KR100222495B1 - Making method for binding the upper of shoes - Google Patents

Making method for binding the upper of shoes Download PDF

Info

Publication number
KR100222495B1
KR100222495B1 KR1019970020887A KR19970020887A KR100222495B1 KR 100222495 B1 KR100222495 B1 KR 100222495B1 KR 1019970020887 A KR1019970020887 A KR 1019970020887A KR 19970020887 A KR19970020887 A KR 19970020887A KR 100222495 B1 KR100222495 B1 KR 100222495B1
Authority
KR
South Korea
Prior art keywords
lower plate
plug
suture
sealing
wrinkled
Prior art date
Application number
KR1019970020887A
Other languages
Korean (ko)
Other versions
KR970058614A (en
Inventor
송성기
Original Assignee
송성기
주식회사거성물산
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 송성기, 주식회사거성물산 filed Critical 송성기
Priority to KR1019970020887A priority Critical patent/KR100222495B1/en
Publication of KR970058614A publication Critical patent/KR970058614A/en
Application granted granted Critical
Publication of KR100222495B1 publication Critical patent/KR100222495B1/en

Abstract

본 발명은 구두의 하판 상부와 플러그를 주름지게 봉합함에 있어서, 봉합시 하판의 주름이 형성되는 부위에 미리 주름선을 성형시켜 주름을 쉽게 잡아가며 하판과 플러그를 봉합시키도록 구두제조용 하판의 주름선 성형방법에 관한 것이다.In the present invention, the upper and lower plate of the shoe pleatly suture, the wrinkles of the lower plate for shoe manufacturing so as to sew the lower plate and the plug easily by forming a wrinkle line in advance to the portion where the pleats of the lower plate is formed when sewing It relates to a molding method.

이러한 본 발명은 구두의 하판상부에 플러그를 봉합하여 하판 봉합부위에 주름을 형성시킴에 있어서, 하판의 프레스 재단 후 하판의 봉합구멍과 봉합구멍사이마다 일정깊이 및 길이를 갖는 주름선을 압착 성형시킴으로써 이루어지는 것으로 주름을 잡는데 따른 작업상의 어려움을 해소하고 시간의 낭비를 줄인 것이다.In the present invention, the plug is sewn on the upper plate of the shoe to form a pleat on the lower plate suture, and after press-cutting the lower plate, a crimp line having a predetermined depth and length is press-molded between the sealing hole and the sealing hole of the lower plate. It eliminates the difficulties of crimping and reduces the waste of time.

Description

구두제조용 하판의 주름선 성형방법Crease line forming method of lower board for shoe manufacturing

본 발명은 구두의 하판 상부를 주름지게 하여 플러그를 봉합함에 있어서, 봉합시 하판의 주름이 형성되는 부위에 미리 주름선을 성형시켜 주름을 쉽게 잡아가며 하판과 플러그를 봉합시키도록 하는 구두제조용 하판의 주름선 성형방법에 관한 것이다.In the present invention, when the upper part of the lower plate of the shoe is wrinkled and the plug is closed, the lower plate for shoe manufacturing which sutures the lower plate and the plug to easily grip the wrinkles by forming a wrinkle line in advance where the wrinkles of the lower plate are formed. It relates to a wrinkle line forming method.

하판상부를 주름지게 하여 플러그를 봉합하는 기존의 주름구두는 제1도에 도시된 바와 같이 구두의 외관을 결정하는 하판(10)과, 상기 하판(10)상부에 봉하되어 발등을 덮어주는 플러그(20)와, 하판(10)하부에 결속되어 밑면을 구성하는 밑판(30)으로 구성되어 있다.Existing wrinkled shoes for closing the upper plate to pleat the plug is the lower plate 10 to determine the appearance of the shoe as shown in Figure 1, and the plug is sealed on the lower plate 10 to cover the foot ( 20) and a bottom plate 30 that is bound to the bottom of the bottom plate 10 and constitutes a bottom surface.

이러한 구성의 기존 주름구두 제조공정은 다음과 같다.The existing wrinkled shoe manufacturing process of this configuration is as follows.

1) 하판(10)과 플러그(20) 준비과정1) Preparation process of the lower plate 10 and the plug 20

하판(10)과 플러그(20)는 가죽원단을 프레스 재단하여 제 2 및 제 3 과 같은 형태로 준비한다.The lower plate 10 and the plug 20 are prepared by press cutting the leather fabric into the second and third shapes.

