KR101368977B1 - Squeeze ring preventing stationary fit between lamina members from separation and, blanking unit having the same - Google Patents

Squeeze ring preventing stationary fit between lamina members from separation and, blanking unit having the same Download PDF

Info

Publication number
KR101368977B1
KR101368977B1 KR1020120046826A KR20120046826A KR101368977B1 KR 101368977 B1 KR101368977 B1 KR 101368977B1 KR 1020120046826 A KR1020120046826 A KR 1020120046826A KR 20120046826 A KR20120046826 A KR 20120046826A KR 101368977 B1 KR101368977 B1 KR 101368977B1
Authority
KR
South Korea
Prior art keywords
squeeze ring
lamina
lamina member
laminated core
inner diameter
Prior art date
Application number
KR1020120046826A
Other languages
Korean (ko)
Other versions
KR20130123587A (en
Inventor
최창일
지정규
강석조
Original Assignee
주식회사 포스코티엠씨
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 주식회사 포스코티엠씨 filed Critical 주식회사 포스코티엠씨
Priority to KR1020120046826A priority Critical patent/KR101368977B1/en
Publication of KR20130123587A publication Critical patent/KR20130123587A/en
Application granted granted Critical
Publication of KR101368977B1 publication Critical patent/KR101368977B1/en

Abstract

본 발명에 따르면, 스퀴즈 링의 내부에서 라미나 부재가 억지끼움으로 서로 결합되어 만들어진 적층코아가 스퀴즈 링의 하단으로부터 배출될 때 상기 억지끼움 결합이 분리되어 라미나 부재가 서로 분리되는 것을 방지할 수 있다는 효과를 가진다. According to the present invention, when the laminated cores made by combining the lamina members with each other in the squeeze ring are discharged from the lower end of the squeeze ring, the interference fit bond is separated to prevent the lamina members from being separated from each other. Has the effect.

Description

라미나 부재 사이의 억지끼움 결합이 분리되는 것을 방지하는 스퀴즈 링 및, 이를 구비하는 블랭킹 유니트{Squeeze ring preventing stationary fit between lamina members from separation and, blanking unit having the same}Squeeze ring preventing stationary fit between lamina members from separation and, blanking unit having the same}

본 발명은 스퀴즈 링에 관한 것으로서, 더욱 구체적으로는 스퀴즈 링의 내부에서 라미나 부재가 억지끼움으로 적층되어 만들어진 적층코아가 스퀴즈 링의 하단에서 배출될 때 라미나 부재 사이의 결합이 분리되는 것을 방지할 수 있는 스퀴즈 링에 관한 것이다. 또한, 본 발명은 이러한 스퀴즈 링을 구비하는 블랭킹 유니트에 대한 것이기도 하다. The present invention relates to a squeeze ring, and more particularly, to prevent the bond between the lamina members from being separated when the laminated core made by laminating the lamina members inside the squeeze ring is discharged from the bottom of the squeeze ring. It is about squeeze ring to be able to do. The invention also relates to a blanking unit having such a squeeze ring.

일반적으로, 라미나 부재를 적층하여 제조되는 적층 코아는 발전기나 모터의 회전자 및 고정자로 사용되며, 이를 제조하는 방법은 당업계에 잘 알려져 있다. In general, laminated cores produced by laminating lamina members are used as rotors and stators of generators or motors, and methods for making them are well known in the art.

도 1에는 라미나 부재(105)가 적층되어 완성된 적층 코아(100)가 도시되어 있다. 원형인 라미나 부재(105)의 중심에는 샤프트 홀(101)이 형성되고, 샤프트 홀(101)의 외곽으로는 라미나 부재(105)의 외주(外周)측에 방사상으로 다수의 슬롯(102)이 형성된다. 1 shows a laminated core 100 completed by laminating a lamina member 105. A shaft hole 101 is formed at the center of the circular lamina member 105, and a plurality of slots 102 are radially disposed on the outer circumferential side of the lamina member 105 at the outside of the shaft hole 101. Is formed.

샤프트 홀(101)을 중심으로 그 외측에는 복수의 인터록 탭(103)이 형성된다. 도 2에 나타난 바와 같이, 인터록 탭(103)은 아래로 엠보싱된 오목부로서, 라미나 부재(105)가 적층될 때 상부 라미나 부재(105)의 인터록 탭(103)이 바로 아래의 라미나 부재(105)에 형성된 인터록 탭(103)과 끼워맞춤 결합되어 적층 코아(100)가 형성되도록 한다. A plurality of interlock tabs 103 are formed on the outer side of the shaft hole 101. As shown in FIG. 2, the interlock tab 103 is a recess embossed down, where the interlock tab 103 of the upper lamina member 105 is directly below the lamina when the lamina member 105 is laminated. The interlock tab 103 formed in the member 105 is fitted and coupled to form the laminated core 100.

상기 적층 코아(100)는 적층 코아 제조 장치에 의하여 제조되는데, 대한민국 특허등록 제10-0578043호, 대한민국 특허등록 제10-0762744호, 대한민국 특허등록 제10-1089903호 등에 제조장치와 제조방법이 개시되어 있다. The laminated core 100 is manufactured by a laminated core manufacturing apparatus, and a manufacturing apparatus and a manufacturing method are disclosed in Korean Patent Registration No. 10-0578043, Korean Patent Registration No. 10-0762744, and Korean Patent Registration No. 10-1089903. It is.

