JPS63238930A - Manufacture of edge ring - Google Patents

Manufacture of edge ring

Info

Publication number
JPS63238930A
JPS63238930A JP7226087A JP7226087A JPS63238930A JP S63238930 A JPS63238930 A JP S63238930A JP 7226087 A JP7226087 A JP 7226087A JP 7226087 A JP7226087 A JP 7226087A JP S63238930 A JPS63238930 A JP S63238930A
Authority
JP
Japan
Prior art keywords
ring
edge
die
female die
annular groove
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP7226087A
Other languages
Japanese (ja)
Other versions
JPH0683859B2 (en
Inventor
Masatoshi Fujine
藤根 正敏
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
FUJINE KOHAN KK
Original Assignee
FUJINE KOHAN KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by FUJINE KOHAN KK filed Critical FUJINE KOHAN KK
Priority to JP62072260A priority Critical patent/JPH0683859B2/en
Publication of JPS63238930A publication Critical patent/JPS63238930A/en
Publication of JPH0683859B2 publication Critical patent/JPH0683859B2/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

PURPOSE:To obtain the edge ring in the necessary sectional shape by one stage by curving the upper and lower edges of a ring with a female die and male die and supporting the side wall of the ring with female die at pressing time. CONSTITUTION:A short cylindrical ring is formed by welding both ends of a tape material, fitted to the inner side of a last female die 3 and the lower edge of the ring is abutted to the annular groove edge in arcuate sectional shape of a 2nd female die 4. With the descent of a mal die 6, then, the upper edge of the ring is formed by curving along annular groove in arcuate sectional shape provided on the lower face of the male die 6. The lower edge of the ring is formed by curving to the inner side by the annular groove. Simultaneously with completing the curved edge 2a of specific curvature by the projection bar of a 3rd female die 9 on the upper edge of the ring like this a curved edge 2b is completed at the lower edge of the ring to obtain a specific edge ring 11 together with a linear side wall 2c.

Description

【発明の詳細な説明】 (産業上の利用分野) この発明は′、硝子蓋縁又はほうろう器の蓋縁および容
器口縁部などに嵌着固定する為に使用する縁リングに関
するもので、縁リングの製造の産業分野で利用される。
Detailed Description of the Invention (Field of Industrial Application) This invention relates to a rim ring used for fitting and fixing to a glass lid rim, an enamel lid rim, a container mouth rim, etc. Used in the industrial field of ring manufacturing.

(従来の技術) 従来、此の種、縁リングの製造法については、本願の発
明者が種々改良を重ねており、金属テープからプレス成
形する方法を発明しく特公昭52−1388号)、その
応用によって装着時に弾性変形可能な縁リングの製造法
も発明した(特開昭60−162541号)。
(Prior Art) The inventor of the present application has made various improvements in the manufacturing method of this type of ring and edge ring, and has invented a method of press-forming from a metal tape (Japanese Patent Publication No. 1388/1988). He also invented a method for manufacturing edge rings that can be elastically deformed when worn depending on the application (Japanese Patent Application Laid-Open No. 162541/1983).

(発明により解決すべき問題点) 前記従来の製造法によっては、側壁を縦直線状にし、上
下縁を屈曲する加工を一組型で一工程で行うことが解決
されず、例えば特開昭60−162541号によれば、
二つの型を用い、更に縁リング嵌着時に巻駒を使用して
屈曲している。
(Problems to be Solved by the Invention) According to the conventional manufacturing method described above, it is not possible to form the side wall into a vertical straight line and bend the upper and lower edges in one process using a set of molds. According to No.-162541,
Two molds are used, and a winding piece is used to bend the edge ring when fitting it.

従って側壁の直線部分を比較的幅広く設ける方法が解決
されていない問題点、および上下両縁を一工程で加工で
きない問題点があった。
Therefore, there was a problem that a method of providing a relatively wide straight portion of the side wall has not been solved, and a problem that both the upper and lower edges cannot be processed in one step.

