JPS5841722B2 - gohanseizohouhou - Google Patents
gohanseizohouhouInfo
- Publication number
- JPS5841722B2 JPS5841722B2 JP7978175A JP7978175A JPS5841722B2 JP S5841722 B2 JPS5841722 B2 JP S5841722B2 JP 7978175 A JP7978175 A JP 7978175A JP 7978175 A JP7978175 A JP 7978175A JP S5841722 B2 JPS5841722 B2 JP S5841722B2
- Authority
- JP
- Japan
- Prior art keywords
- plywood
- hot press
- defective
- hot
- manufacturing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
【発明の詳細な説明】
本発明は新規な合板製造方法に関しその目的とするとこ
ろは合板製造における不良率の低下にある。DETAILED DESCRIPTION OF THE INVENTION The present invention relates to a novel plywood manufacturing method, and its purpose is to reduce the defective rate in plywood manufacturing.
従来の合板製造方法は第1図に示す如くスプレッダ1に
よって表裏面に糊付けされた中板2と表板3、裏板4と
が仕組まれ、1枚の合板素材5となる。In the conventional plywood manufacturing method, as shown in FIG. 1, a middle board 2, a front board 3, and a back board 4, which are glued on the front and back sides by a spreader 1, are assembled to form a single plywood material 5.
これら合板素材5を複数枚重合してコールドプレス6に
て仮圧締し、次いでホットプレス7にて熱圧し、然る後
ダブルソー8によってその四周縁部9の垂直加工をほど
こし、最終製品寸法としてサンダ10によってその表面
を平滑となし合板製品11となしていた。A plurality of these plywood materials 5 are superimposed and temporarily pressed in a cold press 6, then hot pressed in a hot press 7, and then the four peripheral edges 9 are vertically processed by a double saw 8 to obtain the final product dimensions. The surface was smoothed with a sander 10 to form a plywood product 11.
この際、コールドプレス9工程からホットプレス7への
挿入時、第2図に示す如く、合板素材5の挿入方向端部
において表板3、中板2並びに裏板4か不揃いであると
往々にしてその一部がホットプレス7のガイド板12に
つかえて折れまがりそのままホットプレス7によって熱
圧されると、それは第3図に示す如き・不良合板製品1
3となっていた。At this time, when inserting the plywood material 5 from the cold press 9 process into the hot press 7, it is often the case that the top plate 3, middle plate 2, and back plate 4 are not aligned at the end of the plywood material 5 in the insertion direction, as shown in FIG. When a part of the plywood gets caught in the guide plate 12 of the hot press 7, bends, and is hot-pressed by the hot press 7, it becomes a defective plywood product 1 as shown in FIG.
It was 3.
一方、前記合板素材5の挿入方向先端部における各単板
の不揃は各単板の大きさの不揃、仕組工程における作業
形態から現状では不可避である。On the other hand, the unevenness of the veneers at the leading end in the insertion direction of the plywood material 5 is currently unavoidable due to the unevenness of the sizes of the veneers and the work style in the assembly process.
本発明は前記従来方法の欠点を解消するものでその一実
施例を第4図について説明すれば糊付け、仕組並びにコ
ールドプレス6による仮圧締工程までは従来方法と同一
であるが、本発明においては次のホットプレス7への挿
入にあたって合板素材5の四周縁部9をダブルソー8に
よって鋸断し、垂直に加工するものである。The present invention solves the drawbacks of the conventional method, and an embodiment thereof will be described with reference to FIG. When inserting into the next hot press 7, the four peripheral edges 9 of the plywood material 5 are sawed with a double saw 8 and processed vertically.
この垂直加工によって従来方法にみられた如きホットプ
レス7への挿入にあたって単板の一部が折れまがって不
良合板製品13が発生することを防止できるものである
。This vertical processing can prevent a portion of the veneer from bending during insertion into the hot press 7, which occurs in the conventional method, resulting in a defective plywood product 13.
尚、本実施例においては合板素材5の四周縁部9の垂直
加工にあたってダブルソー8の鋸断によってこれを行な
っているが、これはエツヂサンダ等による研削加工によ
っても同等の効果が得られるものである。In this embodiment, the four peripheral edges 9 of the plywood material 5 are vertically processed by sawing with a double saw 8, but the same effect can be obtained by grinding with an edge sander or the like. .
本発明は前記の如くホットプレス7への挿入時、合板素
材5の四周縁部9に垂直加工が施されているので単板の
折れまがりがなくなり不良合板製品13の発生が皆無と
なるすぐれた効果を有するものである。As described above, the present invention is superior in that the four peripheral edges 9 of the plywood material 5 are vertically processed when inserted into the hot press 7, so that the veneer does not bend and there is no occurrence of defective plywood products 13. It is effective.
第1図は従来の合板製造ラインをブロックで表わしたブ
ロック線図、第2図は合板素材のホットプレスへの挿入
状態を示す暗示側面図、第3図は不良合板製品を示す一
部破断側面図、第4図は本発明による合板製造ラインを
ブロックで表わしたブロック線図である。Figure 1 is a block diagram of a conventional plywood production line, Figure 2 is a side view showing the state of plywood material being inserted into a hot press, and Figure 3 is a partially broken side view showing a defective plywood product. FIG. 4 is a block diagram showing a plywood manufacturing line according to the present invention using blocks.
Claims (1)
材縁部垂直加工工程を挿入したことを特長とする合板製
造方法。1. A plywood manufacturing method characterized by inserting a plywood material edge vertical processing step between the cold pressing step and the hot pressing step.