KR101079190B1 - Touchscreen panel having zigzag pattern design - Google Patents

Touchscreen panel having zigzag pattern design Download PDF

Info

Publication number
KR101079190B1
KR101079190B1 KR1020090087243A KR20090087243A KR101079190B1 KR 101079190 B1 KR101079190 B1 KR 101079190B1 KR 1020090087243 A KR1020090087243 A KR 1020090087243A KR 20090087243 A KR20090087243 A KR 20090087243A KR 101079190 B1 KR101079190 B1 KR 101079190B1
Authority
KR
South Korea
Prior art keywords
layer
double
adhesive tape
ito film
touch screen
Prior art date
Application number
KR1020090087243A
Other languages
Korean (ko)
Other versions
KR20110029532A (en
Inventor
석송곤
라상섭
조동현
강용재
Original Assignee
주식회사 모린스
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 주식회사 모린스 filed Critical 주식회사 모린스
Priority to KR1020090087243A priority Critical patent/KR101079190B1/en
Publication of KR20110029532A publication Critical patent/KR20110029532A/en
Application granted granted Critical
Publication of KR101079190B1 publication Critical patent/KR101079190B1/en

Abstract

본 발명은 실버패튼전극의 내측 끝단을 양면접착테이프의 폭과 동일하게 하고, 하부 ITO필름층에 에칭(식각, etching)을 형성시켜 양면접착테이프층에 함유되어 있는 염소 등의 성분과 반응하여 생성되는 화합물인, 즉 예를 들어 염산 등에 의해 상부 및 하부 ITO필름층이 부식 또는 양면접착테이프에 의해 ITO 필름층 코팅층에서의 박리현상 등에 의하여 접착력이 저하되는 것을 방지할 수 있도록 지그재그 패턴(zigzag pattern)을 적용시킨 것을 특징으로 하는 지그재그 패턴 구조를 갖는 터치스크린패널에 관한 것으로, 상부 및 하부 ITO 필름층 간에 전기적 신호가 원활하게 연결될 수 있도록 함으로써, 터치스크린패널의 가시영역(View Area, V/A)에서 광학적 특성의 변화가 없이 영상의 질을 향상시킴으로써, 다양한 종류의 전자기기에 그 적용을 확대할 수 있어 그 수요가 더욱 확대될 것으로 기대된다. The present invention makes the inner end of the silver pattern electrode equal to the width of the double-sided adhesive tape, and forms an etching (etching) on the lower ITO film layer to react with components such as chlorine contained in the double-sided adhesive tape layer. Zigzag pattern (i.e., zigzag pattern) to prevent the adhesion of the upper and lower ITO film layers, such as hydrochloric acid or the like, from being deteriorated due to corrosion or peeling from the ITO film layer coating layer due to double-sided adhesive tape. The present invention relates to a touch screen panel having a zigzag pattern structure, wherein an electrical signal is smoothly connected between the upper and lower ITO film layers, thereby allowing a visible area of the touch screen panel (View Area, V / A). By improving the quality of the image without changing the optical characteristics, the application can be extended to various kinds of electronic devices. Demand is expected to expand further.

터치스크린패널, 양면접착테이프, 에칭, 염소, ITO필름층, 실버패튼전극 Touch screen panel, double-sided adhesive tape, etching, chlorine, ITO film layer, silver pattern electrode

Description

지그재그 패턴 구조를 갖는 터치스크린패널{TOUCHSCREEN PANEL HAVING ZIGZAG PATTERN DESIGN}Touch screen panel with zigzag pattern structure {TOUCHSCREEN PANEL HAVING ZIGZAG PATTERN DESIGN}

본 발명은 지그재그 패턴 구조를 갖는 터치스크린패널에 관한 것으로, 더욱 상세하게는 상부 실버패튼전극의 내측 끝단을 양면접착테이프와 동일하게 하고, 하부 ITO필름층에 에칭(etching)을 형성시켜 양면접착테이프층에 함유되어 있는 염소 등의 성분과 반응하여 생성되는 화합물인, 즉 예를 들어 염산 등에 의해 상부 및 하부 ITO필름층이 반응하며 발생할 수 있는 손상을 방지할 수 있도록 지그재그 패턴(zigzag pattern)을 적용시켜 상부 및 하부 ITO 필름층 간에 전기적 신호가 원활하도록 한 구조인 것을 특징으로 하는 지그재그 패턴 구조를 갖는 터치스크린패널에 관한 것이다. The present invention relates to a touch screen panel having a zigzag pattern structure. More specifically, the inner end of the upper silver pattern electrode is made the same as the double-sided adhesive tape, and an etching is formed on the lower ITO film layer to form a double-sided adhesive tape. A zigzag pattern is applied to prevent damage caused by the reaction of the upper and lower ITO film layers, for example, by hydrochloric acid, which is a compound produced by reacting with a component such as chlorine contained in the layer. The present invention relates to a touch screen panel having a zigzag pattern structure, which is characterized in that the electrical signal is smoothly formed between the upper and lower ITO film layers.

최근 급격한 성장을 하고 있는 산업분야인 터치스크린패널(Touch Screen Panel)은 마우스나 키보드 등의 입력 방식을 대체할 수 있는 새로운 입력 방식으로, 사용자가 스크린을 보면서 손가락을 이용하여 스크린에 원하는 정보를 직접 입 력할 수 있는 새로운 입력 방식이다. 따라서 누구나 쉽게 조작할 수 있기 때문에 GUI(Graphical User Interface) 환경 하에서 가장 이상적인 입력 방식으로 평가받고 있으며, 현재 휴대폰, 네비게이션, PMP, 은행의 현금입출금기, 관공서의 민원서류발급기, 각종 관광 및 주요 기관의 안내기기 등 여러 분야에서 널리 사용되고 있다.Touch Screen Panel, an industry that is rapidly growing recently, is a new input method that can replace the input method such as a mouse or keyboard, and the user directly touches the desired information on the screen by using his / her fingers while looking at the screen. It is a new input method that can be input. Therefore, it is evaluated as the most ideal input method under the GUI (Graphical User Interface) environment because it can be easily operated by anyone, and is currently used as a mobile phone, navigation, PMP, bank teller and dispenser, public information issuing machine, guide of various tourism and major institutions. It is widely used in various fields such as equipment.

이러한 터치스크린패널은 애플의 아이폰이 정전용량 방식 터치스크린패널을 휴대폰에 채용하기 시작하면서 터치스크린패널 시장은 규모 면에서 급격한 성장을 이루었으며, 특히 올해 초부터 보다 많은 휴대폰 업체들이 터치스크린패널을 적용한 다양한 새로운 휴대폰들이 소비자들에게 제공됨에 따라 터치스크린패널이 다양하게 개발되어 특허출원 및 등록되고 있다. The touchscreen panel market has grown rapidly in size as Apple's iPhone began to adopt capacitive touchscreen panels in mobile phones. Especially since early this year, more mobile phone companies have applied touchscreen panels. As various new mobile phones are provided to consumers, various touch screen panels have been developed and patented and registered.