(問題点を解決すべき手段) 然るにこの発明は、短筒状リングを雌型、雄型により湾
曲させるに際し、前記リングの内側壁又は外側を支持し
つ)H型、雄型で加工することにより前記従来の問題点
を解決したのである。
(Means to Solve the Problems) However, the present invention provides a method for bending a short cylindrical ring using a female mold or a male mold, while supporting the inner wall or outer side of the ring, and processing the short cylindrical ring using an H shape or a male mold. The above-mentioned conventional problems have been solved.

即ちこの発明は、縁リングに必要な幅の金属テープを所
定の長さに切断して、その両端を溶接することにより短
筒状リングを形成し、前記短筒状リングを雌型へ、その
側壁を支持する状態でセットし、ついで雄型を下降して
、前記リングの上縁を断面円弧状に湾曲させると共に、
下縁を前記上縁と同一側へ湾曲させることにより縁リン
グの製造性を改良したのである。vi記において、短筒
状リングの上縁および下縁は、外側又は内側に湾曲する
。この湾曲は雌型、雄型の対応部に設けた断面円弧状の
環状溝によって加工される。この場合にリングは補助型
(uI型)などによって側壁を支持されているので、製
品の側壁ははゾ垂直を保つので、目的を達成することが
できる。前記における側壁支持は垂直壁を有する雌型の
側壁による為、プレス中に変形するおそれはない。
That is, in this invention, a short cylindrical ring is formed by cutting a metal tape having the width necessary for the edge ring into a predetermined length and welding both ends of the metal tape, and then inserting the short cylindrical ring into a female mold. The ring is set in a state where it supports the side wall, and then the male mold is lowered to curve the upper edge of the ring into an arcuate cross-section,
Manufacturability of the edge ring was improved by curving the lower edge to the same side as the upper edge. In paragraph vi, the upper and lower edges of the short cylindrical ring are curved outwardly or inwardly. This curvature is created by an annular groove with an arcuate cross section provided in the corresponding parts of the female and male molds. In this case, since the side wall of the ring is supported by an auxiliary mold (uI type) or the like, the side wall of the product remains vertical, so that the purpose can be achieved. Since the side wall support in the above is based on the female side wall having vertical walls, there is no risk of deformation during pressing.

(発明の作用) この発明は筒状に形成したリングを雌型、雄型でプレス
加工するに際し、その上下縁は前記両型の環状溝へ当接
しであるので、同一方向へ湾曲されると共に、リングの
外側壁又は内側壁は支持されているので、加工中に変形
することなく、リングは当初供給した時の、1−の形状
を保持している。
(Function of the invention) When pressing a cylindrical ring with a female mold and a male mold, the upper and lower edges of the ring are in contact with the annular grooves of both molds, so that they are curved in the same direction. Since the outer or inner walls of the ring are supported, the ring retains its original 1-shape as supplied without being deformed during processing.

(実施例1) 次にこの発明の実施例を第1図乃至第4図について説明
する。
(Example 1) Next, an example of the present invention will be described with reference to FIGS. 1 to 4.

