JPS5733935A - Burring method - Google Patents

Burring method

Info

Publication number
JPS5733935A
JPS5733935A JP10666680A JP10666680A JPS5733935A JP S5733935 A JPS5733935 A JP S5733935A JP 10666680 A JP10666680 A JP 10666680A JP 10666680 A JP10666680 A JP 10666680A JP S5733935 A JPS5733935 A JP S5733935A
Authority
JP
Japan
Prior art keywords
burrs
outside
small holes
burr
discharged
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP10666680A
Other languages
Japanese (ja)
Inventor
Shigeki Komeichi
Kunio Hayashi
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toyota Motor Corp
Original Assignee
Toyota Motor Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toyota Motor Corp filed Critical Toyota Motor Corp
Priority to JP10666680A priority Critical patent/JPS5733935A/en
Publication of JPS5733935A publication Critical patent/JPS5733935A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To easily and surely remove a residual object even after burring work, by supplying freezing material to the inside of a hollow member, and then applying pressure from one side of the hollow member, breaking a burr while deforming further circulating the freezing material and discharging the burr to the outside.
CONSTITUTION: In the surroundings of small holes 3, 4, there are formed burrs 5, 6 protruding toward a hollowed part. To remove these burrs 5, 6, the small holes 3, 4 are closed by using gum tapes 7, 8, and then liquid of water or the like is poured into the hollowed part of a cylinder 1 from another opening part 2, lowered its temperature and frozen. Then the gum tapes 7, 8 are removed, and a rod 10 is inserted into the cylinder 1 while applying pressure. As pressurizing force increases a frozen material 9 is discharged from the small holes 3, 4 to the outside, here the burrs 5, 6 are curved around a supporting point in the vicinity of their base part, broken off and discharged to the outside.
COPYRIGHT: (C)1982,JPO&Japio
JP10666680A 1980-08-01 1980-08-01 Burring method Pending JPS5733935A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP10666680A JPS5733935A (en) 1980-08-01 1980-08-01 Burring method

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP10666680A JPS5733935A (en) 1980-08-01 1980-08-01 Burring method

Publications (1)

Publication Number Publication Date
JPS5733935A true JPS5733935A (en) 1982-02-24

Family

ID=14439394

Family Applications (1)

Application Number Title Priority Date Filing Date
JP10666680A Pending JPS5733935A (en) 1980-08-01 1980-08-01 Burring method

Country Status (1)

Country Link
JP (1) JPS5733935A (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6175038U (en) * 1984-10-24 1986-05-21
JPH04129370U (en) * 1991-05-20 1992-11-26 東海旅客鉄道株式会社 Vehicle sliding door device

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6175038U (en) * 1984-10-24 1986-05-21
JPH04129370U (en) * 1991-05-20 1992-11-26 東海旅客鉄道株式会社 Vehicle sliding door device

Similar Documents

Publication Publication Date Title
ATE339919T1 (en) OCCLUSION SYSTEM FOR REPAIRING ANEURYSM
JPS55139160A (en) Internal chilling type casting method
JPS51151384A (en) Process for cultivating organic tissue or cells automatically
JPS5733935A (en) Burring method
BR9005428A (en) PERFECTING IN LOST FOAM MOLDING PROCESS AND UNDER CONTROLLED PRESSURE OF METALLIC PIECES
JPS54138874A (en) Repairing method for leakage of hollow yarn membrane module
JPS5670324A (en) Concrete crushing body and crushing method of concrete structure
DE69705992T2 (en) Device for preventing mold parts from hindering the ejection of mold parts
JPS53102861A (en) Sticking method for ring on hollow shaft
JPS5555727A (en) Removing freezing pipe
JPS5575852A (en) Production of cast pipe joint
JPS5519323A (en) Removing anchor earth extension
JPS5781521A (en) Sludge mixer
JPS53101181A (en) Method of withdrawing molded products from a mold
JPS55143429A (en) Method and device for checking internal-pressure resistance strength of glass container
JPS5732310A (en) Method for repairing wall of blast furnace
CA2023784A1 (en) Method for the removal of aqueous liquids from the sump of an underground cavity
JPS6414002A (en) Slip casting molding method
AU1138697A (en) A method for preparing a non-fibrous porous material
JPH022234Y2 (en)
JPS5656757A (en) Production of sound killed steel ingot
JPS55135617A (en) Method of obtaining constant-amount discharge of liquid material
JPS5242642A (en) Sludge processing method of freezing and melting type
JPS644016A (en) Furnace tube
JPS5619951A (en) Ingotting method of high grade steel