KR101074368B1 - The nail file and that manufacturing method - Google Patents

The nail file and that manufacturing method Download PDF

Info

Publication number
KR101074368B1
KR101074368B1 KR1020090026317A KR20090026317A KR101074368B1 KR 101074368 B1 KR101074368 B1 KR 101074368B1 KR 1020090026317 A KR1020090026317 A KR 1020090026317A KR 20090026317 A KR20090026317 A KR 20090026317A KR 101074368 B1 KR101074368 B1 KR 101074368B1
Authority
KR
South Korea
Prior art keywords
polishing
tempered glass
nail
nail polishing
manufacturing
Prior art date
Application number
KR1020090026317A
Other languages
Korean (ko)
Other versions
KR20100107940A (en
Inventor
이광영
Original Assignee
(주)옵토라인
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by (주)옵토라인 filed Critical (주)옵토라인
Priority to KR1020090026317A priority Critical patent/KR101074368B1/en
Publication of KR20100107940A publication Critical patent/KR20100107940A/en
Application granted granted Critical
Publication of KR101074368B1 publication Critical patent/KR101074368B1/en

Abstract

본 발명은 손톱 연마용 줄 제조방법에 관한 것으로서, 종래에는 금속제에 연마용 해칭홈을 형성하거나 또는 표면에 연마용 가루를 부착시킨 두 가지의 형태가 대표적이었으나 그 수명이 한정적이고 청소가 용이하지 않았던 문제점을 해결하기 위하여 개발된 것으로;The present invention relates to a method for manufacturing a nail polishing file. In the related art, two types in which an abrasive hatching groove is formed on a metal or an abrasive powder is attached to a surface thereof are typical, but their lifespan is limited and not easy to clean. Developed to solve the problem;

일 끝단은 그 폭이 좁아지는 테이퍼부가 형성되고, 상면 또는 저면에는 연마을 위한 가공면이 형성된 긴 판 형상의 몸체로 이루어지는 손톱 연마용 줄에 있어서; 상기 몸체는 강화유리로 이루어지며; 상기 가공면은 그 경계면이 단턱지게 형성되는 미세한 원형의 홈부가 장방형의 배열로 다수 형성됨을 특징으로 하는 손톱 연마용 줄 및; One end is provided with a tapered portion that is narrow in width, the upper or lower surface in the nail polishing string consisting of a long plate-shaped body formed with a processing surface for polishing; The body is made of tempered glass; The processing surface is a nail polishing file, characterized in that a plurality of fine circular grooves are formed in a rectangular arrangement in which the boundary surface is stepped;

강화유리판에 미세한 원이 장방형으로 배열된 패턴을 원을 제외한 부분을 부식을 방지하는 방식액으로 포토 마스킹하는 포토 마스킹단계와; 부식액에 의하여 원형의 홈부를 형성하는 에칭단계와; 필요한 형상으로 강화유리를 절단하는 절단단계와; 절단된 손톱 연마용 줄을 세척하는 세척단계의 일련의 단계가 연속적으로 이루어짐을 특징으로 하는 손톱 연마용 줄 제조방법에 관한 것이다.A photo masking step of photomasking the pattern in which the fine circles are arranged in a rectangular shape on the tempered glass plate with an anticorrosive solution to prevent corrosion except for the circle; An etching step of forming a circular groove part by the corrosion solution; Cutting step of cutting the tempered glass to the required shape; The present invention relates to a method for manufacturing a nail polishing string, characterized in that a series of steps of washing the cut nail polishing string are continuously performed.

손톱, 연마, 줄 Nails, polishing, files

Description

손톱 연마용 줄 제조방법{The nail file and that manufacturing method}The nail file and that manufacturing method

본 발명은 손톱 연마용 줄 제조방법에 관한 것으로서, 좀더 상세하게 설명하면 내마모성이 우수한 강화유리를 사용하여 제조함으로 내구성이 뛰어나고 세척이 용이하며 생산 단가가 저렴한 효과가 있는 손톱 연마용 줄 제조방법에 관한 것이다.The present invention relates to a method for manufacturing a nail polishing file, and more specifically, to a method for manufacturing a nail polishing file having excellent durability and easy cleaning and low production cost by manufacturing using tempered glass having excellent wear resistance. will be.

손톱을 연마하는 줄은 처음에는 쇠로 이루어진 얇고 긴 판의 형상을 가지고 일면에는 해칭홈이 형성되어 있는 형태가 대부분이었다.At first, the file was polished to form a thin, long plate made of iron, and hatching grooves were formed on one side.

