KR20000040244A - Method for bonding an upper plate and a lower plate of a plasma display panel - Google Patents
Method for bonding an upper plate and a lower plate of a plasma display panel Download PDFInfo
- Publication number
- KR20000040244A KR20000040244A KR1019980055823A KR19980055823A KR20000040244A KR 20000040244 A KR20000040244 A KR 20000040244A KR 1019980055823 A KR1019980055823 A KR 1019980055823A KR 19980055823 A KR19980055823 A KR 19980055823A KR 20000040244 A KR20000040244 A KR 20000040244A
- Authority
- KR
- South Korea
- Prior art keywords
- display panel
- plasma display
- plate
- solid bar
- upper plate
- Prior art date
Abstract
Description
본 발명은 플라즈마 디스플레이 패널의 제조에 관한 것으로, 특히 플라즈마 디스플레이 패널 유리의 상하판 합착시 고체 형태의 실링 그래스 바(Sealing Glass Bar)를 이용하여 소성 건조하여 가소성공정을 제거함으로서 소결시 발생하는 가스 및 잔류 응력을 최소화 하도록 한 플라즈마 디스플레이 패널의 제조방법에 관한 것이다.BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to the manufacture of a plasma display panel, and in particular, a gas generated during sintering by removing the plasticity process by firing and drying using a sealing glass bar in a solid form when the upper and lower plates of the glass are bonded together. The present invention relates to a method of manufacturing a plasma display panel to minimize residual stress.
일반적으로 정보를 표시하기 위한 박형의 표시장치로서 플라즈마 디스플레이 패널이 널리 사용되고 있다. 종래의 플라즈마 디스플레이 패널은, 투명한 표시전극이 다수 형성된 표면그래스 기판(상판)과 그 하부에 결합되는 배면 그래스 기판(하판)을 포함하여 이루어진다.In general, a plasma display panel is widely used as a thin display device for displaying information. The conventional plasma display panel includes a surface glass substrate (top plate) having a plurality of transparent display electrodes formed thereon and a back glass substrate (bottom plate) coupled to a lower portion thereof.
종래의 플라즈마 디스플레이 패널의 제조공정중에 있어서, 상판과 하판의 합착방법은, 도 1에 도시된 바와 같이, 그래스 파우더와 유기용제로 이루어진 페이스트 상태의 실링그래스(2)를 디스펜서를 이용하여 상판(2) 또는 하판의 모서리를 따라 두르고, 상판과 하판를 서로 합착하기 전에 각각에 대하여 일정 온도로 가소성하여 실링그래스를 소결하여 딱딱한 고체상태가 되도록 한 후, 상판과 하판를 서로 맞대어 다시 로내에서 소성, 건조하여 합착한다.In the conventional manufacturing process of the plasma display panel, the bonding method of the upper plate and the lower plate, as shown in Figure 1, the sealing plate 2 made of a paste powder made of grass powder and an organic solvent using a dispenser, the upper plate (2) ) Or along the edges of the bottom plate, before firing the top and bottom plates together, plasticize them to a certain temperature and sinter the sealing grass to a hard solid state, and then fire the top and bottom plates together, and then fire and dry them in the furnace again. do.
그런데, 가소성시 페이스트 소멸에 의한 체적의 수축이 심하여 유리에 유해한 잔류 응력을 유발시키고, 페이스트 상태의 실링그래스를 희석시키는 유기 용제가 시간에 따라 증발하므로 점도가 점점 커지므로 공정 조건을 맞추기 힘든 문제점이 있었다.However, when plasticizing, the shrinkage of the volume due to the extinction of the paste is severe, causing harmful residual stress to the glass, and the organic solvent diluting the sealing glass in the paste state evaporates with time, so that the viscosity increases gradually. there was.
한편, 가소성 공정을 거치지 않고서는 상, 하판 합착시 유기 용제가 연소되면서 발생하는 유해 가스가 플라즈마 디스플레이 패널 내부에 잔류하여, 휘도를 떨어뜨리고, 플라즈마 가스의 전기적인 특성을 나쁘게하여 불량의 원인이 되게 한다.On the other hand, without undergoing a plasticity process, harmful gases generated by the combustion of organic solvents during upper and lower plate bonding remain inside the plasma display panel, lowering luminance and deteriorating electrical characteristics of the plasma gas, thereby causing defects. do.