이때 하판(10)과 플러그(20)에는 봉합구멍(11)(21)이 함께 천공되며 플러그(20)를 하판(10)에 봉합시키기 위해 하판(10)과 플러그(20)에 천공되는 봉합구멍(11)(21)의 수는 동일하게 하되 그 사이간격만 틀리게 한다.In this case, the lower plate 10 and the plug 20 are perforated with the sealing holes 11 and 21, and the sealing hole perforated in the lower plate 10 and the plug 20 to seal the plug 20 to the lower plate 10. The number of (11) (21) should be the same but only the gap between them is wrong.

2) 내피 준비과정2) Endothelial Preparation

하판(10)과 플러그(20)의 내측에 접착제로 접착되는 내피도 프레스 재단하여 준비하되 봉합부위를 고려하여 내피는 하판(10)과 플러그(20)보다는 면적이 좁게된다.The endothelial is adhered to the inner side of the lower plate 10 and the plug 20 by press-cutting preparation, but the area is narrower than the lower plate 10 and the plug 20 in consideration of the suture.

3) 봉합부위 절단공정3) Cutting process of suture

가죽과 가죽이 서로 맞대어 봉합되는 부위를 내측에서 약간씩 깍아주어 두개의 가죽이 맞닿는 봉합부위의 두께가 두꺼워지는 것을 방지한다.The skin and the skin where the leather is stitched against each other slightly cut away from the inside to prevent the thickening of the seal between the two leather contact.

4) 외피와 내부 봉합과정4) Outer shell and internal suture process

준비된 외피의 내측에 내피를 접착제로 접착시킨다.The inner skin is glued to the inside of the prepared skin.

5) 하판(10)봉합과정5) Bottom plate (10) stitching process

하판(10)의 뒷축부위와 전면상부에 형성되는 봉합부위를 재봉질하여 봉합처리한다.The suture portion formed on the rear shaft portion and the front upper portion of the lower plate 10 is sewn by sewing.

6) 하판(10)과 플러그(20)봉합과정6) The bottom plate 10 and plug 20 sealing process

하판(10)의 봉합구멍(11)과 플러그(20)의 봉합구멍(21)을 맞추어가며 수작업으로 재봉실을 이용하여 하판(10)과 플러그(20)를 결합시킨다.The sewing plate 11 of the lower plate 10 and the sealing hole 21 of the plug 20 are aligned, and the lower plate 10 and the plug 20 are coupled by using a sewing thread by hand.

이때 하판(10)의 봉합구멍(11)간격과 플러그(20)의 봉합구멍(21)간격이 서로 달라 하판(10)의 봉합구멍(11)사이마다 주름을 주어야만 하판(10)과 플러그(20)를 봉합시킬 수 있게 된다.At this time, the gap between the sealing hole 11 of the lower plate 10 and the sealing hole 21 of the plug 20 are different from each other, so that the lower plate 10 and the plug 20 have to be wrinkled between the sealing holes 11 of the lower plate 10. ) Can be sealed.

그러나 하판(10)을 이루는 가죽을 봉합구멍(11)이 나타날때 마다 주름주기 위해서는 송곳등으로 일일이 주름부위를 잡아가며 봉합시켜야 하므로 작업이 어렵고 작업시간 또한 많이 걸리게 되어 주름구두 제조시 가장 큰 어려움으로 나타나고 있다.However, in order to wrinkle the leather constituting the lower plate 10 every time the suture hole 11 appears, it must be sutured by holding the wrinkles with an awl and so on, which makes the work difficult and takes a lot of working time. Appearing.

7) 하판(10)과 밑판(30)결속과정7) Bottom plate (10) and bottom plate (30) binding process

하판(10)하부에 밑판(30)을 결속시켜 구두를 제작하게 된다.The bottom plate 30 is bound to the bottom plate 10 to produce shoes.

이같이 주름구두의 일반적인 제작공정을 살펴본 바와 같이 어렵고 시간이 많이 소모되는 공정이 6)번 공정에서의 하판(10)에 주름을 잡아주는 공정이다.As described in the general manufacturing process of the wrinkled shoes as described above, the difficult and time-consuming process is to wrinkle the lower plate 10 in step 6).

