KR200328295Y1 - Jig for reforming Open Section of Hemisphere - Google Patents

Jig for reforming Open Section of Hemisphere Download PDF

Info

Publication number
KR200328295Y1
KR200328295Y1 KR20-2003-0022562U KR20030022562U KR200328295Y1 KR 200328295 Y1 KR200328295 Y1 KR 200328295Y1 KR 20030022562 U KR20030022562 U KR 20030022562U KR 200328295 Y1 KR200328295 Y1 KR 200328295Y1
Authority
KR
South Korea
Prior art keywords
jig
head
opening
deformed
slot
Prior art date
Application number
KR20-2003-0022562U
Other languages
Korean (ko)
Inventor
김대중
Original Assignee
두산중공업 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 두산중공업 주식회사 filed Critical 두산중공업 주식회사
Priority to KR20-2003-0022562U priority Critical patent/KR200328295Y1/en
Application granted granted Critical
Publication of KR200328295Y1 publication Critical patent/KR200328295Y1/en

Abstract

본 고안은 열처리된 단조품의 치수 변형을 교정하는 지그에 있어서, 반구형 단조품의 개방부가 열처리 과정 중에 변형되었을 경우 변형된 개방부를 진원에 가깝도록 치수 교정하는 지그를 제공하는 데 그 목적이 있다.The object of the present invention is to provide a jig for correcting the dimensional deformation of the heat-treated forging product, when the opening of the semi-spherical forging is deformed during the heat treatment process, the jig for dimensional correction of the deformed opening close to the source.

상기와 같은 목적을 달성하기 위한 본 고안은 개방부(3)가 타원형으로 변형된 고압용기의 헤드(1)를 소정의 곡률반경을 갖는 진원의 형태로 교정하기 위한 지그에 있어서, 일측면(100S)이 상기 곡률반경으로 가공되고, 슬롯(103)이 저면(100B)에서 상면(100H)으로 소정의 깊이만큼 상기 곡률반경으로 전면(100F)에서 후면(100R)으로 형성되어 상기 일측면(100S)과 상기 슬롯(103)의 내측면(100I)이 평행하게 구성된 것을 기술적 특징으로 한다.The present invention for achieving the above object in the jig for straightening the head 1 of the high-pressure container in which the opening portion 3 is deformed in an elliptical shape in the form of a circle having a predetermined radius of curvature, one side (100S) ) Is processed into the curvature radius, the slot 103 is formed from the front surface (100F) to the rear surface (100R) with the curvature radius by a predetermined depth from the bottom surface (100B) to the upper surface (100H) And the inner surface 100I of the slot 103 are configured in parallel.

이와 같이 구성된 본 고안의 반구형 단조품의 개방부 치수교정용 지그는 타원형의 개방부를 갖는 헤드를 교정함에 있어서, 블록의 일측면에서 슬롯의 내측면까지의 두께가 다양한 여러 지그를 제작하여 준비해 둠으로써, 교정용 별도의 치구를 제작할 필요없이 헤드를 단조함에 사용된 동일 치수의 치구를 이용하여 변형된 헤드를 교정할 수 있다는 장점이 있다.The opening part dimensional calibration jig of the hemispherical forging of the present invention configured as described above is prepared by preparing various jigs having various thicknesses from one side of the block to the inner side of the slot in calibrating a head having an elliptical opening, There is an advantage that the deformed head can be corrected by using the jig of the same size used to forge the head without having to manufacture a separate jig for calibration.

Description

반구형 단조품의 개방부 치수교정용 지그{Jig for reforming Open Section of Hemisphere}Jig for reforming Open Section of Hemisphere

본 고안은 열처리된 단조품의 치수 변형을 교정하는 지그에 관한 것이며, 특히 반구형 단조품의 개방부가 열처리 과정 중에 변형되었을 경우 변형된 개방부를 진원에 가깝도록 치수 교정하는 지그를 제공하는 데 그 목적이 있다.The present invention relates to a jig for correcting the dimensional deformation of the heat-treated forging, and particularly to provide a jig for dimensional correction of the deformed opening close to the origin when the opening of the hemispherical forging is deformed during the heat treatment process.

일반적으로 고압용기는 관형 쉘의 양단부에 반구형 상하부 헤드가 각각 용접 고정되어 제작된다. 이런 쉘과 상하부 헤드는 단조제작된 단조품이다. 이러한 제품을 단조작업을 통해 제작하기 위해서는 수차례의 열처리작업이 필요하다.In general, the high-pressure container is manufactured by welding the hemispherical upper and lower heads respectively at both ends of the tubular shell. These shells and upper and lower heads are forged parts. Forging these products requires several heat treatments.