그리고, 터치스크린패널을 적용시킨 전자제품 및 기기류는 고가의 제품들로 수요자의 욕구를 충족시키기 위해서는 기기의 성능이 우수하면서 외관의 결점이 없어야 한다. 즉 고가의 전자제품이나 기기류들이 사소한 외관의 결점에 의해 수요자로부터 크레임에 의한 반품으로 막대한 손실을 입을 수 있기 때문이다. In addition, the electronic products and devices to which the touch screen panel is applied are expensive products, and in order to satisfy consumer's needs, the device should have excellent performance and no defects in appearance. In other words, expensive electronic products and devices may suffer huge losses due to minor defects from customers due to minor defects in appearance.

한편, 터치스크린패널을 적용시킨 전자제품으로 대표적인 휴대폰의 구조를 살펴보면, 종래의 휴대폰에서 터치스크린패널(100)은 도 1에 도시된 바와 같이 구조를 갖고 있으며, 상기와 같은 종래의 터치스크린패널의 광학구조물의 적층구조는 도 2에 도시된 바와 같이 상부 OCA층(10)(Optically Clear Adhesive Layer, 이하 'OCA층'이라 한다), 상부 ITO 필름층(20)(PET층과 ITO층으로 구성, Indium Tin Oxide Film Layer, 이하 'ITO 필름층'이라 한다), 상부 실버패튼전극(30), 양면접착테이프층(40), 하부 실버패튼전극(50), 하부 ITO 필름층(PET층과 ITO 층으로 구성)(60), 하부 OCA층(70) 및 플라스틱 PC 또는 강화유리 보강판(80)이 적층된 구조로서, 상부 실버패턴전극(30)과 하부 실버패턴전극(50)의 폭이 같으며, 상부 실버패턴전극(30)과 하부 실버패턴전극(50) 사이에 적층된 양면접착테이프층(40)의 폭이 넓은 구조로 이루어져 있다.On the other hand, when looking at the structure of a typical mobile phone as an electronic product to which the touch screen panel is applied, the touch screen panel 100 in the conventional mobile phone has a structure as shown in Figure 1, the conventional touch screen panel As shown in FIG. 2, the laminated structure of the optical structure includes an upper OCA layer 10 (Optically Clear Adhesive Layer, hereinafter referred to as an 'OCA layer'), an upper ITO film layer 20 (PET layer and ITO layer), Indium Tin Oxide Film Layer, hereinafter referred to as "ITO Film Layer", upper silver pattern electrode 30, double-sided adhesive tape layer 40, lower silver pattern electrode 50, lower ITO film layer (PET layer and ITO layer) (60), the lower OCA layer 70 and the plastic PC or tempered glass reinforcement plate 80 is laminated, the width of the upper silver pattern electrode 30 and the lower silver pattern electrode 50 is the same , A double-sided adhesive tape layer 40 stacked between the upper silver pattern electrode 30 and the lower silver pattern electrode 50. ) Has a wide structure.

또한 상기와 같은 구조를 갖는 터치스크린패널에서 ITO 필름층은 산화인듐주석(Indium Tin Oxide)을 PET 필름에 얇게 입힌 필름층으로, 터치스크린에서 외부 압력을 가하게 되면 상,하부의 ITO 필름층(20, 60)이 서로 접촉되면서 전기적 신호로 연결하는 역할을 하는 층이다. In addition, in the touch screen panel having the above structure, the ITO film layer is a thin film layer coated with indium tin oxide (Indium Tin Oxide) on the PET film, and when the external pressure is applied on the touch screen, the upper and lower ITO film layers 20 , 60) is a layer that serves to connect with each other as an electrical signal.

이와 같이 종래의 터치스크린패널(100)은 도 1에 도시된 바와 같은 구조에 의해 양면접착테이프층(40)과 상부 및 하부 ITO 필름층(20, 60) 사이에 각각 형성된 a 및 b 부분과 같은 이격공간에 의해 양면접착테이프층(40)이 상부 및 하부 ITO 필름층(20, 60)과 직접 닿게 될 경우, 특히 습도가 많은 환경에서 양면접착테이프 자체에 포함되어 있는 성분과 반응하여 생성될 수 있는 성분이 ITO 필름층과 화학반응을 일으켜 ITO 필름층을 부식시키거나 또는 ITO층과 PET 필름간의 밀착성을 저 하시켜 해당부분의 저항값이 올라가면서 제품의 전기적 특성이 나빠지거나 또는 ITO 필름층이 손상될 경우 실버패턴전극이 제 역활을 제대로 하지 못하고, 터치스크린패널의 전체적인 성능에도 영향을 미쳐 문제점이 발생할 우려가 있다. As such, the conventional touch screen panel 100 has a structure as shown in FIG. 1, such as a and b portions formed between the double-sided adhesive tape layer 40 and the upper and lower ITO film layers 20 and 60, respectively. When the double-sided adhesive tape layer 40 is directly in contact with the upper and lower ITO film layers 20 and 60 by the space, it may be generated by reacting with the components included in the double-sided adhesive tape itself in a humid environment. Chemicals react with the ITO film layer to corrode the ITO film layer or reduce the adhesion between the ITO layer and the PET film, resulting in deterioration of the electrical properties of the product as the resistance value of the part increases, or the ITO film layer If damaged, the silver pattern electrode may not function properly and may affect the overall performance of the touch screen panel, causing problems.

이와 같이 종래의 터치스크린패널은 양면접착테이프가 상부 및 하부 ITO 필름층에 직접 닿게 되고, 양면접착테이프 자체에 함유되어 있는 성분(예를 들어 염소 등의 성분)과 반응하여 생성될 수 있는 성분이 ITO 필름층을 부식시킴으로써 고가의 전자제품 가치를 상실시키는 문제점들이 발생되고 있지만 이를 개선시키기 위한 기술들이 아직까지 제대로 개발되지 않고 있는 실정이었다. As described above, in the conventional touch screen panel, the double-sided adhesive tape is directly in contact with the upper and lower ITO film layers, and the components that can be generated by reacting with the components (for example, chlorine or the like) contained in the double-sided adhesive tape itself are included. Problems that cause the loss of expensive electronic products by the corrosion of the ITO film layer has been generated, but techniques for improving the situation have not been properly developed yet.

따라서, 상기와 같은 문제점을 개선하기 위한 방안으로 본 발명은 상부 실버패턴전극의 내측 끝단이 가시영역(V/A, View Area) 쪽으로 양면접착테이프(DAT)층의 내측과 동일한 끝단에서 적층되도록 확장 설계함으로써, 양면접착테이프가 상부 ITO필름층에 직접 접촉되지 아니하여 양면접착테이프에 함유되어 있는 각종 물질로부터 상부 ITO필름층의 손상을 방지하여 상부 및 하부의 ITO 필름층 간의 전기적 신호가 원활하게 연결될 수 있도록 한 구조인 것을 특징으로 하는 지그재그 패턴 구조를 갖는 터치스크린패널을 제공함을 과제로 한다. Accordingly, the present invention extends such that the inner end of the upper silver pattern electrode is stacked at the same end as the inside of the double-sided adhesive tape (DAT) layer toward the visible area (V / A, View Area). By design, the double-sided adhesive tape is not in direct contact with the upper ITO film layer, thereby preventing damage to the upper ITO film layer from various materials contained in the double-sided adhesive tape, so that electrical signals between the upper and lower ITO film layers can be smoothly connected. An object of the present invention is to provide a touch screen panel having a zigzag pattern structure, which is characterized in that it has a structure such that the structure can be made.