본 발명은 주름구두 제조에 있어서, 하판의 주름이 잡힐 부위에 미리 주름선을 성형시킨 후 하판과 플러그를 봉합시키도록 하므로써 주름선에 의해 자연스럽게 주름이 잡혀지게 되어 주름을 잡아주는데 따른 어려움과 시간낭비를 줄이도록 한 것이다.In the present invention, in the manufacture of wrinkled shoes, by forming a wrinkle line in the wrinkled portion of the lower plate in advance to seal the lower plate and the plug by being wrinkled naturally by the wrinkle line is difficult and time wasted due to the wrinkles To reduce the

이러한 본 발명은 구두의 하판상부에 플러그를 봉합하여 하판 봉합부위에 주름을 형성시킴에 있어서, 하판의 프레스 재단 후 하판의 봉합구멍과 봉합구멍 사이마다 일정깊이 및 길이를 갖는 주름선을 압착 성형시킴으로써 이루어지며 하판의 주름형성시 상기된 주름선이 밀리면서 자연스럽게 주름이 형성되므로 하판과 플러그 봉합시 봉합구멍마다 하판에 주름을 잡아주는데 따른 작업상의 어려움을 해소하고 시간의 낭비를 줄인 것이다.In the present invention, the plug is sewn on the upper plate of the shoe to form a pleat on the lower plate suture, and after press-cutting the lower plate, by crimping a wrinkle line having a predetermined depth and length between the sewing hole and the sewing hole of the lower plate. When wrinkles are formed on the bottom plate, the wrinkles are pushed naturally, and thus wrinkles are naturally formed, thereby reducing the waste of time and eliminating the difficulty of wrinkling the bottom plate for each suture hole when sealing the bottom plate and the plug.

제1도는 주름 구두의 사시도.1 is a perspective view of wrinkled shoes.

제2도는 재단된 상태의 하판 설명도.2 is an explanatory bottom view of the cut state.

제3도는 재단된 상태의 플러그 평면도.3 is a plan view of the plug in the cut state.

제4도는 제1도의 요부확대도.4 is an enlarged view of the main part of FIG.

제5도는 주름선 성형 금구 사시도.5 is a perspective view of a wrinkle forming bracket.

제6도는 하판에 주름선이 성형된 상태도.6 is a state in which the wrinkled line formed on the lower plate.

제7도는 제6도의 A-A선 단면도.7 is a cross-sectional view taken along the line A-A of FIG.

제8도는 봉합부위를 깍아준 상태의 하판 저면도.8 is a bottom view of the lower plate in a state of cutting the sutures.

제9도는 플러그 봉합 이전의 하판 상태도.9 is a bottom plate state before plug closure.

* 도면의 주요부분에 대한 부호의 설명* Explanation of symbols for main parts of the drawings

10 : 하판 11 : 봉합구멍10: lower plate 11: suture hole

12 : 주름선 20 : 플러그12: pleat 20: plug

21 : 봉합구멍 30 : 밑판21: seam 30: bottom plate

40 : 성형금구 41 : 눌림편40: forming tool 41: pressed piece

본 발명은 프레스 재단되고 봉합구멍(11)이 형성된 하판(10)에 봉합구멍(11)사이마다 일정길이와 깊이를 갖는 주름선(12)을 형성시킨 것으로 상기 주름선(12)은 눌림편(41)이 일정간격으로 형성된 성형금구(40)를 이용하여 압착 성형시키도록 한다.According to the present invention, a wrinkled line 12 having a predetermined length and depth is formed in each of the sealing holes 11 in the lower plate 10 having the press cut and the sealing holes 11 formed therein. 41) is press-molded using the molding bracket 40 formed at a predetermined interval.

이같이 주름선(12)이 성형된 하판(10)에 플러그(20)를 봉합시킴으로써 자연스럽게 주름이 형성되도록 하는 본 발명의 제작공정은 기존과 동일하며 다만 하판(10)에 주름선(12)을 성형시키는 공정이 추가된다.The fabrication process of the present invention to naturally form wrinkles by sealing the plug 20 to the lower plate 10 in which the wrinkle lines 12 are formed is the same as before, but the wrinkle lines 12 are formed on the lower plate 10. Is added.

이를 상세히 살펴본다.Look at this in detail.