이러한 방식의 연마용 줄의 경우 지금은 그 수가 많이 줄었지만 손톱깎기에서 그 형태를 확인할 수 있으나 이는 사용하다 보면 줄눈이라고도 불리우는 이러한 해칭홈에 이물질이 쉽게 끼어서 연마효과가 떨어지는 단점이 있었다.In the case of this type of abrasive file, the number is reduced a lot now, but the shape of the nail clipper can be confirmed, but this has a disadvantage in that the abrasive effect is easily caught due to foreign matter easily inserted into these hatching grooves, also called joints.

이를 방지하기 위하여 솔로 세척하는 방법이 있으나 줄눈을 형성하는 방법이 화학적 부식에 의한 방법으로 그 표면이 고르지 않아 쉽게 녹이 쓰는 문제점 때문에 세척또한 용이하지 않는 문제점이 있다.In order to prevent this, there is a method of washing with a brush, but the method of forming a joint is a method due to chemical corrosion, so the surface is uneven, so there is a problem that the washing is not easy because of the problem of easy rust.

다른 방식의 손톱 연마용 줄은 스틱형으로 이루어져 쿠션의 역할을 하는 쿠 션층과 그 위에 연마포를 붙여 이루어진다.The other method of nail polishing file is made of a stick shape, and is made of a cushion layer serving as a cushion and an abrasive cloth thereon.

이러한 방식의 경우 연마 능력은 전술한 예와 비교하면 매우 뛰어나며 연마정도를 거친 것부터 광택을 내는 용도에 이르기까지 세분화하여 제조할 수 있는 뛰어난 기능성을 가지고 있다.In this case, the polishing ability is very excellent compared to the above-described examples, and has excellent functionality that can be manufactured by subdividing from the degree of polishing to the use of the gloss.

하지만 부착된 연마포가 떨어지기 쉽고 내구성이 극히 짧은 단점을 가지고 있다.However, the attached abrasive cloth is easy to fall off and has an extremely short durability.

본 발명은 상기와 같은 문제점을 해결하기 위하여 개발된 것으로서, 그 목적은 내구성이 우수하면서도 연마능력이 뛰어난 손톱 연마용 줄 및 그 제조방법을 개발하는 것이다.The present invention has been developed to solve the above problems, the object of the present invention is to develop a nail polishing file and a method for manufacturing the nail having excellent durability and excellent polishing ability.

또한 물로도 용이하게 세척할 수 있는 손톱 연마용 줄 및 그 제조방법을 개발하는 것이다.In addition, it is to develop a nail polishing file and a method of manufacturing the same that can be easily washed with water.

상기와 같은 목적을 달성하기 위하여 본 발명은 일 끝단은 그 폭이 좁아지는 테이퍼부가 형성되고, 상면 또는 저면에는 연마을 위한 가공면이 형성된 긴 판 형상의 몸체로 이루어지는 손톱 연마용 줄에 있어서;In order to achieve the above object, the present invention has a tapered portion of which one end is narrowed in width, the upper or lower surface in the nail polishing string consisting of a long plate-shaped body formed with a processing surface for polishing;

상기 몸체는 강화유리로 이루어지며;The body is made of tempered glass;

상기 가공면은 그 경계면이 단턱지게 형성되는 미세한 원형의 홈부가 장방형의 배열로 다수 형성됨을 특징으로 한다.The processing surface is characterized in that a plurality of fine circular grooves in which the interface is formed stepwise in a rectangular arrangement.

아울러, 상기 홈부의 직경은 50~100㎛로 형성되고 인접한 홈부와의 간격은 100~150㎛로 이루어짐을 특징으로 한다.In addition, the groove portion has a diameter of 50 ~ 100㎛ and the interval with the adjacent groove portion is characterized in that made of 100 ~ 150㎛.

또한, 강화유리판에 미세한 원이 장방형으로 배열된 패턴을 원을 제외한 부분을 부식을 방지하는 방식액으로 포토 마스킹하는 포토 마스킹단계와;In addition, the photo masking step of photo-masking the pattern in which the fine circles are arranged in a rectangular shape on the tempered glass plate with the anticorrosive solution to prevent corrosion except the circle;

부식액에 의하여 원형의 홈부를 형성하는 에칭단계와;An etching step of forming a circular groove part by the corrosion solution;

필요한 형상으로 강화유리를 절단하는 절단단계와;Cutting step of cutting the tempered glass to the required shape;

절단된 손톱 연마용 줄을 세척하는 세척단계의 일련의 단계가 연속적으로 이루어짐을 특징으로 한다.It is characterized in that a series of steps of the washing step for cleaning the cut nail polish string is made in succession.

