JPS5370040A - Granular rectifier molten flux used in casting of steel and casted ingot with redused surface defficiency - Google Patents
Granular rectifier molten flux used in casting of steel and casted ingot with redused surface defficiencyInfo
- Publication number
- JPS5370040A JPS5370040A JP14461276A JP14461276A JPS5370040A JP S5370040 A JPS5370040 A JP S5370040A JP 14461276 A JP14461276 A JP 14461276A JP 14461276 A JP14461276 A JP 14461276A JP S5370040 A JPS5370040 A JP S5370040A
- Authority
- JP
- Japan
- Prior art keywords
- redused
- defficiency
- rectifier
- granular
- casting
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 229910000831 Steel Inorganic materials 0.000 title 1
- 238000005266 casting Methods 0.000 title 1
- 230000004907 flux Effects 0.000 title 1
- 239000010959 steel Substances 0.000 title 1
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14461276A JPS5370040A (en) | 1976-12-03 | 1976-12-03 | Granular rectifier molten flux used in casting of steel and casted ingot with redused surface defficiency |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP14461276A JPS5370040A (en) | 1976-12-03 | 1976-12-03 | Granular rectifier molten flux used in casting of steel and casted ingot with redused surface defficiency |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5370040A true JPS5370040A (en) | 1978-06-22 |
| JPS5726183B2 JPS5726183B2 (enrdf_load_stackoverflow) | 1982-06-03 |
Family
ID=15366066
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP14461276A Granted JPS5370040A (en) | 1976-12-03 | 1976-12-03 | Granular rectifier molten flux used in casting of steel and casted ingot with redused surface defficiency |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5370040A (enrdf_load_stackoverflow) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5666362A (en) * | 1979-11-02 | 1981-06-04 | Nippon Thermo Chem Kk | Testing method of melting of additive for ingotting |
Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4928808A (enrdf_load_stackoverflow) * | 1972-07-12 | 1974-03-14 | ||
| JPS49115028A (enrdf_load_stackoverflow) * | 1973-03-09 | 1974-11-02 |
-
1976
- 1976-12-03 JP JP14461276A patent/JPS5370040A/ja active Granted
Patent Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS4928808A (enrdf_load_stackoverflow) * | 1972-07-12 | 1974-03-14 | ||
| JPS49115028A (enrdf_load_stackoverflow) * | 1973-03-09 | 1974-11-02 |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5666362A (en) * | 1979-11-02 | 1981-06-04 | Nippon Thermo Chem Kk | Testing method of melting of additive for ingotting |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5726183B2 (enrdf_load_stackoverflow) | 1982-06-03 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS5340630A (en) | Method of augmenting width of cast piece in continuous casting | |
| JPS5340633A (en) | Method of preventing segregation in continuous casting of steel or alloy and device for embodying the method | |
| JPS5323825A (en) | Method and device for indicating end of pouring in case of casting molten metal from molten metal pouring vessel | |
| NZ180524A (en) | Liquid support for and cooling of reuerse surfaces of belts used in continuous casting of metal strip | |
| JPS5370040A (en) | Granular rectifier molten flux used in casting of steel and casted ingot with redused surface defficiency | |
| ZA818652B (en) | Method of cooling castings in the continuous casting of steel | |
| JPS51147431A (en) | Mould for continuous iron and steel casting | |
| JPS5252829A (en) | Continuous casting mould for iron and steel | |
| JPS5288223A (en) | Method of casting steel ingot with few surface defects and granular stratification molten flux for embodying the method | |
| GB1528928A (en) | Methods of and chill moulds for casting metal ingots billets and the like | |
| JPS5345627A (en) | Method of improving solidification structure of steel in continuous casting | |
| JPS5332830A (en) | Method and equipment for maintenance of tundish in continuous casting method | |
| JPS5557363A (en) | Device that cool strand in continuous casting installation of steel | |
| JPS5250929A (en) | Continuous casting mould for metals in which differece between melting temperature and solidifying temerature is large | |
| JPS5342131A (en) | Method of cooling cast piece in continuous casting | |
| JPS5285024A (en) | Method of highhspeed bottom pouring casting of steel ingot with less slag invasion and large interposed substance under surface | |
| JPS52114425A (en) | Pouring method of molten steel in continuous casting | |
| JPS5364621A (en) | Preventing of center segregation in continuous casting | |
| JPS5370928A (en) | Casting of composite metal casted ingot | |
| JPS5285022A (en) | Equipment of supporting and cooling cast piece in continuous casting eqipment | |
| JPS5342133A (en) | Method of cooling cast piece in continuous casting | |
| FR2289270A1 (fr) | Lingotiere a plaques pour la coulee continue de metal et en particulier d'acier | |
| JPS534726A (en) | Method of replacing tundish in continuous casting | |
| JPS545827A (en) | Method of making steel ingot free of surface deficiency and flux for casting steel ingot | |
| JPS52146725A (en) | Measuring method of molten steel in tundish of continuous casting |