적층 코아 제조 장치는 슬롯(102)을 형성하는 슬롯 형성부, 카운터 홀(106)을 형성하는 카운터홀 형성부, 샤프트 홀(101)을 형성하는 샤프트홀 형성부, 인터록 탭(103)을 형성하는 인터록 탭 형성부 및, 금속 스트립을 블랭킹하여 라미나 부재(105)를 형성하고 라미나 부재(105)를 스퀴즈 링의 내부에서 억지끼움으로 서로 결합시키는 블랭킹 유니트를 구비한다. The laminated core manufacturing apparatus forms a slot forming portion forming the slot 102, a counter hole forming portion forming the counter hole 106, a shaft hole forming portion forming the shaft hole 101, and an interlock tab 103. And an interlock tab forming portion, and a blanking unit for blanking the metal strip to form the lamina member 105 and forcing the lamina member 105 to be bonded to each other in the interior of the squeeze ring.

상기 슬롯 형성부, 카운터홀 형성부, 샤프트홀 형성부, 인터록 탭 형성부, 블랭킹 유니트는 상기 특허등록 공보에 그 구성 및 작동과정이 기재되어 있는데, 아래에서는 본 발명과 직접적으로 관련되는 부분인 블랭킹 유니트만을 설명하기로 한다.The slot forming portion, the counter hole forming portion, the shaft hole forming portion, the interlock tab forming portion, and the blanking unit are described in the patent registration publications, and their construction and operation processes are described below. Only the unit will be described.

상기 블랭킹 유니트는, 도 3에 나타난 바와 같이, 상부 다이(도면에 미도시)에 장착된 블랭크 블록과 협력하여 라미나 부재(105)를 블랭킹하여 만들고, 블랭킹된 라미나 부재(105)를 스퀴즈 링(120)의 내부에서 적층한다.The blanking unit is made by blanking the lamina member 105 in cooperation with a blank block mounted to an upper die (not shown in the figure), as shown in FIG. 3, and squeeze the blanked lamina member 105 into a squeeze ring. Laminate inside of 120.

상기 블랭킹 유니트는 로테이션 다이(130)와, 로테이션 다이(130)의 상단에 설치된 블랭크 다이(140)와, 블랭크 다이(140)의 아래에 설치된 스퀴즈 링(120)과, 로테이션 다이(130)를 선택적으로 회전시키기 위한 회전수단(150) 및, 로테이션 다이(130)를 지지하는 고정부쉬(135)를 구비한다. 상기 구성요소 중에서 회전수단(150)은 선택적인 구성 요소로서, 스트레이트 적층을 하는 경우에는 작동하지 않는다.The blanking unit may include a rotation die 130, a blank die 140 installed on the top of the rotation die 130, a squeeze ring 120 installed below the blank die 140, and a rotation die 130. Rotation means 150 and a fixing bush 135 for supporting the rotation die 130 to rotate. Among the components, the rotation means 150 is an optional component and does not work when the straight lamination is performed.

상기 블랭크 블록은 블랭크 다이(140)에 삽입되면서 금속 스트립을 블랭킹하여 라미나 부재(105)를 만들고, 블랭킹된 라미나 부재(105)는 스퀴즈 링(120)의 내부공간(122)에 밀려 들어가는데, 상기 내부공간(122)에 먼저 블랭킹되어 있던 라미나 부재(105)와 새롭게 블랭킹된 라미나 부재(105)는 억지끼움으로 서로 결합된다. 즉, 상부 라미나 부재(105)의 인터록 탭(103)의 하면 볼록부가 하부 라미나 부재(105)의 인터록 탭(103)의 상면 오목부 내에 삽입되어 억지 끼워맞춤 결합되기 때문에 라미나 부재(105)들이 서로 적층될 수 있다. 소정 매수 예컨대, 20장의 라미나 부재(105)가 동일한 과정에 의해 적층된 뒤에, 상기 카운터 공정에서 인터록 탭(103) 대신에 카운터 홀(106)이 형성된 라미나 부재(105)가 블랭킹 되어 그 위에 적층되면, 상기 라미나 부재(105)에는 인터록 탭(103)이 없으므로 라미나 부재(105)는 더 이상 적층되지 않고 분리되게 된다. 이렇게 분리된 적층 코아(100)는 아래쪽의 배출구를 통해 배출된다.The blank block is inserted into the blank die 140 while blanking a metal strip to form a lamina member 105, and the blanked lamina member 105 is pushed into the inner space 122 of the squeeze ring 120. The lamina member 105 blanked in the inner space 122 and the newly blanked lamina member 105 are coupled to each other by interference fit. That is, since the convex portion of the lower surface of the interlock tab 103 of the upper lamina member 105 is inserted into the upper concave portion of the interlock tab 103 of the lower lamina member 105, the lamina member 105 ) May be stacked on each other. After a predetermined number of sheets, for example, 20 lamina members 105 are laminated by the same process, the lamina member 105 having the counter hole 106 formed in place of the interlock tab 103 in the counter process is blanked and placed thereon. When laminated, the lamina member 105 does not have an interlock tab 103 so that the lamina member 105 is no longer laminated and is separated. The stacked cores 100 separated in this way are discharged through the lower discharge port.

