KR101668392B1 - Multi color decorative letters and method - Google Patents

Multi color decorative letters and method Download PDF

Info

Publication number
KR101668392B1
KR101668392B1 KR1020160075883A KR20160075883A KR101668392B1 KR 101668392 B1 KR101668392 B1 KR 101668392B1 KR 1020160075883 A KR1020160075883 A KR 1020160075883A KR 20160075883 A KR20160075883 A KR 20160075883A KR 101668392 B1 KR101668392 B1 KR 101668392B1
Authority
KR
South Korea
Prior art keywords
letter
decoration
character
syringe
depression
Prior art date
Application number
KR1020160075883A
Other languages
Korean (ko)
Inventor
김홍관
Original Assignee
김홍관
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 김홍관 filed Critical 김홍관
Application granted granted Critical
Publication of KR101668392B1 publication Critical patent/KR101668392B1/en

Abstract

The present invention relates to a multi-color letter decoration and a method for the same. According to the present invention, a colorful decoration differing from a letter or logo is performed on the surface of the metallic letter or logo attached to a bag. The present invention includes: a casting step in which a metallic logo or letter body is produced and a protruding step is caused to protrude to an upper outer side such that a recessed portion is formed on an upper side of the letter body; a step in which the burr and oxide coating of the cast letter body are removed; a step in which a curing paint having a viscosity allowing syringe injection is injected by means of a syringe into the recessed portion of the letter body and then curing is performed for a letter decoration to be formed; a step in which the upper surface of the letter decoration based on the curing paint is ground for the surface of the letter decoration to correspond to the protruding step; a step in which the letter body is plated; and a step in which the surfaces of the letter body and the letter decoration are coated.

Description

{Multi color decorative letters and method}

BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a multicolor character decoration and a method of decorating a color of a character or logo of a metallic material attached to a bag, the character being different from a character or a logo.

In the case of a bag or a handbag, a logo or letter of a manufacturer is made of a metal material, and the logo or trademark is protruded in three dimensions on the surface of the product to ensure high quality. In order to enhance the logo or letter, As shown in FIG. 3 and FIG. 4, after forming a space in which a character ornament is inserted into a character body, a space is formed between the character body and the character body It is made to fix the character decoration with the collar, or to fill the space with the epoxy resin.

That is, as shown in FIGS. 3 and 4, protrusions 11 are protruded on both sides of the letter body 10 made of metal to form a depressed portion 12, The embossed portion 12 is filled with an epoxy resin and is then cured by applying pressure or heat. However, the embossed portion 12, which is prepared in the above-described manner, (20) is fixed between the letter decoration (20) and the depression (12) by using an adhesive (30) such as double-sided tape, the letter decoration (20) There is a problem that the gap between the protruding jaws 11 and the letter decoration 12 is not uniform and thus the quality can not be improved. In addition, a method of filling the recessed portion 12 with epoxy resin, which will be described later, Depending on the characteristics, it is difficult to work, There is a problem that yellowing occurs.

In the method of fixing the character decoration 20 to the depression 12 by fixing the character decoration 20 as described above, it is difficult to attach the character decoration 20 when the width of the character decoration 20 is narrow, Further, there is a problem that the clearance between the character decoration 20 and the protruding jaw 11 is not fixed uniformly while the protruding height of the character decoration 20 is not constantly adhered.

When the epoxy resin is injected into the recessed portion 12 and then cured, the width of the letter body 10 is wide and the width of the recessed portion 12 is not so large. However, Has a narrow width of 0.6 to 2.2 mm, there is a problem that the work can not be performed according to the viscosity of the epoxy resin filled in the depressed portion 12, or the surface is not smooth even when the work is performed.