또한 본 발명은 하부 ITO필름층에 에칭(etching)선을 형성시켜 ITO층을 깍아내고 PET(Polyethylene Terephthalate) 필름층이 노출되도록 하부 ITO필름층의 폭에 직교되는 방향으로 에칭(etching)을 형성시킴으로써, 양면접착테이프가 하부 ITO필름층에 접촉되더라도 에칭(etching)에 의해 노출된 하부 ITO필름층에서 받은 전기적, 물리적 손상이 PET(Polyethylene Terephthalate) 필름층의 절연효과에 의해 하부 ITO필름층의 부식에 의한 전기적, 물리적 손상이 확산되는 것을 방지하여 상부 및 하부의 ITO 필름층 간의 전기적 신호가 원활하게 연결될 수 있도록 한 구조인 것을 특징으로 하는 지그재그 패턴 구조를 갖는 터치스크린패널을 제공함을 다른 과제로 한다. In addition, the present invention by forming an etching line on the lower ITO film layer by scraping the ITO layer and forming an etching in a direction orthogonal to the width of the lower ITO film layer to expose the polyethylene terephthalate (PET) film layer Even though the double-sided adhesive tape is in contact with the lower ITO film layer, the electrical and physical damages received from the lower ITO film layer exposed by etching may cause corrosion of the lower ITO film layer due to the insulation effect of the polyethylene terephthalate (PET) film layer. Another object of the present invention is to provide a touch screen panel having a zigzag pattern structure, which is a structure in which electrical signals between upper and lower ITO film layers can be smoothly connected by preventing electrical and physical damage from spreading.

그리고 위와 같이 상부 ITO 필름층의 실버패턴전극을 양면접착테이프의 내측 끝단과 1 : 1로 형성하고 하부 실버패턴전극 내측으로 에칭(Etching)을 형성시키는 방법을 반대 방향으로 즉, 하부 ITO 필름층의 실버패턴전극을 양면접착테이프와 내측 끝단에서 1 : 1로 형성하고 상부 ITO 필름층에서 실버패턴전극 내측으로 에칭(Etching)을 형성시키는 방법도 가능함을 알아야 한다.As described above, the method of forming the silver pattern electrode of the upper ITO film layer as 1: 1 with the inner end of the double-sided adhesive tape and forming etching into the lower silver pattern electrode in the opposite direction, that is, of the lower ITO film layer It is also possible to form a silver pattern electrode with a 1: 1 on both sides of the double-sided adhesive tape and the inner end, and to form an etching from the upper ITO film layer into the silver pattern electrode.

상기의 과제를 달성하기 위한 본 발명은 상부 OCA층, 상부 ITO 필름층, 상부 실버패튼전극, 양면접착테이프층, 하부 실버패튼전극, 하부 ITO 필름층, 하부 OCA층 및 플라스틱 PC 또는 강화유리 보강판의 순으로 적층된 구조로 이루어진 터치스 크린패널에 있어서,The present invention for achieving the above object is the upper OCA layer, the upper ITO film layer, the upper silver pattern electrode, double-sided adhesive tape layer, lower silver pattern electrode, lower ITO film layer, lower OCA layer and plastic PC or tempered glass reinforcement plate In the touch screen panel consisting of a stacked structure in order of,

상기 상부 실버패턴전극은 그 폭의 길이가 가시영역(View Area) 쪽으로 양면접착테이프층의 폭의 길이와 동일한 길이의 폭으로 적층되도록 하여 양면접착테이프층이 상부 ITO 필름층에 닿지 않도록 한 구조인 것을 특징으로 하는 지그재그 패턴 구조를 갖는 터치스크린패널을 과제 해결 수단으로 한다.The upper silver pattern electrode has a structure in which the width of the double-sided adhesive tape layer does not touch the upper ITO film layer by stacking the width of the double-sided adhesive tape in the same length as the width of the double-sided adhesive tape layer toward the view area. A touch screen panel having a zigzag pattern structure is characterized in that the problem solving means.

또한 본 발명은 지그재그 패턴 구조를 갖는 터치스크린패널은 상부 OCA층, 상부 ITO 필름층, 상부 실버패튼전극, 양면접착테이프층, 하부 실버패튼전극 및 ITO PC 또는 ITO 유리판의 순으로 적층된 구조로 이루어진 터치스크린패널에 있어서,In addition, the present invention is a touch screen panel having a zigzag pattern structure is made of a stacked structure of the upper OCA layer, the upper ITO film layer, the upper silver pattern electrode, the double-sided adhesive tape layer, the lower silver pattern electrode and the ITO PC or ITO glass plate. In the touch screen panel,

상기 상부 실버패턴전극은 그 폭의 길이가 가시영역(View Area) 쪽으로 양면접착테이프층의 폭의 길이와 동일한 길이의 폭으로 적층되도록 하여 양면접착테이프층이 상부 ITO 필름층에 닿지 않도록 한 구조인 것을 특징으로 하는 지그재그 패턴 구조를 갖는 터치스크린패널을 다른 과제 해결 수단으로 한다.The upper silver pattern electrode has a structure in which the width of the double-sided adhesive tape layer does not touch the upper ITO film layer by stacking the width of the double-sided adhesive tape in the same length as the width of the double-sided adhesive tape layer toward the view area. A touch screen panel having a zigzag pattern structure is set as another means for solving the problems.

그리고 본 발명에서 상기 하부 ITO필름층 또는 ITO PC 또는 ITO 유리판은 에칭(etching)부를 형성시킨 것을 특징으로 하고, And in the present invention, the lower ITO film layer or ITO PC or ITO glass plate is characterized in that to form an etching (etching),

또한 상기 에칭(etching)부는 하부 ITO필름층 또는 ITO PC 또는 ITO 유리판의 폭에 직교되는 방향으로 형성시킨 것이 바람직하다.In addition, the etching portion is preferably formed in a direction orthogonal to the width of the lower ITO film layer or the ITO PC or ITO glass plate.

따라서 본 발명에 따른 지그재그 패턴 구조를 갖는 터치스크린패널은 양면접착테이프에 의한 상부 및 하부 ITO필름층이 양면접착테이프에 함유되어 있는 성분에 의하여 손상되는 것을 방지하여 상부 및 하부의 ITO 필름층 간의 전기적 신호가 원활하게 연결될 수 있도록 함으로써, 터치스크린패널의 가시영역(View Area, V/A)에서 광학적 특성의 변화가 없이 영상의 질을 향상시킴으로써, 다양한 종류의 전자기기에 그 적용을 확대할 수 있어 그 수요가 더욱 확대될 것으로 기대된다. Accordingly, the touch screen panel having a zigzag pattern structure according to the present invention prevents the upper and lower ITO film layers by the double-sided adhesive tape from being damaged by the components contained in the double-sided adhesive tape, thereby preventing the electrical contact between the upper and lower ITO film layers. By allowing the signals to be connected smoothly, the quality of the images can be improved without changing the optical characteristics in the view area (V / A) of the touch screen panel. The demand is expected to expand further.