아울러, 상기 포토 마스킹 단계에서는 원의 직경을 50~100㎛로 형성되고 인접한 원과의 간격은 100~150㎛로 형성함을 특징으로 한다.In addition, the photo masking step is characterized in that the diameter of the circle is formed to 50 ~ 100㎛ and the interval with the adjacent circle is formed to 100 ~ 150㎛.

상술한 바와 같이 본 발명은 내마모성이 우수한 강화유리를 사용하여 장기간 사용하더라도 마모가 되지 않아 연마능력은 그대로 유지되면서도 내구성이 뛰어난 효과가 있다.As described above, the present invention does not wear even when used for a long time by using tempered glass having excellent abrasion resistance, and thus has excellent durability while maintaining polishing ability.

또한 부식되지 않는 강화유리로 줄을 제조하여 홈에 이물질이 끼었을 경우에도 용이하게 세척하여 사용할 수 있는 효과가 있다.In addition, since the rope is made of tempered glass that does not corrode, there is an effect that it can be easily washed and used even when foreign matter is caught in the groove.

이에 본 발명의 구성을 첨부된 도면에 의하여 당업자가 용이하게 이해하고 재현할 수 있도록 상세하게 설명하면 다음과 같다.Accordingly, the configuration of the present invention will be described in detail with reference to the accompanying drawings so that those skilled in the art can easily understand and reproduce.

도 1은 본 발명의 일 실시 예에 따른 사시도이고, 도 2는 본 발명의 일 실시 예에 따른 평면도이며, 도 3은 본 발명의 일 실시 예에 따른 단면도이고, 도 4는 본 발명의 일 실시 예에 따른 사용상태도로서, 1 is a perspective view according to an embodiment of the present invention, Figure 2 is a plan view according to an embodiment of the present invention, Figure 3 is a cross-sectional view according to an embodiment of the present invention, Figure 4 is an embodiment of the present invention As a state diagram according to the example,

일 끝단은 그 폭이 좁아지는 테이퍼부(1)가 형성되고, 상면 또는 저면에는 연마을 위한 가공면(2)이 형성된 긴 판 형상의 몸체(3)로 이루어지는 손톱 연마용 줄에 있어서;One end is provided with a tapered portion (1) is narrow in its width, the nail surface for the nail consisting of a long plate-shaped body (3) formed on the upper surface or the bottom surface for processing the polishing (2);

상기 몸체(3)는 강화유리로 이루어지며;The body 3 is made of tempered glass;

상기 가공면(2)은 그 경계면이 단턱지게 형성되는 미세한 원형의 홈부(21)가 장방형의 배열로 다수 형성됨을 특징으로 하는 손톱 연마용 줄을 나타내었다.The processing surface (2) showed a nail polishing string, characterized in that a plurality of fine circular groove portions 21 whose boundaries are formed stepwise are formed in a rectangular arrangement.

본원의 경우 종래 연속된 선의 형태 또는 그 선이 교차된 형태와는 다르게 원형의 미세한 홈이 다수 형성되는 형상을 가지고 있는 것이 특징이다.In the case of the present application, unlike the form of a conventional continuous line or the form in which the line is crossed is characterized in that it has a shape in which a plurality of circular fine grooves are formed.

또한 재질로는 강화유리를 사용한 것을 그 특징으로 한다.In addition, the material is characterized in that the use of tempered glass.

이러한 강화유리는 강도가 우수하면서도 마모가 잘되지 않는 특성을 가지고 있으며 단턱지게 형성할 경우 그 모서리가 매우 날카로워 연마의 효과가 뛰어난 효과를 가지고 있다.Such tempered glass has excellent strength but is not abrasion-resistant, and when it is formed steppedly, its edge is very sharp and has an excellent effect of polishing.

따라서 종래의 연마용 줄과 비교하면 우수한 연마능력과 내구성을 가지게 되는 것이다.Therefore, compared with the conventional polishing file, it will have excellent polishing ability and durability.

보다 구체적인 실시 예로는 상기 홈부(21)의 직경은 50~100㎛로 형성되고 인접한 홈부와의 간격은 100~150㎛로 형성하면 종래 가장 많이 사용되던 손톱 연마용 줄과 연마 능력 및 연마면의 거칠기가 유사한 특성을 가진다.In a more specific embodiment, the groove 21 has a diameter of 50 to 100 μm, and an interval between adjacent grooves is 100 to 150 μm. Has similar characteristics.