한편, 도 4a는 스퀴즈 링(120)의 평면도이고 도 4b는 스퀴즈 링(120)의 종단면도이다. 상기 스퀴즈 링(120)의 내경(D2)은 라미나 부재(105)의 직경(D1)보다 약간 작다. 이것은 스퀴즈 링(120)이 라미나 부재(105)에 측압을 가함으로써 라미나 부재(105)가 스퀴즈 링(120)의 내부에서 억지끼움으로 서로 결합될 수 있도록 하기 위해서이다.4A is a top view of the squeeze ring 120 and FIG. 4B is a longitudinal cross-sectional view of the squeeze ring 120. The inner diameter D2 of the squeeze ring 120 is slightly smaller than the diameter D1 of the lamina member 105. This is for the squeeze ring 120 to apply a lateral pressure to the lamina member 105 so that the lamina members 105 can be coupled to each other by interference fit inside the squeeze ring 120.

그런데, 적층코아(100)가 스퀴즈 링(120)의 하단에서 배출될 때, 스퀴즈 링(120)의 측압이 갑자기 없어지기 때문에 라미나 부재(105) 사이의 결합이 분리되는 문제점이 생기기도 한다. 라미나 부재(105) 사이의 결합이 분리된 적층코아(100)는 정상적인 물성을 갖지 못한다.By the way, when the laminated core 100 is discharged from the lower end of the squeeze ring 120, the side pressure of the squeeze ring 120 suddenly disappears, there is also a problem that the bond between the lamina member 105 is separated. The laminated core 100 in which the bond between the lamina members 105 is separated does not have normal physical properties.

도 5a는 라미나 부재(105a) 사이의 결합이 유지되고 있는 정상적인 품질의 적층코아(100a)를 보여주는 있음에 비해, 도 5b는 라미나 부재(105a) 사이의 결합이 분리된 적층코아(100b)를 보여준다. 5a shows the laminated core 100a of normal quality in which the bond between the lamina members 105a is maintained, while FIG. 5b shows the laminated core 100b in which the bond between the lamina members 105a is separated. Shows.

본 발명은 상기 문제점들을 해결하기 위해 고안된 것으로서, 스퀴즈 링의 내부에서 라미나 부재가 억지끼움으로 적층되어 만들어진 적층코아가 스퀴즈 링의 하단에서 배출될 때 라미나 부재 사이의 결합이 분리되는 것을 방지할 수 있는 스퀴즈 링 및, 이러한 스퀴즈 링을 구비하는 블랭킹 유니트를 제공하는 것에 그 목적이 있다.The present invention has been devised to solve the above problems, it is possible to prevent the bond between the lamina member is separated when the lamination core made by laminating the lamina member in the squeeze ring is ejected from the bottom of the squeeze ring It is an object of the present invention to provide a squeeze ring that can be used and a blanking unit having such a squeeze ring.

본 발명의 또 다른 목적은 적층코아가 스퀴즈 링의 하단에서 배출될 때 스퀴즈 링이 적층코아에 작용하는 측압을 서서히 감소시키는 스퀴즈 링 및, 이러한 스퀴즈 링을 구비하는 블랭킹 유니트를 제공하는 것에 있다.It is still another object of the present invention to provide a squeeze ring which gradually reduces the side pressure acting on the laminated core when the laminated core is discharged from the lower end of the squeeze ring, and a blanking unit having such a squeeze ring.

본 발명은 스퀴즈 링이 적층코아에 가하는 측압을 스퀴즈 링의 하단 부근에서 서서히 감소시킴으로써 적층코아를 이루는 라미나 부재 사이의 결합이 분리되는 것을 방지하는 것에 그 특징이 있다. 이를 위해서 본 발명에 따른 스퀴즈 링은 그 내부공간의 하부에 경사면 및/또는 계단턱이 형성되고, 이에 따라 스퀴즈 링의 하부에서는 아래로 내려갈수록 내부 직경이 커진다. The present invention is characterized in that the side pressure applied by the squeeze ring to the laminated core is gradually reduced near the lower end of the squeeze ring to prevent the bond between the lamina members forming the laminated core from being separated. To this end, the squeeze ring according to the present invention has an inclined surface and / or a stepped step formed in the lower portion of the inner space, and as a result, the inner diameter of the squeeze ring is lowered downward.

본 발명에 따른 스퀴즈 링은 스트레이트 적층, 라미나 부재를 소정 매수 적층할 때마다 로테이션 다이를 소정 각도로 회전시키는 인텍스 적층, 스큐 적층에 모두 사용될 수 있다. The squeeze ring according to the present invention can be used for both straight lamination, index lamination and skew lamination which rotates the rotation die at a predetermined angle every time a lamina member is laminated.

상기 목적들을 달성하기 위해, 본 발명의 바람직한 실시예에 따른 스퀴즈 링은 내부공간(210)의 내경(ID)이 하단(220)으로 갈수록 커진다. In order to achieve the above objects, the squeeze ring according to the preferred embodiment of the present invention becomes larger as the inner diameter (ID) of the inner space 210 toward the lower end (220).

금속 스트립이 블랭킹되어 만들어진 라미나 부재가 스퀴즈 링의 내부공간(210)에 삽입되어 상부 라미나 부재와 하부 라미나 부재가 억지끼움으로 서로 결합되어 적층코아를 이룬다. 상기 내부공간(210)의 내경(ID)은 라미나 부재의 직경(D1) 보다 약간 작다. The lamina member formed by blanking the metal strip is inserted into the inner space 210 of the squeeze ring so that the upper lamina member and the lower lamina member are joined to each other by interference fit to form a laminated core. The inner diameter ID of the inner space 210 is slightly smaller than the diameter D1 of the lamina member.

