3분 후에 진행하게 되며, 상기 2차 투명코팅공정(17)시 보다 짧은 거리인 9∼11cm 바람직하게는 10cm 거리를 유지한 상태에서 투명코팅제를 분사하여 코팅하는 공정이다.The third transparent coating process 18 is carried out after 2 to 4 minutes, preferably 3 minutes after the second transparent coating process 17, 9 is a shorter distance than the second transparent coating process 17 Preferably it is a process of spraying and coating a transparent coating agent in the state which kept the distance of -11cm.
이때, 상기 저압 스프레이건을 가로방향으로 분사하되 상,하 3cm 간격으로 이격하여 분사하며 전체적으로 1회 도포하는 것이 바람직하다.At this time, the low pressure spray gun is sprayed in the horizontal direction, and sprayed at intervals of 3cm apart up and down, it is preferable to apply once.
여기서, 상기 2차 투명코팅공정(17)후 2∼4분 후에 진행하는 것은 상기 2차 투명코팅공정(17)시 코팅된 코팅면이 건조되지 않은 상태에서 보다 짧은 거리인 9∼11cm 거리를 유지하고, 상,하 3cm 간격으로 도장하게 되면 흘러내리기 때문에 이를 방지하기 위함이다.Here, proceeding after 2 to 4 minutes after the second transparent coating process 17 maintains a shorter distance of 9 to 11 cm in a state that the coated surface is not dried during the second transparent coating process 17. And, to prevent this because it flows down when the paint is spaced up and down 3cm.
한편, 상기 투명코팅공정(16)(17)(18)을 3차에 걸쳐 진행하고 또한 도장거리를 점차적으로 짧게 함으로서 투명코팅제 상호간에 부착력이 향상되고 작업과정에서 흘러내리지 않으며 고른 코팅면을 얻을 수 있어 강도가 향상된다.On the other hand, by proceeding the transparent coating process (16) (17) (18) three times and gradually shorten the coating distance, the adhesion between the transparent coating agent is improved and does not flow down in the working process to obtain an even coating surface There is an improvement in strength.
아울러, 상기 투명코팅공정(16)(17)(18)은 반드시 3차에 한정되는 것은 아니며 다수회를 하더라도 점차적으로 도장거리를 짧게 한다는 것이 중요하다.In addition, the transparent coating process (16) (17) (18) is not necessarily limited to the third, it is important to gradually shorten the coating distance even if many times.
2차 열처리공정(19)은 상기 3차 투명코팅공정(18)을 거쳐 코팅된 부분을 열건조기로 대략 20분동안 건조한 후 대략 20분동안 냉각하는 공정이다. 이렇게 코팅된 부분을 신속하게 건조하고 냉각함으로서 아래의 광택공정(20)이 원활히 이루어질 수 있다.The secondary heat treatment process 19 is a process of drying the coated portion through the third transparent coating process 18 with a heat dryer for about 20 minutes and then cooling it for about 20 minutes. By quickly drying and cooling the coated portion, the below gloss process 20 can be performed smoothly.
이때, 상기 열건조기는 가열할 면으로부터 대략 50cm 거리를 유지하는 것이 바람직하다.At this time, it is preferable that the heat dryer maintains a distance of about 50 cm from the surface to be heated.
마지막으로 광택공정(20)은 상기 2차 열처리공정(19)을 거쳐 건조되고 냉각된 코팅부분을 컴파운드로 광택처리하는 공정이다.Finally, the gloss process 20 is a process of polishing the dried and cooled coating part with a compound through the secondary heat treatment process 19.
아울러, 상기 광택공정(20)은 1000매쉬, 2000매쉬, 3000매쉬 컴파운드로 순차적으로 광택하는 것이 바람직하며, 이는 상기 2차 열처리공정(19) 후 코팅면에 남아있는 오랜지필(올록볼록한 현상)을 제거하여 평탄면으로 연마하는 것이다.In addition, the gloss process 20 is preferably polished sequentially with 1000 mesh, 2000 mesh, 3000 mesh compound, which is the orange peel (convex phenomenon) remaining on the coated surface after the secondary heat treatment process (19) It is removed and polished to a flat surface.
실시예 2Example 2
상기한 제 1 실시예는 자동차의 도어 등과 같이 도장할 면이 비교적 넓을 때 전체를 도장하는 공정이며, 제 2 실시예에서는 흠집이 비교적 작은 부분 즉, 부분도장을 할 때 사용하는 도장방법이다.The first embodiment is a process of painting the whole when the surface to be painted, such as a door of a car, is relatively wide, and in the second embodiment, a coating method which is used for a relatively small portion of the scratch, that is, partial coating.
