JPS5550917A - Controlling method of take-up tension of serrated coil - Google Patents

Controlling method of take-up tension of serrated coil

Info

Publication number
JPS5550917A
JPS5550917A JP12535678A JP12535678A JPS5550917A JP S5550917 A JPS5550917 A JP S5550917A JP 12535678 A JP12535678 A JP 12535678A JP 12535678 A JP12535678 A JP 12535678A JP S5550917 A JPS5550917 A JP S5550917A
Authority
JP
Japan
Prior art keywords
tension
take
outside
coil
plate thickness
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP12535678A
Other languages
Japanese (ja)
Inventor
Akishige Yoshida
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JFE Steel Corp
Original Assignee
Kawasaki Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kawasaki Steel Corp filed Critical Kawasaki Steel Corp
Priority to JP12535678A priority Critical patent/JPS5550917A/en
Publication of JPS5550917A publication Critical patent/JPS5550917A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To prevent occurrence of stick and slip by so controlling the take-up tension after the plate thickness change point that the tension integrated value after the plate thickness changing becomes the tension integrated value of the specified tension of the outside wond coil at the time of taking-up the steel plates of different wall thickness to serrated coils.
CONSTITUTION: When an inside wound coil is thicker than an outside wound coil, the inside wound coil is begun to be wound under the initial tension I determined by the specified tension curve 22 and is taken up under the tension gradually decreasing down to the plate thickness change point A. From the plate thickness change point A, an outside wound coil is taken up and this taking up is accomplished in accordance with the take-up tension curve 26. The taking-up ends at the final tension E. The integrated value of the take-up tension curve 26 and outside diameters is so determined as to become equal to the tension integrated value of the specified tension curve 24 of the coil for outside winding. In this way, the take-up tension from the plate thickness change point gradually decreases and unlike in conventional methods, taking up of the outside wound coil under abruptly decreasing take-up tension is obviated and therefore the slip which had hitherto occured at the rewinding in skin-pass rolling mills may be prevented.
COPYRIGHT: (C)1980,JPO&Japio
JP12535678A 1978-10-11 1978-10-11 Controlling method of take-up tension of serrated coil Pending JPS5550917A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP12535678A JPS5550917A (en) 1978-10-11 1978-10-11 Controlling method of take-up tension of serrated coil

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP12535678A JPS5550917A (en) 1978-10-11 1978-10-11 Controlling method of take-up tension of serrated coil

Publications (1)

Publication Number Publication Date
JPS5550917A true JPS5550917A (en) 1980-04-14

Family

ID=14908097

Family Applications (1)

Application Number Title Priority Date Filing Date
JP12535678A Pending JPS5550917A (en) 1978-10-11 1978-10-11 Controlling method of take-up tension of serrated coil

Country Status (1)

Country Link
JP (1) JPS5550917A (en)

Similar Documents

Publication Publication Date Title
JPS5550917A (en) Controlling method of take-up tension of serrated coil
JPS53112253A (en) Controlling method for interstand tension in continuous rolling mill
JPS6289502A (en) Production of steel sheet by continuous casting of thin ingot
JPS5721805A (en) Manufacture of rolled iron core
JPS5343575A (en) Compensating method of coil winding diameter at rolled form detection
JPS5659533A (en) Coiling method for cold rolled strip
KR920004497B1 (en) Controlling method of a taper tension for a cold rolled equipment
JPS55139654A (en) Tape tension control method
JPS574306A (en) Cold rolling apparatus for electrical steel sheet
JPS557122A (en) Winding loop control method for steel coil
JPS55114419A (en) Coiling method of foil material
JPS54148162A (en) Belt plate winder
JPH04131325A (en) Box annealing method of grain-oriented silicon steel plate
JPS5944933B2 (en) How to control the speed of hotsutran table
JPS54118365A (en) Rolling operation
JPS5614005A (en) Cold rolling method for metallic strip for preventing defect due to coil break
JPS5675348A (en) Pirn with tail and manufacture thereof
JPS57103736A (en) Coiling method for hot rolled coil
JPS55109516A (en) Wire drawing machine
Chen et al. Investigation on Buckling of Coiled Strip Under High Winding Tension
CA2027316A1 (en) Process for preparing wound core having low core loss
JPS61249624A (en) Tension controlling method for payoff reel
JPS56136742A (en) Control method for alternately starting winders for coil-shaped treated material
JPS54145353A (en) Rolling method
JPS5556937A (en) Rewinding method for strip coil wound together with paper