상기 하단(220)에는 바깥쪽을 향한 경사면(221)이 형성될 수 있다.An inclined surface 221 facing outward may be formed at the lower end 220.

상기 경사면(221)의 상측에는 적어도 하나의 계단턱(230)(232)이 형성될 수 있고, 이에 따라 계단턱(230)(232)의 위쪽의 내경(ID)보다 아래쪽의 내경(ID)이 커진다.At least one staircase 230 and 232 may be formed above the inclined surface 221, and thus, an inner diameter ID of the lower side of the inclined surface 221 may be lower than an inner diameter ID of the upper side of the staircase 230 and 232. Gets bigger

아울러, 상기 경사면(221)과는 별도로, 내부공간(210)의 하부에는 적어도 하나의 계단턱(230)(232)이 형성될 수 있다. 이 경우, 계단턱(230)(232)의 위쪽의 내경(ID)보다 아래쪽의 내경(ID)이 크다. In addition, apart from the inclined surface 221, at least one staircase 230 and 232 may be formed at a lower portion of the internal space 210. In this case, the inner diameter ID of the lower side is larger than the inner diameter ID of the upper side of the stepped 230 and 232.

본 발명의 다른 측면인 블랭킹 유니트는, 금속 스트립을 블랭킹하여 라미나 부재를 만들기 위한 블랭크 다이; 및 블랭크 다이의 아래에 설치되고, 블랭킹된 라미나 부재가 억지끼움으로 서로 결합되는, 상기 스퀴즈 링;을 구비한다. Another aspect of the present invention is a blanking unit, comprising: a blank die for blanking a metal strip to make a lamina member; And the squeeze ring installed under the blank die, and the blanked lamina members are joined to each other by interference fit.

본 발명에 따른 스퀴즈 링 및, 이러한 스퀴즈 링을 구비하는 블랭킹 유니트는 다음과 같은 효과를 가진다.The squeeze ring and the blanking unit provided with such a squeeze ring according to the present invention have the following effects.

첫째, 스퀴즈 링의 내부에서 라미나 부재가 억지끼움으로 적층되어 만들어진 적층코아가 스퀴즈 링의 하단에서 배출될 때 라미나 부재 사이의 결합이 분리되는 것을 방지할 수 있다.First, it is possible to prevent the bond between the lamina members from being separated when the laminated core made by laminating the lamina members by interference fit inside the squeeze ring is discharged from the lower end of the squeeze ring.

둘째, 적층코아가 스퀴즈 링의 하단에서 배출될 때 스퀴즈 링이 적층코아에 작용하는 측압을 서서히 감소시킬 수 있다. Second, when the laminated core is discharged from the bottom of the squeeze ring, the squeeze ring can gradually reduce the side pressure acting on the laminated core.

도 1은 일반적인 적층 코아를 보여주는 사시도이다.
도 2는 도 1의 II-II'선에 따른 단면도이다.
도 3은 종래 기술에 따른 적층 코아 제조 장치의 블랭킹 유니트를 개략적으로 나타낸 종단면도이다.
도 4a는 도 3의 블랭킹 유니트에 구비된 스퀴즈 링을 보여주는 평면도이다.
도 4b는 도 3의 블랭킹 유니트에 구비된 스퀴즈 링을 보여주는 종단면도이다.
도 5a는 종래 기술에 따른 적층 코아 제조 장치를 이용해서 만들어진 적층코아를 보여주는 사시도로서, 라미나 부재 사이의 결합이 정상적으로 유지되고 있는 적층코아를 보여주는 도면이다.
도 5b는 종래 기술에 따른 적층 코아 제조 장치를 이용해서 만들어진 적층코아를 보여주는 사시도로서, 라미나 부재 사이의 결합이 분리된 적층코아를 보여주는 도면이다.
도 6은 본 발명의 바람직한 실시예에 따른 스퀴즈 링을 보여주는 종단면도이다.
도 7은 도 6의 스퀴즈 링을 보여주는 평면도이다.
도 8은 도 6의 A 부분의 확대도이다.
1 is a perspective view showing a general laminated core.
FIG. 2 is a cross-sectional view taken along the line II-II 'of FIG. 1.
Figure 3 is a longitudinal sectional view schematically showing a blanking unit of the laminated core manufacturing apparatus according to the prior art.
4A is a plan view illustrating a squeeze ring provided in the blanking unit of FIG. 3.
4B is a longitudinal cross-sectional view illustrating a squeeze ring provided in the blanking unit of FIG. 3.
Figure 5a is a perspective view showing a laminated core made using a laminated core manufacturing apparatus according to the prior art, it is a view showing a laminated core in which the bonding between the lamina member is normally maintained.
Figure 5b is a perspective view showing a laminated core made using a laminated core manufacturing apparatus according to the prior art, it is a view showing a laminated core separated bond between the lamina member.
6 is a longitudinal sectional view showing a squeeze ring according to a preferred embodiment of the present invention.
7 is a plan view illustrating the squeeze ring of FIG. 6.
FIG. 8 is an enlarged view of a portion A of FIG. 6.

