JPS6185307U - - Google Patents
Info
- Publication number
- JPS6185307U JPS6185307U JP16842784U JP16842784U JPS6185307U JP S6185307 U JPS6185307 U JP S6185307U JP 16842784 U JP16842784 U JP 16842784U JP 16842784 U JP16842784 U JP 16842784U JP S6185307 U JPS6185307 U JP S6185307U
- Authority
- JP
- Japan
- Prior art keywords
- steel
- around
- shank
- carburizing
- relaxation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Description
第1図は本考案のドリルの一実施例の側面図、
第2図はその刃先端面図である。
1…ドリル、2…刃部、3…ねじれ溝、4…切
れ刃、5…マージン部、6…二番取り面、7…チ
ゼルエツジ、8…シヤンク部、9…タング、10
…首、11…溶接部。
FIG. 1 is a side view of an embodiment of the drill of the present invention.
FIG. 2 is a front view of the tip of the blade. DESCRIPTION OF SYMBOLS 1... Drill, 2... Blade part, 3... Helix groove, 4... Cutting edge, 5... Margin part, 6... Double chamfer, 7... Chisel edge, 8... Shank part, 9... Tang, 10
...Neck, 11...Welding part.
Claims (1)
素鋼または熱間ダイス鋼製のシヤンク部から成る
モールス・テーパーシヤンク、ドリルにおいて、
高速度鋼棒材を溝切り加工および二番取り加工後
750°C前後の温度で表面Cが1.1%前後に
なるような緩和浸炭を施し、ひきつづいて焼入・
焼もどしを施し、溝研摩、ホモ処理後外径研削お
よび刃つけを行ない、220°C前後の大気雰囲
気中で約2時間加熱して黄金色の酸化皮膜を形成
したマージン部およびシヤンク部を有することを
特徴とする緩和浸炭モールス・テーパーシヤンク
ドリル。 In Morse taper shank drills, which consist of a blade made of high-speed steel and a shank made of structural alloy steel, structural carbon steel, or hot die steel,
After grooving and second-cutting high-speed steel bars, they are subjected to relaxation carburizing at a temperature of around 750°C to a surface C of around 1.1%, followed by quenching and
It has margins and shank parts that have been tempered, grooved, homogenized, outer diameter ground and edged, and heated in an air atmosphere around 220°C for about 2 hours to form a golden oxide film. A relaxation carburizing Morse taper shank drill.