That is, when the depression 12 formed on the upper surface of the narrow-width body 10 is filled with the epoxy resin, since the width of the depression 12 is narrow, the epoxy resin is injected using a syringe, Which is excellent in chemical resistance, adhesiveness, and corrosion resistance by bonding polyamine and polyamide, but has a characteristic that weather resistance is lowered and yellowing occurs. The pigment and the curing agent are mixed in the epoxy resin, and then the depression (12 ), It is easy to inject into a syringe, but discoloration tends to occur. On the contrary, when the viscosity of the pigment is increased to increase the viscosity, the ink can not be injected into the syringe, Lt; / RTI >

Korean Patent Publication No. 10-1998-0023964 (published July 6, 1998) Korean Patent Publication No. 10-2009-0015325 (Published Feb. 12, 2009) Korean Patent Publication No. 10-2005-0093080 (published on September 23, 2005) Korea Patent Registration No. 10-0921650 (Registered on October 17, 2009) Korean Patent Publication No. 10-2002-0072141 (disclosed on September 14, 2002)

The present invention relates to a method of fixing a logo or letter body made of metal and forming a depressed portion on an upper side of a bag or a bag and fixing the letter ornament having a color different from that of the letter body to the depressed portion, , The upper surface of the letter decoration is not constantly adhered to the protruding jaw formed on the upper part of the letter body, and the gap between the letter decoration and the protruding jaw is not constantly adhered, while the width of the letter body is narrow The problem that the viscosity of the epoxy resin is so high that it is difficult to inject into the depression by inserting it into a syringe is solved and at the same time the upper side of the letter body can not be maintained smoothly.

The present invention relates to a casting process for forming a logo or a letter body on a metal and forming a depression on an upper side of a letter body by protruding a protruding jaw to the outside of the upper side, A step of injecting a curing paint having a viscosity that can be injected by a syringe into a depression of a letter body by a syringe and then curing to form a letter decoration; polishing the upper surface of the letter decoration made of the cured paint to form a surface The process of plating the letter body and the process of coating the surface of the letter body and the letter decoration are performed. Through this manufacturing process, the letter decoration is completed.

The present invention can be effectively used when the width of the letter body is narrow and the width of the depressed portion is narrow, and a hardening paint having a viscosity that can be injected by a syringe is injected into the depressed portion and then hardened.

The present invention relates to a method for forming a character decoration of a color different from a character body on the upper side of a logo or a letter body attached to a bag or a bag by injecting a curing paint having a viscosity that can be injected by a syringe into a depression of a character body Not only the workability is excellent but also the gap between the protruding jaw and the letter decoration is not generated, and the design can be made beautiful by the formation of the narrow and complicated character decoration.

Particularly, in order to solve the problem of difficulty of injecting into a syringe when viscosity is high and easily discoloring when viscosity is low, it is possible to inject with a syringe And the width of the letter body is as small as 0.6 to 2.2 mm, so that even if the width of the depressed portion is narrow, the injection into the syringe is easy, and discoloration or discoloration occurs after curing due to heat or ultraviolet rays It is not made, and there is an effect that the protruding jaw and the gap of the character decoration do not occur together with the fixing firmly.

FIG. 1 is a photograph showing an embodiment of a conventional single-color letter body
FIG. 2 is a view showing a state in which a character decoration is fixed to an existing character body
FIG. 3 is an exploded perspective view of a conventional character body
Fig. 4 is a cross-sectional view of a state in which character decoration is fixed on an existing letter body
Fig. 5 is a perspective view of a character body of the present invention,
6 is a state diagram of injecting a curing paint into a character body depression of the present invention with a syringe
FIG. 7 is a perspective view of a letter body formed with a character decoration according to the present invention,
8 is a flow chart

The present invention forms a character decoration of a different color on the upper side of a logo or a letter body attached to the surface of a bag or a bag. A letter body is formed of a metal material, and a protrusion protrudes from a side surface of the letter body to form a depression After the casting of the letter body is completed, the burr and the oxide film are removed, and a hardening paint having a viscosity that can be injected by a syringe into the depression of the letter body is injected into the syringe and cured to form a letter decoration. Polishing the surface to match the protruding jaw with the surface of the text, plating the text body, and coating the surface of the text body and the text.