ステンレステープを所定長さに切断したテープ材料1の
両端を溶接することにより短筒状のリング2を形成し、
要すれば溶接部の内外壁を研磨して而−にした後(溶接
状態が良ければ、必ずしも研磨しなくてよい)、第1雌
型3の内側に嵌め(第3図)、リング2の下縁を第2f
i型4の断面弧状の環状溝5縁に当接する。ついで雄型
6を矢示7のように下降すれば、雄型6の下面に設けた
断面弧状の環状溝8に沿って、リング上縁部は湾曲成形
される。然してリング下縁は、前記環状溝5によって外
側へ湾曲成形される。このようにしてリング上縁は第3
雌型9の突条10により所定曲率の湾曲1#2aが完成
すると同時に、リング下縁に湾曲縁2bが完成し、直線
状の側壁2Cと共に、所定の縁リング11ができ上る。
A short cylindrical ring 2 is formed by welding both ends of a tape material 1 obtained by cutting a stainless steel tape to a predetermined length,
After polishing the inner and outer walls of the welded part if necessary (if the welding condition is good, polishing is not necessarily necessary), fit it inside the first female mold 3 (Fig. 3), and then Lower edge to 2nd f
It comes into contact with the edge of the annular groove 5 of the i-type 4, which has an arcuate cross section. Then, when the male mold 6 is lowered as shown by the arrow 7, the upper edge of the ring is curved along the annular groove 8 with an arcuate cross section provided on the lower surface of the male mold 6. The lower edge of the ring is thus curved outwardly by the annular groove 5. In this way, the upper edge of the ring
At the same time that the curve 1#2a of a predetermined curvature is completed by the protrusion 10 of the female mold 9, a curved edge 2b is completed at the lower edge of the ring, and together with the linear side wall 2C, a predetermined edge ring 11 is completed.

前記実施例においては、リング2の上下縁が夫々内方へ
湾曲成形される。前記方法によればリング2を雌型およ
び雄型によって一工程で上下縁を同時に湾曲成形するこ
とができると共に、中央部側壁を比較的幅広く、かつ変
形なく成形することができる。この場合に第1雌型3は
、雄型6の下降に伴いスプリング12を下圧して矢示1
3のように下降(第4図)するので、側壁の直線性は保
たれる。更に第3雌型9も、雄型6の下降に伴いスプリ
ング15を下圧して矢示14のように下降するので、製
品縁リング11の上部湾曲縁2aを所定の形状および寸
法に仕上げることができる。
In the embodiment described above, the upper and lower edges of the ring 2 are each curved inwardly. According to the method described above, the upper and lower edges of the ring 2 can be curved simultaneously in one step using the female mold and the male mold, and the side walls of the center can be molded to be relatively wide and without deformation. In this case, the first female mold 3 presses down the spring 12 as the male mold 6 descends, and the first female mold 3 moves to the direction indicated by the arrow.
3 (FIG. 4), the straightness of the side wall is maintained. Furthermore, as the male die 6 descends, the third female die 9 also presses down the spring 15 and descends as shown by the arrow 14, so that the upper curved edge 2a of the product edge ring 11 can be finished into a predetermined shape and size. can.

(実施例2) 次にこの発明の実施例を第1図および第2図と第5図お
よび第7図について説明する。
(Embodiment 2) Next, an embodiment of the present invention will be described with reference to FIGS. 1, 2, 5, and 7.

ステンレステープを所定長さに切断したテープ材1の両
端を溶接することにより、短筒状のリング2を形成し、
要すれば溶接部の内壁を研磨して面一にした後、その下
縁部内側を第1雌型16の外側へ嵌着すると共に、その
下端を第1雌型16     ゛の側壁部へ設けた断面
弧状の環状溝17に臨ませる。ついで雄型18を矢示1
9のように下降させると、雄型18の断面弧状の環状溝
20の内側にリング2の上端が臨むことになる(第6図
)、そこで雄型18を更に下降させると、リング2の上
縁は環状溝17により湾曲縁2aを形成し、下縁は環状
溝20によって湾曲縁2bを形成する。前記において、
湾曲縁2aは第2雌型21の突条22に当接することに
より曲率を補正される。前記第2雌型21は、雄型18
の下降に伴いスプリング23を下圧して矢示24のよう
に下降するので、湾曲縁2aが過度の変形を受けること
なく、湾曲縁2a、2b間の直線側壁2Cも変形を受け
ることなく正しい形状に成形される。前記実施例はりン
グの上下縁を外側へ湾曲する場合である。
A short cylindrical ring 2 is formed by welding both ends of a tape material 1 made by cutting a stainless steel tape to a predetermined length,
If necessary, after polishing the inner wall of the welding part to make it flush, fit the inside of the lower edge to the outside of the first female mold 16, and attach the lower end to the side wall of the first female mold 16. It faces an annular groove 17 having an arcuate cross section. Next, move the male mold 18 to the arrow 1
When the male die 18 is lowered as shown in 9, the upper end of the ring 2 faces inside the annular groove 20 having an arcuate cross section (Fig. 6).When the male die 18 is further lowered, the upper end of the ring 2 is exposed. The edge forms a curved edge 2a with an annular groove 17, and the lower edge forms a curved edge 2b with an annular groove 20. In the above,
The curvature of the curved edge 2a is corrected by coming into contact with the protrusion 22 of the second female mold 21. The second female mold 21 is the male mold 18
As the curved edges 2a and 2b move downward, the spring 23 is pressed down and moves downward as shown by the arrow 24, so that the curved edge 2a is not excessively deformed, and the straight side wall 2C between the curved edges 2a and 2b is also not deformed and has the correct shape. is formed into. In the above embodiment, the upper and lower edges of the ring are curved outward.

