- JPS6487534A JPS6487534A JP24551887A JP24551887A JPS6487534A JP S6487534 A JPS6487534 A JP S6487534A JP 24551887 A JP24551887 A JP 24551887A JP 24551887 A JP24551887 A JP 24551887A JP S6487534 A JPS6487534 A JP S6487534A
- Authority
- JP
- Japan
- Prior art keywords
- glass body
- cations
- monovalent cations
- chemical durability
- incorporating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Surface Treatment Of Glass (AREA)
- Glass Compositions (AREA)
Abstract
PURPOSE:To prevent the surface of a glass body from being deteriorated and to improve chemical durability of the glass body by ion-exchanging monovalent cations of the surface of the glass body incorporating monovalent cations with bivalent cations and reducing the concn. of the monovalent cations. CONSTITUTION:A glass body incorporating monovalent cations is obtained by immersing e.g. a phosphate glass body incorporating 40mol.% Na2O and 32mol.% P2O5 in melted salt consisting of 40wt.% AgNO3 and 60wt.% KNO3 e.g. at 430 deg.C for 350hr. Then this glass body is immersed in melted salt incorporating bivalent cations consisting of e.g. 17wt.% Ba(NO3)2 and 83wt.% CsNO3 in a prescribed time and the monovalent cations existing within 20mum thickness of the surface are ion-exchanged with the bivalent cations and the concn. of the monovalent cations of the surface is reduced. Thereby the chemical durability of a functional glass body such as a refractive index distribution-type glass body is improved.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP24551887A JPS6487534A (en) | 1987-09-29 | 1987-09-29 | Method for improving chemical durability of glass body |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP24551887A JPS6487534A (en) | 1987-09-29 | 1987-09-29 | Method for improving chemical durability of glass body |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS6487534A true JPS6487534A (en) | 1989-03-31 |
Family
ID=17134875
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP24551887A Pending JPS6487534A (en) | 1987-09-29 | 1987-09-29 | Method for improving chemical durability of glass body |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6487534A (en) |
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH11503403A (en) * | 1996-02-07 | 1999-03-26 | サン−ゴバン ビトラージュ | Glass substrate treatment method |
JP2013238677A (en) * | 2012-05-11 | 2013-11-28 | Asahi Glass Co Ltd | Reflector |
JP2013238678A (en) * | 2012-05-11 | 2013-11-28 | Asahi Glass Co Ltd | Reflector |
CN107721195A (en) * | 2017-10-27 | 2018-02-23 | 福州瑞克布朗医药科技有限公司 | A kind of method for strengthening gear division devitrified glass physicochemical property |
CN108147681A (en) * | 2018-01-25 | 2018-06-12 | 中国科学院上海光学精密机械研究所 | A kind of laser glass ion exchange Enhancement Method |
Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5186512A (en) * | 1975-01-28 | 1976-07-29 | Mitsubishi Heavy Ind Ltd | SERAMITSUKUSUNOKYOKAHOHO |
JPS5628855A (en) * | 1979-08-17 | 1981-03-23 | Toyo Seikan Kaisha Ltd | Laminated bag* which can be sterilized by retort* having excellent stacking pressure resisting property |
JPS62100451A (en) * | 1985-10-28 | 1987-05-09 | Hoya Corp | Glass composition suitable to produce glass having refractive index gradient |
-
1987
- 1987-09-29 JP JP24551887A patent/JPS6487534A/en active Pending
Patent Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5186512A (en) * | 1975-01-28 | 1976-07-29 | Mitsubishi Heavy Ind Ltd | SERAMITSUKUSUNOKYOKAHOHO |
JPS5628855A (en) * | 1979-08-17 | 1981-03-23 | Toyo Seikan Kaisha Ltd | Laminated bag* which can be sterilized by retort* having excellent stacking pressure resisting property |
JPS62100451A (en) * | 1985-10-28 | 1987-05-09 | Hoya Corp | Glass composition suitable to produce glass having refractive index gradient |
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH11503403A (en) * | 1996-02-07 | 1999-03-26 | サン−ゴバン ビトラージュ | Glass substrate treatment method |
JP2013238677A (en) * | 2012-05-11 | 2013-11-28 | Asahi Glass Co Ltd | Reflector |
JP2013238678A (en) * | 2012-05-11 | 2013-11-28 | Asahi Glass Co Ltd | Reflector |
CN107721195A (en) * | 2017-10-27 | 2018-02-23 | 福州瑞克布朗医药科技有限公司 | A kind of method for strengthening gear division devitrified glass physicochemical property |
CN108147681A (en) * | 2018-01-25 | 2018-06-12 | 中国科学院上海光学精密机械研究所 | A kind of laser glass ion exchange Enhancement Method |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
DE3729736C2 (en) | ||
IE810159L (en) | Alkali resistant glass fibres. | |
DE389713T1 (en) | METHOD FOR COATING WITH A BIOACTIVE HYDROXYAPATITE FILM. | |
GB1495125A (en) | Photochromic sheet glass compositions and articles | |
DE19615688A1 (en) | Glass substrate for magnetic disks | |
KR910016640A (en) | Colorless silver-containing glass by ion exchange, preparation method thereof and optical fiber device | |
GB1346747A (en) | Method for strengthening glass by ion exchange | |
US3773489A (en) | Chemically strengthened glass | |
JPS6487534A (en) | Method for improving chemical durability of glass body | |
GB1267387A (en) | Light-conducting glass fibres having a peripheral light-absorbent layer | |
IL40405A (en) | Process of colouring or modifying the colouration of a glass body containing reducing ions by diffusion | |
GB1475500A (en) | Ophthalmic glass compositions | |
JPS57196744A (en) | Surface treatment of glass containing alkali metal | |
JPS57134586A (en) | Production of joined body for electrolysis | |
EP0035241A1 (en) | Method for the activation of titanium surfaces | |
Sharaf et al. | FTIR spectral/structural investigation of the ion exchange/thermal treatment of silver ions into a silicate glass | |
DE3576491D1 (en) | METHOD FOR PRODUCING THE TIN DIOXIDE INTERFERENCE LAYER (S), IN PARTICULAR FROM HEAT-REFLECTING-COATED GLASS DISKS BY REACTIVE MAGNETRONIC SPRAYING AND WITH A TIN DIOXIDE LAYER MISSING ITSELF. | |
ES8303543A1 (en) | Phosphate coating process and composition. | |
ATE47536T1 (en) | FLUID CRACK CATALYST AND METHOD OF MANUFACTURE. | |
DE2900116C2 (en) | Process for increasing the chemical resistance of glass fibers | |
JPS57179055A (en) | Manufacture of refractive index distribution type lens | |
GB1242984A (en) | Method of treating a surface of a glass article | |
KR19990003413A (en) | Method of strengthening the front glass of cathode ray tube | |
GB917388A (en) | A method of treating glass to increase the tensile strength thereof and glass so treated | |
Kozmanyan | Relation between concentration and refractive index gradients in an ion-exchanged alkaline aluminoborosilicate glass |