1) 하판(10)과 플러그(20) 준비과정1) Preparation process of the lower plate 10 and the plug 20

원단가죽을 금형으로 프레스 재단하여 제2도, 제3도와 같은 하판(10)과 플러그(20)를 준비하되 하판(10)과 플러그(20)에는 동일숫자의 봉합구멍(11)(21)이 일정간격으로 천공된다.The fabric is press-cut into a mold to prepare the lower plate 10 and the plug 20 as shown in FIGS. 2 and 3, but the lower plate 10 and the plug 20 have the same number of suture holes 11 and 21. It is drilled at regular intervals.

즉 하판(10)의 봉합구멍(11)과 플러그(20)의 봉합구멍(21)수는 동일하나 다만 그 간격만 상이할 뿐이다.That is, the number of the sealing holes 11 of the lower plate 10 and the number of the sealing holes 21 of the plug 20 are the same, but only the gaps thereof are different.

2) 내피 준비과정2) Endothelial Preparation

하판(10)과 플러그(20) 내부에 부착되는 내피도 프레스 재단하여 준비한다.The inner skin attached to the lower plate 10 and the plug 20 is also prepared by press cutting.

3) 봉합부위 절단과정3) Cutting process of suture

제8도에 도시된 바와 같이 하판(10)의 내측 봉합부위(13)를 일정두께만큼 깍아내어 봉합시 두께가 두꺼워지는 것을 방지한다.As shown in FIG. 8, the inner sealing portion 13 of the lower plate 10 is scraped off by a predetermined thickness to prevent the thickness of the sealing from being thickened.

4) 외피와 내피 봉합과정4) outer skin and endothelial suture process

준비된 외피내측에 내피를 부착시킨다.Attach the endothelial to the prepared inner skin.

5) 하판(10)봉합과정5) Bottom plate (10) stitching process

하판(10)의 뒷굼치 부위 및 상호 봉합부위와 플러그(20)의 돌출부위 선단은 마무리 봉합한다.The back end of the lower plate 10 and the end portion of the mutual suture and the protruding portion of the plug 20 are finished suture.

6) 하판(10)과 플러그(20) 봉합과정6) The bottom plate 10 and plug 20 sewing process

플러그(20)의 외측으로 하판(10)의 선단부위를 감싸고 하판(10)과 플러그(20)의 봉합구멍(11)(21)을 맞추어가며 봉합사로 봉합한다.Wrap the tip portion of the lower plate 10 to the outside of the plug 20 and the suture hole 11 and 21 of the lower plate 10 and the plug 20 are aligned and sutured with a suture.

7) 하판(10)과 밑판(30) 결속과정7) Bonding process of bottom plate 10 and bottom plate 30

하판(10)하부에 밑판(30)을 결속 고정시킨다.The bottom plate 30 is fixed to the bottom of the bottom plate 10.

본 발명은 상기된 3번째 공정인 봉합부위 절단과정과 4번째 공정인 외피와 내피 봉합과정에서 선택적으로 주름선(12)을 형성시킨다.The present invention selectively forms a wrinkled line 12 in the process of cutting the suture site, the third process and the skin and endothelial suture process, the fourth process.

즉 주름선(12)은 하판(10)에 봉합부위(13)를 깍아주고 성형시키거나 내피를 접착시킨 후 성형시키게 되나 하판(10)에만 주름선(12)을 성형시키게 되므로 상기 공정 이외에 하판(10)을 봉합시키기 전의 어떤 공정에서 하판(10)에 주름선(12)을 성형시켜도 무방하다.That is, the wrinkled line 12 is formed by shaving and molding the suture site 13 on the lower plate 10 or by adhering the endothelium, but since the wrinkled line 12 is formed only on the lower plate 10, the lower plate 10 In the step before sealing 10), the wrinkled lines 12 may be formed on the lower plate 10.

하판(10)이 준비된 상태에서 성형금구(40)하부에 하판(10)을 놓고 성형금구(40)를 유압 또는 공압으로 압을 가하며 고주파 가열하면 하판(10)의 표면에는 눌림편(41)의 모양에 의해 제6도와 제7도에 도시된 바와 같이 주름선(12)이 성형된다.When the lower plate 10 is prepared, the lower plate 10 is placed under the molding tool 40, and the molding tool 40 is pressurized by hydraulic or pneumatic pressure and heated at a high frequency so that the surface of the lower plate 10 is pressed. By the shape, the wrinkled lines 12 are formed as shown in FIG. 6 and FIG.