본 발명은 이러한 종래기술의 문제점을 해결하기 위한 것으로, 따라서 미리 소결한 실링 그래스 바(Sealing Glass Bar)를 이용하여 상판과 하판을 합착하므로써 상, 하판에 대한 가소성 공정을 없앨 수 있고, 가소성시 발생하는 가스를 줄여 플라즈마 디스플레이 패널의 휘도를 높이고, 소결시 페이스트의 수축에 의한 잔류 응력을 줄일 수 있는 플라즈마 디스플레이 패널의 상, 하판의 합착방법의 제공을 목적으로 한다.The present invention is to solve the problems of the prior art, and thus, by bonding the upper plate and the lower plate using a pre-sintered sealing glass bar (Sealing Glass Bar), it is possible to eliminate the plasticity process for the upper and lower plates, and occurs during plasticity It is an object of the present invention to provide a method of bonding the upper and lower plates of a plasma display panel to reduce the gas to increase the luminance of the plasma display panel and to reduce residual stress caused by shrinkage of the paste during sintering.
상기 목적을 달성하기 위하여, 본 발명의 플라즈마 디스플레이 패널의 상, 하판의 합착방법은, 그래스파우더와 유기용제로 이루어진 실링 그래스를 가소성시키어, 고체상태의 고체 바(20)를 만들고, 상기 고체 바를, 상판 또는 하판의 어느 하나의 판위의 모서리를 따라 배치하고, 나머지 판을 그 위에 합착시켜 소성, 건조하는 것을 특징으로 한다.In order to achieve the above object, the bonding method of the upper and lower plates of the plasma display panel of the present invention, by plasticizing the sealing glass consisting of a glass powder and an organic solvent, to make a solid bar 20 of a solid state, the solid bar, It is arranged along the edge of any one of the upper plate or the lower plate, and the remaining plate is bonded to it, characterized in that the firing, drying.
도 1 은 페이스트상태의 실링그래스가 도포된 상태의 플라즈마 디스플레이 패널의 상판의 평면도1 is a plan view of an upper plate of a plasma display panel in a state where a paste glass sealing glass is applied;
도 2 는 본 발명에 따른 고체바의 실링그래스가 배치된 상태의 플라즈마 디스플레이 패널의 상판의 평면도2 is a plan view of a top plate of a plasma display panel in a state where a sealing glass of a solid bar according to the present invention is disposed;
도 3 a,b 는 본 발명에 따른 실링 그래스 고체바의 평면도3 a, b is a plan view of a sealing grass solid bar according to the present invention
*** 도면의 주요부분에 대한 부호의 설명 ****** Explanation of symbols for main parts of drawing ***
10 : 상판 20 : 고체바10: top 20: solid bar
21 : 오목단 23 : 볼록단21 concave end 23 convex end
본 발명의 플라즈마 디스플레이 패널의 상, 하판의 합착방법은, 먼저, 그래스파우더와 유기용제로 이루어진 실링 그래스를 가소성시키어, 도 3에 도시된 바와 같이, 고체상태의 일자형 또는 ㄴ자형의 바(20)를 만든다.In the method of bonding the upper and lower plates of the plasma display panel of the present invention, first, the sealing glass made of the glass powder and the organic solvent is plasticized, and as shown in FIG. 3, the solid or straight bar 20 is shown. Make
상기 고체 바(20)를, 도 2에 도시된 바와 같이, 상판(10) 또는 하판의 어느 하나의 판위의 모서리를 따라 배치하고, 나머지 판을 그위에 합착시켜 소성, 건조한다.As shown in FIG. 2, the solid bar 20 is disposed along an edge of one of the upper plates 10 or lower plates, and the remaining plates are bonded and fired and dried.
한편, 일자형 바와, ㄴ자형 바(20)를 소성할 때 한쪽 단부(21)은 오목하게 하고 다른 단부(23)은 볼록하게하여 소성 건조시 실링 그래스간의 응착이 긴밀하도록 하게 한다.On the other hand, when firing the straight bar and the N-shaped bar 20, one end 21 is concave and the other end 23 is convex, so that adhesion between the sealing grasses during plastic drying is tight.
이상, 설명한 바와 같이, 본 발명에 따르면, 미리 가소성된 실링 그래스 바를 사용함으로서 페이스트상태의 실링 글래스의 디스펜싱후의 가소성 공정을 없애 공정 시간을 단축할 수 있으며, 페이스트상태의 실링 그래스보다 정도 관리가 유리하다. 또한 상, 하판 합착시 플라즈마 디스플레이 패널 내부의 잔류 가스의 발생이 없어지며, 미리 수축된 고체 바를 이용하므로서, 페이스트의 소결에 따른 수축에 의한 잔류 응력의 발생을 감소시킬 수 있다.As described above, according to the present invention, by using a plastic sealing bar that has been pre-plasticized, it is possible to shorten the process time by eliminating the plasticizing process after dispensing the sealing glass in the paste state, and the degree of control is better than that of the paste sealing glass. Do. In addition, when the upper and lower plates are bonded together, residual gas inside the plasma display panel is not generated, and since the solid bar that has been previously shrunk is used, the generation of residual stress due to shrinkage due to sintering of the paste can be reduced.
Claims (4)