이하, 첨부된 도면을 참조하여 본 발명의 바람직한 실시예를 첨부한 도면인 도 3 내지 도 7에 의거하여 상세히 설명하며, 동일한 기능을 수행하는 구성 요소에 대해서는 동일한 참조 번호를 병기한다. 한편, 각 도면 및 상세한 설명에서 일반적인 터치스크린패널로부터 이 분야의 종사자들이 용이하게 알 수 있는 구성 및 작용에 대한 도시 및 언급은 간략히 하거나 생략하였다. 특히, 도면의 도시에 있어서 요소들 사이의 크기 비가 다소 상이하게 표현되거나 서로 결합되는 부품들 사이의 크기가 상이하게 표현된 부분도 있으나, 이와 같은 도면의 표현 차이는 이 분야의 종사자들이 용이하게 이해할 수 있는 부분들이므로 별도의 설명을 생략한다.Hereinafter, with reference to the accompanying drawings, a preferred embodiment of the present invention will be described in detail with reference to Figures 3 to 7, which are attached, with the same reference numerals for components that perform the same function. On the other hand, in the drawings and detailed description showing and referring to the configuration and operation that can be easily understood by those skilled in the art from a general touch screen panel is briefly or omitted. In particular, although the size ratio between the elements in the drawings of the drawings are expressed slightly different or the size between the components that are coupled to each other is expressed, the representation of such drawings is easily understood by those skilled in the art The descriptions are omitted since they are possible parts.

또한 본 발명은 상세한 설명의 내용 중에 사용하는 용어 중 'ITO 필름층'과 '접착테이프층'은 문장 전후의 문맥 흐름상 'ITO 필름'과 '접착테이프'로 혼용하여 사용할 수 있음을 이해하여야 한다. In addition, the present invention should be understood that the term 'ITO film layer' and 'adhesive tape layer' among the terms used in the description may be used interchangeably as 'ITO film' and 'adhesive tape' in the context flow before and after the sentence. .

본 발명에서 도 3은 본 발명에 따른 실시예로서, 지그재그 패턴 구조를 갖는 터치스크린패널을 A-A'선방향으로 절단한 면(바탕면 : 하부 ITO 필름층)을 나타내는 단면도이고, 도 4는 본 발명에 따른 다른 실시예로서, 지그재그 패턴 구조를 갖는 터치스크린패널을 A-A'선방향으로 절단한 면(바탕면 : ITO PC 또는 ITO 유리)을 나타내는 단면도이며, 도 5는 도 3 및 도 4의 도면에서 에칭(etching)부를 형성시킨 것을 나타낸 평면도이고, 도 6은 도 3에서 에칭(etching)부를 형성시킨 상태를 나타낸 단면도이며, 도 7은 도 4에서 에칭(etching)부를 형성시킨 상태를 나타낸 단면도에 관한 것이다.In the present invention, Figure 3 is a cross-sectional view showing a surface (base: lower ITO film layer) cut in the A-A 'line direction of the touch screen panel having a zigzag pattern structure as an embodiment according to the present invention, Figure 4 As another embodiment according to the present invention, a cross-sectional view showing a surface (base surface: ITO PC or ITO glass) cut in the A-A 'line direction of the touch screen panel having a zigzag pattern structure, Figure 5 and Figure 3 and Figure 4 is a plan view illustrating the formation of an etching unit in FIG. 4, and FIG. 6 is a cross-sectional view illustrating the state in which an etching unit is formed in FIG. 3, and FIG. 7 illustrates a state in which the etching unit is formed in FIG. 4. Relates to the cross-sectional view shown.

본 발명에 따른 지그재그 패턴 구조를 갖는 터치스크린패널은 도 3에 도시된 바와 같이 상부 OCA층(10), 상부 ITO 필름층(20), 상부 실버패튼전극(30) 및 윈도우 필름층(도면에는 미도시)의 순으로 적층된 구조의 상판 패널과 그리고 하부 실버패튼전극(50), 하부 ITO 필름층(60), 하부 OCA층(70) 및 플라스틱 PC 또는 강화유리 보강판(80)의 순으로 적층된 구조의 하판 패널로 구분되고, 상기 하판 패널과 상판 패널을 양면접착테이프(40)를 사용하여 접착시킨 구조로 이루어진다. As shown in FIG. 3, the touch screen panel having a zigzag pattern structure according to the present invention has an upper OCA layer 10, an upper ITO film layer 20, an upper silver patternon electrode 30, and a window film layer (not shown in the drawing). Top panel of the laminated structure in the order of) and the lower silver pattern electrode 50, the lower ITO film layer 60, the lower OCA layer 70 and the plastic PC or tempered glass reinforcement plate 80 It is divided into a lower panel of the structure, and the lower panel and the upper panel consists of a structure bonded to each other using a double-sided adhesive tape (40).

또한, 본 발명에 따른 지그재그 패턴 구조를 갖는 터치스크린패널의 적층구조는 도 4에 표시된 바와 같이 상부 OCA층(10)(Optically Clear Adhesive Layer, 이하 'OCA층'이라 한다), 상부 ITO 필름층(20), 상부 실버패튼전극(30), 양면접착테이프층(40), 하부 실버패튼전극(50), ITO PC 또는 ITO 유리판(81)(상기의 구조에서 아래쪽에 위치한 ITO 필름층과 OCA층 그리고 플라스틱 PC 또는 강화유리 보강판이 하는 역할을 하나의 층으로 구현)로 적층된 구조에도 적용될 수 있다.In addition, the stacked structure of the touch screen panel having a zigzag pattern structure according to the present invention is an upper OCA layer 10 (Optically Clear Adhesive Layer, hereinafter referred to as 'OCA layer'), the upper ITO film layer as shown in FIG. 20), the upper silver pattern electrode 30, the double-sided adhesive tape layer 40, the lower silver pattern electrode 50, ITO PC or ITO glass plate 81 (in the above structure, the ITO film layer and the OCA layer and It can also be applied to a laminated structure of a plastic PC or a tempered glass reinforcement plate to realize a role of one layer).

본 발명에 따른 지그재그 패턴 구조를 갖는 터치스크린패널의 적층구조는 이외에도 전통적인 4선 저항막방식 터치스크린패널에 모두 적용이 가능하다. 즉 적층 구조에 상관없이 상하부에 각각 2개의 전극을 실버(또는 전극 역할을 할 수 있는 도전 물질)로 형성하고, 상하부에 ITO 층(또는 그와 같은 역할을 할 수 있는 물질, 예를 들어 CNT, 실버 나노 와이어 등)을 포함하는 모든 형태의 터치스크린패널 제품에 적용할 수 있다.The laminated structure of the touch screen panel having a zigzag pattern structure according to the present invention can be applied to both conventional 4-wire resistive touch screen panels. That is, two electrodes are formed of silver (or a conductive material capable of acting as an electrode) on the upper and lower sides, irrespective of the stacked structure, and an ITO layer (or a material capable of acting as such, for example, CNT, on the upper and lower sides). It can be applied to all types of touch screen panel products including silver nano wire.