이하, 첨부된 도면들을 참조로 본 발명에 대해서 상세히 설명하기로 한다. 이에 앞서, 본 명세서 및 청구범위에 사용된 용어나 단어는 통상적이거나 사전적인 의미로 한정해서 해석되어서는 아니되며, 발명자는 그 자신의 발명을 가장 최선의 방법으로 설명하기 위해 용어의 개념을 적절하게 정의할 수 있다는 원칙에 입각하여 본 발명의 기술적 사상에 부합하는 의미와 개념으로 해석되어야만 한다. 따라서, 본 명세서에 기재된 실시예와 도면에 도시된 구성은 본 발명의 실시예들에 불과할 뿐이고 본 발명의 기술적 사상을 모두 대변하는 것은 아니므로, 본 출원시점에 있어서 이들을 대체할 수 있는 다양한 균등물과 변형예들이 있을 수 있음을 이해하여야 한다.
Hereinafter, the present invention will be described in detail with reference to the accompanying drawings. Prior to this, terms and words used in the present specification and claims should not be construed as limited to ordinary or dictionary terms, and the inventor should appropriately interpret the concepts of the terms appropriately It should be interpreted in accordance with the meaning and concept consistent with the technical idea of the present invention based on the principle that it can be defined. Therefore, the embodiments described in the present specification and the configurations shown in the drawings are merely examples of the present invention and are not intended to represent all of the technical ideas of the present invention, so that various equivalents And variations are possible.

본 발명은 적층코아 제조장치의 블랭킹 유니트에 구비되는 스퀴즈 링에 대한 것이다. 상기 적층코아 제조장치와 블랭킹 유니트에 대한 내용은 대한민국 특허등록 제10-0578043호, 대한민국 특허등록 제10-0762744호, 대한민국 특허등록 제10-1089903호 등에 개시되어 있는데, 상기 등록공보에 기재된 내용은 본 명세서에 포함된다. 따라서, 상기 스퀴즈 링과 블랭킹 유니트의 일반적인 구조 및 작동은 상기 등록공보에 기재된 내용을 참조하여 이해하여야 한다.
The present invention relates to a squeeze ring provided in the blanking unit of the laminated core manufacturing apparatus. The stacked core manufacturing apparatus and the blanking unit are disclosed in Korean Patent Registration No. 10-0578043, Korean Patent Registration No. 10-0762744, and Korean Patent Registration No. 10-1089903. Included herein. Therefore, the general structure and operation of the squeeze ring and blanking unit should be understood with reference to the contents described in the above-mentioned registration publication.

도 6은 본 발명의 바람직한 실시예에 따른 스퀴즈 링을 보여주는 종단면도이고, 도 7은 상기 스퀴즈 링을 보여주는 평면도이며, 도 8은 도 6의 A 부분의 확대도이다.6 is a longitudinal cross-sectional view showing a squeeze ring according to a preferred embodiment of the present invention, Figure 7 is a plan view showing the squeeze ring, Figure 8 is an enlarged view of a portion A of FIG.

본 발명에 따른 스퀴즈 링(200)은 로테이션 다이(130)의 내부에 설치되되, 블랭킹 다이(140)의 아래에 설치되는 것으로서, 스퀴즈 링(도 3, 4a, 4b의 120)의 설치 위치와 동일한 위치에 설치된다. The squeeze ring 200 according to the present invention is installed inside the rotation die 130, but is installed below the blanking die 140, the same as the installation position of the squeeze ring (120 in Figs. 3, 4a, 4b) Is installed in position.

한편, 당업자에게 알려진 바와 같이, 상기 로테이션 다이(130)는 라미나 부재를 인덱스 적층하거나 스큐 적층하는 경우에는 회전 수단(150)에 의해 선택적으로 회전될 수 있는데, 로테이션 다이(130)가 회전됨에 따라 스퀴즈 링(200)도 회전하게 된다. 한편, 고정부쉬(135)는 베어링을 통해서 로테이션 다이(130)를 회전 가능하게 지지한다. 이러한 블랭크 다이(140), 스퀴즈 링(200), 로테이션 다이(130), 회전 수단(150) 및, 고정부쉬(135)는 본 발명에 따른 블랭킹 유니트를 구성하는 요소인데, 상기 구성 요소 중에서 블랭크 다이(140), 로테이션 다이(130), 회전 수단(150) 및, 고정부쉬(135)는 '발명의 배경이 되는 기술'에서 설명된 바 있다. On the other hand, as known to those skilled in the art, the rotation die 130 may be selectively rotated by the rotation means 150 in the case of index lamination or skew lamination of the lamina member, as the rotation die 130 is rotated The squeeze ring 200 is also rotated. On the other hand, the fixed bush 135 rotatably supports the rotation die 130 through a bearing. The blank die 140, the squeeze ring 200, the rotation die 130, the rotation means 150, and the fixing bush 135 is a component constituting the blanking unit according to the present invention, the blank die of the components 140, the rotation die 130, the rotation means 150, and the fixing bush 135 has been described in the description 'background to the invention'.

스퀴즈 링(200)은 그 내부에 내부공간(210)이 형성된 통 형상을 가지는데, 상기 내부공간(210)의 상단과 하단이 개방되어 있다. 이에 따라, 상기 개방된 상단을 통해 블랭킹된 라미나 부재(105)가 밀려 들어오고 상기 개방된 하단을 통해 적층코아(100)가 배출된다.The squeeze ring 200 has a cylindrical shape in which an inner space 210 is formed, and the upper and lower ends of the inner space 210 are open. Accordingly, the lamina member 105 blanked through the open top is pushed in and the stacked core 100 is discharged through the open bottom.