(発明の効果) この発明によれば、雌型と雄型によりリングの上下縁を
湾曲させると共に、プレス加工時に雌型によってリング
の側壁を支持するので、所定幅の直線側壁をもったリン
グを成形し得る効果がある。
(Effects of the Invention) According to the present invention, the upper and lower edges of the ring are curved by the female die and the male die, and the side walls of the ring are supported by the female die during press working, so that a ring with straight side walls of a predetermined width can be formed. It has the effect of being moldable.

即ち一工程で所望断面形状の縁リングを得ることができ
る。
That is, an edge ring with a desired cross-sectional shape can be obtained in one step.

【図面の簡単な説明】[Brief explanation of the drawing]

第1図はこの発明の実施に用いるテープ材の一部を省略
した斜視図、第2図は同じくリングの斜視図、第3図は
同じく型の拡大断面図、第4図は同じく型のプレス時の
拡大断面図、第5図は同じく製品の一部拡大斜視図、第
6図は同じく他の実施例の型の拡大断面図、第7図は同
じく型のプレス時の拡大断面図、第8図は同じく製品の
一部拡大斜視図である。
Fig. 1 is a partially omitted perspective view of the tape material used to carry out the present invention, Fig. 2 is a perspective view of a ring, Fig. 3 is an enlarged sectional view of a mold, and Fig. 4 is a press of the same mold. FIG. 5 is an enlarged perspective view of a part of the product, FIG. 6 is an enlarged sectional view of a mold of another embodiment, and FIG. 7 is an enlarged sectional view of the mold when pressed. FIG. 8 is a partially enlarged perspective view of the product.

Claims (1)

【特許請求の範囲】 1 縁リングに必要な幅の金属テープを所定の長さに切
断して、その両端を溶接することにより短筒状リングを
形成し、前記短筒状リングをプレス型へ、その側壁を支
持する状態でセットし、ついで雄型を下降して、前記リ
ングの上縁を断面円弧状に湾曲させると共に、下縁を前
記上縁と同一側へ湾曲させることを特徴とした縁リング
の製造法 2 上縁の湾曲方向は、外側又は内側とした特許請求の
範囲第1項記載の縁リングの製造法 3 側壁支持部は、雄型の下降に伴って下降するように
した特許請求の範囲第1項記載の縁リングの製造法
[Claims] 1. Cut a metal tape with the width necessary for the edge ring into a predetermined length, weld both ends to form a short cylindrical ring, and place the short cylindrical ring into a press mold. , the ring is set in a state where its side walls are supported, and then the male mold is lowered to curve the upper edge of the ring into an arcuate cross-section, and to curve the lower edge to the same side as the upper edge. Method 2 for manufacturing an edge ring Method 3 for manufacturing an edge ring according to claim 1, in which the upper edge is curved outward or inward.The side wall support portion is lowered as the male die is lowered. Method for manufacturing an edge ring according to claim 1
JP62072260A 1987-03-26 1987-03-26 Method for manufacturing edge ring with flat surface Expired - Lifetime JPH0683859B2 (en)