제 2 실시예는 제 1 실시예처럼 1차 이물질 제거공정(10), 흠집제거 공정(11), 1차 도장공정(12), 1차 열처리공정(13), 2차 이물질 제거공정(14), 2차 도장공정(15), 1차 투명코팅공정(16), 2차 투명코팅공정(17), 3차 투명코팅공정(18), 2차 열처리공정(19), 광택공정(20)으로 이루어진다.In the second embodiment, as in the first embodiment, the first foreign matter removing step 10, the scratch removing step 11, the first painting step 12, the first heat treatment step 13, and the second foreign matter removing step 14 are performed. , Secondary coating process (15), primary transparent coating process (16), secondary transparent coating process (17), tertiary transparent coating process (18), secondary heat treatment process (19), polishing process (20) Is done.
즉, 제 2 실시예는 상기한 제 1 실시예와 동일한 공정으로 진행되어 여기서 전체공정에대한 설명은 생략하며, 단, 틀린공정에 대해서만 설명하도록 한다.That is, the second embodiment proceeds to the same process as the first embodiment described above, and the description of the entire process will be omitted here, but only the wrong process will be described.
먼처, 1차 도장공정(12)은 상기 흠집제거 공정(11)을 거치면서 고형화물질이 도포되어 흠집이 제거된 부분을 9∼11cm 바람직하게는 10cm 거리를 유지한 상태에서 차체에 도색된 동일한 색상의 페인트를 분사도장하되 상기 고형화물질의 경계선 보다 4∼6cm 바람직하게는 5cm 를 넘겨서 도장하게 된다.First, the first painting process 12 is the same color painted on the vehicle body while maintaining a distance of 9 to 11 cm, preferably 10 cm, from which the solidified material is applied while the scratch removing process 11 is applied. Spray coating of the coating, but the coating of 4-6cm, preferably 5cm more than the boundary of the solidified material.
즉, 상기 흠집제거 공정(11)에서 고형화물질을 샌드페이퍼로 연마작업을 할때 주변부분까지 연마가 될 수 있기 때문에 상기 1차 도장공정(12)에서는 상기 고형화물질 경계선 보다 4∼6cm 넘겨서 그 주변부위까지 도장을 하는 것이다.That is, since the surface can be polished to the peripheral part when the solidifying material is sandpaper polished in the scratch removal process 11, the peripheral part of the first coating process 12 is 4 to 6 cm beyond the boundary line of the solidified material. Will paint until.
이때, 상기 저압 스프레이건을 가로방향으로 도장하되 상,하 3cm 간격으로 이격하여 도장을 하며 전체적으로 2회 도포하는 것이 바람직하다.At this time, the low-pressure spray gun is coated in the horizontal direction, the upper and lower spaced apart 3cm intervals are preferably applied twice as a whole.
2차 도장공정(15)은 상기 2차 이물질 제거공정(14)을 거쳐 이물질이 제거된 페인트 부분을 저압 스프레이건을 사용하여 상기 1차 도장공정(12)시 보다 먼 거리인 14∼16cm 바람직하게는 15cm 거리를 유지한 상태에서 차체에 도색된 동일한 색상의 페인트를 분사도장하되 상기 상기 1차 도장공정(12)에서 도장된 페인트 경계선 보다 2∼4cm 바람직하게는 3cm 를 넘겨서 도장하게 된다.The secondary coating process 15 preferably uses a low pressure spray gun to remove the foreign matter removed through the secondary foreign material removal process 14, using a low pressure spray gun, which is 14 to 16 cm, which is farther away from the primary coating process 12. While spraying the paint of the same color painted on the vehicle body while maintaining a distance of 15cm, the paint is applied over 2 ~ 4cm, preferably 3cm more than the paint boundary painted in the primary painting process (12).
즉, 상기 2차 이물질 제거공정(14)에서 페인트 부분을 샌드페이퍼로 연마작업을 할때 주변부분까지 연마가 될 수 있기 때문에 상기 2차 도장공정(15)에서는 상기 페인트 경계선 보다 2∼4cm 넘겨서 그 주변부위까지 도장을 하는 것이다.That is, when the paint portion is polished by sand paper in the second foreign matter removing step 14, the peripheral part may be polished, so the second coating step 15 passes 2 to 4 cm more than the paint boundary line, To paint the site.