스퀴즈 링(200)은 만들고자 하는 라미나 부재(105)의 형상과 상응하는 단면형상을 가질 수 있다. 예를 들어, 라미나 부재(105)가 원형인 경우에는 스퀴즈 링(200)도 원형의 단면형상을 가진다. Squeeze ring 200 may have a cross-sectional shape corresponding to the shape of the lamina member 105 to be made. For example, when the lamina member 105 is circular, the squeeze ring 200 also has a circular cross-sectional shape.

또한, 스퀴즈 링(200)의 내경(ID)은 라미나 부재(105)의 직경보다 약간 작다. 이에 따라, 스퀴즈 링(200)이 내부공간(210)에 삽입되어 있는 라미나 부재(105)에 측압을 가하게 되어, 블랭킹된 라미나 부재(105)가 스퀴즈 링(200)에 삽입되면 하부 라미나 부재(105)의 인터록 탭(103)과 억지끼움 결합될 수 있다. 라미나 부재(105)의 적층이 반복되다가 카운터 홀(106)이 형성된 라미나 부재(105)가 블랭킹되어 스퀴즈 링(200)에 삽입되면, 카운터 홀(106)이 형성된 라미나 부재(105)는 인터록 탭(103)이 없기 때문에 하부 라미나 부재(105)와의 결합이 이루어지지 않게 되고, 이에 따라 적층코아(100)의 적층이 완료된다. 적층이 완료된 적층코아(100)는 스퀴즈 링(200)의 하단(220)을 통해 밖으로 배출되고, 카운터 홀(106)이 형성된 라미나 부재(105)에는 라미나 부재(105)의 적층이 새롭게 시작된다. In addition, the inner diameter ID of the squeeze ring 200 is slightly smaller than the diameter of the lamina member 105. Accordingly, the squeeze ring 200 is applied to the lamina member 105 is inserted into the interior space 210, the lower lamina when the blanked lamina member 105 is inserted into the squeeze ring 200 The interlock tab 103 of the member 105 may be interference fit. When the lamina member 105 is repeatedly stacked and the lamina member 105 having the counter hole 106 is blanked and inserted into the squeeze ring 200, the lamina member 105 having the counter hole 106 is formed. Since there is no interlock tab 103, the lower lamina member 105 is not bonded, and thus the lamination core 100 is laminated. The lamination core 100 after the lamination is completed is discharged out through the lower end 220 of the squeeze ring 200, and lamination of the lamina member 105 is newly started on the lamina member 105 on which the counter hole 106 is formed. do.

이 때, 본 발명에 따른 스퀴즈 링(200)은 적층코아(100)가 하단(220)을 통해 배출될 때 라미나 부재(적층코아)에 가해지는 상기 측압을 서서히 감소시킨다는 특징을 갖는다. 즉, 스퀴즈 링(200)의 하부에서는 내부공간(210)의 내경(ID)이 하단(220)으로 갈수록 증가한다. At this time, the squeeze ring 200 according to the present invention has a characteristic of gradually reducing the side pressure applied to the lamina member (laminated core) when the laminated core 100 is discharged through the lower end 220. That is, in the lower portion of the squeeze ring 200, the inner diameter ID of the inner space 210 increases toward the lower portion 220.

도 8에 나타난 바와 같이, 내부공간(210)의 하부에는 경사면(221)과 계단턱(230)(232)이 형성된다. 경사면(221)은 아래쪽 방향으로 진행할 경우 내경(ID)이 점차로 넓어지도록 바깥쪽으로 형성된다. 또한, 계단턱(230)(232)은 계단턱(230)(232)의 위쪽 내경(ID) 보다 아래쪽의 내경(ID)이 커지도록 형성된다. As shown in FIG. 8, the inclined surface 221 and the stepped walls 230 and 232 are formed below the inner space 210. The inclined surface 221 is formed outward so that the inner diameter ID gradually widens when traveling downward. In addition, the staircases 230 and 232 are formed to have a larger inner diameter ID than the upper inner diameter ID of the staircases 230 and 232.

상기 경사면(221)은 0도 30분 정도의 각도(θ)로 형성될 수 있다. 또한, 계단턱(230)은 0.018mm ∼ 0.02mm 정도의 높이(H1)를 갖고 계단턱(232)은 0.013mm ∼ 0.015mm 정도의 높이(H2)를 가지는 것이 바람직하다.The inclined surface 221 may be formed at an angle θ of about 0 degrees 30 minutes. In addition, the step jaw 230 preferably has a height H1 of about 0.018 mm to 0.02 mm, and the step jaw 232 has a height H2 of about 0.013 mm to 0.015 mm.

상기 경사면(221)과 계단턱(230)(232)에 의해서 증가되는 전체 내경 중에서 계단턱(230)에 의해서 30%∼40%의 내경이 증가되고, 계단턱(232)에 의해서 30%∼40%의 내경이 증가되며, 경사면(221)에 의해서 나머지 내경 부분이 증가될 수 있다. Of the total inside diameters increased by the inclined surface 221 and the stepped jaw 230, 232, the inner diameter of 30% to 40% is increased by the stepped jaw 230, and 30% to 40 by the stepped jaw 232. The inner diameter of% is increased, and the remaining inner diameter portion may be increased by the inclined surface 221.

