JPS5477268A - Continuous manufacture of welded angular steel tube - Google Patents
Continuous manufacture of welded angular steel tubeInfo
- Publication number
- JPS5477268A JPS5477268A JP14483577A JP14483577A JPS5477268A JP S5477268 A JPS5477268 A JP S5477268A JP 14483577 A JP14483577 A JP 14483577A JP 14483577 A JP14483577 A JP 14483577A JP S5477268 A JPS5477268 A JP S5477268A
- Authority
- JP
- Japan
- Prior art keywords
- steel
- steel tube
- welded
- depth
- steel plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 229910000831 Steel Inorganic materials 0.000 title abstract 13
- 239000010959 steel Substances 0.000 title abstract 13
- 238000004519 manufacturing process Methods 0.000 title 1
- 210000003127 knee Anatomy 0.000 abstract 2
- 238000000034 method Methods 0.000 abstract 2
- 238000003466 welding Methods 0.000 abstract 2
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14483577A JPS5477268A (en) | 1977-12-02 | 1977-12-02 | Continuous manufacture of welded angular steel tube |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14483577A JPS5477268A (en) | 1977-12-02 | 1977-12-02 | Continuous manufacture of welded angular steel tube |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5477268A true JPS5477268A (en) | 1979-06-20 |
JPS6125444B2 JPS6125444B2 (enrdf_load_stackoverflow) | 1986-06-16 |
Family
ID=15371534
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP14483577A Granted JPS5477268A (en) | 1977-12-02 | 1977-12-02 | Continuous manufacture of welded angular steel tube |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5477268A (enrdf_load_stackoverflow) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5481157A (en) * | 1977-12-13 | 1979-06-28 | Sumitomo Metal Ind Ltd | Manufacture of welded box-shaped steel |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0492941U (enrdf_load_stackoverflow) * | 1990-12-26 | 1992-08-12 |
-
1977
- 1977-12-02 JP JP14483577A patent/JPS5477268A/ja active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5481157A (en) * | 1977-12-13 | 1979-06-28 | Sumitomo Metal Ind Ltd | Manufacture of welded box-shaped steel |
Also Published As
Publication number | Publication date |
---|---|
JPS6125444B2 (enrdf_load_stackoverflow) | 1986-06-16 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5477268A (en) | Continuous manufacture of welded angular steel tube | |
JPS5481156A (en) | Manufacture of welded box-shaped steel | |
JPS53113734A (en) | One-side arc welding method for 9% ni steel | |
JPS571572A (en) | Arc welding method of thick steel plate | |
JPS5429859A (en) | Diffusion welding method utilizing transformation | |
JPS5477269A (en) | Continuous manufacture of welded angular steel tube | |
JPS53104531A (en) | Surface processing method decreasing stress corrosion cracking | |
JPS5439366A (en) | Method of forming sheet spring material and sheet spring material | |
JPS53106352A (en) | Forming method for reverse strain in welding steel plate | |
JPS5645296A (en) | Welding method of t-joint | |
JPS5335122A (en) | Oiling electric machine tank | |
JPS5435146A (en) | Seal welding method of tube plate and tube | |
JPS5411846A (en) | Welding means with low weld crack susceptibility and method of making same | |
JPS57137028A (en) | Shape steel straightening method by roller straightening machine | |
JPS5417348A (en) | Internal build-up welding process for austenitic stainless steel pipes | |
JPS5561390A (en) | Butt welding method of stationary pipe | |
JPS54131557A (en) | Manufacture of clad steel pipe | |
JPS5395850A (en) | Multiple wire submerged arc welding method | |
Barborka et al. | Weldability of Ni-Cr-Mo-V Steels(1-3 per cent Ni) for Tig Welding | |
JPS5429868A (en) | Relieving method for distorsion of steel sheet | |
JPS53147901A (en) | Method and apparatus for correcting motor-rotor unbalance | |
JPS52156740A (en) | Welding process for austenite steel tubes | |
JPS5747529A (en) | Forming method of pipe of thin plate | |
JPS57207123A (en) | Relieving method for stress remaining in weld zone of stainless steel | |
JPS5290112A (en) | Method of joining steel sheet pile |