이때, 상기 저압 스프레이건을 가로방향으로 도장하되 상,하 5cm 간격으로 이격하여 도장을 하며 전체적으로 3회 도포하는 것이 바람직하다.At this time, the low-pressure spray gun is applied in the horizontal direction, spaced apart at intervals of 5cm up and down, it is preferable to apply three times as a whole.
1차 투명코팅공정(16)은 상기 2차 도장공정(15)을 거친 페인트 부분을 도장할 면으로부터 19∼21cm 바람직하게는 20cm 거리를 유지한 상태에서 투명코팅제를 분사하여 코팅하되 상기 2차 도장공정(15)에서 도장된 페인트 부분의 경계선 보다 4∼6cm 바람직하게는 5cm 넘겨서 코팅하게 된다.The first transparent coating process 16 is sprayed with a transparent coating agent while maintaining a distance of 19 to 21 cm, preferably 20 cm, from the surface to be painted the second part of the coating process 15, the second coating The coating is carried out 4-6 cm, preferably 5 cm, beyond the boundary of the painted portion painted in the step (15).
즉, 상기 2차 도장공정(15)에서 도장된 페인트 부분에만 코팅을 하게 되면 그 부분에서 층이 생기기 때문에 상기 1차 투명코팅공정(16)에서는 상기 페인트 경계선 보다 4∼6cm 넘겨서 그 주변부위까지 코팅을 하는 것이다.That is, when the coating is applied only to the painted portion painted in the secondary coating process 15, a layer is formed at the portion, so that the first transparent coating process 16 passes over 4 to 6 cm above the paint boundary and coats the peripheral portion thereof. To do.
이때, 상기 저압 스프레이건을 가로방향으로 분사하되 상,하 5cm 간격으로 이격하여 분사하며 전체적으로 2회 도포하는 것이 바람직하다.At this time, it is preferable to spray the low pressure spray gun in the horizontal direction, spaced apart at intervals of 5cm up and down, and to apply twice as a whole.
이후, 2차 투명코팅공정(17)은 상기 1차 투명코팅공정(16)에서 코팅된 코팅 경계선 보다 1∼2cm 작게 코팅을 하게 되고, 3차 투명코팅공정(18)에서는 상기 2차 투명코팅공정(17)에서 코팅된 코팅 경계선 보다 1∼2cm 작게 코팅을 진행하여 코팅이 완료된 후에 층이 생기지 않도록 한다.Subsequently, the second transparent coating process 17 coats 1 to 2 cm smaller than the coating boundary line coated in the first transparent coating process 16, and in the third transparent coating process 18, the second transparent coating process. The coating is carried out 1 ~ 2 cm smaller than the coating boundary coated in (17) so that no layer is formed after the coating is completed.
상기한 본 발명에 따르면, 자동차 표면의 흠집을 제거하기 위해 저압 스프레이건을 이용하여 페인트와 투명코팅제를 코팅함에 있어 도장두께를 보상함으로서 일정한 외력이 작용해도 도장부위가 파손되지 않고, 새로 도포된 페인트와 기존의 주변 페인트의 색상이 균일하고 편차가 없음은 물론 층이 생기지 않으며 작업성도 향상된다.According to the present invention described above, by coating a paint and a transparent coating agent using a low pressure spray gun to remove scratches on the surface of the car, the coating area is not damaged even when a certain external force is applied, and the newly applied paint And the color of the existing paint is uniform, there is no deviation, there is no layer and workability is improved.
도 1 은 본 발명에 따른 저압 스프레이건을 이용한 자동차 흠집 도장방법을 나타내는 공정도이다.1 is a process chart showing a scratch coating method for a vehicle using a low pressure spray gun according to the present invention.
<도면의 주요 부분에 대한 부호설명><Code Description of Main Parts of Drawing>
10: 1차 이물질 제거공정 11: 흠집제거 공정10: first foreign matter removal process 11: scratch removal process
12: 1차 도장공정 13: 1차 열처리 공정12: 1st coating process 13: 1st heat treatment process
14: 2차 이물질 제거공정 15: 2차 도장공정14: 2nd foreign matter removal process 15: 2nd painting process
16: 1차 투명코팅 공정 17: 2차 투명코팅 공정16: 1st transparent coating process 17: 2nd transparent coating process
18: 3차 투명코팅 공정 19: 2차 열처리 공정18: 3rd transparent coating process 19: 2nd heat treatment process
20: 광택공정20: polishing process
Claims (8)