한편, 전술한 바와 같이, 본 발명은 적층코아(100)가 스퀴즈 링(200)의 하단에서 배출될 때 스퀴즈 링(200)이 적층코아(100)에 가하는 측압을 서서히 감소시키는 것에 그 특징이 있다. 따라서, 본 발명에 따른 기술적 사상에는 내부공간(210)의 하단(220)에 경사면만 형성되고 계단턱이 형성되지 않은 경우, 계단턱이 형성되지 않고 경사면이 반복적으로 형성된 경우, 계단턱만이 형성된 경우, 하단(220)에 계단턱이 형성되고 계단턱의 상측에 경사면이 형성된 경우 등도 포함되는 것으로 이해되어야 한다. 즉, 적층코아(100)가 스퀴즈 링(200)의 하단(220)에서 배출될 때 스퀴즈 링(200)이 적층코아(100)에 가하는 측압을 서서히 감소시킬 수 있는 구성은 본 발명의 권리범위에 포함되는 것으로 이해되어야 한다.On the other hand, as described above, the present invention is characterized in that the squeeze ring 200 when the laminated core 100 is discharged from the lower end of the squeeze ring 200 is gradually reduced the side pressure applied to the laminated core 100 . Therefore, in the technical concept according to the present invention, when only the inclined surface is formed at the bottom 220 of the inner space 210 and the staircase is not formed, when the inclined surface is repeatedly formed without the stepped jaw, only the stepped jaw is formed. In this case, it should be understood that the stepped jaw is formed at the lower end 220 and the inclined surface is formed above the stepped jaw. That is, when the laminated core 100 is discharged from the lower end 220 of the squeeze ring 200, the configuration that can gradually reduce the side pressure applied to the laminated core 100 is within the scope of the present invention. It should be understood to be included.

그러면, 본 발명에 따른 스퀴즈 링(200)을 이용하여 적층코아를 제조하는 과정을 설명하기로 한다. Then, a process of manufacturing a laminated core using the squeeze ring 200 according to the present invention will be described.

먼저, 금속 스트립을 이송시키면서 금속 스트립에 샤프트 홀(101), 슬롯(102), 인터록 탭(103) 등을 순차적으로 형성한다. 한편, 소정 매수의 라미나 부재(105)에 해당하는 금속 스트립에 인터록 탭(103)을 형성한 후에는 인터록 탭(103)을 형성하지 않고 카운터 홀(106)을 형성한다. 예를 들어, 20매의 라미나 부재에 해당하는 금속 스트립에 인터록 탭을 형성하고 21매 째의 라미나 부재에 해당하는 금속스트립 부분에는 카운터 홀(106)을 천공한다. 이러한 과정은 대한민국 특허등록 제10-0578043호, 대한민국 특허등록 제10-0762744호, 대한민국 특허등록 제10-1089903호 등에 개시되어 있는데, 상기 등록공보에 기재된 내용은 본 명세서에 포함된다. First, the shaft hole 101, the slot 102, the interlock tab 103, etc. are sequentially formed in the metal strip while transferring the metal strip. On the other hand, after the interlock tab 103 is formed in the metal strip corresponding to the predetermined number of lamina members 105, the counter hole 106 is formed without forming the interlock tab 103. For example, an interlock tab is formed in a metal strip corresponding to twenty lamina members, and a counter hole 106 is drilled in the metal strip portion corresponding to the twenty-first lamina member. This process is disclosed in the Republic of Korea Patent Registration No. 10-0578043, Republic of Korea Patent Registration No. 10-0762744, Republic of Korea Patent Registration No. 10-1089903, etc., the contents described in the registered publication is included herein.

샤프트 홀(101), 슬롯(102), 인터록 탭(103)이 형성된 금속 스트립이 블랭킹 유니트에 이송되면 블랭킹 블록이 블랭크 다이(140)와 협력하여 금속 스트립을 블랭킹하여 라미나 부재(105)를 형성한 후 블랭킹된 라미나 부재(105)를 스퀴즈 링(200)에 밀어 넣는다. 이 때, 스퀴즈 링(200)은 라미나 부재(105)에 소정의 측압을 가한다.When the metal strip having the shaft hole 101, the slot 102 and the interlock tab 103 is transferred to the blanking unit, the blanking block cooperates with the blank die 140 to blank the metal strip to form the lamina member 105. The blanked lamina member 105 is then pushed into the squeeze ring 200. At this time, the squeeze ring 200 exerts a predetermined side pressure on the lamina member 105.