상기에서 상, 하부 OCA층(10, 70)은 각각 광학 투명 접착제인 OCA(Optically Clear Adhesive)를 이용하여 상, 하부 ITO 필름층(20, 60)과 플라스틱 PC 또는 강화유리 보강판(80) 및 윈도우 필름층(도면에는 미도시, 상부 OCA층의 상부에 적층되는 층)을 접착시키기 위한 층이다. In the above, the upper and lower OCA layer (10, 70) is the upper and lower ITO film layer (20, 60) and the plastic PC or tempered glass reinforcement plate 80 and using the optically clear adhesive OCA (Optically Clear Adhesive), respectively It is a layer for adhering a window film layer (the layer laminated | stacked on top of the upper OCA layer not shown in drawing).

그리고 ITO 필름층은 필름에 산화인듐주석(Indium Tin Oxide)을 입힌 층으로써, 터치스크린에서 외부 압력을 가하게 되면 상, 하부의 ITO 필름층(20, 60)이 서로 접촉되면서 전기신호로 연결하는 역할을 한다. In addition, the ITO film layer is a layer coated with indium tin oxide (Indium Tin Oxide) on the film, and when the external pressure is applied on the touch screen, the upper and lower ITO film layers 20 and 60 come into contact with each other and connect with electric signals. Do it.

또한 본 발명에서 연성회로기판(도면에는 미도시)은 상, 하부의 실버패튼전극(30, 50)과 접속되는 부분의 연성회로기판의 선단 상하부에 접착된 이방 도전성 필름(ACF, Anisotropic Conductive Film)(도면에는 미도시)에 함유되어 있는 도전성 볼이 압력에 의해 터지면서 연성회로기판과 상, 하부의 실버패튼전극(30, 50) 사이에 전류가 흐르게 되며, 상기와 같은 구성은 통상적인 기술로서 본 발명의 특징이 되지 아니하므로 여기서는 그 설명을 생략하기로 한다. In the present invention, the flexible circuit board (not shown in the drawing) is an anisotropic conductive film (ACF) bonded to the upper and lower ends of the flexible circuit board of the portion connected to the upper and lower silver pattern electrodes (30, 50) The conductive balls contained in (not shown in the drawing) are blown by pressure, and current flows between the flexible circuit board and the upper and lower silver pattern electrodes 30 and 50. The above configuration is a conventional technique. Since it is not a feature of the present invention, description thereof will be omitted.

따라서 본 발명에 따른 실시예로서, 도 3에 도시된 바와 같은 지그재그 패턴 구조를 갖는 터치스크린패널은 상부 OCA층(10), 상부 ITO 필름층(20), 상부 실버패튼전극(30), 양면접착테이프층(40), 하부 실버패튼전극(50), 하부 ITO 필름(60), 하부 OCA층(70) 및 플라스틱 PC 또는 강화유리 보강판(80)의 순으로 적층된 구조로 이루어진 터치스크린패널에 있어서,Therefore, as an embodiment according to the present invention, the touch screen panel having a zigzag pattern structure as shown in Figure 3 is the upper OCA layer 10, the upper ITO film layer 20, the upper silver patternon electrode 30, both sides adhesive In the touch screen panel having a structure in which a tape layer 40, a lower silver pattern electrode 50, a lower ITO film 60, a lower OCA layer 70, and a plastic PC or tempered glass reinforcement plate 80 are stacked in this order. In

상기 상부 실버패턴전극(30)은 그 폭의 길이가 가시영역(View Area) 쪽으로 양면접착테이프층(40)의 폭의 길이와 동일한 길이의 폭으로 적층되도록 하여 양면접착테이프층(40)이 상부 ITO 필름층(20)에 닿지 않도록 한 구조인 것을 특징으로 한다. The upper silver pattern electrode 30 has a width of the double-sided adhesive tape layer 40 on the upper side so that the length of the width is laminated with a width equal to the length of the width of the double-sided adhesive tape layer 40 toward the view area. It is characterized by having a structure not to contact the ITO film layer 20.

그리고 본 발명에 따른 다른 실시예로서, 도 4에 도시된 바와 같은 지그재그 패턴 구조를 갖는 터치스크린패널은 상부 OCA층(10), 상부 ITO 필름층(20), 상부 실버패튼전극(30), 양면접착테이프층(40), 하부 실버패튼전극(50) 및 ITO PC 또는 ITO 유리판(81)의 순으로 적층된 구조로 이루어진 터치스크린패널에 있어서,And as another embodiment according to the present invention, the touch screen panel having a zigzag pattern structure as shown in Figure 4 is the upper OCA layer 10, the upper ITO film layer 20, the upper silver patternon electrode 30, both sides In the touch screen panel having a structure in which the adhesive tape layer 40, the lower silver pattern electrode 50, and the ITO PC or ITO glass plate 81 are stacked in this order,

상기 상부 실버패턴전극(30)은 그 폭의 길이가 가시영역(View Area) 쪽으로 양면접착테이프층(40)의 폭의 길이와 동일한 길이의 폭으로 적층되도록 하여 양면접착테이프층(40)이 상부 ITO 필름층(20)에 닿지 않도록 한 구조인 것을 특징으로 한다. The upper silver pattern electrode 30 has a width of the double-sided adhesive tape layer 40 on the upper side so that the length of the width is laminated with a width equal to the length of the width of the double-sided adhesive tape layer 40 toward the view area. It is characterized by having a structure not to contact the ITO film layer 20.

본 발명에서 '지그재그 패턴 구조'라 함은 도 2와 같이 광학구조물의 적층구조가 대칭형 적층구조인 종래의 터치스크린패널과는 달리 도 3 및 도 4에 도시된 바와 같이 광학구조물의 적층구조가 상부 실버패턴전극에 의해 비대칭형 적층구조인 것을 의미한다.In the present invention, the zigzag pattern structure is different from the conventional touch screen panel in which the stacked structure of the optical structure is a symmetrical stacked structure as shown in FIG. 2, and the stacked structure of the optical structure is shown in FIGS. 3 and 4. The silver pattern electrode means an asymmetrical laminated structure.

즉, 본 발명에 따른 터치스크린패널은 상부 실버패턴전극(30)의 폭의 길이가 가시영역(V/A, View Area) 쪽으로 양면접착테이프층(40)의 폭의 길이와 동일한 폭의 길이로 적층되도록 확장설계함으로써, 양면접착테이프층(40)이 상부 ITO필름층(20)에 직접 접촉되지 아니하여 양면접착테이프에 함유되어 있는 성분과 반응하여 생성될 수 있는 화합물 등에 의한 상부 ITO필름층(20)의 손상을 방지하여 상부 및 하부의 ITO 필름층(20, 60) 간의 전기적 신호가 원활하게 연결될 수 있도록 한 구조인 것이 특징이다. That is, in the touch screen panel according to the present invention, the width of the upper silver pattern electrode 30 is equal to the length of the width of the double-sided adhesive tape layer 40 toward the view area (V / A, View Area). By the expansion design to be laminated, the upper ITO film layer by the compound or the like that can be produced by reacting with the components contained in the double-sided adhesive tape without the direct double-sided adhesive tape layer 40 is in direct contact with the upper ITO film layer 20 ( It is characterized in that the structure to prevent the damage of the 20) so that the electrical signal between the upper and lower ITO film layer (20, 60) can be connected smoothly.