한편 반구형의 헤드로 단조된 비완제품을 열처리하게 되면, 진원에 가까워야 할 반구형 헤드의 개방부가 타원형으로 변형된다. 이와 같이 변형된 헤드는 쉘의 단부에 맞대응하지 않기 때문에 용접할 수 없어 폐기하거나 교정작업을 통해 진원에 가깝도록 교정한 후 쉘에 용접 고정한다.On the other hand, when heat treatment of the finished product forged by the hemispherical head, the opening of the hemispherical head to be close to the round shape is deformed into an oval shape. Since the deformed head does not correspond to the end of the shell, it cannot be welded, so it is discarded, or the head is calibrated to be close to the original through the calibration operation, and then welded to the shell.

종래에는 타원형으로 변형된 반구형 헤드를 진원으로 교정하기 위해 완제품의 반경과 동일한 반경을 갖는 반구형의 치구를 이용하여 헤드의 안쪽면을 가압한다.Conventionally, the inner surface of the head is pressed by using a hemispherical jig having a radius equal to the radius of the finished product in order to correct the elliptical deformed hemispherical head in a circle.

이런 치구를 타원형으로 변형된 헤드의 개방부에 삽입하여 가압함에 있어서, 개방부의 단축은 반구형 치구의 직경으로 늘어나 소성변형되지만, 장축은 치구의 직경으로 수축되지 않는다.In inserting and pressing such jig into the opening of the elliptically deformed head, the short axis of the opening extends to the diameter of the hemispherical jig and plastic deformation, but the long axis does not contract to the diameter of the jig.

이는 치구로 가압함에 있어서, 치구와 접하는 헤드 개방부의 두 지점은 변형된 타원의 단축에 위치하며 치구의 가압에 의한 응력이 집중되어 치구의 형상대로 단축은 확장되어 소성변형되지만, 개방부의 장축방향의 두 지점은 자유면 상태로서 응력이 수축하는 방향으로 집중되지 않고 분산되기 때문에 장축방향은 원하는 치수 즉 치구의 치수대로 소성변형되지 않는다.In pressurizing the jig, the two points of the head opening contacting the jig are located at the short axis of the deformed ellipse and the stress of the jig is concentrated so that the short axis is expanded to the shape of the jig and the plastic deformation is performed. Since the two points are free surface states and are dispersed without being concentrated in the direction of stress contraction, the long axis direction does not plastically deform to the desired dimension, that is, the jig.

이와 같은 이유에서 개방부를 진원의 형상을 갖는 헤드로 변형하기 위해서는 설계상의 치수보다 직경이 큰 치구가 필요한다. 하지만, 이런 교정용 치구를 별도로 제작하여 사용하기에는 비용이 많이 소요되며, 또한 다양한 크기의 압력용기를 제작함에 있어서 교정용 치구를 다양하게 보유하고 있어야 한다는 단점이 있다.For this reason, in order to deform the opening into a head having a round shape, a jig having a diameter larger than the design dimension is required. However, it is costly to manufacture and use such orthodontic jig separately, and there is a disadvantage in that various orthodontic jig should be held in manufacturing pressure vessels of various sizes.

본 고안은 앞서 설명한 바와 같은 종래 기술의 문제점을 해결하기 위하여 제안된 것으로서, 개방부가 타원형으로 변형된 헤드를 진원으로 교정하기 위한 지그에 있어서, 타원형의 장축과 단축의 차를 보상하여 진원의 반구형 헤드로 소성변형하는 반구형 단조품의 치수교정용 지그를 제공하는 데 그 목적이 있다.The present invention has been proposed to solve the problems of the prior art as described above, in the jig for correcting the head of the elliptical deformed opening to the round, the hemispherical head of the round by compensating the difference between the long and short axis of the elliptical It is an object of the present invention to provide a jig for dimensional calibration of hemispherical forged products that are plastically deformed in the

도 1은 본 발명의 한 실시예에 따른 반구형 단조품의 치수교정용 지그를 이용하여 열변형된 헤드를 교정하는 과정을 나타낸 개략도이고,1 is a schematic diagram showing a process of calibrating a heat-deformed head using a dimensional calibration jig of a hemispherical forging according to an embodiment of the present invention,

도 2는 도 1에 도시된 반구형 단조품의 치수교정용 지그를 나타낸 사시도이다.Figure 2 is a perspective view showing a jig for dimensional calibration of the hemispherical forging shown in FIG.

