JPS5614082A - Inert gas metal arc welding method - Google Patents
Inert gas metal arc welding methodInfo
- Publication number
- JPS5614082A JPS5614082A JP8921979A JP8921979A JPS5614082A JP S5614082 A JPS5614082 A JP S5614082A JP 8921979 A JP8921979 A JP 8921979A JP 8921979 A JP8921979 A JP 8921979A JP S5614082 A JPS5614082 A JP S5614082A
- Authority
- JP
- Japan
- Prior art keywords
- arc
- welding
- electrodes
- globule
- consumable
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To achieve the stabilization of the arc and make possible the controlling of globule migration mode, deposition amount, etc. by providing a consumable electrode for MIG welding and plural consumable electrodes for TIG welding respectively to the central part and its circumference and encircling the wire tip and arc of the former by the arc of the latter. CONSTITUTION:For example, consumable electrodes 3, 6 and 7 for MIG and TIG welding are disposed as shown in the figure, and with these as anode, and the welding work 1 as cathode or by making these to the opposite polarities, the welding is performed. This causes the arc A generated by the central electrode 3 to be effectively converged by the arcs B, C having the directivity in the central direction generated by the surrounding electrodes 6, 7, thereby enabling powerful arc throttling power, that is, pinch force, to be obtained. This pinch force and the wire tip are effectively preheated by the surrounding arc and are thereby pointed at the end, by which the stable spray arc may be maintained and globule migration mode is improved. Further, the amount and shape of penetration may be controlled by dispersing the welding current to the electrodes 3 and 6, 7.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8921979A JPS5614082A (en) | 1979-07-16 | 1979-07-16 | Inert gas metal arc welding method |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP8921979A JPS5614082A (en) | 1979-07-16 | 1979-07-16 | Inert gas metal arc welding method |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5614082A true JPS5614082A (en) | 1981-02-10 |
Family
ID=13964607
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP8921979A Pending JPS5614082A (en) | 1979-07-16 | 1979-07-16 | Inert gas metal arc welding method |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5614082A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4547654A (en) * | 1981-11-13 | 1985-10-15 | Westinghouse Electric Corp. | Method and apparatus for arc welding |
-
1979
- 1979-07-16 JP JP8921979A patent/JPS5614082A/en active Pending
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4547654A (en) * | 1981-11-13 | 1985-10-15 | Westinghouse Electric Corp. | Method and apparatus for arc welding |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CA2073840A1 (en) | Method of Welding Nickel or Nickel Alloy Products | |
JP2912693B2 (en) | Gas metal arc welding method for aluminum base material | |
GB1101036A (en) | Electric arc welding | |
ES8200252A1 (en) | Non-consumable composite welding electrode. | |
US4147917A (en) | Method and device for plasma-MIG-welding | |
US3539756A (en) | Welding apparatus | |
JPS5614082A (en) | Inert gas metal arc welding method | |
GB1439575A (en) | Method of and device for plasma mig welding | |
JPH0641032B2 (en) | Non-consumable electrode arc welding method | |
US3309490A (en) | Arc welding with a.c. power and cored electrode | |
JP2001018067A (en) | Method and device for narrow gap welding | |
US3019330A (en) | Electrode for inert gas shielded electric welding and cutting | |
JP3211318B2 (en) | Torch for TIG arc welding and pulse TIG arc welding method | |
GB1340794A (en) | Plasma-mig arc welding | |
US4002878A (en) | Gas tungsten arc welding electrode | |
GB912915A (en) | Electric arc welding | |
US3137783A (en) | Methods of arc welding | |
JPS61108475A (en) | Inert gas shield welding method | |
JPS564380A (en) | Tig-mig welding method | |
JPS60210370A (en) | Tig multielectrode torch | |
US3610868A (en) | Submerged-welding method | |
SU1004051A1 (en) | Non-consumable electrode for arc and plasma working in inert gas medium | |
FR2314016A1 (en) | Submerged arc deposition welding - using two consumable electrodes connected to obtain high deposition rate but very low dilution | |
JPS582551Y2 (en) | Equipment for arc welding or arc welding surface treatment | |
SU536911A1 (en) | Method of arc fusion welding |