JPS58208935A - Magnetic recording medium - Google Patents
Magnetic recording mediumInfo
- Publication number
- JPS58208935A JPS58208935A JP57090820A JP9082082A JPS58208935A JP S58208935 A JPS58208935 A JP S58208935A JP 57090820 A JP57090820 A JP 57090820A JP 9082082 A JP9082082 A JP 9082082A JP S58208935 A JPS58208935 A JP S58208935A
- Authority
- JP
- Japan
- Prior art keywords
- layer
- oxide
- ferromagnetic
- magnetic recording
- recording medium
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Description
【発明の詳細な説明】
本発明は保護層を有する磁気記録媒体に関するものであ
る。DETAILED DESCRIPTION OF THE INVENTION The present invention relates to a magnetic recording medium having a protective layer.
プラスチックフィルム等の基体に強磁性体金属な真空蒸
着法やイオンブレーティング法等によって斜めに付着さ
せた磁気記録媒体は、一般に抗磁力や角形化、磁気記録
密度が共に従来の塗布型のものI(比べて犬ざいという
長所がある。Magnetic recording media, which are made by diagonally attaching ferromagnetic metal to a substrate such as a plastic film by vacuum evaporation or ion blating, generally have better coercive force, squareness, and magnetic recording density than conventional coated media. (In comparison, it has the advantage of being dog-friendly.
ところで、基体に設けられた強磁性体金属は空気−中に
晒されると酸化するが、酸化物が生じると飽和磁化か減
少する欠点があり、さらにこのようにして生じた酸化物
は剥離し易く、磁気へ、F等により!II 1lllt
されさらに内側の強磁性体金属が酸化され飽和磁化が益
々減少する。また、擦られた酸化物のために磁気へラド
等が目づまりを起こす欠点もあった。By the way, the ferromagnetic metal provided on the substrate oxidizes when exposed to air, but it has the disadvantage that the saturation magnetization decreases when oxides are formed, and furthermore, the oxides formed in this way are easy to peel off. , to magnetism, by F etc.! II 1llllt
Furthermore, the inner ferromagnetic metal is oxidized and the saturation magnetization further decreases. There was also the drawback that the rubbed oxide caused the magnetic helad, etc. to become clogged.
本発明は1以上の欠点を改良し2強磁性体金属層の酸化
を防止しつる磁気記録媒体の提供を目的とする。SUMMARY OF THE INVENTION It is an object of the present invention to provide a magnetic recording medium which improves one or more disadvantages and prevents oxidation of the two ferromagnetic metal layers.
本発明は、上記の目的を達成するために2強磁性体金属
層の表面に主として強磁性体金属の酸化物からなる保護
層を設けることを特徴とする磁気記録媒体を提供するも
のである。In order to achieve the above object, the present invention provides a magnetic recording medium characterized in that a protective layer mainly made of ferromagnetic metal oxide is provided on the surface of two ferromagnetic metal layers.
以下1本発明の実施例を図面に基づ(・て説明する。An embodiment of the present invention will be described below based on the drawings.
第1図((おいて、1は厚さ6〜40μのプラスチック
フィルムからなる基体である。2は基体10表面に、真
空蒸着法やイオンプレーティング法。In FIG. 1, 1 is a substrate made of a plastic film with a thickness of 6 to 40 μm. 2 is a substrate 10 that is coated on the surface by vacuum evaporation or ion plating.
スハノタリング法等により鉄や二、ケル、コノ、ルト等
の強磁性体金属を斜めに付着させ形成した強磁性体金1
1である。5は強磁性体金属層2の表而eこ予じめブ7
’J−’J中等において設けられた1強磁性体金媚の酸
化物からなる保護層である。Ferromagnetic gold 1 formed by obliquely adhering ferromagnetic metals such as iron, ferromagnetic metal, ferromagnetic metal, ferromagnetic metal, etc. using the Suhanota ring method etc.
It is 1. 5 is the surface of the ferromagnetic metal layer 2.
'J-' This is a protective layer made of a ferromagnetic metal oxide provided in J, etc.
すなわち、予じめ強磁性体金属層20表面に酸化フハル
トや酸化二、ケル等の酸化物の保護層3を真空蒸着法等
(・こより設けているが、このような酸化物lま1強磁
性体金属層2の一部が酸化したものと異なり、剥離強度
が非常−に大き−1<、磁気へットに擦られたとしても
保護層3はほとんど制れることかなく1強磁性体金属層
2の酸化を防止でき。That is, a protective layer 3 of oxides such as Fhard oxide, dioxide, Kel oxide, etc. is previously provided on the surface of the ferromagnetic metal layer 20 by vacuum evaporation method. Unlike the part of the magnetic metal layer 2 that is oxidized, the peel strength is extremely high.Even if it is rubbed by a magnetic field, the protective layer 3 is almost unrestrained and remains a ferromagnetic material. Oxidation of the metal layer 2 can be prevented.
飽和磁化の低下を防止できる。Decrease in saturation magnetization can be prevented.
以上の通り1本発明によれば2強磁性体金属層の酸(ヒ
を防止飽和磁化の低下を防ぐことができ。As described above, according to the present invention, it is possible to prevent the acid in the ferromagnetic metal layer and to prevent the saturation magnetization from decreasing.
磁気へ、ト等による刺離を防止しつる磁気記録媒体か得
られる。A magnetic recording medium can be obtained that prevents pricking due to magnetism, etc.
図は本発明の実施例の断面図を示す。 1・・・基体、2・・・・・・強磁性体金属層。 6・・・・・保護層。 特許出願人 日立コンデンサ株式会社 The figure shows a cross-sectional view of an embodiment of the invention. 1...Substrate, 2...Ferromagnetic metal layer. 6...Protective layer. Patent applicant: Hitachi Capacitor Co., Ltd.
Claims (1)
において1強磁性体金属の表面に主として強磁性体金属
の酸化物からなる保護層を設けることを特徴とする磁気
記録媒体。(1) A magnetic recording medium having a ferromagnetic metal attached to a base, characterized in that a protective layer mainly consisting of an oxide of the ferromagnetic metal is provided on the surface of the ferromagnetic metal.