JPS5395120A - Tough steel having excellent resistance for becoming brittle owing to sr - Google Patents

Tough steel having excellent resistance for becoming brittle owing to sr

Info

Publication number
JPS5395120A
JPS5395120A JP1010277A JP1010277A JPS5395120A JP S5395120 A JPS5395120 A JP S5395120A JP 1010277 A JP1010277 A JP 1010277A JP 1010277 A JP1010277 A JP 1010277A JP S5395120 A JPS5395120 A JP S5395120A
Authority
JP
Japan
Prior art keywords
excellent resistance
tough steel
becoming brittle
owing
brittle owing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP1010277A
Other languages
Japanese (ja)
Other versions
JPS594487B2 (en
Inventor
Yasuo Otani
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Sumitomo Metal Industries Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sumitomo Metal Industries Ltd filed Critical Sumitomo Metal Industries Ltd
Priority to JP52010102A priority Critical patent/JPS594487B2/en
Publication of JPS5395120A publication Critical patent/JPS5395120A/en
Publication of JPS594487B2 publication Critical patent/JPS594487B2/en
Expired legal-status Critical Current

Abstract

PURPOSE: The tough steel of which the tendency to become brittle after the annealing for stress relieving (SR) has been reduced in the use at a low temperature to the extent of-100°C, by lowering the content of C and, at the same time, by making Mo contained.
COPYRIGHT: (C)1978,JPO&Japio
JP52010102A 1977-01-31 1977-01-31 Manufacturing method for strong steel with excellent SR embrittlement resistance Expired JPS594487B2 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP52010102A JPS594487B2 (en) 1977-01-31 1977-01-31 Manufacturing method for strong steel with excellent SR embrittlement resistance

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP52010102A JPS594487B2 (en) 1977-01-31 1977-01-31 Manufacturing method for strong steel with excellent SR embrittlement resistance

Publications (2)

Publication Number Publication Date
JPS5395120A true JPS5395120A (en) 1978-08-19
JPS594487B2 JPS594487B2 (en) 1984-01-30

Family

ID=11740944

Family Applications (1)

Application Number Title Priority Date Filing Date
JP52010102A Expired JPS594487B2 (en) 1977-01-31 1977-01-31 Manufacturing method for strong steel with excellent SR embrittlement resistance

Country Status (1)

Country Link
JP (1) JPS594487B2 (en)

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS53110917A (en) * 1977-03-11 1978-09-28 Nippon Kokan Kk <Nkk> Steel of excellent sr embrittlement resistance
JPS5763664A (en) * 1981-08-14 1982-04-17 Nippon Kokan Kk <Nkk> Steel products with superior resistance to sr embrittlement
JPS5763663A (en) * 1981-08-14 1982-04-17 Nippon Kokan Kk <Nkk> Steel products with superior rewistance to sr embrittlement

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP6608497B1 (en) 2018-08-22 2019-11-20 三菱重工業株式会社 Method for disassembling plastic composites

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5039618A (en) * 1973-08-15 1975-04-11
JPS50145314A (en) * 1974-05-14 1975-11-21

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5039618A (en) * 1973-08-15 1975-04-11
JPS50145314A (en) * 1974-05-14 1975-11-21

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS53110917A (en) * 1977-03-11 1978-09-28 Nippon Kokan Kk <Nkk> Steel of excellent sr embrittlement resistance
JPS6035423B2 (en) * 1977-03-11 1985-08-14 日本鋼管株式会社 Steel material with excellent SR embrittlement resistance
JPS5763664A (en) * 1981-08-14 1982-04-17 Nippon Kokan Kk <Nkk> Steel products with superior resistance to sr embrittlement
JPS5763663A (en) * 1981-08-14 1982-04-17 Nippon Kokan Kk <Nkk> Steel products with superior rewistance to sr embrittlement

Also Published As

Publication number Publication date
JPS594487B2 (en) 1984-01-30

Similar Documents

Publication Publication Date Title
JPS52131912A (en) T# alloy with high internal friction and heat treatment thereof
JPS5226506A (en) Lubricating oil composition for compressor
JPS5395120A (en) Tough steel having excellent resistance for becoming brittle owing to sr
JPS522822A (en) Wear resistant steel
JPS5395121A (en) Preparation of high tensile steel sheet
JPS53147051A (en) 1alpha-hydroxy-24-dehydro-vitamin d3 and its preparation
JPS5389815A (en) Steel bar for low temperature
JPS5386605A (en) Sintered alloy having wear resistance at high temperature
JPS5365213A (en) Low alloy high toughness steel with excellent delayed fracture resistantproperty
JPS5716152A (en) Austenite-containing stainless steel having deep drawing property
JPS53133524A (en) Austenitic stainless steel for cold forging
JPS5335613A (en) Sheathing for watch
JPS52117831A (en) Preparation of strong and tough low nickel high tensile steel
JPS5445612A (en) Low-alloy steel free of post-stress-removing-anneal embrittlement in heat affected zone
JPS5411015A (en) Iron alloy
JPS52138421A (en) Two-phased stainless steeel
JPS5284111A (en) W-base casting alloy for bit used to opening tap hole of balst furnace
JPS5385714A (en) Free-cutting nickel-chromium alloy
JPS52156121A (en) High tensile steel for low temperature use
JPS5410304A (en) Method of preventing the deterioration of lubricant
JPS53103966A (en) Preparation of steel wire having high toughness
JPS5397917A (en) Alloy steel for low temperature use
JPS53115612A (en) Method for manufacturing thick, hot-rolled, high-tension steel band excellent in tenacity at low temperature
JPS5411824A (en) Magnetic alloy
JPS5438206A (en) Alloy magnet