In the present invention, the depression formed on the upper side of the character body is filled with a curing paint having a viscosity that can be injected by a syringe, so that the character decoration can be made in various colors, And the surface of the character decoration and the protruding jaw of the character body are polished to be polished to be beautiful, while the character body is plated with the character decoration and the color, and the character decoration of the body of the plated character body is coated Thereby preventing the discoloration of the character decoration.

Unlike the method of adhering letter ornament to a plated letter body with a glue, a curved paint having a viscosity that can be injected by a syringe is filled into a depression of a letter body by a syringe, It can be easily filled with the syringe at the narrowed depression portion to improve the workability and to solve the problem that the interval between the protruding jaw of the character body and the character decoration can not be kept constant, and after the character decoration is formed, The surface of the body is plated, and then the surface is coated after the plating is performed. This is a characteristic feature of the present invention.

DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, the present invention will be described in detail with reference to the accompanying drawings.

The character decoration 20 of the present invention is filled with a curing paint having a viscosity that can be injected by a syringe into a depression 12 formed on the upper side of the character body 10 and is cured by heat or ultraviolet rays. The curing paint constituting the curing paint is filled with the syringe to the depression 12 and is integrally adhered and fixed to the character body 10 at the same time and the character decoration 20 is completed without a gap with the protrusion 11.

The character body 10 of the present invention is provided with a known fixing structure 13 which is fixed to a bag or a bag on the lower side and a depression 12 is formed on the upper side, A curing paint having a viscosity capable of being injected into a syringe is formed so as to be filled into a syringe and then injected into a depression 12. The cured paint is filled in accordance with the height of the protrusion 11, Since the liquid curing paint is used, the character decoration 20 is formed so that a gap with the protruding protrusion 11 is not generated.

The character decoration 20 of the present invention can be expressed in any color by hardening a curing paint having a viscosity that can be injected by a syringe. Even if the width of the character decoration 20 is narrow to 0.6 to 2.2 mm, It is possible to express the narrow and thin letter decoration 20, which enables the expression of various designs, in particular, the expression of a desired color.

The character body 10 of the present invention has a narrow width of 0.6 to 2.2 mm and the depressed portion 12 is formed on the upper surface of the character body 10, Therefore, when the cured paint is filled in the depression grooves 12, it can not be directly filled, and it is inevitable to fill the cured paint with a syringe. Therefore, in the present invention, since the cured paint having a viscosity that can be injected by a syringe is used, The concave portion 12 can be easily filled with the narrow width.

The present invention is characterized in that a casting process is performed in which the logo or letter body 10 is made of metal and the protruding jaws 11 are protruded outside the upper part to form a depression 12 on the upper side of the letter body 10, A process of removing the burr and the oxide film generated in the casting process of the body 10 is carried out and a curing paint having a viscosity that can be injected into the syringe is filled into the depression 12 of the character body 10 with a syringe The surface of the letter decoration 20 formed by curing the hardening paint and the upper surface of the letter body 10 are polished to form a protrusion 11 and a letter decoration 20 and the surface of the text body 10 is coated with the surface of the text body 10 after the plating process is performed on the text body 10, do.

The present invention is characterized in that the letter body 10 is made by casting metal and has a fixing structure 13 on the lower side and a protrusion 11 on the upper side to form a depression 12, The burr and the oxide film of the character body 10 are removed and the depression 12 formed on the upper surface of the textured body 10 is filled with a hardener by a syringe And is then cured by ultraviolet rays to form a character decoration 20 made of a curing paint having a viscosity capable of being injected into the upper side of the character body 10 by a syringe.

The letter body 10 according to the present invention has a narrow width so that the width of the recessed portion 12 must be narrow and it is difficult to fill the recessed recess 12 with resin. (12) can be filled with a curing paint using a syringe.

