JPS55152118A - Preparation of high chromium steel by vacuum oxygen lancing method - Google Patents
Preparation of high chromium steel by vacuum oxygen lancing methodInfo
- Publication number
- JPS55152118A JPS55152118A JP5926979A JP5926979A JPS55152118A JP S55152118 A JPS55152118 A JP S55152118A JP 5926979 A JP5926979 A JP 5926979A JP 5926979 A JP5926979 A JP 5926979A JP S55152118 A JPS55152118 A JP S55152118A
- Authority
- JP
- Japan
- Prior art keywords
- oxygen lancing
- chromium steel
- high chromium
- oxygen
- vacuum
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To refine the low carbon high chromium steel economically while the oxidation loss of Cr is reduced by a method wherein a preliminary decarburized amount by the oxygen lancing in the atmosheric pressure is reduced and a decarburized amount is increased by a vacuum oxygen lancing.
CONSTITUTION: In case of preparing the low carbon high chromium steel, as a stock material, steel scraps, high carbon Fe-Cr, high carbon Fe-Ni or the like are used and molten by an arc furnace. In this time, if a molten C amount is 0.80% or below, a vacuum oxygen lancing method (VOD) is directly applied to decarburize and refine to a low carbon range and, if 0.80W1.20% or more, the oxygen lancing is carried out in the atmospheric pressure to decarburize. In the C content of this degree, the oxidation of Cr is low even by the oxygen lancing decarburization under the atmospheric pressure. Particularly, after a high Cr steel containing C: 0.30W 1.20% is subjected to the oxygen lancing in an oxygen quantity 0.5Nm3/min., the vacuum natural decarburization is carried out at least for 10 or more min. to prepare a low carbon high chromium steel without oxidizing Cr.
COPYRIGHT: (C)1980,JPO&Japio
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP54059269A JPS5921368B2 (en) | 1979-05-14 | 1979-05-14 | Manufacturing method of high chromium steel by vacuum oxygen blowing method |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP54059269A JPS5921368B2 (en) | 1979-05-14 | 1979-05-14 | Manufacturing method of high chromium steel by vacuum oxygen blowing method |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS55152118A true JPS55152118A (en) | 1980-11-27 |
| JPS5921368B2 JPS5921368B2 (en) | 1984-05-19 |
Family
ID=13108474
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP54059269A Expired JPS5921368B2 (en) | 1979-05-14 | 1979-05-14 | Manufacturing method of high chromium steel by vacuum oxygen blowing method |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5921368B2 (en) |
-
1979
- 1979-05-14 JP JP54059269A patent/JPS5921368B2/en not_active Expired
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5921368B2 (en) | 1984-05-19 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| ES2006217A6 (en) | Method for deoxidizing tantalum material | |
| DE69809909D1 (en) | STAINLESS STEEL POWDER | |
| WO1997028285A3 (en) | Producing stainless steels in parallel operated vessels | |
| JPS54160514A (en) | Decarburization and annealing method for directional electromagnetic steel plate | |
| ES8302787A1 (en) | Process for refining high-chromium steels | |
| JPS55152118A (en) | Preparation of high chromium steel by vacuum oxygen lancing method | |
| JPS5579821A (en) | Manufacture of low-carbon high-chromium alloy steel by heat-insulated furnace for molten steel | |
| JPS56142815A (en) | Refining method of stainless steel | |
| AU531039B2 (en) | Process for the decarburization of chromium containing cast-irons | |
| TW346505B (en) | Process for producing low-carbon chromium-containing steel | |
| DE3572996D1 (en) | Rapid decarburization steelmaking process | |
| JPS56156701A (en) | Decarburizing method for cast iron powder | |
| Korousic et al. | Operational aspects of experience in vacuum technology by production of high quality stainless and alloyed steels | |
| JPS55161001A (en) | Production of steel powder for powder metallurgy | |
| JPS5763620A (en) | Denitriding and refining method for high chromium steel | |
| JPS57123954A (en) | Manufacture of low-titanium and high-carbon ferrochromium | |
| Schleimer | Process for Producing High Quality Steel | |
| Masuda et al. | Process for Refining High-Chromium Steels | |
| JPS53125215A (en) | Dephosphorizing method for molten high chromium steel | |
| Kaito | Production of Super Ferritic Stainless Steels by S. D.--VOD Process | |
| ES8403162A1 (en) | Process to produce low hydrogen steel by argon-oxygen decarburization. | |
| JPS51140815A (en) | Decarburization of molten steel at reduced pressur | |
| Presern | The Influence of Slag Composition on CaSi Injection into the Ladle | |
| Bauer et al. | Method for the Refining of Steel | |
| JPS5638413A (en) | Prevention of increase in carbon content of molten steel by addition of iron alloy |