JPS5410218A - Quench hardening method for steel tube with occurence of no quenching crack - Google Patents
Quench hardening method for steel tube with occurence of no quenching crackInfo
- Publication number
- JPS5410218A JPS5410218A JP7583977A JP7583977A JPS5410218A JP S5410218 A JPS5410218 A JP S5410218A JP 7583977 A JP7583977 A JP 7583977A JP 7583977 A JP7583977 A JP 7583977A JP S5410218 A JPS5410218 A JP S5410218A
- Authority
- JP
- Japan
- Prior art keywords
- steel tube
- occurence
- quench hardening
- hardening method
- quenching crack
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To prevent the occurrence of quenching crack in quench hardening of a steel tube by spraying the outside of the tube with cooling water, by cooling the tube while regulating a difference in temp. between the inside and outside when the inside temp. is in the transformation range.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7583977A JPS5929085B2 (en) | 1977-06-25 | 1977-06-25 | Quenching method for steel pipes that does not cause quench cracking |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7583977A JPS5929085B2 (en) | 1977-06-25 | 1977-06-25 | Quenching method for steel pipes that does not cause quench cracking |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5410218A true JPS5410218A (en) | 1979-01-25 |
JPS5929085B2 JPS5929085B2 (en) | 1984-07-18 |
Family
ID=13587758
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP7583977A Expired JPS5929085B2 (en) | 1977-06-25 | 1977-06-25 | Quenching method for steel pipes that does not cause quench cracking |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5929085B2 (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN110629008A (en) * | 2019-09-06 | 2019-12-31 | 达力普石油专用管有限公司 | Method for improving quenching uniformity of internal-spraying and external-spraying quenching system |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH08188827A (en) * | 1995-01-09 | 1996-07-23 | Sumitomo Metal Ind Ltd | Production of martensitic stainless steel tube |
-
1977
- 1977-06-25 JP JP7583977A patent/JPS5929085B2/en not_active Expired
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN110629008A (en) * | 2019-09-06 | 2019-12-31 | 达力普石油专用管有限公司 | Method for improving quenching uniformity of internal-spraying and external-spraying quenching system |
Also Published As
Publication number | Publication date |
---|---|
JPS5929085B2 (en) | 1984-07-18 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS52152814A (en) | Thermo-mechanical treatment of seamless steel pipe | |
JPS5333919A (en) | Production of cold rolled aluminum killed steel sheet with excellent deep drawability | |
JPS5410218A (en) | Quench hardening method for steel tube with occurence of no quenching crack | |
JPS5248507A (en) | Method for cooling outer surface of metallic pipe or large diameter | |
JPS5270914A (en) | Heat treatment of pipe | |
JPS5253712A (en) | Equipment for continuous annealing containingoverage treatment | |
JPS5323817A (en) | Production of low yield ratio, high toughness, high tensile steel plate | |
JPS52143908A (en) | Cooling apparatus in metal heat treatment equipment | |
JPS53119219A (en) | Manufacture of weldable high tensile steel | |
GB1188574A (en) | Method of Toughening Steel by Rolling | |
JPS52138428A (en) | Production of rail having excellent wear resistance and damage resistance as rolled | |
JPS53119254A (en) | Repairing method for nodular graphite cast steel roll | |
JPS5429812A (en) | Cooler for pipe | |
JPS5362726A (en) | Method and apparatus for preparatment of temper rolling | |
JPS5385711A (en) | Manufacture of non-refined high tensile steel sheet with toughness | |
JPS54107411A (en) | Tempering of large diameter steel tube | |
JPS54112364A (en) | Roll for sendzimir mill and its heat treating method | |
JPS5437023A (en) | Production of cold-rolled steel plate to be drawn | |
JPS51112723A (en) | Process for hardening steel pipes | |
JPS5385710A (en) | Heat treating method for low alloy steel | |
JPS5311811A (en) | Carburizing method for molten steel | |
JPS53119216A (en) | Manufacture of steel sheet with excellent mechanical properties | |
JPS5693853A (en) | Steel pipe for oil well with excellent compression strength | |
JPS56119739A (en) | Manufacture of high-strength steel strip | |
JPS53119207A (en) | Method and apparatus for cooling steel belt at continuous annealing |