도 5는 본 발명의 일 실시 예에 따른 블록도로서, 전술한 제품을 만들기 위한 방법은 강화유리판에 미세한 원이 장방형으로 배열된 패턴을 원을 제외한 부분 을 부식을 방지하는 방식액으로 포토 마스킹하는 포토 마스킹단계와;Figure 5 is a block diagram according to an embodiment of the present invention, the method for making the above product is to mask the portion of the pattern except the circle in the pattern of fine circles arranged in a rectangular glass on the tempered glass plate with a corrosion-resistant solution to prevent corrosion A photo masking step;

부식액에 의하여 원형의 홈부를 형성하는 에칭단계와;An etching step of forming a circular groove part by the corrosion solution;

필요한 형상으로 강화유리를 절단하는 절단단계와;Cutting step of cutting the tempered glass to the required shape;

절단된 손톱 연마용 줄을 세척하는 세척단계의 일련의 단계가 연속적으로 이루어짐으로 제조된다.A series of steps of a washing step for cleaning the cut nail polish string is made in succession.

이러한 방법의 가장 큰 장점은 상기 포토 마스킹단계과 에칭단계를 넓은 판 형상의 강화유리에서 수행하도록 하고 필요한 제품은 그 후에 절단하여 다수 형성하는 것으로 생산성이 매우 뛰어나며 기존의 제품과 비교하면 단가도 대폭 줄어들어 저렴하고도 우수한 제품을 공급할 수 있다.The biggest advantage of this method is that the photo masking step and the etching step are performed in a wide plate-shaped tempered glass, and the necessary products are cut afterwards to form a large number, which is very productive, and the unit cost is significantly reduced compared to existing products. It can supply excellent products.

또 홈부를 형성하는 단계에서는 전술한 실시 예와 같이 상기 포토 마스킹 단계에서는 원의 직경을 50~100㎛로 형성되고 인접한 원과의 간격은 100~150㎛로 형성하고 있다.In the step of forming the groove portion, as in the above-described embodiment, in the photo masking step, the diameter of the circle is formed to be 50 to 100 μm, and the distance between adjacent circles is formed to be 100 to 150 μm.

또한 통상의 지식을 가진자라면 동일한 배열로 이를 형성하지 않고 점차 조밀해지는 배열로 홈부를 형성하여 부분적으로 연마 능력이 차이가 나는 제품의 제조를 용이하게 할 수 있을 것이다.In addition, those skilled in the art will be able to facilitate the manufacture of products having partial polishing ability by forming grooves in an increasingly dense arrangement without forming them in the same arrangement.

도 1은 본 발명의 일 실시 예에 따른 사시도1 is a perspective view according to an embodiment of the present invention

도 2는 본 발명의 일 실시 예에 따른 평면도2 is a plan view according to an embodiment of the present invention;

도 3은 본 발명의 일 실시 예에 따른 단면도3 is a cross-sectional view according to an embodiment of the present invention.

도 4는 본 발명의 일 실시 예에 따른 사용상태도4 is a state diagram used in accordance with an embodiment of the present invention

도 5는 본 발명의 일 실시 예에 따른 블록도5 is a block diagram according to an embodiment of the present invention.

<도면 중 주요 부분에 대한 부호의 설명><Explanation of symbols for main parts of the drawings>

1 : 테이퍼부1: Taper part

2 : 가공면2: machining surface

21 : 홈부     21: groove

3 : 몸체3: body

Claims (4)

삭제delete 삭제delete 강화유리판에 미세한 원이 장방형으로 배열된 패턴을 원을 제외한 부분을 부식을 방지하는 방식액으로 포토 마스킹하는 포토 마스킹단계와;A photo masking step of photomasking the pattern in which the fine circles are arranged in a rectangular shape on the tempered glass plate with an anticorrosive solution to prevent corrosion except for the circle; 부식액에 의하여 원형의 홈부를 형성하는 에칭단계와;An etching step of forming a circular groove part by the corrosion solution; 필요한 형상으로 강화유리를 절단하는 절단단계와;Cutting step of cutting the tempered glass to the required shape; 절단된 손톱 연마용 줄을 세척하는 세척단계의 일련의 단계가 연속적으로 이루어짐을 특징으로 하는 손톱 연마용 줄 제조방법.A method of manufacturing a nail polishing file, characterized in that a series of steps of washing step for cleaning the cut nail polishing file is performed continuously. 제 3항에 있어서, 상기 포토 마스킹 단계에서는 원의 직경을 50~100㎛로 형 성되고 인접한 원과의 간격은 100~150㎛로 형성함을 특징으로 하는 손톱 연마용 줄 제조방법.4. The method of claim 3, wherein in the photomasking step, the diameter of the circle is formed in a range of 50 to 100 µm and the distance from the adjacent circle is formed in a range of 100 to 150 µm.
KR1020090026317A 2009-03-27 2009-03-27 The nail file and that manufacturing method KR101074368B1 (en)