JPS5453315A - Long pipe material for continuous stretch reducer - Google Patents
Long pipe material for continuous stretch reducerInfo
- Publication number
- JPS5453315A JPS5453315A JP11956677A JP11956677A JPS5453315A JP S5453315 A JPS5453315 A JP S5453315A JP 11956677 A JP11956677 A JP 11956677A JP 11956677 A JP11956677 A JP 11956677A JP S5453315 A JPS5453315 A JP S5453315A
- Authority
- JP
- Japan
- Prior art keywords
- pipe
- mother
- joint
- stretch reducer
- pipe material
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To obtain a steel pipe material for a stretch reducer prevented from breaking at and near a welded part by giving a proper balance between strengthes of a mother pipe and a joint.
CONSTITUTION: For the continuous manufacturing of a small-diameter pipe by a stretch reducer, the strength rate of a welded joint part to a mother material part in a high temperature of 800W900 degrees C in a pipe material previously prolonged by welding is taken in 1.00W1.30. Material A steel is given by connecting carbon steel pipes by friction pressure welding, and is processed by stretch reducing after external beads are cut off. In this case, since the mother pipe and the joint part are given an essentially equal quality, the strength of the pipe joint is almost equal to that of the mother pipe in a high temperature of 800W900 degrees C
COPYRIGHT: (C)1979,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11956677A JPS5453315A (en) | 1977-10-05 | 1977-10-05 | Long pipe material for continuous stretch reducer |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11956677A JPS5453315A (en) | 1977-10-05 | 1977-10-05 | Long pipe material for continuous stretch reducer |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5453315A true JPS5453315A (en) | 1979-04-26 |
Family
ID=14764496
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP11956677A Pending JPS5453315A (en) | 1977-10-05 | 1977-10-05 | Long pipe material for continuous stretch reducer |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5453315A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6046802A (en) * | 1983-08-26 | 1985-03-13 | Nippon Steel Corp | Rolling method of pipe |
-
1977
- 1977-10-05 JP JP11956677A patent/JPS5453315A/en active Pending
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6046802A (en) * | 1983-08-26 | 1985-03-13 | Nippon Steel Corp | Rolling method of pipe |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5453315A (en) | Long pipe material for continuous stretch reducer | |
JPS53113734A (en) | One-side arc welding method for 9% ni steel | |
JPS57175094A (en) | Improving method for residual stress in welded joint part of pipes | |
JPS5221210A (en) | High tensile strength cast steel for low temperature having superior w elding property | |
JPS53141140A (en) | Process for forming weld joint of pipeline or vessel | |
JPS53116264A (en) | Tack welding method for seam of steel pipe | |
JPS53130242A (en) | Welding method for manufacture of thick-walled large diameter welded steel pipe | |
JPS5639192A (en) | Continuous repetitive bending process method for welding joint steel band | |
JPS5429859A (en) | Diffusion welding method utilizing transformation | |
JPS5443844A (en) | Welded joint structure | |
JPS51142715A (en) | Pipe joint | |
SU1823326A1 (en) | Method of making large-dimension constructions from different-kind steels | |
JPS57112990A (en) | Method for welding of piping and support fitting used in high temperature atmosphere | |
JPS5420945A (en) | Seam tack welding method for steel pipe | |
JPS53119772A (en) | Manufacture of force welded pipe | |
JPS53129136A (en) | Construction of welded joint for piping and elbow | |
JPS5719155A (en) | Welding method using refining packing member | |
JPS57103791A (en) | Double blank pipe for production of pipe clad steel and forming method of said pipe | |
JPS5411045A (en) | Preventing method for crack initiation of deposited metal | |
JPS5413433A (en) | Welding method for stainless steel | |
JPS5530388A (en) | One side welding method using refractory material | |
JPS5318814A (en) | Strengthening structure for steel pipe bending | |
JPS5395850A (en) | Multiple wire submerged arc welding method | |
JPS5397963A (en) | Arc welding method of pipes | |
JPS5550976A (en) | Insert welding method |