그리고 본 발명에 따른 실시예에서 상기 하부 ITO필름층(60)은 도 3에 도시된 바와 같이 에칭(etching)부(63)를 형성시키고, 또한 본 발명에 따른 다른 실시예에서 도 4에 도시된 바와 같이 ITO PC 또는 ITO 유리판(81)에 에칭(etching)부(63)를 형성시키는 것이 바람직하다.In the embodiment according to the present invention, the lower ITO film layer 60 forms an etching portion 63 as shown in FIG. 3, and is also shown in FIG. 4 in another embodiment according to the present invention. As described above, it is preferable to form an etching portion 63 on the ITO PC or the ITO glass plate 81.

상기 에칭(etching)부(63)는 도 5에 도시된 바와 같이 하부 ITO필름층(60)에서 에칭(etching)을 하여 ITO층(61)의 면을 깍아낸 다음 PET 필름층(62)이 노출되도록 하여 하부 ITO필름층(60)의 폭에 직교되는 방향(도 1의 A-A'의 직교방향)으로 에칭(etching)선을 형성시킴으로써, 양면접착테이프층(40)이 하부 ITO필름층(60)에 접촉되더라도 도 6에 도시된 바와 같이 에칭(etching)부(63)에 의해 ITO층(Indium Tin Oxide Layer)(61)이 깍여지고, 노출되는 PET 필름층(62)의 절연효과에 의해 하부 ITO필름층(60)의 부식에 의한 손상이 확산되는 것을 방지하여 상부 및 하부의 ITO 필름층(20, 60) 간의 전기적 신호가 원활하게 연결될 수 있도록 한 구조인 것이 특징이다. As shown in FIG. 5, the etching part 63 is etched from the lower ITO film layer 60 to scrape off the surface of the ITO layer 61 and then expose the PET film layer 62. By forming an etching line in a direction orthogonal to the width of the lower ITO film layer 60 (orthogonal to A-A 'of FIG. 1), the double-sided adhesive tape layer 40 is formed by the lower ITO film layer ( 6, the indium tin oxide layer 61 is scraped off by the etching portion 63 as shown in FIG. 6, and the insulation effect of the exposed PET film layer 62 is reduced. It is characterized in that the structure to prevent the damage caused by corrosion of the lower ITO film layer 60 is spread so that the electrical signal between the upper and lower ITO film layer (20, 60) can be connected smoothly.

또는 다른 실시예로서도 5에 도시된 바와 같이 ITO PC 또는 ITO 유리판(81)에서 ITO PC 또는 ITO 유리판(81)의 폭에 직교되는 방향(도 1의 A-A'의 직교방향)으로 에칭(etching)선을 형성시켜 도 7에 도시된 바와 같이 ITO PC 또는 ITO 유리판(81)의 면을 깍아낸다.Alternatively, as shown in FIG. 5, etching is performed in the direction orthogonal to the width of the ITO PC or the ITO glass plate 81 in the ITO PC or the ITO glass plate 81 (orthogonal to A-A 'in FIG. 1). ) And cut off the surface of the ITO PC or ITO glass plate 81 as shown in FIG.

그리고 상기 에칭(etching)부(63)는 습식 식각(Wet Etching) 방식, 또는 건식 식각(Dry) 방식으로 형성시키는 것이 바람직하다. 상기에서 습식 식각(Wet Etching) 방식 및 건식 식각(Dry) 방식은 통상적인 방법에 의해 실시되어진다. In addition, the etching portion 63 may be formed by a wet etching method or a dry etching method. Wet etching (Wet Etching) method and dry etching (Dry) method is performed by a conventional method.

또한 상기의 방법에 의해 형성되는 에칭부는 도 3 및 도 4에 도시된 바와 같이 일정 간격의 폭에 식각하거나 또는 가는 선의 형태로 식각할 수도 있다. In addition, as shown in FIGS. 3 and 4, the etching portion formed by the above method may be etched in a width of a predetermined interval or in the form of a thin line.

참고로 본 발명에서 터치스크린패널에 사용되는 광학구조물의 적층체의 두께는 통상적으로 일반적인 터치스크린패널에 사용되는 광학구조물의 적층체로서, 상부 및 하부 실버패튼전극(30, 50)의 두께는 각각 20 ㎛ 이하인 것이 바람직하고, 양면접착테이프층(40)의 두께는 50~150 ㎛인 것이 바람직하며, 상부 및 하부 ITO필름층(20, 60)의 두께는 100~200 ㎛ 사이의 것을 사용하고, 그리고 상부 및 하부 ITO필름층(20, 60)에서 ITO층(61)의 두께는 수백 ㎚인 것이 바람직하며, 사용 목적에 따라 상기에서 한정한 두께의 치수 이외에도 적용되어질 수 있다. For reference, in the present invention, the thickness of the stack of optical structures used in the touch screen panel is typically a stack of optical structures used in a general touch screen panel, and the thicknesses of the upper and lower silver pattern electrodes 30 and 50 are respectively. It is preferable that it is 20 micrometers or less, The thickness of the double-sided adhesive tape layer 40 is 50-150 micrometers, The thickness of the upper and lower ITO film layers 20 and 60 uses between 100-200 micrometers, In addition, the thickness of the ITO layer 61 in the upper and lower ITO film layers 20 and 60 is preferably several hundred nm, and may be applied in addition to the above-defined thickness according to the purpose of use.

한편, 종래의 터치스크린패널은 도 2에 도시된 바와 같이 폭의 길이가 동일한 상부 실버패튼전극(30) 및 하부 실버패튼전극(50) 사이에 상기 상부 및 하부 실버패튼전극(30, 50)의 폭의 길이보다 긴 양면접착테이프층(40)이 적층됨으로써, 상기 양면접착테이프층(40)이 상부 및 하부 ITO 필름층(20, 60)에 접촉되면서 양면접착테이프층(40)에 함유되어 있는 성분이 상기 상부 및 하부 ITO 필름층(20, 60)의 ITO층(61)을 부식시키게 되고, 이러한 부식현상에 의해 상부 및 하부의 ITO 필름층(20, 60) 간의 전기적 신호가 불규칙해지고 이로 인해 터치 오인식, 미감지 등의 문제점들이 발생하게 되며, 양면접착테이프가 화합물을 생성하면서 부가적으로 본연의 접착력을 저해시키는 현상을 유발할 수도 있다. Meanwhile, in the conventional touch screen panel, as shown in FIG. 2, the upper and lower silver pattern electrodes 30 and 50 are disposed between the upper silver pattern electrode 30 and the lower silver pattern electrode 50 having the same width. By laminating the double-sided adhesive tape layer 40 longer than the length of the width, the double-sided adhesive tape layer 40 is contained in the double-sided adhesive tape layer 40 while contacting the upper and lower ITO film layers 20, 60. A component causes corrosion of the ITO layer 61 of the upper and lower ITO film layers 20 and 60, and this corrosion phenomenon causes irregular electrical signals between the upper and lower ITO film layers 20 and 60. Problems such as touch misunderstanding and undetected will occur, and the double-sided adhesive tape may cause a phenomenon that additionally inhibits the original adhesion while generating the compound.

