JPS5827486Y2 - glass sealed terminal - Google Patents

glass sealed terminal

Info

Publication number
JPS5827486Y2
JPS5827486Y2 JP2533079U JP2533079U JPS5827486Y2 JP S5827486 Y2 JPS5827486 Y2 JP S5827486Y2 JP 2533079 U JP2533079 U JP 2533079U JP 2533079 U JP2533079 U JP 2533079U JP S5827486 Y2 JPS5827486 Y2 JP S5827486Y2
Authority
JP
Japan
Prior art keywords
glass
outer ring
iron
nickel
metal outer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP2533079U
Other languages
Japanese (ja)
Other versions
JPS55124181U (en
Inventor
雅男 西山
Original Assignee
日本電気ホームエレクトロニクス株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 日本電気ホームエレクトロニクス株式会社 filed Critical 日本電気ホームエレクトロニクス株式会社
Priority to JP2533079U priority Critical patent/JPS5827486Y2/en
Publication of JPS55124181U publication Critical patent/JPS55124181U/ja
Application granted granted Critical
Publication of JPS5827486Y2 publication Critical patent/JPS5827486Y2/en
Expired legal-status Critical Current

Description

【考案の詳細な説明】 本考案はガスセンサ用ステムに好適するガラス封止端子
に関する。
DETAILED DESCRIPTION OF THE INVENTION The present invention relates to a glass-sealed terminal suitable for a stem for a gas sensor.

ガスセンサ用のガラス封止端子は、例えば第1図に示す
ように、金属外環1にリード線2をガラス3を介して、
かつ金属外環1とリード線2との間の沿面距離を大きく
するために、ガラス3が金属外環1から突出状に封止さ
れており、金属外環1およびリード線2が鉄・ニッケル
・コバルト合金よりなり、ガラス3がホウケイ酸ガラス
からなるのが普通である。
For example, as shown in FIG. 1, a glass-sealed terminal for a gas sensor includes a lead wire 2 connected to a metal outer ring 1 through a glass 3.
In addition, in order to increase the creepage distance between the metal outer ring 1 and the lead wires 2, the glass 3 is sealed in a protruding manner from the metal outer ring 1, and the metal outer ring 1 and the lead wires 2 are made of iron/nickel. - It is made of cobalt alloy, and the glass 3 is usually made of borosilicate glass.

ところが、金属材料として鉄・ニッケル・コバルト合金
を用いると、硫酸や硝酸のミストによって、ガラス封止
界面やメツシュ状キャップの溶接界面で発錆しやすいの
みならず、鉄・ニッケル・コバルト合金が高価なため、
ガラス封止端子が高価になるという問題点があった。
However, when iron, nickel, and cobalt alloys are used as metal materials, they not only tend to rust at glass sealing interfaces and welded interfaces of mesh caps due to sulfuric acid or nitric acid mist, but also make iron, nickel, and cobalt alloys expensive. For some reason,
There was a problem that the glass-sealed terminal was expensive.

本考案はこのような問題点を解決するために提案された
もので、以下実施例を図面により説明する。
The present invention was proposed to solve these problems, and embodiments thereof will be described below with reference to the drawings.

第2図に示す第1の実施例において、11は鉄・ニッケ
/L、−クロム合金(Fe 52%、Ni42%、Cr
5%。
In the first embodiment shown in FIG.
5%.

a −89X 10 ’cm/cm/deg)よりなる
金属外環で、絞り加工による筒状部12に、上記と同様
の鉄・ニッケル・クロム合金または鉄・ニッケル合金(
Fe48〜52%、Ni52〜48%。
The cylindrical part 12 is made of a metal outer ring made of a -89
Fe48-52%, Ni52-48%.

α=52〜105cm/cm/deg)よりなるリード
線13が、ソーダライムガラス(810273,6%、
Na2O17,2%、CaO3,4%。
The lead wire 13 made of soda lime glass (810273, 6%,
Na2O 17.2%, CaO3.4%.

Mg03.7%、Al2031%。Mg03.7%, Al2031%.

a = 92 cm/cm/deg)または高鉛ガラス
(810257%、Pb029.4%、V2O7,3%
、Na204.1%、Al2031.5%、Ca00.
2%。
a = 92 cm/cm/deg) or high lead glass (810257%, Pb029.4%, V2O7,3%
, Na204.1%, Al2031.5%, Ca00.
2%.