* 도면의 주요부분에 대한 부호의 설명 *Explanation of symbols on the main parts of the drawings

1 : 헤드 3 : 개방부1: Head 3: Opening

100 : 지그 100S : 지그의 측면100: jig 100S: side of the jig

100B : 지그의 저면 100H : 지그의 상면100B: bottom of jig 100H: top of jig

100F : 지그의 전면 100R : 지그의 후면100F: front of jig 100R: rear of jig

100I : 지그의 내측면 103 : 슬롯100I: inner side of jig 103: slot

상기와 같은 목적을 달성하기 위한 본 고안은 개방부가 타원형으로 변형된 고압용기의 헤드를 소정의 곡률반경을 갖는 진원의 형태로 교정하기 위한 지그에 있어서, 일측면이 상기 곡률반경으로 가공되고, 슬롯이 저면에서 상면으로 소정의 깊이만큼 상기 곡률반경으로 전면에서 후면으로 형성되어 상기 일측면과 상기 슬롯의 내측면이 평행하게 구성된 것을 기술적 특징으로 한다.The present invention for achieving the above object is a jig for correcting the head of the high-pressure container in which the opening is deformed into an elliptical shape in the form of a circle having a predetermined radius of curvature, one side is processed into the radius of curvature, the slot The lower surface to the upper surface is formed from the front to the rear with the radius of curvature by a predetermined depth, characterized in that the one side and the inner surface of the slot is configured in parallel.

아래에서, 본 고안에 따른 반구형 단조품의 개방부 치수교정용 지그의 양호한 실시예를 첨부한 도면을 참조로 하여 상세히 설명하겠다.In the following, with reference to the accompanying drawings, a preferred embodiment of the opening jig for calibration of the hemispherical forging according to the present invention will be described in detail.

도면에서, 도 1은 본 고안의 한 실시예에 따른 반구형 단조품의 치수교정용 지그를 이용하여 열변형된 헤드를 교정하는 과정을 나타낸 개략도이고, 도 2는 도 1에 도시된 반구형 단조품의 치수교정용 지그를 나타낸 사시도이다.1 is a schematic diagram showing a process of calibrating a heat-deformed head using a dimensional calibration jig of a hemispherical forging according to an embodiment of the present invention, Figure 2 is a dimensional calibration of the hemispherical forging shown in FIG. It is a perspective view which shows the dragon jig.

도 1에 도시된 바와 같이, 열처리되어 개방부가 타원형으로 변형된 헤드(1)는 진원형의 중공이 형성된 받침대(10)에 안착되며, 타원형상을 갖는 개방부(3)에서 단축방향에 위치한 개방부(3)의 두 지점에 지그(100)를 설치한다.As shown in FIG. 1, the head 1, which is heat-treated and the opening is deformed into an elliptical shape, is seated on a pedestal 10 having a circular hollow, and is opened in a uniaxial direction in the opening 3 having an elliptical shape. The jig 100 is installed at two points of the unit 3.

여기에서 지그(100)는 도 2에 도시된 바와 같다. 지그(100)는 직육면체의 블록(101)이 아래와 같이 가공된 형상을 갖는다.The jig 100 is as shown in FIG. 2. The jig 100 has a shape in which a block 101 of a rectangular parallelepiped is processed as follows.

블록(101)의 일측면(100S)은 치구(20)의 곡률반경과 동일하게 가공되며, 슬롯(103)이 상기 블록(101)의 저면(100B)에 형성되는데, 슬롯(103)은 블록(101)의 저면(100B)에서 상면(100H)으로 소정의 깊이만큼 상기 곡률반경으로 블록(101)의 전면(100F)에서 후면(100R)으로 관통하여 형성된다.One side surface 100S of the block 101 is processed in the same manner as the radius of curvature of the jig 20, the slot 103 is formed in the bottom surface 100B of the block 101, the slot 103 is a block ( It is formed by penetrating from the front surface 100F of the block 101 to the rear surface 100R with the curvature radius from the bottom surface 100B of the 101 to the upper surface 100H by a predetermined depth.

따라서, 블록(101)의 일측면(100S)과 슬롯(103)의 내측면(100I)은 진원의 곡률반경과 동일하게 만곡된 형태로 형성되며, 블록(101)의 일측면(100S)과 내측면(100I) 사이의 두께가 헤드(1) 교정치수의 두께가 된다.Accordingly, the one side surface 100S of the block 101 and the inner surface 100I of the slot 103 are formed in the same curved shape as the curvature radius of the round shape, and the one side surface 100S of the block 101 and the inner surface 100I of the slot 101 are formed. The thickness between the side surfaces 100I becomes the thickness of the head 1 calibration dimension.

아래에서는 이와 같이 구성된 블록과 받침대를 이용하여 변형된 헤드를 교정하는 과정에 대해 설명한다.Hereinafter, a process of calibrating the deformed head using the block and the pedestal thus constructed will be described.

진원의 중공이 형성된 받침대(10)에 열변형된 헤드(1)를 안착한다. 이때 개방부(3)가 상부방향을 향하도록 위치하며, 개방부(3)의 단축방향으로 헤드(1)의 2지점에 블록(101)을 설치하는데, 블록(101)의 슬롯(103)에 헤드(1)의 개방부 가장자리를 삽입하여 설치한다.The thermally deformed head 1 is seated on a pedestal 10 having a hollow hollow. In this case, the opening part 3 is positioned to face upward, and the block 101 is installed at two points of the head 1 in the short axis direction of the opening part 3, and is provided in the slot 103 of the block 101. Insert the edge of the opening of the head (1) and install it.