In the present invention, since the cured paint can be filled in the recessed groove 12 by filling the hardened paint in the syringe, the hardened paint can be easily filled into the narrow and long depression grooves 12, and coloration is not made after curing due to the nature of the hardened paint.

Here, the curing paint having a viscosity that can be injected by a syringe may be made of various colors, and a color that matches with the plating color of the character body 10 and has the best color contrast effect is selected.

When the character decoration 20 is formed on the upper side of the character body 10 according to the present invention, the upper side of the protrusion 11 and the upper side of the character decoration 20 are polished by a polishing process, The height of the surface 20 can be matched to make it possible to express a beautiful surface.

That is, the protruding jaw 11 of the character body 10 is made to coincide with the height of the character decoration 20, and the surface is smoothly polished. Thus, the character decoration is fixed to the depression by using an adhesive or the like In this case, there is a gap between the protruding jaw and the letter decoration, and at the same time, since the size of the clearance differs depending on the position, the problem of not being seen as a sophisticated and high-quality character decoration is solved.

The present invention relates to a method for plating a character body (10) after a surface of a character decoration (20) is made to correspond to a height of a protrusion (11) of a character body (10) and polished to have a smooth surface, The metal body 10 of the metal is plated and the text decoration 20 made of the cured paint is not plated.

When the text body 10 having the text decoration 20 is formed, the text decoration 20 maintains its original color and texture while the text body 10 is plated with a desired texture and color A character body 10 of various textures and a character decoration 20 can be expressed, thereby providing a high-level representation of logos or letters.

After the plating of the text body 10 is completed, a surface coating process is performed to prevent corrosion of the plated text body 10, while preventing discoloration of the text decoration 20 and enhancing the adhesive force .

As described above, since the letter decoration 20 is formed by filling the depression 12 of the letter decoration 20 with a curing paint having a viscosity that can be injected by a syringe, the protrusion 11 of the letter body 10 It is possible to express the natural boundary that the letter decoration (20) is integrated, and it is possible to express the decoration of narrow letters by providing the advantage of having a constant height and surface due to the surface polishing and expressing narrow character. You can.

10: letter body 11: protruding jaw
12: depression 20: letter decoration

Claims (2)

The letter body 10, which is attached to the surface of the bag and has a narrow width of 0.6 to 2.2 mm, protrudes outwardly from the upper side to form a depression 12 on the upper side of the character body 10 A casting process for forming the fixing structure 13 on the lower side is performed,
A process of removing burrs and an oxide film generated in the casting process of the character body 10 is performed,
A step of filling a curing paint having a viscosity that can be injected by a syringe into a depression 12 of a letter body 10 from which burrs and an oxide film are removed is filled with a syringe and then cured to form a letter decoration 20,
The surface of the character decoration 20 and the top surface of the character body 10 are polished to align the protrusion 11 and the surface of the character decoration 20,
A process of plating the character body 10 is performed,
And coating the surface of the text body (10) and the surface of the text decoration (20) after the plating process.
The letter body 10, which is attached to the surface of the bag and has a narrow width of 0.6 to 2.2 mm, protrudes outwardly from the upper side to form a depression 12 on the upper side of the character body 10 On the other hand, the fixing structure 13 is formed on the lower side,
After the burr and the oxide film which are generated in the casting process of the character body 10 are removed, a curved paint having a viscosity that can be injected into the syringe is filled into the depression 12 of the character body 10 with a syringe and cured, The decoration 20 is formed,
The surface of the character decoration 20 and the upper surface of the character body 10 are polished so that the height of the protrusions 11 and the surface of the character decoration 20 are matched,
The character body 10 is plated and then the surface of the character body 10 and the character decoration 20 are coated after the projecting jaws 11 of the character body 10 and the surface of the character decoration 20 are polished Multicolor letters decorated with.
KR1020160075883A 2016-02-29 2016-06-17 Multi color decorative letters and method KR101668392B1 (en)