Maoo、2%。Maoo, 2%.

a = 89 X 10−7cm/cm/deg)より
なるガラス14により、ガラス14が金属外環11から
突出状に封止されている。
a = 89 x 10 -7 cm/cm/deg) The glass 14 is sealed in a protruding manner from the metal outer ring 11 .

すなわち、本考案は発錆および材料費の観点から、金属
外環11およびリード線13の材質を特定し、かつこの
金属材料との封着性を考慮してガラス14の材質を特定
したものである。
That is, in the present invention, the material of the metal outer ring 11 and the lead wire 13 is specified from the viewpoint of rust generation and material cost, and the material of the glass 14 is specified in consideration of the sealing property with the metal material. be.

このような構成であると、金属外環11およびリード線
13が硫酸や硝酸のミストによって発錆することがなく
、シかも鉄・ニッケル・クロム・合金や鉄・ニッケル合
金は鉄・ニッケル・コバルト合金に比較して安価である
ので、従来と比べて品質の良いガラス封止端子が安価に
提供できる。
With such a configuration, the metal outer ring 11 and the lead wire 13 will not rust due to sulfuric acid or nitric acid mist, and iron/nickel/chromium alloy or iron/nickel alloy may be replaced by iron/nickel/cobalt. Since it is cheaper than alloys, it is possible to provide glass-sealed terminals of better quality at a lower cost than conventional ones.

第3図は第2の実施例で金属外環21が、鉄・ニッケル
・クロム合金をキャップ状にプレス成型した点を除いて
は、第2図と同様であるため、第2図と同一部分または
対応部分に同一参照符号を付したので、その説明を省略
する。
Figure 3 shows the second embodiment, which is the same as Figure 2 except that the metal outer ring 21 is press-molded from an iron-nickel-chromium alloy into a cap shape, so the parts are the same as in Figure 2. Or, since corresponding parts are given the same reference numerals, the explanation thereof will be omitted.

第4図は第3の実施例で、金属外環31が比較的厚い金
属板をプレス加工して製作されている点を除いては第2
図と同様であるため、第2図と同一部分または対応部分
に同一参照符号を付したので、その説明を省略する。
FIG. 4 shows the third embodiment, which is similar to the second embodiment except that the metal outer ring 31 is manufactured by pressing a relatively thick metal plate.
Since it is similar to the figure, the same reference numerals are given to the same or corresponding parts as in FIG. 2, and the explanation thereof will be omitted.

本考案は以上のように、発錆のないガラス封止端子が安
価に提供できるという効果を奏する。
As described above, the present invention has the effect of providing a rust-free glass-sealed terminal at a low cost.

【図面の簡単な説明】[Brief explanation of the drawing]

第1図は本考案の前提となるガラス封止端子の縦断面図
、第2図ないし第4図は本考案の異なる実施例のガラス
封止端子の縦断面図である。 11.21.31・・・・・・金属外環、13・・・・
・・リード線、14・・・・・・ガラス。
FIG. 1 is a longitudinal cross-sectional view of a glass-sealed terminal, which is the premise of the present invention, and FIGS. 2 to 4 are longitudinal cross-sectional views of glass-sealed terminals according to different embodiments of the present invention. 11.21.31...Metal outer ring, 13...
...Lead wire, 14...Glass.

Claims (1)

【実用新案登録請求の範囲】[Scope of utility model registration request] 鉄・ニッケル・クロム合金よりなる金属外環に、鉄・ニ
ッケル合金および鉄・ニッケル・クロム合金から選択さ
れたリード線を、ソーダライムガラスおよび鉛ガラスか
ら選択されたガラスを用いて、かつガラスが金属外環か
ら突出状になるように封止してなるガラス封止端子。
A lead wire selected from an iron-nickel alloy and an iron-nickel-chromium alloy is attached to a metal outer ring made of an iron-nickel-chromium alloy using a glass selected from soda-lime glass and lead glass. A glass-sealed terminal that is sealed so that it protrudes from a metal outer ring.
JP2533079U 1979-02-27 1979-02-27 glass sealed terminal Expired JPS5827486Y2 (en)