JPS58127747A - 腐食防止シ−ル材 - Google Patents

腐食防止シ−ル材

Info

Publication number
JPS58127747A
JPS58127747A JP891782A JP891782A JPS58127747A JP S58127747 A JPS58127747 A JP S58127747A JP 891782 A JP891782 A JP 891782A JP 891782 A JP891782 A JP 891782A JP S58127747 A JPS58127747 A JP S58127747A
Authority
JP
Japan
Prior art keywords
fine
gap
corrosion
powder
sealing material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP891782A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0222782B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html
Inventor
Nobuyoshi Hosaka
保坂 信義
Yuichi Ishikawa
雄一 石川
Shigeru Shida
志田 茂
Osamu Nishida
西田 「あ」
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hitachi Ltd
Original Assignee
Hitachi Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hitachi Ltd filed Critical Hitachi Ltd
Priority to JP891782A priority Critical patent/JPS58127747A/ja
Priority to DE8383100543T priority patent/DE3376336D1/de
Priority to EP83100543A priority patent/EP0090912B1/en
Priority to US06/460,017 priority patent/US4433093A/en
Publication of JPS58127747A publication Critical patent/JPS58127747A/ja
Publication of JPH0222782B2 publication Critical patent/JPH0222782B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Compositions Of Macromolecular Compounds (AREA)
  • Sealing Material Composition (AREA)
JP891782A 1982-01-25 1982-01-25 腐食防止シ−ル材 Granted JPS58127747A (ja)

Priority Applications (4)

Application Number Priority Date Filing Date Title
JP891782A JPS58127747A (ja) 1982-01-25 1982-01-25 腐食防止シ−ル材
DE8383100543T DE3376336D1 (en) 1982-01-25 1983-01-21 Anti-crevice corrosion sealant, and method of using it
EP83100543A EP0090912B1 (en) 1982-01-25 1983-01-21 Anti-crevice corrosion sealant, and method of using it
US06/460,017 US4433093A (en) 1982-01-25 1983-01-21 Anti-crevice corrosion sealant and method for anti-crevice corrosion

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP891782A JPS58127747A (ja) 1982-01-25 1982-01-25 腐食防止シ−ル材

Publications (2)

Publication Number Publication Date
JPS58127747A true JPS58127747A (ja) 1983-07-29
JPH0222782B2 JPH0222782B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) 1990-05-21

Family

ID=11706002

Family Applications (1)

Application Number Title Priority Date Filing Date
JP891782A Granted JPS58127747A (ja) 1982-01-25 1982-01-25 腐食防止シ−ル材

Country Status (1)

Country Link
JP (1) JPS58127747A (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2009185249A (ja) * 2008-02-08 2009-08-20 Asahi Rubber Kk プラスチゾルシール材組成物

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2009185249A (ja) * 2008-02-08 2009-08-20 Asahi Rubber Kk プラスチゾルシール材組成物

Also Published As

Publication number Publication date
JPH0222782B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) 1990-05-21

Similar Documents

Publication Publication Date Title
AU2009316522B2 (en) Composition and method for controlling copper discharge and erosion of copper alloys in industrial systems
Smart et al. The anaerobic corrosion of carbon steel and cast iron in artificial groundwaters
Tyusenkov Chemical resistance of steel 13CrV (rus 13ХФА)
Khadom et al. Modeling of corrosion inhibition of copper-nickel alloy in hydrochloric acid by benzotriazole
US5435941A (en) Tobacco extract composition and method
JPS58127747A (ja) 腐食防止シ−ル材
CN105684091B (zh) 通过组合的溶解与机械的靶向换热器沉积物去除
EP0090912B1 (en) Anti-crevice corrosion sealant, and method of using it
McChesney et al. Internal cathodic protection to study the erosion‐corrosion of AISI 1018 carbon steel
Neal Pipeline coating failure-not always what you think it is
US12234243B1 (en) Diorganyl diselenide-clubbed quaternary purines as corrosion inhibitors
JPS5887281A (ja) 金属接合面の隙間腐食防止法
Mainier et al. Performance of Propargyl Alcohol as Corrosion Inhibitor for Electroless Nickel-Phosphorus (NiP) Coating in Hydrochloric Acid Solution
Jano et al. Test of inhibition efficiency of pineapple crown extract as green inhibitor for two kinds of low allow carbon steel in acidic media.
El-Sherbini et al. The corrosion of copper metal in hcl solutions and the effect of molybdate and chromate
JPS6316470B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html)
JPS59113309A (ja) 耐食性ボルト
JPS5939303B2 (ja) 防食石綿ジヨイントシ−トの製造法
Lee et al. Determining the Coupling Current as a Means of Detecting Crevice Activity and Inhibition
JPS6360280B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html)
JPS5983780A (ja) アルミニウム又はアルミニウム合金タンクの防食方法
JPS58147567A (ja) アルミニウム又はアルミニウム合金タンク用防食剤
Afolabi et al. Effect Of Ammonium Molybdate Inhibition On Corrosion Behaviour Of Mild Steel In Chloride And Sulphide Media
JPH0261080A (ja) ステンレス鋼のカソード防食法
Charng et al. Review of CorrosionCausesandCorrosionControl In a Technical Facility