JPS6090860A - 高温度用低比重セメントの品質劣化を防止する方法 - Google Patents

高温度用低比重セメントの品質劣化を防止する方法

Info

Publication number
JPS6090860A
JPS6090860A JP19839683A JP19839683A JPS6090860A JP S6090860 A JPS6090860 A JP S6090860A JP 19839683 A JP19839683 A JP 19839683A JP 19839683 A JP19839683 A JP 19839683A JP S6090860 A JPS6090860 A JP S6090860A
Authority
JP
Japan
Prior art keywords
specific gravity
cement
low specific
high temperatures
high temperature
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP19839683A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0541583B2 (cg-RX-API-DMAC7.html
Inventor
小林 和一
茂生 岡林
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Ube Corp
Original Assignee
Ube Industries Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ube Industries Ltd filed Critical Ube Industries Ltd
Priority to JP19839683A priority Critical patent/JPS6090860A/ja
Publication of JPS6090860A publication Critical patent/JPS6090860A/ja
Publication of JPH0541583B2 publication Critical patent/JPH0541583B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Curing Cements, Concrete, And Artificial Stone (AREA)
JP19839683A 1983-10-25 1983-10-25 高温度用低比重セメントの品質劣化を防止する方法 Granted JPS6090860A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP19839683A JPS6090860A (ja) 1983-10-25 1983-10-25 高温度用低比重セメントの品質劣化を防止する方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP19839683A JPS6090860A (ja) 1983-10-25 1983-10-25 高温度用低比重セメントの品質劣化を防止する方法

Publications (2)

Publication Number Publication Date
JPS6090860A true JPS6090860A (ja) 1985-05-22
JPH0541583B2 JPH0541583B2 (cg-RX-API-DMAC7.html) 1993-06-23

Family

ID=16390429

Family Applications (1)

Application Number Title Priority Date Filing Date
JP19839683A Granted JPS6090860A (ja) 1983-10-25 1983-10-25 高温度用低比重セメントの品質劣化を防止する方法

Country Status (1)

Country Link
JP (1) JPS6090860A (cg-RX-API-DMAC7.html)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6502636B2 (en) * 1999-09-07 2003-01-07 Halliburton Energy Services, Inc. Methods and compositions for grouting heat exchange pipe
JP2003506527A (ja) * 1999-07-29 2003-02-18 ソフィテック、ナムローゼ、フェンノートシャップ 油井等のための低密度および低間隙率セメンティングスラリー
JP2009530220A (ja) * 2006-03-21 2009-08-27 ハルリブルトン エネルギ セルビセス インコーポレーテッド 低水和熱セメント組成物、及び該組成物の使用方法
EP3070065A1 (de) * 2015-03-17 2016-09-21 HeidelbergCement AG Verzögerermischung für alkali-aktivierte bindemittel

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5788052A (en) * 1980-11-14 1982-06-01 Ube Industries Manufacture of heat-resistant gypsum composition
JPS5815049A (ja) * 1981-07-16 1983-01-28 宇部興産株式会社 坑井用セメント組成物
JPS5869753A (ja) * 1981-10-19 1983-04-26 電気化学工業株式会社 コンクリ−トのワ−カビリテイ改良方法

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5788052A (en) * 1980-11-14 1982-06-01 Ube Industries Manufacture of heat-resistant gypsum composition
JPS5815049A (ja) * 1981-07-16 1983-01-28 宇部興産株式会社 坑井用セメント組成物
JPS5869753A (ja) * 1981-10-19 1983-04-26 電気化学工業株式会社 コンクリ−トのワ−カビリテイ改良方法

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2003506527A (ja) * 1999-07-29 2003-02-18 ソフィテック、ナムローゼ、フェンノートシャップ 油井等のための低密度および低間隙率セメンティングスラリー
US6502636B2 (en) * 1999-09-07 2003-01-07 Halliburton Energy Services, Inc. Methods and compositions for grouting heat exchange pipe
JP2009530220A (ja) * 2006-03-21 2009-08-27 ハルリブルトン エネルギ セルビセス インコーポレーテッド 低水和熱セメント組成物、及び該組成物の使用方法
EP3070065A1 (de) * 2015-03-17 2016-09-21 HeidelbergCement AG Verzögerermischung für alkali-aktivierte bindemittel
WO2016146251A1 (de) * 2015-03-17 2016-09-22 Heidelbergcement Ag Verzögerermischung für alkali-aktivierte bindemittel

Also Published As

Publication number Publication date
JPH0541583B2 (cg-RX-API-DMAC7.html) 1993-06-23

Similar Documents

Publication Publication Date Title
US6405801B1 (en) Environmentally acceptable well cement fluid loss control additives, compositions and methods
AU738096B2 (en) Light weight high temperature well cement compositions and methods
US4234344A (en) Lightweight cement and method of cementing therewith
US5900053A (en) Light weight high temperature well cement compositions and methods
US6457523B1 (en) Delayed thixotropic cement compositions and methods
US4450009A (en) Method of preparing a light weight cement composition from sea water
US6656265B1 (en) Cementation product and use for cementing oil wells or the like
US6957702B2 (en) Cement compositions with improved mechanical properties and methods of cementing in a subterranean formation
US4114692A (en) Method for cementing high temperature wells
US4131578A (en) Aqueous hydraulic cement slurry
US20050109507A1 (en) Methods of using cement compositions having long-term slurry-state stability
US4125160A (en) Method of cementing a high temperature borehole
US7357834B2 (en) Cement composition for use with a formate-based drilling fluid comprising an alkaline buffering agent
JPS6090860A (ja) 高温度用低比重セメントの品質劣化を防止する方法
US5109042A (en) Fluid loss additive for cement slurries containing a n-vinyl-2-pyrrolidone-ω-2-acrylamido-2-methylpropane sulfonate-ω-acrylic acid-ω-acrylamide polymer
CA2523086C (en) Biodegradable cement retarder compositions and methods of cementing in a subterranean formation
US11084758B1 (en) Fly ash-cement for oil and gas cementing applications
JPS6238314B2 (cg-RX-API-DMAC7.html)
US11466192B2 (en) Cements for oil and gas cementing applications
JPS59128248A (ja) 高温度用の超低比重セメント及びセメントスラリ−
JPS59128249A (ja) 高温度用超低比重セメント及びセメントスラリ−