여기서 주름선(12)은 정확히 봉합구멍(11)과 봉합구멍(11)사이에 성형되어야하고 주름선(12)의 길이는 눌림편(41)의 길이에 의해 결정되며 주름선(12)의 깊이는 성형금구(40)를 누르는 압에 의하여 결정되어진다.Here, the wrinkle line 12 should be exactly formed between the suture hole 11 and the suture hole 11 and the length of the wrinkle line 12 is determined by the length of the pressing piece 41 and the depth of the wrinkle line 12. Is determined by the pressing force of the molding tool 40.

이같이 하판(10)의 봉합구멍(11)사이마다 일정길이 및 깊이를 갖는 주름선(12)을 성형시킨 경우 하판(10)과 플러그(20)의 봉합구멍(11)(21)을 맞추어가며 봉합시키면 하판(10)에 형성된 주름선(12)에서 하판(10)이 자연스럽게 주름지어지게 되므로 기존과 같이 송곳등으로 주름을 잡아주어야 하는 어려움 없이 자연스럽게 주름이 잡히게 된다.As such, when the corrugated wire 12 having a predetermined length and depth is formed between each of the sealing holes 11 of the lower plate 10, the lower plate 10 and the sealing holes 11 and 21 of the plug 20 are fitted to each other. When the lower plate 10 is naturally wrinkled in the fold line 12 formed on the lower plate 10 will be wrinkled naturally without the difficulty of having to pleat with an awl or the like as before.

즉 봉합구멍(11)의 사이간격이 넓은 하판(10)과 봉합구멍(21)의 사이간격이 좁은 플러그(20)의 봉합구멍(11)(21)을 맞추어가며 봉합시킬 때 하판(10)의 주름이 잡힐 부위에 미리 주름선(12)을 성형시킴으로써 하판(10)과 플러그(20)의 봉합시 자연스럽게 주름선(12)에 의해 하판(10)에는 주름이 잡히게 된다.That is, the lower plate 10 of the lower plate 10 when the suture holes 11 and 21 of the plug 20 having a wide interval between the sealing holes 11 and the sealing hole 21 are fitted to each other while being stitched together. By forming the wrinkled line 12 in advance to the portion to be wrinkled, the lower plate 10 is naturally wrinkled by the wrinkled line 12 when the lower plate 10 and the plug 20 are closed.

따라서 별도로 주름을 잡아주기 위한 노력을 기울이지 않아도 되고 균일한 형태의 주름을 잡아줄 수 있어 제품의 품질을 향상시키게 된다.Therefore, it is not necessary to make an effort to pleat separately, and it is possible to grasp a uniform form of wrinkles, thereby improving the product quality.

본 발명은 주름구두의 하판에 천공된 봉합구멍 사이마다 미리 주름선을 성형시켜 플러그와의 봉합시 간단히 주름이 잡아지도록 하므로써 주름을 억지로 잡아줄때에 비하여 작업이 쉬워지고 작업시간 또한 크게 단축시킬 수 있는 것이다.The present invention by forming a wrinkle line in advance between the perforated stitching hole in the lower plate of the wrinkled shoe to be easily caught wrinkles when sutured with the plug, so that the operation is easier and the working time can be significantly shortened compared to when the wrinkle is forcibly held. will be.

Claims (1)

봉합구멍이 천공된 하판 상부에 동일갯수의 봉합구멍이 천공된 플러그를 각각의 봉합구멍을 맞추어가며 봉합시킴에 있어서, 하판의 봉합구멍과 봉합구멍 사이에 일정한 길이 및 깊이를 갖는 주름선을 형성시켜 봉합구멍의 사이간격이 다른 하판과 플러그를 봉합시킬 때 하판의 주름선에서 주름이 형성되게 하는 것을 특징으로 하는 구두 제조용 하판의 주름선 성형방법.In sealing the plugs with the same number of sealing holes in the upper part of the lower plate where the sealing holes are perforated to fit each sewing hole, a wrinkle line having a constant length and depth is formed between the sealing hole and the sealing hole of the lower plate. A method of forming a wrinkled line of a lower plate for shoe manufacturing, characterized in that wrinkles are formed in the lines of wrinkles of the lower plate when the gap between the suture holes and the lower plate is closed.
KR1019970020887A 1997-05-23 1997-05-23 Making method for binding the upper of shoes KR100222495B1 (en)