계속해서 블랭킹이 이루어지면, 먼저 블랭킹되어 스퀴즈 링(200)에 삽입된 하부 라미나 부재(105)에 새롭게 블랭킹된 라민나 부재(105)가 억지끼움으로 결합하게 된다. 즉, 하부 라미나 부재(105)의 인터록 탭(103)과 상부 라미나 부재(105)의 인터록 탭(103)이 억지끼움 결합된다. 한편, 인터록 탭(103)이 형성된 라미나 부재(105)가 블랭킹된 경우에는 이러한 억지끼움 결합이 계속되면서 적층코아(100)가 아래로 이동하게 되고, 카운터 홀(106)이 형성된 라미나 부재(105)가 블랭킹되어 스퀴즈 링(200)에 삽입되면 하부 라미나 부재(105)와 결합될 수 없기 때문에 하부의 적층코아는 스퀴즈 링(200)의 하단(220)을 통해 밖으로 배출된다.Subsequently, if blanking is made, the newly blanked laminna member 105 is forcibly fitted to the lower lamina member 105 blanked and inserted into the squeeze ring 200. That is, the interlock tab 103 of the lower lamina member 105 and the interlock tab 103 of the upper lamina member 105 are interference fit. On the other hand, when the lamina member 105 on which the interlock tab 103 is formed is blanked, the lamination core 100 moves downward while the interference fitting is continued, and the lamina member on which the counter hole 106 is formed ( When the 105 is blanked and inserted into the squeeze ring 200, the laminated core of the lower part is discharged out through the lower end 220 of the squeeze ring 200 because it cannot be combined with the lower lamina member 105.

이 때, 스퀴즈 링(200)의 하단(220)은 아래쪽으로 갈수록 내경(ID)이 점차로 증가하고, 이에 따라 스퀴즈 링(200)의 하단(220)이 적층코아(100)에 가하는 측압이 아래쪽으로 갈수록 작아진다. 따라서, 적층코아(100)가 상기 하단(220)에서 배출될 때 측압의 변화가 서서히 이루어지기 때문에 적층코아(100)를 이루는 라미나 부재(105) 사이의 결합이 분리되는 것을 방지할 수 있게 된다. At this time, the inner diameter (ID) of the lower end 220 of the squeeze ring 200 gradually increases toward the lower side, and thus the side pressure applied to the laminated core 100 by the lower end 220 of the squeeze ring 200 downwards. It gets smaller. Therefore, when the laminated core 100 is discharged from the lower end 220, since the change in the side pressure is gradually made, it is possible to prevent the bonding between the lamina members 105 forming the laminated core 100 to be separated. .

100, 100a, 100b : 적층 코아 105, 105a : 라미나 부재
200 : 스퀴즈 링 210 : 내부공간
220 : 하단 221 : 경사면
230, 232 : 계단턱
100, 100a, 100b: laminated core 105, 105a: lamina member
200: squeeze ring 210: inner space
220: bottom 221: slope
230, 232: staircase

Claims (6)

금속 스트립이 블랭킹되어 만들어진 라미나 부재가 내부공간(210)에 삽입되어 상부 라미나 부재와 하부 라미나 부재가 억지끼움으로 서로 결합되어 적층코아를 이루고, 상기 내부공간(210)의 하부에서는 상기 내부공간(210)의 내경(ID)이 하단(220)으로 갈수록 증가하는 것을 특징으로 하는 스퀴즈 링.The lamina member formed by blanking the metal strip is inserted into the inner space 210 so that the upper lamina member and the lower lamina member are joined to each other by interference fit to form a lamination core. Squeeze ring, characterized in that the inner diameter (ID) of the space 210 increases toward the lower end (220). 제1항에 있어서,
상기 라미나 부재의 직경(D1) 보다 상기 내부공간(210)의 내경(ID)이 작은 것을 특징으로 하는 스퀴즈 링.
The method of claim 1,
Squeeze ring, characterized in that the inner diameter (ID) of the inner space 210 is smaller than the diameter (D1) of the lamina member.
제2항에 있어서,
상기 하단(220)에는 바깥쪽을 향한 경사면(221)이 형성된 것을 특징으로 하는 스퀴즈 링.
3. The method of claim 2,
The squeeze ring, characterized in that the lower surface 220 is formed with an inclined surface 221 facing outward.
제3항에 있어서,
상기 경사면(221)의 상측에는 적어도 하나의 계단턱(230)(232)이 형성되어 계단턱(230)(232)의 위쪽의 내경(ID)보다 아래쪽의 내경(ID)이 큰 것을 특징으로 하는 스퀴즈 링.
The method of claim 3,
At least one stairwell 230 and 232 is formed above the inclined surface 221, and an inner diameter ID of a lower portion is greater than an inner diameter ID of an upper portion of the stairwell 230 and 232. Squeeze Ring.
제2항에 있어서,
상기 내부공간(210)의 하부에는 적어도 하나의 계단턱(230)(232)이 형성되어 계단턱(230)(232)의 위쪽의 내경(ID)보다 아래쪽의 내경(ID)이 큰 것을 특징으로 하는 스퀴즈 링.
3. The method of claim 2,
At least one stairwell 230 and 232 is formed at the lower portion of the internal space 210, and an inner diameter ID of a lower portion is greater than an inner diameter ID of an upper portion of the stairwell 230 and 232. Squeeze ring.
금속 스트립을 블랭킹하여 라미나 부재를 만들기 위한 블랭크 다이; 및
블랭크 다이의 아래에 설치되고, 블랭킹된 라미나 부재가 억지끼움으로 서로 결합되는, 제1항 내지 제5항 중 어느 한 항의 스퀴즈 링;을 구비하는 것을 특징으로 하는 블랭킹 유니트.
A blank die for blanking the metal strip to make a lamina member; And
A squeeze ring according to any one of claims 1 to 5, which is installed under the blank die and in which the blanked lamina members are joined to each other by interference fit.
KR1020120046826A 2012-05-03 2012-05-03 Squeeze ring preventing stationary fit between lamina members from separation and, blanking unit having the same KR101368977B1 (en)