본 발명에서 도 2 내지 도 4에 도시된 바와 같은 V/A(View Area) 경계면이란 가시영역의 경계면으로서, 터치스크린 외곽의 프레임과 하부 LCD 화면과의 경계되는 면을 의미한다. In the present invention, as shown in FIGS. 2 to 4, the V / A (View Area) boundary surface is a boundary surface of the visible area, and means a boundary surface between the frame of the touch screen and the lower LCD screen.

그리고 본 발명에서 상기 상부 ITO 필름층(20) 또는 하부 ITO 필름층(60)의 ITO는 투명도전막으로 대체할 수 있다. 본 발명에서 사용가능한 투명도전막의 예를 들면 ITO층, CNT(탄소 나노 튜브), 실버 나노 와이어, 박막 니켈 등이 있으며, 상기에서 나열한 종류 이외에도 ITO와 동등 이상의 물성을 갖는 투명도전막인 경우에는 모두 적용되어질 수 있다.In the present invention, the ITO of the upper ITO film layer 20 or the lower ITO film layer 60 may be replaced with a transparent conductive film. Examples of the transparent conductive film usable in the present invention include an ITO layer , CNT (carbon nanotube), silver nanowires, thin film nickel, and the like. In addition to the above-mentioned types, all of the transparent conductive films having the same or higher properties as those of ITO are applicable. Can be done.

또한 본 발명에서 상기 상부 및 하부 실버패튼전극(30, 50)은 실버 이외의 대체소재로서 도전성 소재를 이용하여 전극을 형성시키는 것이 가능하다, 즉, 백금, 구리, 알루미늄과 같은 소재를 사용하거나 또는 폴리아닐린, 폴리아세틸렌, 폴리피롤, 폴리티오펜, 폴리-3-알킬티오펜, 폴리페닐렌 설파이드, 폴리퓨란, 폴리티에닐렌비닐렌,폴리다이에틸렌로 이루어진 군에 1종을 선택하여 사용하는 전도성 고 분자 화합물을 사용하는 것이 바람직하며, 상기에서 열거한 종류 이외의 소재라도 도전성 특성이 있는 소재일 경우에는 사용이 가능하다.In addition, in the present invention, the upper and lower silver pattern electrodes 30 and 50 may be formed of an electrode using a conductive material as an alternative material other than silver, that is, using a material such as platinum, copper, aluminum, or Conductive high molecular weight polymer selected from the group consisting of polyaniline, polyacetylene, polypyrrole, polythiophene, poly-3-alkylthiophene, polyphenylene sulfide, polyfuran, polythienylenevinylene and polydiethylene It is preferable to use a compound, and in the case of a material having conductive properties, even a material other than the above-mentioned types can be used.

또한 상기 패튼전극은 실버 또는 이외의 도전성 소재를 이용하여 인쇄 또는 증착의 방법으로 전극을 형성시킨다. 상기에서 전극을 형성시키기 위한 방법인 인쇄 또는 증착의 방법은 통상적인 방법에 의해 실시되어진다. In addition, the pattern electrode is formed of a method of printing or vapor deposition using a silver or other conductive material. The method of printing or vapor deposition, which is a method for forming an electrode in the above, is carried out by a conventional method.

그리고 본 발명에서 양면접착테이프층(40)에서 사용하는 양면접착테이프는 그 대체소재로서, 통상적인 접착제를 사용할 수 있으며, 상기 접착제의 경우에는 인쇄방식에 의해 접착층을 형성시킨다. 상기에서 접착층의 형성은 통상적인 인쇄방식에 의해 실시되어진다. In the present invention, the double-sided adhesive tape used in the double-sided adhesive tape layer 40 may be a conventional adhesive as the substitute material, and in the case of the adhesive, an adhesive layer is formed by a printing method. Formation of the adhesive layer in the above is carried out by a conventional printing method.

따라서, 본 발명은 상기에서 상술한 바와 같이 양면접착테이프 또는 접착제에 의해 상부 및 하부 ITO 필름층이 손상되지 않는 구조의 터치스크린패널로서, 상부 및 하부 ITO 필름층간의 전기적 신호의 연결이 원활하여 영상의 질을 향상된 것이 특징이다. Accordingly, the present invention is a touch screen panel having a structure in which the upper and lower ITO film layers are not damaged by the double-sided adhesive tape or adhesive as described above, and the connection of the electrical signals between the upper and lower ITO film layers is smooth. It is characterized by improved quality.

상술한 바와 같은, 본 발명의 바람직한 실시예에 따른 터치스크린패널을 상기한 설명 및 도면에 따라 도시하였지만, 이는 예를 들어 설명한 것에 불과하며 본 발명의 기술적 사상을 벗어나지 않는 범위 내에서 다양한 변화 및 변경이 가능하다 는 것을 이 분야의 통상적인 기술자들은 잘 이해할 수 있을 것이다. As described above, the touch screen panel according to a preferred embodiment of the present invention has been shown in accordance with the above description and drawings, but this is merely described, for example, and various changes and modifications within the scope without departing from the technical spirit of the present invention. It will be appreciated by those skilled in the art that this is possible.

도 1은 종래의 터치스크린패널에서 터치스크린의 평면을 나타내기 위한 도면;1 is a view showing a plane of a touch screen in a conventional touch screen panel;

도 2는 상기 도 1의 A-A'선을 절단한 면을 나타내는 단면도;       2 is a cross-sectional view showing a plane taken along the line AA ′ of FIG. 1;

도 3은 본 발명에 따른 실시예로서, 지그재그 패턴 구조를 갖는 터치스크린패널을 A-A'선방향으로 절단한 면(바탕면 : 하부 ITO 필름층)을 나타내는 단면도;       3 is a cross-sectional view showing a surface (base surface: lower ITO film layer) cut along a line A-A 'of a touch screen panel having a zigzag pattern structure as an embodiment according to the present invention;

도 4는 본 발명에 따른 다른 실시예로서, 지그재그 패턴 구조를 갖는 터치스크린패널을 A-A'선방향으로 절단한 면(바탕면 : ITO PC 또는 ITO 유리판)을 나타내는 단면도;       4 is a cross-sectional view showing a surface (base surface: ITO PC or ITO glass plate) cut in the direction A-A 'of a touch screen panel having a zigzag pattern structure as another embodiment according to the present invention;

도 5는 도 3 및 도 4의 도면에서 에칭(etching)부를 형성시킨 것을 나타낸 평면도;FIG. 5 is a plan view showing an etching part formed in the drawings of FIGS. 3 and 4;

도 6는 도 3에서 에칭(etching)부를 형성시킨 상태를 나타낸 단면도; FIG. 6 is a cross-sectional view illustrating a state in which an etching part is formed in FIG. 3; FIG.

도 7은 도 4에서 에칭(etching)부를 형성시킨 상태를 나타낸 단면도에 관한 것이다.FIG. 7 is a cross-sectional view illustrating a state in which an etching part is formed in FIG. 4.

