JPS62127325U - - Google Patents

Info

Publication number
JPS62127325U
JPS62127325U JP1344386U JP1344386U JPS62127325U JP S62127325 U JPS62127325 U JP S62127325U JP 1344386 U JP1344386 U JP 1344386U JP 1344386 U JP1344386 U JP 1344386U JP S62127325 U JPS62127325 U JP S62127325U
Authority
JP
Japan
Prior art keywords
thin
plate
thin metal
metal
joining
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP1344386U
Other languages
Japanese (ja)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to JP1344386U priority Critical patent/JPS62127325U/ja
Publication of JPS62127325U publication Critical patent/JPS62127325U/ja
Pending legal-status Critical Current

Description

【図面の簡単な説明】[Brief explanation of the drawing]

第1図ないし第4図は、この考案の第1の実施
例を示し、第1図は接合構造の斜視図であり、第
2図は第1図とは上下逆の方向から見た斜視図で
あり、第3図は第4図に対応する箇所を示す断面
図であり接合工程の途中の状態を示し、第4図は
第1図の線―に沿う断面図である。第5図は
、この考案の第2の実施例を示す断面図である。
第6図は、この考案の第3の実施例を示す断面図
である。第7図は、この考案の第4の実施例を示
す断面図である。第8図は、この考案の第5の実
施例を示す断面図である。第9図は、この考案の
第6の実施例を示す断面図である。第10図ない
し第12図は、この考案の第7の実施例を示し、
第10図はバーリング加工前の状態を示し、第1
1図はバーリング加工後の状態を示し、第12図
は接合片9の先端部を折曲げた後の状態を示す。 図において、1は第1の金属薄板、2は第2の
金属薄板、3は折曲げ線、4は折重ね部分、5は
一方または他方片側(下方片側)、6は一方また
は他方片側(上方片側)、7,8は貫通孔、9は
接合片、11は端縁部、12はバーリングポンチ
である。
Figures 1 to 4 show a first embodiment of this invention, with Figure 1 being a perspective view of the joint structure, and Figure 2 being a perspective view seen from the upside down direction from Figure 1. 3 is a sectional view showing a portion corresponding to FIG. 4, showing a state in the middle of the joining process, and FIG. 4 is a sectional view taken along the line - in FIG. 1. FIG. 5 is a sectional view showing a second embodiment of this invention.
FIG. 6 is a sectional view showing a third embodiment of this invention. FIG. 7 is a sectional view showing a fourth embodiment of this invention. FIG. 8 is a sectional view showing a fifth embodiment of this invention. FIG. 9 is a sectional view showing a sixth embodiment of this invention. 10 to 12 show a seventh embodiment of this invention,
Figure 10 shows the state before burring, and the first
1 shows the state after burring, and FIG. 12 shows the state after the tip of the joining piece 9 is bent. In the figure, 1 is the first metal thin plate, 2 is the second metal thin plate, 3 is the bending line, 4 is the folded part, 5 is one or the other side (lower side), 6 is one or the other side (upper side) (one side), 7 and 8 are through holes, 9 is a joint piece, 11 is an edge portion, and 12 is a burring punch.

Claims (1)

【実用新案登録請求の範囲】 (1) 第1の金属薄板が折曲げられて形成された
折重ね部分に第2の金属薄板が挾み込まれた状態
で、第1の金属薄板と第2の金属薄板とが接合さ
れる、金属薄板の接合構造において、 第1の金属薄板の折重ね部分の一方片側と第2
の金属薄板とには、一連の貫通孔が形成され、第
1の金属薄板の折重ね部分の他方片側には、前記
貫通孔内に挿入される接合片が第1の金属薄板か
ら一体に形成され、前記接合片の先端部が前記一
方片側の外面に沿つて折曲げられてなることを特
徴とする、金属薄板の接合構造。 (2) 前記第2の金属薄板の端縁部は、前記折重
ね部分の折曲げ線の内側に当接する、実用新案登
録請求の範囲第1項記載の金属薄板の接合構造。 (3) 前記接合片は、前記貫通孔の周縁部であつ
て、前記折重ね部分の折曲げ線が位置する側の周
縁部に接触する、実用新案登録請求の範囲第1項
または第2項記載の金属薄板の接合構造。 (4) 前記接合片は、前記貫通孔の周縁部であつ
て、前記折重ね部分の折曲げ線が位置する側とは
反対側の周縁部に接触する、実用新案登録請求の
範囲第1項または第2項記載の金属薄板の接合構
造。 (5) 前記接合片は、前記第1の金属薄板の一部
を切り起こして形成したものである、実用新案登
録請求の範囲第1項ないし第4項のいずれかに記
載の金属薄板の接合構造。 (6) 前記接合片は、前記第1の金属薄板の一部
をバーリング加工して形成したものである、実用
新案登録請求の範囲第1項または第2項記載の金
属薄板の接合構造。
[Claims for Utility Model Registration] (1) In a state where the second thin metal plate is sandwiched between the folded portion formed by bending the first thin metal plate, the first thin metal plate and the second thin metal plate are In the metal thin plate joining structure in which two metal thin plates are joined, one side of the folded portion of the first metal thin plate and the second metal thin plate are joined.
A series of through holes are formed in the thin metal plate, and a joining piece to be inserted into the through hole is formed integrally with the first thin metal plate on the other side of the folded portion of the first thin metal plate. A joining structure for thin metal plates, characterized in that the tip of the joining piece is bent along the outer surface of the one side. (2) The metal thin plate joining structure according to claim 1, wherein the edge portion of the second metal thin plate abuts on the inside of the folding line of the folded portion. (3) The joining piece contacts the peripheral edge of the through hole on the side where the folding line of the folded portion is located, as claimed in claim 1 or 2 of the utility model registration claim. The bonded structure of the metal thin plates described. (4) The joining piece contacts the peripheral edge of the through hole on the side opposite to the side where the folding line of the folded portion is located, Claim 1 of the Utility Model Registration Claim. Or the joining structure of thin metal plates according to item 2. (5) The joining of thin metal sheets according to any one of claims 1 to 4 of the utility model registration claims, wherein the joining piece is formed by cutting and raising a part of the first thin metal sheet. structure. (6) The joining structure of thin metal plates according to claim 1 or 2, wherein the joining piece is formed by burring a part of the first thin metal plate.
JP1344386U 1986-01-31 1986-01-31 Pending JPS62127325U (en)