JPS60143739U - Outlet side sealing device of belt furnace for metal powder reduction - Google Patents
Outlet side sealing device of belt furnace for metal powder reductionInfo
- Publication number
- JPS60143739U JPS60143739U JP3097884U JP3097884U JPS60143739U JP S60143739 U JPS60143739 U JP S60143739U JP 3097884 U JP3097884 U JP 3097884U JP 3097884 U JP3097884 U JP 3097884U JP S60143739 U JPS60143739 U JP S60143739U
- Authority
- JP
- Japan
- Prior art keywords
- belt
- metal powder
- sealing
- inert gas
- outlet side
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。(57) [Summary] This bulletin contains application data before electronic filing, so abstract data is not recorded.
Description
第1図は従来の出口シール装置を示す断面図、 −第2
図は第1図の■−■線矢視拡大断面図、第3図は本考案
実施例の出口シール装置を示す断面図 。
である。
2・・・スチールベルト、4・・・ケーキ、6・・・破
砕機、16・・・第・1シール室、18・・・第2シー
ル室、20−・・第3シール室、24A、24B、24
C−・・自動開閉タンパ−126・・・シールロール、
28・・・ヘルドシール室、32A、32B、32cm
・・圧力検出器、34・・・差圧発信器、36・・・N
2ガス配管、38B、38C・・・自動供給弁、40・
・・排出ガス配管、42B、42C・・・3方切替弁、
44B。
44C・・・自動排気弁、46・・・酸素濃度計。
第1図
第2図 −Figure 1 is a sectional view showing a conventional outlet sealing device;
The figure is an enlarged sectional view taken along the line ■--■ in FIG. 1, and FIG. 3 is a sectional view showing the outlet sealing device according to the embodiment of the present invention. It is. 2...Steel belt, 4...Cake, 6...Crusher, 16...First seal chamber, 18...Second seal chamber, 20-...Third seal chamber, 24A, 24B, 24
C-... Automatic opening/closing tamper 126... Seal roll,
28...Heald seal chamber, 32A, 32B, 32cm
...Pressure detector, 34...Differential pressure transmitter, 36...N
2 gas piping, 38B, 38C... automatic supply valve, 40.
...Exhaust gas piping, 42B, 42C...3-way switching valve,
44B. 44C...Automatic exhaust valve, 46...Oxygen concentration meter. Figure 1 Figure 2 -
Claims (1)
元脱炭する金属粉未還元用ベルト炉の出′ °ロ側シー
ル装置において、前記還元性雰囲気に連通し還元脱炭さ
れ固着したケーキを破砕し該粉砕ケーキ排出用の自動開
閉ダンパーと前記スチールベルトのシールロールを有す
る第1シール室ト、前記第1シール室の下部に設けられ
前記破砕ケーキ人出用の自動開閉ダンパーを有する1室
以上の・ 後続シール室と、前記シールロールに接続
するベルトシール室と、圧力検出器、差圧発信器、不活
性ガス配管および自動供給弁等より成り前記シール室に
不活性ガスを供給する不活性ガス供給装置と、排気ガス
配管、3方切替弁、排気弁および酸へ素濃度計より成り
前記後続シール室の不活性ガスを前記ベルトシール室も
゛しくは大気中に排出する排出装置と、前記スチールベ
ルトの速度に応じて前記自動開閉ダンパーおよび弁を制
御するインク、−パルタイマーと、を有して成ることを
特徴とする金属粉未還元用ベルト炉の出口側シール装置
。In a sealing device on the outlet side of a belt furnace for unreduced metal powder in which metal powder is reduced and decarburized on a steel belt in a reducing atmosphere, the cake is communicated with the reducing atmosphere to crush the fixed cake that has been reduced and decarburized. a first sealing chamber having an automatic opening/closing damper for discharging the crushed cake and a seal roll of the steel belt; and one or more chambers provided at the lower part of the first sealing chamber and having an automatic opening/closing damper for discharging the crushed cake. An inert gas supply that supplies inert gas to the sealing chamber, which is comprised of a subsequent sealing chamber, a belt sealing chamber connected to the sealing roll, a pressure detector, a differential pressure transmitter, an inert gas piping, an automatic supply valve, etc. a discharge device comprising an exhaust gas pipe, a three-way switching valve, an exhaust valve, and an oxy-heloxide concentration meter for discharging the inert gas in the subsequent seal chamber into the belt seal chamber or into the atmosphere; 1. An outlet side sealing device for a belt furnace for unreduced metal powder, comprising: an ink-pal timer that controls the automatic opening/closing damper and valve according to the speed of the belt.