JPS6487226A - Manufacture of hollow molded product - Google Patents
Manufacture of hollow molded productInfo
- Publication number
- JPS6487226A JPS6487226A JP62245563A JP24556387A JPS6487226A JP S6487226 A JPS6487226 A JP S6487226A JP 62245563 A JP62245563 A JP 62245563A JP 24556387 A JP24556387 A JP 24556387A JP S6487226 A JPS6487226 A JP S6487226A
- Authority
- JP
- Japan
- Prior art keywords
- molding die
- manufacture
- molded product
- density
- polyethylene
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To manufacture a hollow molded product of good surface gloss without lengthening molding cycle by using a parison of polyolefin resin as a blow molding die and also using a molding die constituted of a fluorine resin molded product for part or the whole of the molding die including the end of the upper inner surface. CONSTITUTION:A molding die constituted of a fluorine resin molded material covering part or the whole of the same including its end of the upper inner surface as a blow molding die to extrude a parison composed of polyolefin resin is used. As for polyolefin, polyethylene consisting of 30-90wt.% of high density polyethylene having 0.945g/cm<3> or more of density, and 0.01-3.0g/10min of melt index, and 70-10wt.% of a straight-chain low density or middle density polyethylene having 0.910-0.940g/cm<3> of density, 0.1-10.0g/10min of melt index and 6.0 or less of the ratio (Mw/Mn) between the weight-average mol. wt. Mw and the number-average mol. wt. Mn should be used to manufacture a polyethylene hollow molded material of particularly good surface gloss.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP62245563A JPH0617057B2 (en) | 1987-09-29 | 1987-09-29 | Hollow molded product manufacturing method |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP62245563A JPH0617057B2 (en) | 1987-09-29 | 1987-09-29 | Hollow molded product manufacturing method |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6487226A true JPS6487226A (en) | 1989-03-31 |
JPH0617057B2 JPH0617057B2 (en) | 1994-03-09 |
Family
ID=17135567
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP62245563A Expired - Lifetime JPH0617057B2 (en) | 1987-09-29 | 1987-09-29 | Hollow molded product manufacturing method |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPH0617057B2 (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2007223073A (en) * | 2006-02-21 | 2007-09-06 | Sekisui Chem Co Ltd | Extrusion mold and long article manufacturing method using the same |
Citations (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2820252A (en) * | 1954-10-18 | 1958-01-21 | Polymer Corp | Method of extrusion |
JPS5023462A (en) * | 1973-07-03 | 1975-03-13 | ||
JPS5882734A (en) * | 1981-11-12 | 1983-05-18 | Mitsui Petrochem Ind Ltd | Blow molding method for ethylene-alpha-olefin copolymer |
JPS60110421A (en) * | 1983-11-01 | 1985-06-15 | デユポン・カナダ・インコーポレーテツド | Die for extruding and molding polymer |
JPS6110432A (en) * | 1984-06-27 | 1986-01-17 | Mitsui Petrochem Ind Ltd | Manufacture of blow-molded container |
-
1987
- 1987-09-29 JP JP62245563A patent/JPH0617057B2/en not_active Expired - Lifetime
Patent Citations (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2820252A (en) * | 1954-10-18 | 1958-01-21 | Polymer Corp | Method of extrusion |
JPS5023462A (en) * | 1973-07-03 | 1975-03-13 | ||
JPS5882734A (en) * | 1981-11-12 | 1983-05-18 | Mitsui Petrochem Ind Ltd | Blow molding method for ethylene-alpha-olefin copolymer |
JPS60110421A (en) * | 1983-11-01 | 1985-06-15 | デユポン・カナダ・インコーポレーテツド | Die for extruding and molding polymer |
JPS6110432A (en) * | 1984-06-27 | 1986-01-17 | Mitsui Petrochem Ind Ltd | Manufacture of blow-molded container |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2007223073A (en) * | 2006-02-21 | 2007-09-06 | Sekisui Chem Co Ltd | Extrusion mold and long article manufacturing method using the same |
Also Published As
Publication number | Publication date |
---|---|
JPH0617057B2 (en) | 1994-03-09 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS55152735A (en) | Polyethylene composition | |
ES8300124A1 (en) | Polyethylene compositions for extrusion in particular for blow moulding. | |
ES448160A1 (en) | Blends of copolyesters and ethylene/carboxylic acid copolymers which are at least ten percent neutralized | |
EP0297363A3 (en) | High temperature resistant thermoplastic moulding masses with improved melt stability | |
DE3666926D1 (en) | Process for the preparation of blown film | |
ES485708A1 (en) | Polypropylene molding composition and process for its preparation | |
DE59707768D1 (en) | High molecular weight ethylene / propylene reactor blend with a broad molecular weight distribution | |
DE3376485D1 (en) | Process for producing a shaped article of beta-hydroxybutyrate polymer | |
ES2091289T3 (en) | POLYMERIC COMPOSITIONS. | |
ES2083430T3 (en) | COMPOSITIONS OF THERMOPLASTIC POLYMERS CONTAINING MODIFIERS OF THE RHEOLOGY OF THE MELTING MASS. | |
ES448159A1 (en) | Blends of copolyesters, ethylene/carboxylic acid copolymers and a polycarbodiimide | |
JPS55144045A (en) | Forming material containing styreneeacrylnitrile copolymer and ethylene oxide*propylene oxide triblock copolymer | |
JPS6487226A (en) | Manufacture of hollow molded product | |
JPS545713A (en) | Keyboard apparatus | |
AU7441887A (en) | Molding compositions providing improved surface characteristics | |
JPS5670044A (en) | Polystyrene resin composition for extrusion molding | |
JPS5379939A (en) | Blow molding resin composition | |
EP0417319A4 (en) | Blown polypropylene resin container | |
JPS53102948A (en) | Polypropylene molding material | |
JPS5573741A (en) | Polypropylene composition | |
GB838141A (en) | Improvements in or relating to synthetic resinous monofilaments | |
JPS57201632A (en) | Manufacture of blow molded article | |
JPS5511945A (en) | Lid for globe box | |
AU1755088A (en) | Composition comprising polymer of 4-methyl-pentene-1 | |
JPS6429445A (en) | Polyolefin composition |