그리고 반구형 치구(20)를 헤드(1)의 개방부(3)에 진입하여 가압한다. 이때, 치구(20)는 가장 먼저 블록(101)의 일측면(100S)과 접하게 되는데, 이때 가압력을점차 낮추면서 가압한다. 이런 과정에서 가압력은 블록(101)을 통해 단축방향은 늘어나고, 이에 대해 상대적으로 장축방향은 수축된다.Then, the hemispherical jig 20 enters and opens the opening 3 of the head 1. At this time, the jig 20 is first in contact with one side (100S) of the block 101, at this time pressurized while gradually lowering the pressing force. In this process, the pressing force is increased in the short axis direction through the block 101, and the long axis direction is contracted relative thereto.

이런 과정에 있어서, 단축을 최대로 늘릴 수 있는 거리는 치구(20)의 반경과 두 블록(101)의 일측면(100S)과 슬롯(103)의 내측면(100I)까지의 두께를 합한 거리이다. 따라서 치구(20)의 반경보다 큰 직경으로 헤드(1)의 개방부를 확장할 수 있으며, 또한 치구(20)가 헤드(1)의 개방부로 진입을 조절하여 헤드(1) 개방부(3)의 장단축의 거리를 조절함으로써 타원형으로 변형된 헤드(1)의 개방부(3)를 진원에 가깝게 교정한다.In this process, the distance to maximize the short axis is the sum of the radius of the jig 20 and the thickness between the one side (100S) of the two blocks 101 and the inner surface (100I) of the slot 103. Therefore, the opening of the head 1 can be expanded to a diameter larger than the radius of the jig 20, and the jig 20 controls the entry into the opening of the head 1 so that the opening of the head 1 opening 3 can be extended. By adjusting the distance of the short and short axis, the opening 3 of the head 1 deformed into an elliptical shape is corrected close to the origin.

앞서 상세히 설명한 바와 같이, 본 고안의 반구형 단조품의 개방부 치수교정용 지그는 타원형의 개방부를 갖는 헤드를 교정함에 있어서, 블록의 일측면에서 슬롯의 내측면까지의 두께가 다양한 여러 지그를 제작하여 준비해 둠으로써, 교정용 별도의 치구를 제작할 필요없이 헤드를 단조함에 사용된 동일 치수의 치구를 이용하여 변형된 헤드를 교정할 수 있다는 장점이 있다.As described in detail above, the opening part dimensional calibration jig of the hemispherical forging according to the present invention is prepared by preparing various jigs having various thicknesses from one side of the block to the inner side of the slot in calibrating the head having an elliptical opening. By doing so, there is an advantage that the deformed head can be corrected by using the jig of the same size used to forge the head without having to manufacture a separate jig for calibration.

이상에서 본 고안의 반구형 단조품의 개방부 치수교정용 지그에 대한 기술사상을 첨부도면과 함께 서술하였지만, 이는 본 고안의 가장 양호한 실시예를 예시적으로 설명한 것이지 본 고안을 한정하는 것은 아니다.The technical idea of the opening jig for dimensional calibration of the hemispherical forging of the present invention has been described with the accompanying drawings, but this is only illustrative of the best embodiment of the present invention and is not intended to limit the present invention.

Claims (1)

개방부(3)가 타원형으로 변형된 고압용기의 헤드(1)를 소정의 곡률반경을 갖는 진원의 형태로 교정하기 위한 지그에 있어서,In the jig for correcting the head (1) of the high-pressure container in which the opening (3) is deformed into an elliptical shape in the form of a circle having a predetermined radius of curvature, 일측면(100S)이 상기 곡률반경으로 가공되고, 슬롯(103)이 저면(100B)에서 상면(100H)으로 소정의 깊이만큼 상기 곡률반경으로 전면(100F)에서 후면(100R)으로 형성되어 상기 일측면(100S)과 상기 슬롯(103)의 내측면(100I)이 평행한 것을 특징으로 하는 반구형 단조품의 개방부 치수교정용 지그.One side (100S) is processed into the curvature radius, the slot 103 is formed from the front surface (100F) to the rear surface (100R) with the curvature radius by a predetermined depth from the bottom surface (100B) to the work An opening part dimensional calibration jig of a semi-spherical forged product, characterized in that the side surface (100S) and the inner surface (100I) of the slot 103 is parallel.
KR20-2003-0022562U 2003-07-12 2003-07-12 Jig for reforming Open Section of Hemisphere KR200328295Y1 (en)