* 도면의 주요부분에 대한 부호의 설명 *Explanation of symbols on the main parts of the drawings

100 : 터치스크린패널 10 : 상부 OCA층100: touch screen panel 10: upper OCA layer

20 : 상부 ITO 필름층 30 : 상부 실버패튼전극20: upper ITO film layer 30: upper silver pattern electrode

40 : 양면접착테이프층 50 : 하부 실버패튼전극40: double-sided adhesive tape layer 50: lower silver pattern electrode

60 : 하부 ITO 필름층 61 : ITO층60: lower ITO film layer 61: ITO layer

62 : PET 필름층 63 : 에칭부 62: PET film layer 63: etching portion

70 : 하부 OCA층 80 : 플라스틱 PC 또는 강화유리 보강판70: lower OCA layer 80: plastic PC or tempered glass reinforcement plate

81 : ITO PC 또는 ITO 유리판81: ITO PC or ITO Glass Plate

Claims (11)

상부 OCA층, 상부 ITO 필름층, 상부 실버패튼전극, 양면접착테이프층, 하부 실버패튼전극, 하부 ITO 필름층, 하부 OCA층 및 플라스틱 PC 또는 강화유리 보강판의 순으로 적층된 구조로 이루어진 터치스크린패널에 있어서,Touch screen consisting of laminated structure of upper OCA layer, upper ITO film layer, upper silver pattern electrode, double-sided adhesive tape layer, lower silver pattern electrode, lower ITO film layer, lower OCA layer and plastic PC or tempered glass reinforcement plate In the panel, 상기 상부 실버패턴전극은 그 폭의 길이가 가시영역(View Area) 쪽으로 양면접착테이프층의 폭의 길이와 동일한 길이의 폭으로 적층되도록 하여 양면접착테이프층이 상부 ITO 필름층에 닿지 않도록 한 구조이고, The upper silver pattern electrode is structured such that the width of the double-sided adhesive tape layer does not touch the upper ITO film layer by stacking the width of the upper side of the double-sided adhesive tape layer in the same length as the width of the double-sided adhesive tape layer toward the view area. , 상기 하부 ITO필름층의 폭에 직교되는 방향으로 습식 식각(Wet Etching) 방식, 또는 건식 식각(Dry) 방식에 의해 에칭(etching)부를 형성시킨 것을 특징으로 하는 지그재그 패턴 구조를 갖는 터치스크린패널.A touch screen panel having a zigzag pattern structure, wherein an etching part is formed by a wet etching method or a dry etching method in a direction orthogonal to the width of the lower ITO film layer. 지그재그 패턴 구조를 갖는 터치스크린패널은 상부 OCA층, 상부 ITO 필름층, 상부 실버패튼전극, 양면접착테이프층, 하부 실버패튼전극 및 ITO PC 또는 ITO 유리판의 순으로 적층된 구조로 이루어진 터치스크린패널에 있어서,The touch screen panel having a zigzag pattern structure is a touch screen panel which is formed by stacking an upper OCA layer, an upper ITO film layer, an upper silver pattern electrode, a double-sided adhesive tape layer, a lower silver pattern electrode, and an ITO PC or ITO glass plate. In 상기 상부 실버패턴전극은 그 폭의 길이가 가시영역(View Area) 쪽으로 양면접착테이프층의 폭의 길이와 동일한 길이의 폭으로 적층되도록 하여 양면접착테이프층이 상부 ITO 필름층에 닿지 않도록 한 구조이고, The upper silver pattern electrode is structured such that the width of the double-sided adhesive tape layer does not touch the upper ITO film layer by stacking the width of the upper side of the double-sided adhesive tape layer in the same length as the width of the double-sided adhesive tape layer toward the view area. , 상기 ITO PC 또는 ITO 유리판의 폭에 직교되는 방향으로 습식 식각(Wet Etching) 방식, 또는 건식 식각(Dry) 방식에 의해 에칭(etching)부를 형성시킨 것을 특징으로 하는 지그재그 패턴 구조를 갖는 터치스크린패널.A touch screen panel having a zigzag pattern structure, wherein an etching part is formed by a wet etching method or a dry etching method in a direction orthogonal to the width of the ITO PC or the ITO glass plate. 삭제delete 삭제delete 삭제delete 제 1항에 있어서,The method of claim 1, 상기 하부 ITO필름층은 PET 필름층이 노출되는 위치까지 에칭시키는 것을 특징으로 하는 지그재그 패턴 구조를 갖는 터치스크린패널.The lower ITO film layer is a touch screen panel having a zigzag pattern structure, characterized in that the etching to the position where the PET film layer is exposed. 삭제delete 제 1항에 있어서,The method of claim 1, 상기 상부 ITO 필름층 또는 하부 ITO 필름층의 ITO는 투명도전막으로 대체할 수 있는 것을 특징으로 하는 지그재그 패턴 구조를 갖는 터치스크린패널.Touch screen panel having a zigzag pattern structure, characterized in that the ITO of the upper ITO film layer or the lower ITO film layer can be replaced by a transparent conductive film. 제 1항에 있어서,The method of claim 1, 상기 실버패튼전극은 실버의 대체소재로서 백금, 구리, 알루미늄과 같은 소재를 사용하거나 또는 폴리아닐린, 폴리아세틸렌, 폴리피롤, 폴리티오펜, 폴리-3-알킬티오펜, 폴리페닐렌 설파이드, 폴리퓨란, 폴리티에닐렌비닐렌,폴리다이에틸렌의 전도성 고분자 화합물로 이루어진 군에 1종을 선택하여 전극을 형성시키는 것을 특징으로 하는 지그재그 패턴 구조를 갖는 터치스크린패널.The silver patternon electrode may be made of a material such as platinum, copper, or aluminum as an alternative material of silver, or polyaniline, polyacetylene, polypyrrole, polythiophene, poly-3-alkylthiophene, polyphenylene sulfide, polyfuran, poly A touch screen panel having a zigzag pattern structure, wherein an electrode is formed by selecting one kind from a group consisting of a conductive polymer compound of thienylenevinylene and polydiethylene. 제 9항에 있어서,The method of claim 9, 상기 실버패튼전극은 실버 또는 백금, 구리, 알루미늄과 같은 소재를 사용하거나 또는 폴리아닐린, 폴리아세틸렌, 폴리피롤, 폴리티오펜, 폴리-3-알킬티오펜, 폴리페닐렌 설파이드, 폴리퓨란, 폴리티에닐렌비닐렌,폴리다이에틸렌의 전도성 고분자 화합물로 이루어진 군에 1종을 선택하여 인쇄 또는 증착의 방법으로 전극을 형성하는 것을 특징으로 하는 지그재그 패턴 구조를 갖는 터치스크린패널.The silver patternon electrode may be made of silver or platinum, copper, aluminum, or polyaniline, polyacetylene, polypyrrole, polythiophene, poly-3-alkylthiophene, polyphenylene sulfide, polyfuran, polythienylenevinyl Touch screen panel having a zigzag pattern structure, characterized in that the electrode is formed by a method of printing or deposition by selecting one of the group consisting of a conductive polymer compound of lene, polydiethylene. 제 1항에 있어서,The method of claim 1, 상기 양면접착테이프층은 양면접착테이프의 대체소재로서, 접착제를 사용하여 인쇄하여 층을 형성시키는 것을 특징으로 하는 지그재그 패턴 구조를 갖는 터치스크린패널.The double-sided adhesive tape layer is a substitute material for the double-sided adhesive tape, the touch screen panel having a zigzag pattern structure, characterized in that to form a layer by printing using an adhesive.
KR1020090087243A 2009-09-15 2009-09-15 Touchscreen panel having zigzag pattern design KR101079190B1 (en)