JPS6434514A - Manufacture of wear resistant bent duplex pipe - Google Patents
Manufacture of wear resistant bent duplex pipeInfo
- Publication number
- JPS6434514A JPS6434514A JP19206487A JP19206487A JPS6434514A JP S6434514 A JPS6434514 A JP S6434514A JP 19206487 A JP19206487 A JP 19206487A JP 19206487 A JP19206487 A JP 19206487A JP S6434514 A JPS6434514 A JP S6434514A
- Authority
- JP
- Japan
- Prior art keywords
- pipe
- bent
- pieces
- wear resistant
- inner pipe
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To improve working efficiency and to reduce manufacturing cost by disposing wear resistant pieces on a recessed part of outside a bent pipe to form an inner pipe, then by joining the outer pipe and the bent inner pipe. CONSTITUTION:The recessed part 5 is provided on the outer surface of the bent pipe 3 and the pieces 4 of the wear resistant material are bonded on its surface by bonding agent. At this time, the outer diameter of the bent inner pipe 2 to be formed is nearly approximated to the bent outer pipe 1. A heating system 6 and cooling water injecting means 7, 7 are set up on the outer periphery of the outer bent pipe 1, and the inner pipe 2 is inserted into the outer pipe 1 and moved. In this way, the outer pipe 1 and the inner pipe 2 are joined through compressive force, a microelastic deformation of the thin part of the recessed part 5 prevents displacement and breaking of the pieces 4. Therefore, as the working efficiency of the duplex pipe is improved and the amount to be used of the pieces 4 of the resistant material is cut down, the manufacturing cost is reduced.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP19206487A JPS6434514A (en) | 1987-07-31 | 1987-07-31 | Manufacture of wear resistant bent duplex pipe |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP19206487A JPS6434514A (en) | 1987-07-31 | 1987-07-31 | Manufacture of wear resistant bent duplex pipe |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6434514A true JPS6434514A (en) | 1989-02-06 |
JPH0576387B2 JPH0576387B2 (en) | 1993-10-22 |
Family
ID=16285023
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP19206487A Granted JPS6434514A (en) | 1987-07-31 | 1987-07-31 | Manufacture of wear resistant bent duplex pipe |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6434514A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5978349A (en) * | 1982-10-27 | 1984-05-07 | Dainippon Printing Co Ltd | Plate making system for video picture |
-
1987
- 1987-07-31 JP JP19206487A patent/JPS6434514A/en active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5978349A (en) * | 1982-10-27 | 1984-05-07 | Dainippon Printing Co Ltd | Plate making system for video picture |
Also Published As
Publication number | Publication date |
---|---|
JPH0576387B2 (en) | 1993-10-22 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS6434514A (en) | Manufacture of wear resistant bent duplex pipe | |
JPS55154119A (en) | Supersonic processor | |
JPS57135291A (en) | Manufacture of scroll compressor | |
JPS646537A (en) | Manufacture of spring made of ceramic | |
JPS6434513A (en) | Manufacture of wear resistant bent duplex pipe | |
JPS56144881A (en) | Joining method | |
FR2424814A1 (en) | METHOD FOR MAKING A LINK OF A CERTAIN EXTENT BETWEEN TWO SURFACES | |
JPS54150761A (en) | Liquid receiver for refrigeration cycle | |
JPS5684135A (en) | Manufacture of bent pipe | |
JPS6487991A (en) | Hose and manufacture thereof | |
JPS57161680A (en) | Hand of time piece and manufacture thereof | |
SU1064103A1 (en) | Rotating furnace band | |
JPS5639131A (en) | Manufacture of coaxial reducing pipe | |
JPS5441232A (en) | Metallic material covering method | |
JPS57154385A (en) | Joining method for composite material | |
JPS56127825A (en) | Manufacture of rotor of electromagnetic clutch for car cooler | |
JPS55154121A (en) | Preparation of metal-covered plastic pipe | |
JPS57156879A (en) | Manufacture of clad material | |
JPS5731436A (en) | Production of roller | |
JPS56122632A (en) | Construction for joining of platelike body and its formation | |
JPS5448661A (en) | Manufacture of clad pipe | |
JPS55117622A (en) | Forming method of engaging portion at end portion of pipe made of synthetic resin | |
JPS5677088A (en) | Manufacture of complex electric contact point by cold pressure welding | |
JPS5597890A (en) | Electromagnetic bonding method | |
JPS53141343A (en) | Improvement in bond strength |