JPS54159360A - Automatic one side welding method - Google Patents

Automatic one side welding method

Info

Publication number
JPS54159360A
JPS54159360A JP6766678A JP6766678A JPS54159360A JP S54159360 A JPS54159360 A JP S54159360A JP 6766678 A JP6766678 A JP 6766678A JP 6766678 A JP6766678 A JP 6766678A JP S54159360 A JPS54159360 A JP S54159360A
Authority
JP
Japan
Prior art keywords
weld
deformation
temperature
residual stress
welding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP6766678A
Other languages
Japanese (ja)
Inventor
Kyo Matsuzaka
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hitachi Ltd
Original Assignee
Hitachi Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hitachi Ltd filed Critical Hitachi Ltd
Priority to JP6766678A priority Critical patent/JPS54159360A/en
Publication of JPS54159360A publication Critical patent/JPS54159360A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To prevent the deformation to be caused while the welding work, to prevent the crack at the toe of weld, and to uniformize the distribution of the residual stress, by keeping the temperature of the groove covering whole length of weld at 350W450°C until the welding is finished, at the automatic one side welding method.
CONSTITUTION: The generation of the crack at the toe of weld, a large deformation 3, an angular deformation 5, and the residual stress, with the progress of the welding work of the parent metal 1 in the arrowed direction, quickly develops from a point when the temperature of weld zone is cooled down to under 350°C. This fact is due to the Young's modulus quickly reducing at the temperature above 350°C; therefore, the weld zone is heated by the burner, etc., so as to keep the temperature of whole area at 350W450°C, until the welding work is finished; hereby, the plastic deformation due to the shrinking is made easy. According to this method, the generation of the deformation and the residual stress is almost prevented.
COPYRIGHT: (C)1979,JPO&Japio
JP6766678A 1978-06-07 1978-06-07 Automatic one side welding method Pending JPS54159360A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP6766678A JPS54159360A (en) 1978-06-07 1978-06-07 Automatic one side welding method

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP6766678A JPS54159360A (en) 1978-06-07 1978-06-07 Automatic one side welding method

Publications (1)

Publication Number Publication Date
JPS54159360A true JPS54159360A (en) 1979-12-17

Family

ID=13351545

Family Applications (1)

Application Number Title Priority Date Filing Date
JP6766678A Pending JPS54159360A (en) 1978-06-07 1978-06-07 Automatic one side welding method

Country Status (1)

Country Link
JP (1) JPS54159360A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2018114555A (en) * 2017-01-17 2018-07-26 株式会社神戸製鋼所 One-face submerge arc welding method and one-face submerge arc welding device

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2018114555A (en) * 2017-01-17 2018-07-26 株式会社神戸製鋼所 One-face submerge arc welding method and one-face submerge arc welding device

Similar Documents

Publication Publication Date Title
DK567878A (en) PROCESS FOR HEAT WELDING TO ATTACH TWO INSERTED PIPE PARTS INTO EACH OTHER AND THE APPARATUS FOR PERFORMING THE PROCEDURE
BR8603648A (en) PROCESS FOR ASSEMBLING A GAS CIRCULATION BLOCK
ES230586U (en) Cable joinder assembly
JPS54159360A (en) Automatic one side welding method
JPS5311328A (en) Heater and resin-packing metal mold equipped with heater
NO823140L (en) PROGRAM FOR HEAT TREATMENT OF NICKEL-COBOLT-IRON alloys
JPS57112960A (en) Heat resistant roll having spiral internal water groove
JPS5425236A (en) Method of improving toughness of welded joint
JPS53102247A (en) Diffusion welder with internal cooler
JPS53149141A (en) Manufacture of welded structure
JPS5399054A (en) Diffusion welding method of iron base material
JPS52155880A (en) Incinerator of melting type
JPS5337106A (en) Repairing method of blast furnace shell
JPS53109830A (en) Welding method for prevention of reheating crack
JPS53119433A (en) Liquid fuel combustor
JPS5230163A (en) Method for junction of semiconductor parts
JPS54162008A (en) Welding method of anticorrosive shield material of steam turbine blade
JPS549146A (en) Method of producing forge-welded pipes
JPS5518535A (en) Setting-up method for converter
JPS56160872A (en) Repairing welding method
JPS5410442A (en) Enclosing process of sheathed heater
JPS55162449A (en) Joining method for detachable type roof having sash around glass
JPS52112850A (en) Forming connection in heat insulating material
JPS52155657A (en) Fiber glass reinforced polybutylene threphthalate composition
JPS5397066A (en) Method of shrinking heat-shrinkable sleeve with heating